Reinforcement detail drawings are one important part of the design of hydraulic structures and the important basis of construction and management. However, the efficiency of the traditional creation of engineering dra...Reinforcement detail drawings are one important part of the design of hydraulic structures and the important basis of construction and management. However, the efficiency of the traditional creation of engineering drawings is very low and the workload is heavy. There is no satisfactory software for hydraulic engineering because of the irregularity and diversity of hydraulic structures' shape. An automatic generation system of reinforcement detail drawings for hydraulic structures is introduced. Its functions and modules are introduced first. The related technologies such as automatic driensioning are discussed in detail. At the end of the paper, an example is given.展开更多
In this study,a numerical analysis was conducted on the ductile fracture of a 2-mm diameter Mg-1Zn-0.5Mn-0.5Sr-0.1Ca alloy wire during drawing.The hexagonally close-packed crystal structure of Mg alloys causes asymmet...In this study,a numerical analysis was conducted on the ductile fracture of a 2-mm diameter Mg-1Zn-0.5Mn-0.5Sr-0.1Ca alloy wire during drawing.The hexagonally close-packed crystal structure of Mg alloys causes asymmetric fracture behavior,especially in the compression region.The aim of this study is to develop a comprehensive damage model for Mg alloy wire that accurately predicts ductile fracture,with a focus on the compression region.A novel experimental method was introduced to measure the ductile fracture of Mg alloy wires under different stress states.The wire drawing process was simulated using the Generalized Incremental Stress-State dependent damage(GISSMO)Model and the Semi-Analytical Model for Polymers(SAMP)model.The damage model's prediction and the experimental results were found to be in excellent agreement,especially in determining crack initiation.Computational analysis established a safe zone diagram for die angle and reduction ratio,and experimental validation confirmed the feasibility of this approach.The proposed damage model can provide a practical and reliable analysis for optimizing the drawing process of Mg alloy wire.展开更多
A specific revised HFCVD apparatus and a novel process combining HFCVD and polishing technique were presented to deposit the micro-and nano-crystalline multilayered ultra-smooth diamond(USCD) film on the interior-ho...A specific revised HFCVD apparatus and a novel process combining HFCVD and polishing technique were presented to deposit the micro-and nano-crystalline multilayered ultra-smooth diamond(USCD) film on the interior-hole surface of WC-Co drawing dies with aperture ranging from d1.0 mm to 60 mm.Characterization results indicate that the surface roughness values(Ra) in the entry zone,drawing zone and bearing zone of as-fabricated USCD coated drawing die were measured as low as 25.7,23.3 and 25.5 nm,respectively.Furthermore,the friction properties of USCD films were examined in both dry sliding and water-lubricating conditions,and the results show that the USCD film presents much superior friction properties.Its friction coefficients against ball-bearing steel,copper and silicon nitride balls(d4 mm),is always lower than that of microcrystalline diamond(MCD) or WC-Co sample,regardless of the lubricating condition.Meanwhile,it still presents competitive wear resistance with the MCD films.Finally,the working lifetime and performance of as-fabricated USCD coated drawing dies were examined under producing low-carbon steel pipes in dry-sliding and water-lubricating conditions.Under the water-lubricating drawing condition,its production significantly increases by about 20 times compared with the conventional WC-Co drawing dies.展开更多
The development of microstructure and texture during cold deep drawing of commercially pure titanium(CP-Ti) was investigated.Three parts,stretching region,drawing region and flange region,were sequentially formed in...The development of microstructure and texture during cold deep drawing of commercially pure titanium(CP-Ti) was investigated.Three parts,stretching region,drawing region and flange region,were sequentially formed in the deep drawing process of the hemispheric surface part,with reference to deformation modes and strain regimes.Results show that the plastic strain is accommodated by dislocation slip and deformation twinning in the whole deep drawing process.The texture of the CP-Ti sheet and its drawn part consists of rolling texture component and recrystallization texture component.The intensity and type of the initial texture varied during the drawing process are related to the production of deformation twinning and dislocation slip.Twinning weakens the initial texture by randomizing the orientations of crystals,especially for the recrystallization texture.The recrystallization texture in the drawing region disappears due to the significant forming of twinning.Furthermore,over drawing would result in the predominance of dislocation slip and the texture is strengthened.展开更多
