期刊文献+
共找到331篇文章
< 1 2 17 >
每页显示 20 50 100
Mathematical Modelling and 3D FEM Analysis of the Influence of Initial Stresses on the ERR in a Band Crack’s Front in the Rectangular Orthotropic Thick Plate 被引量:2
1
作者 Arzu Turan Dincel Surkay DAkbarov 《Computers, Materials & Continua》 SCIE EI 2017年第3期249-270,共22页
This paper deals with the mathematical modelling and 3D FEM study of the energy release rate(ERR)in the band crack’s front contained in the orthotropic thick rectangular plate which is stretched or compressed initial... This paper deals with the mathematical modelling and 3D FEM study of the energy release rate(ERR)in the band crack’s front contained in the orthotropic thick rectangular plate which is stretched or compressed initially before the loading of the crack's edge planes.The initial stretching or compressing of the plate causes uniformly distributed normal stress to appear acting in the direction which is parallel to the plane on which the band crack is located.After the appearance of the initial stress in the plate it is assumed that the crack's edge planes are loaded with additional uniformly distributed normal forces and the ERR caused with this additional loading is studied.The corresponding boundary value problem is formulated within the scope of the so-called 3D linearized theory of elasticity which allows the initial stress on the values of the ERR to be taken into consideration.Numerical results on the influence of the initial stress,anisotropy properties of the plate material,the crack’s length and its distance from the face planes of the plate on the values of the ERR,are presented and discussed.In particular,it is established that for the relatively greater length of the crack’s band,the initial stretching of the plate causes a decrease,but the initial compression causes an increase in the values of the ERR. 展开更多
关键词 band crack energy release rate stress intensity factor initial stress orthotropic material rectangular plate 3D FEM
下载PDF
TEM OBSERVATION OF LOCAL DEFORMATION BAND AT CRACK TIP 被引量:1
2
作者 YAO Kefu University of Science and Technology Beijing,Beijing,ChinaTANG Naivong CHEN Nanping Tsinghua University,Beijing,China 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 1992年第3期147-153,共7页
The thin foil specimen of a ferrite-austenite duplex stainless steel was tensiled under transmis- sion electron microscope(TEM).It was found that both in ferrite and austenite the local deformation band at crack tip w... The thin foil specimen of a ferrite-austenite duplex stainless steel was tensiled under transmis- sion electron microscope(TEM).It was found that both in ferrite and austenite the local deformation band at crack tip was formed near to the crack propagating direction.Its forma- tion was related with the crack tip Schmid factor,dislocation shielding,latent hardening and hardening coefficient.When the crack tip emitted dislocations to a slip system by the action of pure mode Ⅱ stress resolute,and the decreasing rate of hardening coefficient was suitable,lo- cal deformation band was easy to form. 展开更多
关键词 crack tip local deformation band dislocation shielding
下载PDF
