Objective To compare the long-term clinical effects of two kinds of crowns and bridges made of porcelain fused to Au-Pt alloy and Ni-Cr alloy. Methods A total of 131 teeth (64 patients) were rehabilitated using porcel...Objective To compare the long-term clinical effects of two kinds of crowns and bridges made of porcelain fused to Au-Pt alloy and Ni-Cr alloy. Methods A total of 131 teeth (64 patients) were rehabilitated using porcelain-fused-to-metal crowns, among which 59 were rehabilitated with Au-Pt alloy metal ceramic crown and 72 with Ni-Cr alloy metal ceramic crown. The porcelain fracture, shade, marginal adaptation, gingival discoloration, and gingival status after finishing restoration and 36 months of follow-up were evaluated. Results After 36 months of restoration, porcelain fused to Au-Pt alloy crown showed better clinical effects than porcelain fused to Ni-Cr alloy crown in shade, marginal adaptation, gingival discoloration, as well as gingival status (all P<0.05). Conclusion The Au-Pt alloy ceramic crown is superior to Ni-Cr alloy ceramic crown in long-term clinical effects.展开更多
The keeper and cast dowel-coping, as a primary component for a magnetic attachment, is easily subjected to corrosion in a wet environment, such as the oral cavity, which contains electrolyte-rich saliva, complex micro...The keeper and cast dowel-coping, as a primary component for a magnetic attachment, is easily subjected to corrosion in a wet environment, such as the oral cavity, which contains electrolyte-rich saliva, complex microflora and chewing behaviour and so on. The objective of this in vitro study was to examine the corrosion resistance of a dowel and coping-keeper complex fabricated by finish keeper and three alloys (cobalt-chromium, CoCr; silver-palladium-gold, PdAu; gold-platinum, AuPt) using a laser- welding process and a casting technique. The surface morphology characteristics and microstructures of the samples were examined by means of metallographic microscope and scanning electron microscope (SEM). Energy-dispersive spectroscopy (EDS) with SEM provided elements analysis information for the test samples after 10% oxalic acid solution etching test. Tafel polarization curve recordings demonstrated parameter values indicating corrosion of the samples when subjected to electrochemical testing. This study has suggested that massive oxides are attached to the surface of the CoCr-keeper complex but not to the AuPt-keeper complex. Only the keeper area of cast CoCr-keeper complex displayed obvious intergranular corrosion and changes in the Fe and Co elements, Both cast and laser-welded AuPt-keeper complexes had the highest free corrosion potential, followed by the PdAu-keeper complex. We concluded that although the corrosion resistance of the CoCr-keeper complex was worst, the keeper surface passive film was actually preserved to its maximum extent. The laser-welded CoCr- and PdAu-keeper complexes possessed superior corrosion resistance as compared with their cast specimens, but no significant difference was found between the cast and laser-welded AuPt-keeper complexes. The Fe-poor and Cr-rich band, appearing on the edge of the keeper when casting, has been proven to be a corrosion-prone area.展开更多
文摘Objective To compare the long-term clinical effects of two kinds of crowns and bridges made of porcelain fused to Au-Pt alloy and Ni-Cr alloy. Methods A total of 131 teeth (64 patients) were rehabilitated using porcelain-fused-to-metal crowns, among which 59 were rehabilitated with Au-Pt alloy metal ceramic crown and 72 with Ni-Cr alloy metal ceramic crown. The porcelain fracture, shade, marginal adaptation, gingival discoloration, and gingival status after finishing restoration and 36 months of follow-up were evaluated. Results After 36 months of restoration, porcelain fused to Au-Pt alloy crown showed better clinical effects than porcelain fused to Ni-Cr alloy crown in shade, marginal adaptation, gingival discoloration, as well as gingival status (all P<0.05). Conclusion The Au-Pt alloy ceramic crown is superior to Ni-Cr alloy ceramic crown in long-term clinical effects.
基金funded by the National Natural Science Foundation of China (Grant No. 81000456)the Science and Technology Department of Sichuan Province (Grant No. 2015JY0146)the Science and Technology Bureau of Chengdu (Grant No. 2014-HM01-00203-SF)
文摘The keeper and cast dowel-coping, as a primary component for a magnetic attachment, is easily subjected to corrosion in a wet environment, such as the oral cavity, which contains electrolyte-rich saliva, complex microflora and chewing behaviour and so on. The objective of this in vitro study was to examine the corrosion resistance of a dowel and coping-keeper complex fabricated by finish keeper and three alloys (cobalt-chromium, CoCr; silver-palladium-gold, PdAu; gold-platinum, AuPt) using a laser- welding process and a casting technique. The surface morphology characteristics and microstructures of the samples were examined by means of metallographic microscope and scanning electron microscope (SEM). Energy-dispersive spectroscopy (EDS) with SEM provided elements analysis information for the test samples after 10% oxalic acid solution etching test. Tafel polarization curve recordings demonstrated parameter values indicating corrosion of the samples when subjected to electrochemical testing. This study has suggested that massive oxides are attached to the surface of the CoCr-keeper complex but not to the AuPt-keeper complex. Only the keeper area of cast CoCr-keeper complex displayed obvious intergranular corrosion and changes in the Fe and Co elements, Both cast and laser-welded AuPt-keeper complexes had the highest free corrosion potential, followed by the PdAu-keeper complex. We concluded that although the corrosion resistance of the CoCr-keeper complex was worst, the keeper surface passive film was actually preserved to its maximum extent. The laser-welded CoCr- and PdAu-keeper complexes possessed superior corrosion resistance as compared with their cast specimens, but no significant difference was found between the cast and laser-welded AuPt-keeper complexes. The Fe-poor and Cr-rich band, appearing on the edge of the keeper when casting, has been proven to be a corrosion-prone area.