Microstructures and properties analysis of dissimilar metal joint in the friction stir welded copper to aluminum alloy 被引量:9
1
作者 王希靖 张忠科 +1 位作者 达朝炳 李晶 《China Welding》 EI CAS 2007年第1期57-62,共6页
This paper mainly concentrated on the feasibility of friction stir welding of dissimilar metal of aluminum alloy to copper (I2) and a preliminary analysis of welding parameters influencing on the microstructures and... This paper mainly concentrated on the feasibility of friction stir welding of dissimilar metal of aluminum alloy to copper (I2) and a preliminary analysis of welding parameters influencing on the microstructures and properties of joint was carried out. The results indicated that the thickness of workpiece played an important role in the welding parameters which could succeed in the friction stir welding of dissimilar metal of copper to aluminum alloy, and the parameters were proved to be a narrow choice. The interfacial region between copper and aluminum in the dissimilar joint was not uniformly mixed, constituted with part of incomplete mixing zone, complete mixing zone, dispersion zone and the most region' s boundary was obvious. Meantime a kind banded structure with inhomogeneous width was formed. The intermetallic compounds generated during friction stir welding in the interfacial region were mainly CugAl4, Al2Cu etc, and their hardness was higher than oihers. 展开更多
关键词 friction stir welding dissimilar metals copper aluminum alloy
下载PDF
Analysis of Laser Micro Welding of Copper-Aluminum Dissimilar Metals and Its Mechanism
2
作者 Jiang Huang Wenqing Shi +2 位作者 Yuping Xie Zhigang Liang Jinming Zhan 《Journal of Applied Mathematics and Physics》 2019年第12期3192-3200,共9页
Micro welding of dissimilar metals can meet many performance requirements for modern engineering structures. In this experiment, laser micro welding of copper-aluminum dissimilar metals was conducted with an HWLW-300A... Micro welding of dissimilar metals can meet many performance requirements for modern engineering structures. In this experiment, laser micro welding of copper-aluminum dissimilar metals was conducted with an HWLW-300A energy negative feedback Nd:YAG pulse laser. By using the overlap