Effect of Rare Earth on Void Band of Diffusion Layer and Properties of Aluminized Steel 被引量:4
3
作者 ZHANG Wei FAN Zhi-kang +3 位作者 HU Peng-fei LONG Yong-qiang LIU Hua WEN Jiu-ba 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2006年第5期60-64,78,共6页
The effects of the addition of rare earth (RE) elements on the void band in the diffusion layer, and the re sistances to both oxidation and spalling of aluminized steel were investigated through high temperature oxi... The effects of the addition of rare earth (RE) elements on the void band in the diffusion layer, and the re sistances to both oxidation and spalling of aluminized steel were investigated through high temperature oxidation and spalling tests. The results showed that RE had significant effects on the void band in the diffusion layer and the properties of aluminized steel. After diffusion treatment, a considerable number of the voids between the middle layer and transitional layer of pure aluminized coating, aggregated into wavy-line-shaped void bands parallel to the outer surface. For the RE added aluminized coating, only a few voids aggregated into intermittent block shapes. During high temperature oxidation at 800 ℃ for 200 h, the wavy void band of pure aluminized coating aggregated further into a linear crack parallel to the outer surface, and the internal oxidation occurred within them; the open cracks perpendicular to the surface penetrated through the diffusion layer. For the RE added aluminized coating, only a few voids aggregated into intermittent meniscus shapes. During cyclic spalling tests, the peeling, spallation, and pulver ulent cracking occurred along the void band in the diffusion layer of pure aluminized coating, but only a little spallation occurred in the diffusion layer of the RE-added aluminized coating, in which cracks perpendicular to the surface were much smaller than those of pure aluminized coating and did not penetrate through the diffusion layer. It is evident that RE addition can restrain the formation and aggregation of voids and subsequently improve the resistances to oxidation and spalling. The mechanism of the RE effect on the void band in the diffusion layer is also discussed. 展开更多
关键词 rare earth void band crack internal oxidation oxidation resistance spalling resistance aluminized steel
下载PDF
Metallurgical analysis of a failed maraging steel shear screw used in the band separation system of a satellite launch vehicle 被引量:5
4
作者 S.V.S. Narayana MURTY Sushant K. MANWATKAR E Ramesh NARAYANAN 《Defence Technology(防务技术)》 SCIE EI CAS CSCD 2016年第5期380-387,共8页
Maraging steels have excellent combination of strength and toughness and are extensively used for a variety of aerospace applications. In one such critical application, this steel was used to fabricate shear screws of... Maraging steels have excellent combination of strength and toughness and are extensively used for a variety of aerospace applications. In one such critical application, this steel was used to fabricate shear screws of a stage separation system in a satellite launch vehicle. During assembly preparations, one of the shear screws which connected the separation band and band end block has failed at the first thread. Microstructural analysis revealed that the crack originated from the root of the thread and propagated in an intergranular mode. The failure is attributed to combined effect of stress and corrosion leading to stress corrosion cracking. 展开更多