The texture evolution of cold drawing copper wires produced by continuous casting was measured by X-ray diffractometry and electron back-scatter diffractometry,and was simulated using Taylor model.The results show tha...The texture evolution of cold drawing copper wires produced by continuous casting was measured by X-ray diffractometry and electron back-scatter diffractometry,and was simulated using Taylor model.The results show that in the drawn poly-crystal copper wires produced by traditional continuous casting,111 and 100 duplex fiber texture forms,and with increasing strain,the intensities of 111 and 100 increase.In the drawn single-crystal copper wires produced by Ohno continuous casting,100 rotates to 111,and there is inhomogeneous distribution of fiber texture along radial direction of the wires,which is caused by the distribution of shear deformation.Compared with 100,111 fiber texture is more stable in the drawn copper wires.Comparison of the experimental results with the simulated results shows that the simulation by Taylor model can analyze the texture evolution of drawn copper wires.展开更多
A crystal plasticity finite element model was developed for the drawing deformation of pure copper micro wire,based on rate-dependent crystal plasticity theory.The impact of wire diameter compression ratio on the micr...A crystal plasticity finite element model was developed for the drawing deformation of pure copper micro wire,based on rate-dependent crystal plasticity theory.The impact of wire diameter compression ratio on the micro-mechanical deformation behavior during the wire drawing process was investigated.Results indicate that the internal deformation and slip of the drawn wire are unevenly distributed,forming distinct slip and non-slip zones.Additionally,horizontal strain concentration bands develop within the drawn wire.As the wire diameter compression ratio increases,the strength of the slip systems and the extent of slip zones inside the deformation zone also increase.However,the fluctuating stress state,induced by contact pressure and frictional stress,results in a rough and uneven wire surface and diminishes the stability of the drawing process.展开更多
Prandtl-Reuss flow rule and Hill’s yield criterion were adopted and combined with the concept of finite deformation theory, updated Lagrangian formulation, and a three-dimensional finite element analytical model was ...Prandtl-Reuss flow rule and Hill’s yield criterion were adopted and combined with the concept of finite deformation theory, updated Lagrangian formulation, and a three-dimensional finite element analytical model was established by application of quadrilateral four-node degenerated shell elements coupling into a rigid matrix to deal with the sheet metal forming problems. The fractured thickness of a specimen obtained from a simple tension test was used to be the fracture criterion for the numerical analysis to explore the relationship between punch load and stroke, the thickness distribution, the deformation history and the forming limit of work-piece in the elliptical cup drawing process. The numerical analysis and experiment results show that the punch load increases with the increase of punch stroke, and when the load reaches its maximum, the blank continues to deform with the increase of the punch stroke, resulting in a reduced load until the extension is completed. The minimum thickness of the work-piece concentrates in the contact region of the work-piece and long axis of the punch due to the smaller radius of the curvature of the long axis than the short axis. So the blanks bore the maximum tensile stress in the long axis. Through the limit drawing ratio defined by perimeter of the elliptical punch, the limit drawing ratio of this elliptical cup drawing is defined to be 2.136.展开更多
Electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM) were used to investigate effect of electropulsing on microstructure and texture evolution of Ti-6Al-4V during cold drawing. Rese...Electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM) were used to investigate effect of electropulsing on microstructure and texture evolution of Ti-6Al-4V during cold drawing. Research results demonstrate that the electropulsing treatment (EPT) can enhance the deformability of the grains with unfavorable orientations, which makes the compatibility of deformation among grains much better. A comparison in texture evolution between conventional cold drawing and EPT cold drawing indicates that the EPT promotes prismatic 〈a〉 slip moving, restricts pyramidal 〈c+a〉 slip occurring and accommodates the deformation with c-component by grain boundary sliding. The fraction decrease of low-angle grain boundaries for samples deformed with EPT reveals that the application of electropulsing restricts the formation of the incidental dislocation boundaries and the geometrically necessary boundaries.展开更多
