The optimum technique for silk finishing with a silicone -containing epoxide A is as follows: The silk fabrics is twodipped - two - nipped in a finishing liquid with 6 % (w/w) of the silicone - containing epoxide A, a...The optimum technique for silk finishing with a silicone -containing epoxide A is as follows: The silk fabrics is twodipped - two - nipped in a finishing liquid with 6 % (w/w) of the silicone - containing epoxide A, and 0.3 % ofcatalyst with a pick- up of 100% ± 2%, then drying at60℃ for 3.5 min, finally steaming at 110℃ for 7 min.After crease resistant finishing with the silicone-contain-ing epoxide A, silk can greatly improve both the dry andwet resiliencies. The finished fabrics can endure 20 timeshome laundry and still have good wrinkle resistant prop-erties, while other physical properties such as展开更多
基金Supported by the Foundation of Huo Yingdong Youth Teacher and Shanghai Youth Teacher
文摘The optimum technique for silk finishing with a silicone -containing epoxide A is as follows: The silk fabrics is twodipped - two - nipped in a finishing liquid with 6 % (w/w) of the silicone - containing epoxide A, and 0.3 % ofcatalyst with a pick- up of 100% ± 2%, then drying at60℃ for 3.5 min, finally steaming at 110℃ for 7 min.After crease resistant finishing with the silicone-contain-ing epoxide A, silk can greatly improve both the dry andwet resiliencies. The finished fabrics can endure 20 timeshome laundry and still have good wrinkle resistant prop-erties, while other physical properties such as