关键词 M250 grade maraging steel Shear screw Separation system Mermen band Stress corrosion cracking
下载PDF
Some Observations of Flow Localization and Shear Cracking in Pearlite during Deformation
5
作者 徐永波 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 1989年第2期135-137,共3页
Flow localization, which is an importantmode of deformation in engineering materi-als, has been the interesting subject ofa number of experimental observationsand theoretical investigations in recentyears. However, th... Flow localization, which is an importantmode of deformation in engineering materi-als, has been the interesting subject ofa number of experimental observationsand theoretical investigations in recentyears. However, the basic mechanism ofthe phenomena is not well understood atpresent. In a tensile test, the initiationand growth of a shear band are often simul-taneous. Therefore, it is rather difficult 展开更多
关键词 flow localization shear deformation band crack fracture DISLOCATION
下载PDF
Crack Prediction Model for Concrete Affected by Reinforcement Corrosion
6
作者 Jeb M. Stefan Luz M. Calle +4 位作者 Sven E. Eklund Mark R. Kolody Kunal Kupwade-Patil Eliza L. Montgomery Henry E. Cardenas 《Materials Sciences and Applications》 2019年第6期475-495,共21页
The purpose of this study was to develop an analytical model to predict the time required for cracking of concrete due to corrosion of the iron reinforcement. The concrete and cement specimens used for this study were... The purpose of this study was to develop an analytical model to predict the time required for cracking of concrete due to corrosion of the iron reinforcement. The concrete and cement specimens used for this study were batched with cover material ranging from 0.75 to 1.3 in (1.91 to 3.30 cm). The extent of cover material was not formulated into the model under the assumption that crack initiation would tend to produce visible cracking within a relatively short time period. The model was derived using both Hooke’s Law and the volume expansion induced by the corrosion oxides. Correlation achieved with specimen cracking data from the literature was relatively good with a 95% level of confidence. This model presents a key benefit to facility and infrastructure managers by enabling them to plan the time when corrosion mitigating actions are required. It also provides a significant convenience as the condition of the concrete structure or its environment changes over time. The only parameter that needs to be updated over time is the corrosion rate measurement. This single parameter captures the most influential impact that stems from several other parameters which tend to be required in models that are more mechanistically definitive. 展开更多
关键词 crackING Model CONCRETE Corrosion Marine PORE band Green RUST
下载PDF
脉冲电流对高速冲击下2A10铝绝热剪切带作用规律研究
7