welding method with copper on aluminum, with the laser energy being distributed unevenly, good weld joints were obtained. In this paper, the welding mechanism was analyzed from aspects such as welding temperature and the specific heat capacity of the solid metal. Existing defects were identified, and a feasible improvement scheme was proposed. 展开更多
关键词 Mciro WELDING LASER WELDING copper-aluminum dissimilar metalS MECHANISM
下载PDF
铝/铜异种金属搅拌摩擦焊接头腐蚀行为研究
3
作者 毛悦 郭瀚林 +1 位作者 吴润 傅莉 《热加工工艺》 北大核心 2024年第12期125-128,共4页
采用搅拌摩擦焊接技术实现了3 mm厚6061-T6铝合金与T2紫铜的焊接,研究了Al/Cu搅拌摩擦焊接头的宏观成形、电化学腐蚀以及浸泡腐蚀行为。结果表明,Al/Cu搅拌摩擦焊接接头成形良好,未见裂纹、孔洞等缺陷。Cu的腐蚀电位高于Al,导致Al/Cu之... 采用搅拌摩擦焊接技术实现了3 mm厚6061-T6铝合金与T2紫铜的焊接,研究了Al/Cu搅拌摩擦焊接头的宏观成形、电化学腐蚀以及浸泡腐蚀行为。结果表明,Al/Cu搅拌摩擦焊接接头成形良好,未见裂纹、孔洞等缺陷。Cu的腐蚀电位高于Al,导致Al/Cu之间形成宏观电偶。Al/Cu接头的腐蚀电位低于两种母材,腐蚀电流密度大于两种母材,接头中的宏观电偶效应加速了接头的腐蚀。在浸泡24 h内,接头的腐蚀主要发生在铝合金侧,其中铝侧热影响区的腐蚀最严重,形成的点蚀坑尺寸较大。铝侧焊核区和铝母材也发生了局部点蚀,腐蚀程度相对较轻。铝侧表面腐蚀产物为Al(OH)3/Al2O3。 展开更多
关键词 铝/铜异种金属 搅拌摩擦焊 腐蚀行为
下载PDF
纳米颗粒增强的铝铜异种金属等离子弧熔钎焊接头性能优化研究
4
作者 赵颖 《山西冶金》 CAS 2024年第4期22-24,共3页
铝铜异种金属连接技术因工程应用的需求而备受关注,但传统焊接方法难以满足日益增长的性能要求。纳米颗粒增强技术为优化铝铜异种金属焊接接头性能提供了新的可能。研究通过向铝铜异种金属等离子弧熔钎焊接头中添加不同种类和浓度的纳... 铝铜异种金属连接技术因工程应用的需求而备受关注,但传统焊接方法难以满足日益增长的性能要求。纳米颗粒增强技术为优化铝铜异种金属焊接接头性能提供了新的可能。研究通过向铝铜异种金属等离子弧熔钎焊接头中添加不同种类和浓度的纳米颗粒,深入分析其对接头力学性能、微观组织和耐腐蚀性的影响。实验结果表明,适量和适当种类的纳米颗粒可以显著提高接头的力学性能、微观组织稳定性和耐腐蚀性,为铝铜异种金属等离子弧熔钎焊接头的性能优化提供了有效解决方案。 展开更多
关键词 纳米颗粒 铝铜异种金属 等离子弧熔钎
下载PDF
Effect of the Welding Parameters on the Structural and Mechanical Properties of Aluminium and Copper Sheet Joints by Electromagnetic Pulse Welding
5
作者 Irene Kwee Verena Psyk Koen Faes 《World Journal of Engineering and Technology》 2016年第4期538-561,共24页
Aluminium-copper hybrid parts, as a substitution to copper parts, result in weight and cost reduction, and are relevant in applications related to the electronic, heating and cooling sector. However, aluminium to copp... Aluminium-copper hybrid parts, as a substitution to copper parts, result in weight and cost reduction, and are relevant in applications related to the electronic, heating and cooling sector. However, aluminium to copper joined by thermal welding processes presents challenges in terms of achieving good joint quality. This is attributed