制备工艺对0-3型压电复合材料的d_(33)的影响 被引量:4
1
作者 何政 陈文 +2 位作者 徐庆 周静 孙华君 《压电与声光》 CSCD 北大核心 2003年第5期400-402,共3页
采用固化、热压、冷压工艺制备0-3型PZNN/PVDF压电复合材料,用准静态压电测试仪测试了压电复合材料的压电应变常数d_(33),通过对以上三种制备工艺的对比,结果表明:在无机和有机压电材料的体积比大于70%时,冷压工艺优于固化和热压工艺,... 采用固化、热压、冷压工艺制备0-3型PZNN/PVDF压电复合材料,用准静态压电测试仪测试了压电复合材料的压电应变常数d_(33),通过对以上三种制备工艺的对比,结果表明:在无机和有机压电材料的体积比大于70%时,冷压工艺优于固化和热压工艺,在它们的体积比小于70%时,热压工艺优于冷压和固化工艺。 展开更多
关键词 制备工艺 0-3型 压电复合材料 压电应变常数d33
下载PDF
K_(0.9)Li_(0.1)(Ta_(0.5)Nb_(0.5))O_3晶体压电应变系数的测量 被引量:2
2
作者 尹鑫 魏景谦 王继扬 《压电与声光》 CSCD 北大核心 1994年第5期55-56,共2页
用准静态d_(33)测量仪和干涉法相结合。测量了K_(0.9)Li_(0.1)(Ta_(0.5)Nb_(0.5)Nb_(0.5))O_3晶体的压电应变系数。结果为:d_(33)=86.0,d_(33)=一29.5,d... 用准静态d_(33)测量仪和干涉法相结合。测量了K_(0.9)Li_(0.1)(Ta_(0.5)Nb_(0.5)Nb_(0.5))O_3晶体的压电应变系数。结果为:d_(33)=86.0,d_(33)=一29.5,d_(15)=112.9×10 ̄(-12)C/N. 展开更多
关键词 KLiO晶体 压电应变系数 准静态 测量仪
下载PDF
Outstanding electromechanical performance in piezoelectric ceramics via synergistic effects of defect engineering and domain miniaturization
3
作者 Zhifei Zhang Liang Chen +5 位作者 Huajie Luo Yueyun Zhang Yonghao Yao Guanfu Liu He Qi Jun Chen 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2023年第27期1-8,共8页
Piezoelectric ceramics with high mechanical quality factor Q_(m) and large piezoelectric coefficient d_(33) are urgently required for advanced piezoelectric applications.However,obtaining both of these prop-erties sim... Piezoelectric ceramics with high mechanical quality factor Q_(m) and large piezoelectric coefficient d_(33) are urgently required for advanced piezoelectric applications.However,obtaining both of these prop-erties simultaneously remains a difficult challenge due to their mutually restrictive relationship.Here 0.5Pb(Ni_(1/3)Nb_(2/3))O_(3)-0.5Pb(Zr_(0.3)Ti_(0.7))O_(3) piezoceramic with tetragonal(T)-rich MPB is designed as a matrix to construct the defect engineering by doping low-valent Mn ions.The strong coupling of defect dipole and T-rich phase can effectively hinder the rotation of P_(s),restrict domain wall motion and improve Q_(m).At the same time,the substituted Mn ions will introduce local random field,destroying the long-range or-dering of ferroelectric domain and reducing domain size.The miniaturized domain structure can increase poling efficiency and inhibit the reduction of d_(33).Guided by this strategy,Q_(m) has increased by more than 10 times and d_(33) has only decreased by about 25%.The optimized electromechanical performance with Q_(m)=822,d_(33)=502 pC/N,k_(p)=0.55 and tanδ=0.0069 can be obtained in the present study. 展开更多