作者 胡前程 李伟昊 +2 位作者 李成成 陈立 李兴文 《电工技术学报》 EI CSCD 北大核心 2024年第19期5937-5946,共10页
材料在高速冲击下产生绝热剪切带,电辅助电磁成形技术通过在试样变形同时通入电流可增强材料塑性变形能力,但脉冲电流对绝热剪切带的作用规律目前尚不明晰,制约了材料在超高速冲击环境下的应用。该文设计了一种偏轴长杆箍件试样,通过脉... 材料在高速冲击下产生绝热剪切带,电辅助电磁成形技术通过在试样变形同时通入电流可增强材料塑性变形能力,但脉冲电流对绝热剪切带的作用规律目前尚不明晰,制约了材料在超高速冲击环境下的应用。该文设计了一种偏轴长杆箍件试样,通过脉冲功率源和电磁斥力盘开展了2A10铝合金在极端多物理场环境下即电流密度为10^(8)~10^(9) A/m^(2),应变率≥10^(4)/s的动态变形特性研究。对试样进行金相处理后可观测到材料微观特征的演化过程,对比不同条件下微观特征分布得到了极端多物理场条件下电流密度对材料动态变形的作用规律。结果表明,施加电流后裂纹和绝热剪切带的长度减少,且长度随电流密度增大而逐渐减少。 展开更多
关键词 超高速冲击 电流密度 绝热剪切带 裂纹
下载PDF
冻融作用下条带状磁铁石英岩破裂失稳过程裂纹演化特征试验研究
8
作者 邵国梁 夏冬 +2 位作者 贾淯斐 李铸熙 严加驹 《黄金科学技术》 CSCD 北大核心 2024年第6期1030-1045,共16页
为探究冻融作用对条带状磁铁石英岩破裂失稳过程裂纹演化特征的影响规律,对冻融温度区间为-20~20℃、最长冻融周期为280次的岩石开展了力学与声发射试验研究。结果表明:单轴抗压强度和弹性模量自干燥状态时的200.93 MPa和21.67 GPa下降... 为探究冻融作用对条带状磁铁石英岩破裂失稳过程裂纹演化特征的影响规律,对冻融温度区间为-20~20℃、最长冻融周期为280次的岩石开展了力学与声发射试验研究。结果表明:单轴抗压强度和弹性模量自干燥状态时的200.93 MPa和21.67 GPa下降至冻融280次时的106.64 MPa和8.24 GPa;低冻融周期(冻融循环≤40次)作用下,岩样在裂纹演化过程中以拉伸裂纹为主、剪切裂纹为辅,裂纹破裂主要发生在微裂隙加速扩展阶段,该阶段中、高频信号的出现时间稍早于中、低频信号,且高频条带所对应的幅值较高;高冻融周期(冻融循环>40次)作用下,岩样裂纹演化同样以拉伸裂纹为主,但剪切裂纹占比低于低冻融周期岩样,随着冻融周期的增加,岩样裂纹总量呈降低趋势,在微裂隙加速扩展阶段,中、高频信号与中、低频信号基本上同时大量出现,岩样超高频信号所对应的幅值随着冻融周期的增加而降低;低冻融周期作用下,高能信号主要产生于微裂隙加速扩展阶段,而高冻融周期作用下,高能信号的分布较为分散,且岩样自身声发射能量跨度以及大能量声发射事件出现的概率相较低冻融周期岩样均有所下降。 展开更多
关键词 条带状磁铁石英岩 冻融损伤 裂纹演化 声发射 抗压强度
下载PDF
轴承滚子冲压裂纹形成机理及控制工艺研究
9
作者 董小波 史亚妮 +3 位作者 魏建文 王超 尤蕾蕾 崔广发 《热处理技术与装备》 2024年第4期26-30,共5页
某批轴承冲压滚子端面出现裂纹,通过分析其冲压过程,观察其裂纹处及断口的形貌和显微组织,对裂纹产生的主要原因进行分析。结果表明,原材料局部存在的碳化物液析和碳化物带状超标导致该部位塑韧性变差;并且冷镦过程中大端面的变形较大,... 某批轴承冲压滚子端面出现裂纹,通过分析其冲压过程,观察其裂纹处及断口的形貌和显微组织,对裂纹产生的主要原因进行分析。结果表明,原材料局部存在的碳化物液析和碳化物带状超标导致该部位塑韧性变差;并且冷镦过程中大端面的变形较大,加工硬化作用强,在二者叠加作用下产生裂纹。提出了解决裂纹的措施,需要严格控制原材料质量,保证材料组织和成分的均匀性,避免类似问题再次发生。 展开更多
关键词 冲压滚子 大端面 裂纹 碳化物带状 碳化物液析
下载PDF
水化热引起的大体积混凝土墙应力与开裂分析 被引量:62
10
作者 张子明 郭兴文 杜荣强 《河海大学学报(自然科学版)》 CAS CSCD 北大核心 2002年第5期12-16,共5页
应用基于Arrhenius理论的混凝土绝热温升和徐变模型 ,考虑温度对早期混凝土水化热化学反应速率和徐变特性的影响 ,研究了大体积混凝土墙的温度应力和温度开裂问题 ,并提出了求解非线性微分方程的半解析法 .研究中采用Bazant教授提出的... 应用基于Arrhenius理论的混凝土绝热温升和徐变模型 ,考虑温度对早期混凝土水化热化学反应速率和徐变特性的影响 ,研究了大体积混凝土墙的温度应力和温度开裂问题 ,并提出了求解非线性微分方程的半解析法 .研究中采用Bazant教授提出的裂缝带模型计算温度裂缝 ,采用半解析迭代法逐步加载计算温度、应力和裂缝的产生与扩展 .研究结果表明 ,浇筑温度极大地影响材料的热学力学性质和结构的温升、温度应力和开裂 .研究还揭示了不同养护条件对温度。 展开更多
关键词 大体积混凝土墙 应力 水化热 裂缝带模型 半解析法 混凝土结构
下载PDF
基于加工图的Ti-40阻燃钛合金热变形机理研究 被引量:27
11
作者 曾卫东 周义刚 +3 位作者 舒滢 赵永庆 杨锦 张学敏 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2007年第1期1-6,共6页
采用热模拟压缩试验研究了Ti-40阻燃钛合金在温度900℃~1100℃、应变速率0.01s-1~10s-1范围内的高温变形特性,发现合金的流动应力-应变曲线具有应力峰和流变软化特征,在高温、高应变速率下,出现不连续屈服现象。根据动态材料模型(DMM... 采用热模拟压缩试验研究了Ti-40阻燃钛合金在温度900℃~1100℃、应变速率0.01s-1~10s-1范围内的高温变形特性,发现合金的流动应力-应变曲线具有应力峰和流变软化特征,在高温、高应变速率下,出现不连续屈服现象。根据动态材料模型(DMM)建立的Ti-40合金加工图大致可以分为5个区域:(1)在温度900℃~950℃,应变速率大于1s-1时,易发生45o角剪切开裂,出现明显的剪切变形带,功率耗散率达最小值。(2)在温度1000℃~1100℃、应变速率大于1s-1时,易出现“豆腐渣”式和纵向开裂,大变形时出现局部塑性流动。这2个区域为流动失稳区,在制定热加工工艺时应尽量避免。(3)在高温(≥1050℃)、低应变速率区(≤0.1s-1),功率耗散率为46%~76%,达到最大值,呈现连续再结晶的特征。(4)在900℃~950℃、应变速率0.01s-1~0.1s-1区域内主要发生动态回复,功率耗散率为22%~32%。(5)在温度950℃~1050℃、应变速率0.1s-1~1s-1范围为再结晶区域,功率耗散率为36%~50%。结果表明,加工图是控制材料组织演变和优化工艺的一种有效手段。 展开更多
关键词 Ti-40合金 加工图 变形机理 开裂 剪切变形带 再结晶
下载PDF
基于等效时间的早期混凝土温度裂缝分析 被引量:11
12
作者 张子明 郑国芳 宋智通 《水利水运工程学报》 CSCD 北大核心 2004年第1期41-44,共4页
基于等效时间的混凝土绝热温升、热传导方程,考虑温度对早期混凝土水化热化学反应速率和徐变特性的影响,计算了大体积混凝土墙中心的温升.采用裂缝带模型计算温度裂缝,用半解析迭代法进行了混凝土墙的温度应力和开裂计算.