to their dissimilar mechanical and thermal properties which result in large stress gradients during heating. This study investigated joining of aluminium to copper sheets by electromagnetic pulse welding, which is a solid-state process that uses electromagnetic forces for joining of dissimilar materials. Hybrid sheet welds were obtained for all parameters conditions, selected according to a Taguchi L18 design. The structural and mechanical characteristics were examined and related to the welding parameters by means of a Pareto analysis and response graphs. The welded zone started with a wavy interface with interfacial layers and defects and evolved to a flat interface without interfacial layers. The maximum transferable force depended on the minimum specimen thickness and the strength of the hybrid sheet weld. In case of aluminium sheet thickness reduction, the maximum transferable force was linearly correlated with the aluminium sheet thickness. High quality joints were obtained for no aluminium sheet thickness reduction and for a sheet weld strength which was at least as high as that of the base material. The most effective way to increase the transferable force was to lower the initial gap and to increase the free length, which resulted in no aluminium sheet thickness reduction. Alternatively, the use of a rounded spacer decreased the effect of the aluminium sheet thickness on the transferable force. An increase in weld width was achieved for an increase in capacitor charging energy and gap, whereas an increase in weld length was obtained for a decrease in gap. An increase in weld width did not necessarily result in an increase in the transferable force. In the regarded cases, a hybrid sheet with narrow weld width could therefore have higher quality. 展开更多
关键词 Electromagnetic Pulse Sheet Welding aluminum-to-copper Welds dissimilar metal Welds Transferable Force Interfacial Morphology
下载PDF
超声波辅助钎焊铜/铝异种金属接头界面组织性能及强化机制 被引量:5
6
作者 张汇文 崔炜 闫久春 《焊接学报》 EI CAS CSCD 北大核心 2015年第1期101-104,118,共5页
