Rutting is one of the most damages in the asphalt surfaces for the orthotropic steel bridge decks. With Hamburg wheel tracking device, the suitable test conditions for Gussasphalt in Germany are pointed out, the high ...Rutting is one of the most damages in the asphalt surfaces for the orthotropic steel bridge decks. With Hamburg wheel tracking device, the suitable test conditions for Gussasphalt in Germany are pointed out, the high temperature behaviour of Gussasphalt with different binders are tested and compared. The polymer modified binder has higher resistance stability to rutting. The retained time and mixed frequency have obvious effects on Gussasphalt behaviour during Gussasphalt retained period.展开更多
Using a Hamburg wheel-track test device, the resistance to rutting of Gussasphalt is tested and compared. Gussasphalt with hard bitumen has good resistance to rutting. The related resistance abilities to cracking at ...Using a Hamburg wheel-track test device, the resistance to rutting of Gussasphalt is tested and compared. Gussasphalt with hard bitumen has good resistance to rutting. The related resistance abilities to cracking at low temperature of Gussasphalt are tested and compared through flexural experiments and the composite structure fatigue test with temperature dropping. Gussasphalt with high performance polymer modified bitumen has a longer fatigue life and a lower breaking temperature; they can be used in the future surfaces for steel bridge decks in Germany.展开更多
The normal asphalt index test, DSR test, FTIR and the GPC distribution analysis of molecular weight on the extraction and recovery of asphalt of the gussasphalt, SMA extraction and recovery of asphalt and the rotary-t...The normal asphalt index test, DSR test, FTIR and the GPC distribution analysis of molecular weight on the extraction and recovery of asphalt of the gussasphalt, SMA extraction and recovery of asphalt and the rotary-thin-film-oven-aged asphalt above 240 ℃ were introduced. The results indicate the rutting factor and fatigue factor of the extraction and recovery of asphalt of the gussasphalt are greatly improved, and an obvious absorption peak of carbonyl and a further decrease of the SBS molecular weight of the gussasphalt are found.展开更多
With the development of steel deck paving technology, the associated gussasphalt pavement system also develops maturely. In this paper, the structure characteristics and performance advantages are thoroughly explained...With the development of steel deck paving technology, the associated gussasphalt pavement system also develops maturely. In this paper, the structure characteristics and performance advantages are thoroughly explained by introducing the development course of gussasphalt. The material composition, properties and application effect of three typical pavement methods are analyzed. This paper is intended to give a relatively clear understanding regarding the specific features of gussasphalt, and provide some guidance to further expansion concerning gussasphalt pavement.展开更多
Four-point flexural fatigue test for Gussasphalt mixture specimen was carried out at a straincontrolled mode system. The results showed that the development of the tested stiffness modulus and phase angle of the mixtu...Four-point flexural fatigue test for Gussasphalt mixture specimen was carried out at a straincontrolled mode system. The results showed that the development of the tested stiffness modulus and phase angle of the mixtures with increasing load cycles exhibited three periods, initial generation, slow development and failure period. The fatigue crack generation zone formed in the third period, in which the macro mechanical properties were signifi cantly decreased. Moreover, we also analyzed the effects of asphalt content and mixing temperature on the fatigue life of the mixture. The results showed that the fi rst period when the specimen's initial stiffness modulus was reduced to 80% accounted for 5%-10% of the total fatigue life; the second period in which the reduction became slow and demonstrated a liner relationship with load cycles occupied 70%-85% of the fatigue life; and the third period was about 5%-10%. The results indicated that the lower the mixing temperature, the longer the fatigue life of Gussasphalt mixture. Besides, the increasing of asphalt content has a minor effect on the fatigue life of Gussasphalt mixture展开更多
文摘Rutting is one of the most damages in the asphalt surfaces for the orthotropic steel bridge decks. With Hamburg wheel tracking device, the suitable test conditions for Gussasphalt in Germany are pointed out, the high temperature behaviour of Gussasphalt with different binders are tested and compared. The polymer modified binder has higher resistance stability to rutting. The retained time and mixed frequency have obvious effects on Gussasphalt behaviour during Gussasphalt retained period.
文摘Using a Hamburg wheel-track test device, the resistance to rutting of Gussasphalt is tested and compared. Gussasphalt with hard bitumen has good resistance to rutting. The related resistance abilities to cracking at low temperature of Gussasphalt are tested and compared through flexural experiments and the composite structure fatigue test with temperature dropping. Gussasphalt with high performance polymer modified bitumen has a longer fatigue life and a lower breaking temperature; they can be used in the future surfaces for steel bridge decks in Germany.
基金Funded by the Science and Technology Project of Zhejiang Provincial Communication Department (No. 2007H28)
文摘The normal asphalt index test, DSR test, FTIR and the GPC distribution analysis of molecular weight on the extraction and recovery of asphalt of the gussasphalt, SMA extraction and recovery of asphalt and the rotary-thin-film-oven-aged asphalt above 240 ℃ were introduced. The results indicate the rutting factor and fatigue factor of the extraction and recovery of asphalt of the gussasphalt are greatly improved, and an obvious absorption peak of carbonyl and a further decrease of the SBS molecular weight of the gussasphalt are found.
文摘With the development of steel deck paving technology, the associated gussasphalt pavement system also develops maturely. In this paper, the structure characteristics and performance advantages are thoroughly explained by introducing the development course of gussasphalt. The material composition, properties and application effect of three typical pavement methods are analyzed. This paper is intended to give a relatively clear understanding regarding the specific features of gussasphalt, and provide some guidance to further expansion concerning gussasphalt pavement.
基金Funded by the National Natural Science Foundation of China(No.51202214)
文摘Four-point flexural fatigue test for Gussasphalt mixture specimen was carried out at a straincontrolled mode system. The results showed that the development of the tested stiffness modulus and phase angle of the mixtures with increasing load cycles exhibited three periods, initial generation, slow development and failure period. The fatigue crack generation zone formed in the third period, in which the macro mechanical properties were signifi cantly decreased. Moreover, we also analyzed the effects of asphalt content and mixing temperature on the fatigue life of the mixture. The results showed that the fi rst period when the specimen's initial stiffness modulus was reduced to 80% accounted for 5%-10% of the total fatigue life; the second period in which the reduction became slow and demonstrated a liner relationship with load cycles occupied 70%-85% of the fatigue life; and the third period was about 5%-10%. The results indicated that the lower the mixing temperature, the longer the fatigue life of Gussasphalt mixture. Besides, the increasing of asphalt content has a minor effect on the fatigue life of Gussasphalt mixture
文摘为了研究浇注式沥青胶浆的高温性能及评价指标,采用动态力学分析(DMA)方法,通过动态剪切流变试验,探讨了不同温度、沥青种类、粉胶比对浇注式沥青胶浆高温性能的影响.分析了广义剪切模量与浇注式沥青混合料高温变形之间的相关性,探讨了该指标作为浇注式胶浆高温性能评价指标的适用性,并以车辙深度为控制标准,对广义剪切模量以及60℃条件下的贯入度提出了建议值.结果表明:浇注式沥青胶浆复数剪切模量和相位角受温度、沥青种类、粉胶比因素影响明显;广义剪切模量与混合料永久变形呈良好的线性关系,能作为一种合适的劲度指标评价浇注式沥青胶浆的高温稳定性;60℃条件下,浇注式沥青混合料贯入度指标建议值不大于3.29 mm.