Combining solid granule medium forming technology with ultrasonic vibration plastic forming technology, ultrasonic vibration granule medium forming (UGMF) technology was proposed. To reveal the effect of ultrasonic ...Combining solid granule medium forming technology with ultrasonic vibration plastic forming technology, ultrasonic vibration granule medium forming (UGMF) technology was proposed. To reveal the effect of ultrasonic vibration on flexible-die deep drawing, an ultrasonic vibration with a frequency of 20 kHz and a maximum output of 1.5 kW was on the solid granule medium deep drawing of AZ31B magnesium alloy sheet. The results revealed that ultrasonic vibration promotes the pressure transmission performance of the granule medium and the formability of the sheet. The forming load declines with the ultrasonic amplitude during the drawing process as a result of the combined influence of the "surface effect" and the "softening" of the "volume effect".展开更多
To decrease the size effects of friction in microforming, three kinds of surface coatings, such as diamond-like carbon(DLC), TiN and MoS2, were deposited on surfaces of dies with plasma based ion implantation and de...To decrease the size effects of friction in microforming, three kinds of surface coatings, such as diamond-like carbon(DLC), TiN and MoS2, were deposited on surfaces of dies with plasma based ion implantation and deposition(PBII D) method and magnetron sputtering technique, respectively. The tribological behavior of surface coatings was analyzed considering plastic deformation of specimen at contact interface. The analyses indicate that there is a lower coefficient of friction(COF) and a high wear resistance under the condition of large strain/stress when using the DLC film. The graphitization of DLC film occurs after 100 times of tests. The mechanism of graphitization was analyzed considering energy induced by friction work. The effects of DLC film properties on qualities of micro-deep drawn parts were investigated by analyzing the reduction of wall thickness, etc. The results indicate that DLC film is very helpful for improving the qualities of the micro-parts.展开更多
Although line drawings consist of only line segments on a plane, they convey much information about the three-dimensional object structures. For a computer interpreting line drawings, some intelligent mechanism is req...Although line drawings consist of only line segments on a plane, they convey much information about the three-dimensional object structures. For a computer interpreting line drawings, some intelligent mechanism is required to extract three-dimensional information from the two-dimensional line drawings. In this paper, a new labeling theory and method are proposed for the two-dimensional line drawing with hidden-part-draw of a three-dimensional planar object with trihedral vertices. Some rules for labeling line drawing are established. There are 24 kinds of possible junctions for line drawing with hidden-part-draw, in which there are 8 possible Y and 16 W junctions. The three problems are solved that Sugihara's line drawing labeling technique exists. By analyzing the projections of the holes in manifold planar object, we have put forward a labeling method for the line drawing. Our labeling theory and method can discriminate between correct and incorrect hidden-part-draw natural line drawings. The hidden-part-draw natural line drawings can be labeled correctly by our labeling theory and method, whereas the labeling theory of Sugihara can only label the hidden-part-draw unnatural line drawings in which some visible lines must be drawn as hidden lines, and some invisible lines must be drawn as continuous lines.展开更多
Simulating the traditional painting art by computer graphics is a challenging and attractive subject. Basing on the experience in the ink wash drawing, in this paper, we expound the artistic characters of ink wash p...Simulating the traditional painting art by computer graphics is a challenging and attractive subject. Basing on the experience in the ink wash drawing, in this paper, we expound the artistic characters of ink wash painting and particularly analyze the characteristics of the materials used in the ink wash drawing and the relationships between them. A simulation model is presented and some typical visual effects of the ink wash painting are realized.展开更多