为了研究铜/铝异种金属钎焊接头界面金属间化合物层组织结构对接头性能的影响,从化合物结构出发,提出了一种预涂敷钎料的超声波辅助钎焊复合工艺.结果表明,采用Sn-9Zn共晶钎料,得到细小金属间化合物弥散地分布在铜表面的界面结构,增强... 为了研究铜/铝异种金属钎焊接头界面金属间化合物层组织结构对接头性能的影响,从化合物结构出发,提出了一种预涂敷钎料的超声波辅助钎焊复合工艺.结果表明,采用Sn-9Zn共晶钎料,得到细小金属间化合物弥散地分布在铜表面的界面结构,增强了界面强度,其接头抗拉强度甚至超过传统工艺下将金属间化合物层减薄到极限厚度(1~2μm)时的强度.提出了一种基于超声预涂敷工艺的界面化合物结构调控方法,研究了化合物在钎焊过程中的演变规律,以及金属间化合物层在不同结构和分布情况下对接头力学性能的影响,探索了铜/铝异种金属低温焊接的新途径. 展开更多
关键词 铜/铝异种金属 超声波辅助钎焊 金属间化合物 钎料预涂敷
下载PDF
铝-铜脉冲旁路耦合电弧MIG熔钎焊接头组织分析 被引量:1
7
作者 石玗 许瑾 +1 位作者 黄健康 顾玉芬 《兰州理工大学学报》 CAS 北大核心 2015年第3期6-9,共4页
采用脉冲旁路耦合电弧MIG熔钎焊方法,利用ER4047铝合金焊丝在T2铜板上进行平板堆焊实验,通过调节焊接参数获得良好焊缝成形.利用SEM、EDS和XRD等测试手段对连接界面区的微观组织进行观察和分析.结果表明:在连接界面区从铜侧到铝侧依次... 采用脉冲旁路耦合电弧MIG熔钎焊方法,利用ER4047铝合金焊丝在T2铜板上进行平板堆焊实验,通过调节焊接参数获得良好焊缝成形.利用SEM、EDS和XRD等测试手段对连接界面区的微观组织进行观察和分析.结果表明:在连接界面区从铜侧到铝侧依次生成条状的Cu9Al4、块状的CuAl2金属间化合物和絮状的α(Al)+θ(CuAl2)共晶体,且金属间化合物层的厚度随着母材热输入的增加而增大,同时块状脆性金属间化合物尺寸变大.对熔钎焊接头进行显微维氏硬度测量,结果显示,铝-铜熔钎焊焊接接头金属间化合物区域显微硬度最高达406.7HV,说明铝-铜熔钎焊连接界面区出现脆硬相. 展开更多
关键词 脉冲旁路耦合电弧MIG熔钎焊 铝-铜异种金属焊接 微观组织 金属间化合物
下载PDF
铜-铝异种金属超声波焊缝成型机制与接头性能研究 被引量:1
8
作者 王锡岭 刘驰 +1 位作者 许祥平 杨少伟 《轻合金加工技术》 CAS 2021年第4期60-67,共8页
对铜箔-铝箔进行超声波焊接试验研究,优化设计工艺参数;采用金相显微镜、能谱仪、扫描电镜等分析焊接接头的微观组织;采用高速摄影系统实时监控焊接过程,研究超声波焊缝成型机制。结果表明:焊接压力,焊接振幅、焊接时间对接头性能影响很... 对铜箔-铝箔进行超声波焊接试验研究,优化设计工艺参数;采用金相显微镜、能谱仪、扫描电镜等分析焊接接头的微观组织;采用高速摄影系统实时监控焊接过程,研究超声波焊缝成型机制。结果表明:焊接压力,焊接振幅、焊接时间对接头性能影响很大,这些工艺参数过大或过小都会使接头强度降低。当焊接压力0.20 MPa,焊接振幅30 um,焊接时间0.05 s时,接头强度达到最大值,破断拉伸力为200 N。保持压力和振幅不变,随着焊接时间的增加,铜-铝接头的有效连接长度增加,接头强度增加;进一步增加焊接时间,铜-铝接头有效连接长度没有明显变化,接头强度下降。超声波焊接可分为四个过程:初始接触,摩擦产热,焊接软化,固相结合。 展开更多
关键词 铜-铝异种金属超声波焊接 力学性能 微观组织 高速摄影
下载PDF
异种金属的钎焊 被引量:3
9
作者 庄鸿寿 《焊接》 北大核心 2009年第2期22-25,共4页
连接异种金属时,由于材料物理性能的不同以及连接时发生的冶金反应,比较困难。钎焊是最实用的方法。阐述了常用的异种金属组合:铝-铜、铝-不锈钢、铝-钛、不锈钢-钛合金的钎焊技术,同时列出了这些接头的图片。
关键词 异种金属 铝-铜 铝-不锈钢 铝-钛 不锈钢-钛合金 钎焊
下载PDF
铝硅焊丝成分对铜铝异种金属焊接接头性能影响分析 被引量:1
10
作者 徐宏彤 晏丽琴 王世荣 《世界有色金属》 2017年第22期224-225,共2页
随着社会的发展,对焊接接头的性能要求越来越高,其中焊接材料是影响其性能的关键因素之一,但由于传统焊接材料落后,导致焊接接头表面凹凸不平,存在不饱满的缺陷,影响美观。因此为满足人们工作的需要,文章研究在焊丝中加入铝硅成分后,对... 随着社会的发展,对焊接接头的性能要求越来越高,其中焊接材料是影响其性能的关键因素之一,但由于传统焊接材料落后,导致焊接接头表面凹凸不平,存在不饱满的缺陷,影响美观。因此为满足人们工作的需要,文章研究在焊丝中加入铝硅成分后,对铜铝异种金属焊接接头性能产生的影响。结果表明:对焊接材料进行调整、优化可以改善焊接接头的质量。与传统的焊接材料相比较,利用铝硅焊丝焊接的接头,包括焊缝、熔合区和热影响区都比较平整和饱满,没有出现较大的缺陷,更重要的是焊接接头较密实,质量较高。 展开更多
关键词 铝硅焊丝成分 铜铝异种金属 焊接接头 性能 影响
下载PDF
汽车用铝-铜异种材料摩擦焊接微结构和力学性能研究 被引量:1
11
作者 齐凯丽 李静 《铸造技术》 CAS 北大核心 2016年第6期1232-1235,共4页