关键词 混凝土 水化热 等效时间 裂缝带模型 应力 混凝土墙 温度裂缝
下载PDF
石油专用管材的氢致开裂研究 被引量:10
13
作者 张旺峰 梁永芳 朱金华 《西安公路交通大学学报》 EI CAS CSCD 北大核心 1998年第3期91-93,共3页
研究了五种材料在NACE溶液中的氢致开裂(HIC)行为。结果表明:当材料中存在带状组织时,HIC敏感性增高。为避免带状组织及HIC,要控制Mn、P含量。给出了Mn、P含量的推荐值:Mn≤1.3%,P≤0.016%。
关键词 氢致开裂 石油工业 套管 油气管
下载PDF
基于温度应力仿真分析的碾压混凝土重力坝诱导缝开裂研究 被引量:19
14
作者 周伟 常晓林 +2 位作者 刘杏红 范五一 丁福珍 《岩石力学与工程学报》 EI CAS CSCD 北大核心 2006年第1期122-127,共6页
考虑彭水水电站碾压混凝土坝的实际碾压浇筑过程,采用混凝土钝裂缝带模型,在三维瞬态有限元温度应力仿真分析的基础上,对大坝诱导缝的开裂及裂缝扩展进行了跟踪计算。计算结果表明,坝体的上游面诱导缝缝端应力强度因子局部超过混凝土的... 考虑彭水水电站碾压混凝土坝的实际碾压浇筑过程,采用混凝土钝裂缝带模型,在三维瞬态有限元温度应力仿真分析的基础上,对大坝诱导缝的开裂及裂缝扩展进行了跟踪计算。计算结果表明,坝体的上游面诱导缝缝端应力强度因子局部超过混凝土的断裂韧度而发生开裂,且诱导缝的开裂明显减小了坝段中部区域的拉应力。根据诱导缝的开裂分析结果,建议诱导缝的设置长度为4.5m。 展开更多
关键词 水利工程 碾压混凝土重力坝 诱导缝 温度仿真 钝裂缝带模型
下载PDF
疲劳过程中垂直晶界Cu双晶形变带中位错组态与裂纹形核 被引量:5
15
作者 李勇 李守新 李广义 《金属学报》 SCIE EI CAS CSCD 北大核心 2004年第5期462-466,共5页
采用电子通道衬度技术对垂直晶界Cu双晶在疲劳过程中位错组态的演化与裂纹的形核进行了研究,结果表明,形变带中墙结构的间距从形成之初到疲劳裂纹出现始终保持恒定;穿晶裂纹与沿晶裂纹尖端的位错组态均为胞结构;裂纹优先从形变带产生。
关键词 Cu双晶 位错组态 裂纹 形变带
下载PDF
沥青路面裂缝贴缝带的性能评价及技术要求 被引量:6
16
作者 李峰 石小培 徐剑 《北京工业大学学报》 CAS CSCD 北大核心 2013年第12期1855-1860,共6页
为了评价沥青路面裂缝贴缝带的路用性能,进行了裂缝修补工程试验及跟踪观测,结果表明:贴缝带施工效率高、次生病害少、路用性能良好.针对贴缝带的3种主要失效模式,参考交通行业密封胶标准和相关企业标准,提出了锥入度、软化点、拉拔和... 为了评价沥青路面裂缝贴缝带的路用性能,进行了裂缝修补工程试验及跟踪观测,结果表明:贴缝带施工效率高、次生病害少、路用性能良好.针对贴缝带的3种主要失效模式,参考交通行业密封胶标准和相关企业标准,提出了锥入度、软化点、拉拔和低温拉伸等4个评价方法.收集了6种贴缝带样品进行室内试验,根据试验结果,参考加热型密封胶的技术要求,提出了相应的技术要求. 展开更多
关键词 沥青路面 裂缝 贴缝带 失效模式 性能评价方法
下载PDF
应用加工图理论研究Ti_2AlNb基合金的高温变形特性 被引量:17
17
作者 曾卫东 徐斌 +4 位作者 何德华 梁晓波 李世琼 张建伟 周义刚 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2007年第4期592-596,共5页