The effect of friction coefficient on the deep drawing of aluminum alloy AA6111 at elevated temperatures was analyzed based on the three conditions using the finite element analysis and the experimental approach.Resul...The effect of friction coefficient on the deep drawing of aluminum alloy AA6111 at elevated temperatures was analyzed based on the three conditions using the finite element analysis and the experimental approach.Results indicate that the friction coefficient and lubrication position significantly influence the minimum thickness,the thickness deviation and the failure mode of the formed parts.During the hot forming process,the failure modes are draw mode,stretch mode and equi-biaxial stretch mode induced by different lubrication conditions.In terms of formability,the optimal value of friction coefficient determined in this work is 0.15.At the same time,the good agreement is performed between the experimental and simulated results.Fracture often occurs at the center of cup bottom or near the cup corner in a ductile mode or ductile-brittle mixed mode,respectively.展开更多
Using high-speed oil-filled spinning method,high quality micro copper tube with straight grooves(MCTSG) with an outer diameter of 6 mm was obtained.Then,MCTSG with an outer diameter of 3-6 mm was fabricated successf...Using high-speed oil-filled spinning method,high quality micro copper tube with straight grooves(MCTSG) with an outer diameter of 6 mm was obtained.Then,MCTSG with an outer diameter of 3-6 mm was fabricated successfully by multi-pass drawing processing method.The influence of drawing parameters on the forming of micro straight grooves was investigated based on the forming mechanism.The results show that the values of groove depth and width decrease,while the wall thickness increases as the drawing diameter decreases.At the same time,the groove depth and width increase,while the wall thickness decreases as the die angle increases.The drawing force increases as the reduction increases.Excessive copper tube reduction may results in groove folding and segmental teeth.The drawing force decreases firstly and then increases with the increases in die angle.When the die angle α is 16°,the drawing force is the smallest,indicating 16° is the optimal angle.展开更多
In this paper, the forming features of tapered rectangular box during hydrodynamic deep drawing are studied by means of FEM.The effect rules of square blank corner corner amount on body wrinkling are recognized and co...In this paper, the forming features of tapered rectangular box during hydrodynamic deep drawing are studied by means of FEM.The effect rules of square blank corner corner amount on body wrinkling are recognized and corresponding methods are discussed. At last, the results of FEM are verified by experi- ment.展开更多
Three different stress states of the combination of tensile(t) stress and compressive(c) stress,t t,t c and t c c,exist in the deformed commercially pure titanium(CP-Ti) sheet during cold drawing-bulging.The tex...Three different stress states of the combination of tensile(t) stress and compressive(c) stress,t t,t c and t c c,exist in the deformed commercially pure titanium(CP-Ti) sheet during cold drawing-bulging.The textures and microstructures in the different stress state regions were investigated by means of XRD and TEM analysis.Similar development of texture and microstructure is achieved with less thickness strain under multiaxial stresses in drawing-bulging than in cold rolling.The results show that texture and microstructure are much sensitive to multiaxial stresses.Twinning is more easily activated under compressive stress than tensile stress.Prism a slip is heavily affected by tensile stress,resulting in a remarkable change of the intensity of(0°,35°,0°) texture,while pyramidal c+a slip,forming(20°,35°,30°) texture,weakens with the increase of thickness strain in spite of stress state.展开更多
In sheet metal forming, drawbeads are often used to control uneven material flow which may cause defects such as wrinkles, fracture, surface distortion and springback. Appropriate setting and adjusting the drawbead ...In sheet metal forming, drawbeads are often used to control uneven material flow which may cause defects such as wrinkles, fracture, surface distortion and springback. Appropriate setting and adjusting the drawbead force is one of the most important pa- rameters in sheet metal forming process control. This paper derives the model of loop drawbead restraining force (DBRF) using plastic forming theory, and gives the min imum blankholding force. Experiments are carried out to verify the proposed DBRF model. The good agreement between the calculated values and experiments data justi- fies the proposed loop drawbead restraining force model.展开更多