以6082-T6铝和商业纯铜为对象,研究了Al-Cu的连续驱动摩擦焊,利用光学显微镜、扫描电子显微镜和X射线衍射分析技术分析了焊接界面的微结构。结果表明,接头的拉伸强度比铝母材的强度高3.8%。焊接接头的拉伸断裂位置发生在铝侧,断裂形貌... 以6082-T6铝和商业纯铜为对象,研究了Al-Cu的连续驱动摩擦焊,利用光学显微镜、扫描电子显微镜和X射线衍射分析技术分析了焊接界面的微结构。结果表明,接头的拉伸强度比铝母材的强度高3.8%。焊接接头的拉伸断裂位置发生在铝侧,断裂形貌表明失效形式为韧窝状结构的韧性断裂。 展开更多
关键词 异种金属 力学性能 摩擦焊
下载PDF
铝/铜异种金属熔钎焊研究现状 被引量:1
12
作者 徐文虎 杨瑾 +4 位作者 肖明 彭铭建 赵一璇 刘红兵 陆汉龙 《上海工程技术大学学报》 CAS 2021年第3期215-228,共14页
由于铝合金和铜异种金属之间的物化性能差异较大,铝合金具有强氧化性等因素,铝/铜异种金属连接是焊接领域的研究难点.综述近年来铝/铜异种金属熔钎焊的研究现状,介绍了铝合金和铜异种金属的焊接性,评述了铝/铜异种金属电弧和激光熔钎焊... 由于铝合金和铜异种金属之间的物化性能差异较大,铝合金具有强氧化性等因素,铝/铜异种金属连接是焊接领域的研究难点.综述近年来铝/铜异种金属熔钎焊的研究现状,介绍了铝合金和铜异种金属的焊接性,评述了铝/铜异种金属电弧和激光熔钎焊的研究进展,讨论了铝/铜异种金属熔钎焊仍然存在的共性问题;通过采用合适的焊接工艺配合合金元素调控是解决铝/钢异种金属熔钎焊问题的关键,并对该领域的研究发展进行展望和评述. 展开更多
关键词 铝铜异种金属 电弧熔钎焊 激光熔钎焊 合金化 力学性能
下载PDF
铝与铜异种金属激光焊性能与工艺 被引量:1
13
作者 龚建平 《焊接技术》 2021年第8期37-40,I0015,共5页
为了提升铝与铜异种金属激光焊效率及质量,研究铝与铜异种金属激光焊性能与工艺。根据0.5 mm铝板与2 mm铜板,采用单模激光设备和多模激光设备进行焊接试验,通过调节激光焊的单模与双模、激光功率、焊接速度这3个工艺参数,研究工艺参数... 为了提升铝与铜异种金属激光焊效率及质量,研究铝与铜异种金属激光焊性能与工艺。根据0.5 mm铝板与2 mm铜板,采用单模激光设备和多模激光设备进行焊接试验,通过调节激光焊的单模与双模、激光功率、焊接速度这3个工艺参数,研究工艺参数对焊缝成形的影响以及焊接接头处拉伸性能和硬度的变化规律。根据焊缝成形效果以及焊接接头拉伸性能综合评价焊接质量。试验测得,最佳的激光焊设备是单模激光设备,功率在1 800 W以上、焊接速度50 mm/s时的焊缝成形较好,拉力值在1 700 N以上。采用此参数激光焊焊接铝铜异种金属,能够得到较好的焊缝质量。 展开更多
关键词 铝铜异种金属 激光焊 焊缝性能 拉伸性能
下载PDF
铜铝异种金属搅拌摩擦焊工艺研究 被引量:4
14
作者 张强 徐洪雨 +3 位作者 莫新东 江传斌 秦若东 王金凤 《轻合金加工技术》 CAS 北大核心 2018年第12期51-55,共5页
对2 mm厚的纯铝板和紫铜板的搭接接头的搅拌摩擦焊进行试验研究,分析了工艺参数对焊接质量的影响。结果表明:在试验条件下,焊接速度为60 mm/min、搅拌头旋转速度为700 r/min、下压量为2. 80 mm时,焊接接头抗拉强度达到最大值(96 N/mm2)... 对2 mm厚的纯铝板和紫铜板的搭接接头的搅拌摩擦焊进行试验研究,分析了工艺参数对焊接质量的影响。结果表明:在试验条件下,焊接速度为60 mm/min、搅拌头旋转速度为700 r/min、下压量为2. 80 mm时,焊接接头抗拉强度达到最大值(96 N/mm2),其为铝母材强度的78%,焊接接头成形良好,无明显缺陷。 展开更多
关键词 搅拌摩擦焊 铜铝异种金属焊接 焊接参数 力学性能
下载PDF
铜铝异种金属激光焊接头形貌及性能研究 被引量:1
15
作者 王文明 刘兰胜 +1 位作者 程根健 薛金磊 《装备制造技术》 2021年第12期144-146,共3页
研究了铜铝异种金属激光穿透焊的主要工艺参数:激光功率、焊接速度、光斑直径、焦距等对焊缝成形的影响规律,并以焊接接头的剪切力为目标对工艺参数进行了优化。结果表明:当焊接功率为1275 W、焊接速度为50 mm/s、焦距为200 mm、光斑直... 研究了铜铝异种金属激光穿透焊的主要工艺参数:激光功率、焊接速度、光斑直径、焦距等对焊缝成形的影响规律,并以焊接接头的剪切力为目标对工艺参数进行了优化。结果表明:当焊接功率为1275 W、焊接速度为50 mm/s、焦距为200 mm、光斑直径为0.4 mm时,铜铝异种金属激光焊接接头的焊缝成形最好并获得最大剪切力,为2153.85 N,承载能力达到母材的97%,焊接接头的承载能力与母材基本匹配。 展开更多
关键词 铜铝异种金属 激光焊 剪切力
下载PDF
无缝药芯铜铝焊丝线坯挤压模具的设计
16
作者 张强 冯隽 +1 位作者 戴登峰 董光明 《有色金属加工》 CAS 2013年第6期43-45,共3页
药芯铜铝焊丝用于铜铝异种金属焊接的材料,文中设计的挤压模具,可制取无缝药芯铜铝焊丝线坯,在制取线坯的同时将钎剂注入其芯部,线坯经拉拔减径至焊丝。该技术具有生产效率高、产品性能稳定、质量可靠等特点。
关键词 药芯铜铝焊丝 铜铝异种金属焊接 挤压模具 无缝线坯
下载PDF