基于动态材料模型(DMM),建立了Ti2AlNb基合金(Ti-22Al-25Nb)在温度94012-1060℃,应变速率0.001s^-1-10s^-1范围内的加工图,并利用该图分析了合金的高温变形特性。结果发现:在温度94012~97012,应变速率0.4s^-1~10s^-1和温度... 基于动态材料模型(DMM),建立了Ti2AlNb基合金(Ti-22Al-25Nb)在温度94012-1060℃,应变速率0.001s^-1-10s^-1范围内的加工图,并利用该图分析了合金的高温变形特性。结果发现:在温度94012~97012,应变速率0.4s^-1~10s^-1和温度970℃—1060℃,应变速率1s^-1~10s^-1范围为流动失稳区,前者范围内主要发生绝热剪切变形和45°角剪切开裂,功率耗散率达到最小值;后者区域内以局部塑性流动和纵向开裂为主,功率耗散率小于33%。热加工图的其余部分为塑性加工的“安全区”,主要发生再结晶。在温度94012~970℃,应变速率0.001s^-1-0.4s^-1范围,以α2/O相板条球化为主;在温度970℃~1030℃,应变速率0.001s^-1~1S^-1范围,功率耗散率为35%-45%,呈现连续再结晶特征。在温度1030℃~1060℃。麻蛮谏率0.001s^-1-0.1s^-1范围。功率耗散率为45%~66%。达最大值,发生连续再结晶晶粒长大。 展开更多
关键词 TI2ALNB基合金 Ti-22Al-25Nb 加工图 开裂 绝热剪切变形 再结晶
下载PDF
管线用钢显微组织对氢致裂纹影响的研究 被引量:17
18
作者 顾宝兰 徐学东 周莉 《理化检验(物理分册)》 CAS 2006年第1期8-11,共4页
选用了四种不同显微组织的国产同牌号管线用钢,根据美国腐蚀工程师协会标准NACE TM0284-2003,对其进行氢致开裂实验,并用光学显微镜和扫描电镜对其断面组织进行了观察,分析其显微组织对抗氢致裂纹性能的影响。认为,带状组织以及组织不... 选用了四种不同显微组织的国产同牌号管线用钢,根据美国腐蚀工程师协会标准NACE TM0284-2003,对其进行氢致开裂实验,并用光学显微镜和扫描电镜对其断面组织进行了观察,分析其显微组织对抗氢致裂纹性能的影响。认为,带状组织以及组织不均匀性是引起材料抗氢致裂纹性能下降的主要因素,但这两种因素引起开裂的方式和机理不同。同时发现晶粒度大小对该材料抗氢致裂纹性能没有明显影响。 展开更多
关键词 氢致裂纹 显微组织 带状组织
下载PDF
聚环氧乙烷球晶的带状结构与球晶内部的环形裂纹 被引量:8
19
作者 丁建东 朱军祥 杨玉良 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 1996年第3期498-499,共2页
聚环氧乙烷球晶的带状结构与球晶内部的环形裂纹丁建东,朱军祥,杨玉良(复旦大学高分子科学系、国家教委聚合物分子工程开放实验室,上海,200433)关键词聚合物,带状球晶,裂纹聚环氧乙烷(PEO)具有高度的柔顺性,易于结... 聚环氧乙烷球晶的带状结构与球晶内部的环形裂纹丁建东,朱军祥,杨玉良(复旦大学高分子科学系、国家教委聚合物分子工程开放实验室,上海,200433)关键词聚合物,带状球晶,裂纹聚环氧乙烷(PEO)具有高度的柔顺性,易于结晶,因而被人们选作研究聚合物结晶的... 展开更多
关键词 带状球晶 裂纹 聚环氧乙烷
下载PDF
穿甲试验靶板中绝热剪切带特征及与裂纹的关系 被引量:4
20
作者 李金泉 彭守凡 +1 位作者 黄德武 王敏杰 《兵器材料科学与工程》 CAS CSCD 北大核心 2007年第6期29-32,共4页
采用14.5mm弹道枪发射7.6mm次口径93W穿甲弹,对603钢进行穿甲侵彻试验。结果表明:在一定的条件下,绝热剪切带交叉分布,剪切带内变形极大且不均匀,成为微裂纹和微孔洞的起源,这些微裂纹和微孔洞相互连接,导致裂纹沿绝热剪切带萌生、扩展... 采用14.5mm弹道枪发射7.6mm次口径93W穿甲弹,对603钢进行穿甲侵彻试验。结果表明:在一定的条件下,绝热剪切带交叉分布,剪切带内变形极大且不均匀,成为微裂纹和微孔洞的起源,这些微裂纹和微孔洞相互连接,导致裂纹沿绝热剪切带萌生、扩展,最终形成沿整个绝热剪切带的大裂纹,使部分穿孔表面形成碎片,造成靶板的损伤,降低靶板的力学性能,是靶板破坏的先兆;但绝热剪切带与裂纹并不完全等同,有些剪切带由于变形量不大,不产生裂纹。 展开更多
关键词 靶板 侵彻 绝热剪切带 裂纹