The Effect of Annealing under Non-vacuum on the Optical Properties of TiAlN Non-vacuum Solar Selective Absorbing Coating Prepared by Cathodic Arc Evaporation 被引量:2
1
作者 宫殿清 程旭东 +2 位作者 YE Weiping ZHANG Pu LUO Gan 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2013年第2期256-260,共5页
TiAIN solar selective absorbing coatings which were deposited on 304L stainless steel using cathodic arc evaporation method were annealed under non-vacuum at different temperatures with different times. The optical pr... TiAIN solar selective absorbing coatings which were deposited on 304L stainless steel using cathodic arc evaporation method were annealed under non-vacuum at different temperatures with different times. The optical properties (absorptance and emittance) of the coatings were measured by a spectrophotometer. It was found that, after being annealed for 2 hours at different temperatures, the absorptance of the coatings reached the highest value of 0.92 at 700 ℃ while the emittance got the lowest value of 0.38 at 800 ℃. When the coatings were annealed at 600 ℃ for 24 hours, the optical properties changed to 0.92/0.44 (absorptance/ emittance). By measuring the structure, morphology, elements and surface roughness of the coatings, it was found that both the elemental composition and the surface roughness of the coatings changed as a result of annealing, and these changes caused the change of the optical properties of the coatings. 展开更多
关键词 ANNEALING optiCal properties cathodic arc evaporation solar selective absorbing coating
下载PDF
Effect of 10% Si addition on cathodic arc evaporated TiAlSiN coatings 被引量:8
2
作者 朱丽慧 宋诚 +1 位作者 倪旺阳 刘一雄 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2016年第6期1638-1646,共9页
The effect of 10% Si (mole fraction) addition on TiAlSiN coatings was studied. Ti0.5Al0.5N, Ti0.5Al0.4Si0.1N and Ti0.55Al0.35Si0.1N coatings were deposited on WC?Co substrates by cathodic arc evaporation. The mi... The effect of 10% Si (mole fraction) addition on TiAlSiN coatings was studied. Ti0.5Al0.5N, Ti0.5Al0.4Si0.1N and Ti0.55Al0.35Si0.1N coatings were deposited on WC?Co substrates by cathodic arc evaporation. The microstructure and mechanical properties were characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), nano-indentation measurement and scratch test. The mechanisms of how Si affects the properties and failure modes of TiAlSiN coatings were also discussed. The results show that the addition of 10% Si results in the formation of nc-(Ti,Al,Si)N/a-Si3N4 nano-composite structure. The hardness and toughness of TiAlSiN coatings increase, whereas the coating adhesion strength decreases. Compared with Ti0.55Al0.35Si0.1N coating, Ti0.5Al0.4Si0.1N coating has higher hardness but lower toughness. The dominant failure mode of TiAlN coating is wedging spallation due to low toughness and strong interfacial adhesion. The dominant failure mode of TiAlSiN coatings is buckling spallation due to improved toughness and weakened interfacial adhesion. 展开更多
关键词 TiAlSiN coating TiAlN coating cathodic arc evaporation adhesion strength
下载PDF
Structure,mechanical and thermal properties of Y-doped CrAlN coatings 被引量:3
3
作者 Jin-lian TIAN Chun HU +2 位作者 Li CHEN Yu-min LOU Ning-ning ZHAO 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2021年第9期2740-2749,共10页
CrAlYN coatings with different Y contents(0,5 and 12 at.%)were deposited by cathodic arc evaporation to investigate the influence of Y-addition on the structure,mechanical and thermal properties of CrAlN coatings by u... CrAlYN coatings with different Y contents(0,5 and 12 at.%)were deposited by cathodic arc evaporation to investigate the influence of Y-addition on the structure,mechanical and thermal properties of CrAlN coatings by using X-ray diffraction,scanning electron microscopy,differential scanning calorimetry,thermal gravimetric analysis and nanoindentation.The structural transformation of single phase cubic Cr_(0.42)Al_(0.58)N and Cr_(0.39)Al_(0.56)Y_(0.05)N coatings to cubic−wurtzite mixed Cr_(0.32)Al_(0.56)Y_(0.12)N coating leads to a drop in hardness from(30.2±0.7)GPa of Cr_(0.42)Al_(0.58)N and(32.0±1.0)GPa of Cr_(0.39)Al_(0.56)Y_(0.05)N to(25.2±0.7)GPa of Cr_(0.32)Al_(0.56)Y_(0.12)N.The incorporation of 5 at.%Y retards the thermal decomposition of CrAlN,verified by the postponed precipitation of w-AlN and N-loss upon annealing.Correspondingly,Cr_(0.39)Al_(0.56)Y_(0.05)N coating consistently exhibits the highest hardness value during thermal annealing.Nevertheless,alloying with Y exerts an adverse effect on the oxidation resistance of CrAlN. 展开更多
关键词 CrAlYN coatings cathodic arc evaporation structural evolution HARDNESS thermal stability oxidation resistance