The deformation characteristic of bland in deep drawing is discussed. It is pointed out that the friction and lubrication conditions in for drawing are different from that in mechanical motion or machine work or other...The deformation characteristic of bland in deep drawing is discussed. It is pointed out that the friction and lubrication conditions in for drawing are different from that in mechanical motion or machine work or other plastic process. The common test methods in laboratories are analyzed. It shows that though all those test methods can test the friction coefficient, the probe test method is most suitable for the research of friction and lubrication and the process in deep drawing, for this method is identical with the actual work condition either from the test principle or deformation status of the blank. Last the successful application in the deep drawing simulator newly developed the the probe method are intro- duced in detail.展开更多
A solid-state powerful supercapacitor(SC) is fabricated with a substrate of Xerox paper. Its current collector based on a foldable electronic circuit is developed by simply pencil drawing. Thin graphite sheets on pape...A solid-state powerful supercapacitor(SC) is fabricated with a substrate of Xerox paper. Its current collector based on a foldable electronic circuit is developed by simply pencil drawing. Thin graphite sheets on paper provide effective channels for electron transmission with a low resistance of 95 X sq-1. The conductive organic material of polypyrrole coated on thin graphite sheets acts as the electrode material of the device. The as-fabricated SC exhibits a high specific capacitance of 52.9 F cm-3at a scan rate of 1 m V s-1. An energy storage unit fabricated by three full-charged series SCs can drive a commercial light-emitting diode robustly. This work demonstrated a simple, versatile and costeffective method for paper-based devices.展开更多
Basing on warm mechanical property of SUS304 stainless steel and hydro-mechanical deep drawing process, warm hydro-mechanical deep drawing process is proposed and discussed with experiments in this paper. The experime...Basing on warm mechanical property of SUS304 stainless steel and hydro-mechanical deep drawing process, warm hydro-mechanical deep drawing process is proposed and discussed with experiments in this paper. The experiments are performed at four different temperatures. The results show that the formability of stainless steel is improved under the condition of warm temperature. Warm hydro-mechanical deep drawing raises limiting drawing ratio of SUS304 effectively, and limiting drawing ratio 3.3 is obtained, which is beyond 2.0 with conventional deep drawing. The temperature of 90℃ is beneficial to the forming of SUS304 stainless steel, the strain-induced martensite is controlled effectively, and the thickness distribution is more uniform.展开更多
文摘Reinforcement detail drawings are one important part of the design of hydraulic structures and the important basis of construction and management. However, the efficiency of the traditional creation of engineering drawings is very low and the workload is heavy. There is no satisfactory software for hydraulic engineering because of the irregularity and diversity of hydraulic structures' shape. An automatic generation system of reinforcement detail drawings for hydraulic structures is introduced. Its functions and modules are introduced first. The related technologies such as automatic driensioning are discussed in detail. At the end of the paper, an example is given.
基金supported by the National Research Foundation of Korea(NRF)grant funded by the Korea government(MSIT)(Nos.2020R1A2C2010986,2022M3H4A1A04085301)。
文摘In this study,a numerical analysis was conducted on the ductile fracture of a 2-mm diameter Mg-1Zn-0.5Mn-0.5Sr-0.1Ca alloy wire during drawing.The hexagonally close-packed crystal structure of Mg alloys causes asymmetric fracture behavior,especially in the compression region.The aim of this study is to develop a comprehensive damage model for Mg alloy wire that accurately predicts ductile fracture,with a focus on the compression region.A novel experimental method was introduced to measure the ductile fracture of Mg alloy wires under different stress states.The wire drawing process was simulated using the Generalized Incremental Stress-State dependent damage(GISSMO)Model and the Semi-Analytical Model for Polymers(SAMP)model.The damage model's prediction and the experimental results were found to be in excellent agreement,especially in determining crack initiation.Computational analysis established a safe zone diagram for die angle and reduction ratio,and experimental validation confirmed the feasibility of this approach.The proposed damage model can provide a practical and reliable analysis for optimizing the drawing process of Mg alloy wire.
