The flotation behavior of Xixia andalusite was studied with different collectors.The tests were conducted with a pure andalusite sample in micro-flotation cell and then with an ore sample in a mechanical flotation cel...The flotation behavior of Xixia andalusite was studied with different collectors.The tests were conducted with a pure andalusite sample in micro-flotation cell and then with an ore sample in a mechanical flotation cell.The surface charge was measured on pure andalusite sample and the isoelectric point(IEP) was found to be pH 5.2.Andalusite is floated with an amine collector above IEP where mineral surface is negatively charged.In contrast,an alkyl sulfonate collector(sodium dodecyl benzene sulfonate) is effective in the pH range where andalusite surface is positively charged.Furthermore,andalusite is floated with oleate in neutral and mildly alkaline pH values.55.3% Al2O3 is produced with 75.6% andalusite recovery when using the alkyl benzene sulfonate collector.Starch is found to be an effective depressant for gangue minerals in alkyl benzene sulfonate flotation.Moreover,slimes are found to have an adverse effect on the flotation of andalusite.Therefore,pretreatment by desliming and pre-float(to remove carbonaceous species) prior to andalusite flotation is necessary.展开更多
In light of the problems of low-quality and low degree of comprehensive utilization of Guangdong muscovite-type kaolin, the reasons affecting the quality of kaolin were found to be a small amount of maroon powdery goe...In light of the problems of low-quality and low degree of comprehensive utilization of Guangdong muscovite-type kaolin, the reasons affecting the quality of kaolin were found to be a small amount of maroon powdery goethite adhering to the surface of kaolin and minor muscovite affecting the firing whiteness of products. The ores were dealt with by using the new combined process of attritioning-classifieation-bleaching and flotation. The separation of kaolin from muscovite, quartz and feldspar can come true through the new process. The high-quality kaolin with the firing whiteness of 91% can be obtained, and the muscovite is comprehensively recovered by adopting the key technology of flotation. The content of high-purity muscovite produced is over 99%. The muscovite discarded by original process can be comprehensively recovered.展开更多
The Kansanshi mixed copper sulfide-oxide ore contains significant proportions of fine material manifesting in a variety of processing challenges. This paper presents the work which was carried out to evaluate the effi...The Kansanshi mixed copper sulfide-oxide ore contains significant proportions of fine material manifesting in a variety of processing challenges. This paper presents the work which was carried out to evaluate the efficacy of desliming in improving the flotation response of the ore. Two modes of desliming were investigated, namely;sieving and elutriation after which the deslimed material was subjected to Kansanshi standard laboratory flotation conditions. The minimum copper feed grade for the mixed copper ore was 0.5% Total Copper (TCu). The outcome of this work has shown that desliming improves the flotation response of the Kansanshi mixed copper ore. At a rougher copper concentrate grade of 8%, copper metal recoveries obtained with desliming were in excess of 70% compared to 58% achieved with baseline tests without desliming. It was further observed that desliming resulted in improved flotation rates for the sulfide minerals. For a flotation time of 3 minutes, recoveries of 69% and 74% were obtained with elutriation and sieving respectively compared to 58% recovery for baseline tests. From the same results it was also evident that, of the two modes of desliming investigated, sieving yielded better performance than elutriation.展开更多
文摘The flotation behavior of Xixia andalusite was studied with different collectors.The tests were conducted with a pure andalusite sample in micro-flotation cell and then with an ore sample in a mechanical flotation cell.The surface charge was measured on pure andalusite sample and the isoelectric point(IEP) was found to be pH 5.2.Andalusite is floated with an amine collector above IEP where mineral surface is negatively charged.In contrast,an alkyl sulfonate collector(sodium dodecyl benzene sulfonate) is effective in the pH range where andalusite surface is positively charged.Furthermore,andalusite is floated with oleate in neutral and mildly alkaline pH values.55.3% Al2O3 is produced with 75.6% andalusite recovery when using the alkyl benzene sulfonate collector.Starch is found to be an effective depressant for gangue minerals in alkyl benzene sulfonate flotation.Moreover,slimes are found to have an adverse effect on the flotation of andalusite.Therefore,pretreatment by desliming and pre-float(to remove carbonaceous species) prior to andalusite flotation is necessary.
文摘In light of the problems of low-quality and low degree of comprehensive utilization of Guangdong muscovite-type kaolin, the reasons affecting the quality of kaolin were found to be a small amount of maroon powdery goethite adhering to the surface of kaolin and minor muscovite affecting the firing whiteness of products. The ores were dealt with by using the new combined process of attritioning-classifieation-bleaching and flotation. The separation of kaolin from muscovite, quartz and feldspar can come true through the new process. The high-quality kaolin with the firing whiteness of 91% can be obtained, and the muscovite is comprehensively recovered by adopting the key technology of flotation. The content of high-purity muscovite produced is over 99%. The muscovite discarded by original process can be comprehensively recovered.
文摘The Kansanshi mixed copper sulfide-oxide ore contains significant proportions of fine material manifesting in a variety of processing challenges. This paper presents the work which was carried out to evaluate the efficacy of desliming in improving the flotation response of the ore. Two modes of desliming were investigated, namely;sieving and elutriation after which the deslimed material was subjected to Kansanshi standard laboratory flotation conditions. The minimum copper feed grade for the mixed copper ore was 0.5% Total Copper (TCu). The outcome of this work has shown that desliming improves the flotation response of the Kansanshi mixed copper ore. At a rougher copper concentrate grade of 8%, copper metal recoveries obtained with desliming were in excess of 70% compared to 58% achieved with baseline tests without desliming. It was further observed that desliming resulted in improved flotation rates for the sulfide minerals. For a flotation time of 3 minutes, recoveries of 69% and 74% were obtained with elutriation and sieving respectively compared to 58% recovery for baseline tests. From the same results it was also evident that, of the two modes of desliming investigated, sieving yielded better performance than elutriation.