基金Project(51005154) supported by the National Natural Science Foundation of ChinaProject(12CG11) supported by the Chenguang Program of Shanghai Municipal Education Commission,ChinaProject(201104271) supported by the China Postdoctoral Science Foundation Special Funded Project
文摘A specific revised HFCVD apparatus and a novel process combining HFCVD and polishing technique were presented to deposit the micro-and nano-crystalline multilayered ultra-smooth diamond(USCD) film on the interior-hole surface of WC-Co drawing dies with aperture ranging from d1.0 mm to 60 mm.Characterization results indicate that the surface roughness values(Ra) in the entry zone,drawing zone and bearing zone of as-fabricated USCD coated drawing die were measured as low as 25.7,23.3 and 25.5 nm,respectively.Furthermore,the friction properties of USCD films were examined in both dry sliding and water-lubricating conditions,and the results show that the USCD film presents much superior friction properties.Its friction coefficients against ball-bearing steel,copper and silicon nitride balls(d4 mm),is always lower than that of microcrystalline diamond(MCD) or WC-Co sample,regardless of the lubricating condition.Meanwhile,it still presents competitive wear resistance with the MCD films.Finally,the working lifetime and performance of as-fabricated USCD coated drawing dies were examined under producing low-carbon steel pipes in dry-sliding and water-lubricating conditions.Under the water-lubricating drawing condition,its production significantly increases by about 20 times compared with the conventional WC-Co drawing dies.
基金Project(SKLSP200906) supported by the Fund of State Key Laboratory of Solidification Processing in NWPUProject(B08040) supported by Program of Introducing Talents of Discipline in the Project of Advanced Materials and Their Forming Technology
文摘The development of microstructure and texture during cold deep drawing of commercially pure titanium(CP-Ti) was investigated.Three parts,stretching region,drawing region and flange region,were sequentially formed in the deep drawing process of the hemispheric surface part,with reference to deformation modes and strain regimes.Results show that the plastic strain is accommodated by dislocation slip and deformation twinning in the whole deep drawing process.The texture of the CP-Ti sheet and its drawn part consists of rolling texture component and recrystallization texture component.The intensity and type of the initial texture varied during the drawing process are related to the production of deformation twinning and dislocation slip.Twinning weakens the initial texture by randomizing the orientations of crystals,especially for the recrystallization texture.The recrystallization texture in the drawing region disappears due to the significant forming of twinning.Furthermore,over drawing would result in the predominance of dislocation slip and the texture is strengthened.
基金Projects(50771076,50901055)supported by the National Natural Science Foundation of ChinaProject(07JK274)supported by the Education Department Foundation of Shaanxi Province,China
文摘The texture evolution of cold drawing copper wires produced by continuous casting was measured by X-ray diffractometry and electron back-scatter diffractometry,and was simulated using Taylor model.The results show that in the drawn poly-crystal copper wires produced by traditional continuous casting,111 and 100 duplex fiber texture forms,and with increasing strain,the intensities of 111 and 100 increase.In the drawn single-crystal copper wires produced by Ohno continuous casting,100 rotates to 111,and there is inhomogeneous distribution of fiber texture along radial direction of the wires,which is caused by the distribution of shear deformation.Compared with 100,111 fiber texture is more stable in the drawn copper wires.Comparison of the experimental results with the simulated results shows that the simulation by Taylor model can analyze the texture evolution of drawn copper wires.
基金the National Natural Science Foundation of China(Nos.U21A2051,52173297,52071133)the R&D Projects of Henan Academy of Sciences of China(No.220910009)+2 种基金the Key R&D and Promotion Projects of Henan Province of China(No.212102210441)the Joint Fund of Henan Science and Technology R&D Plan of China(No.222103810037)the Zhongyuan Scholar Workstation Funded Project of China(No.214400510028).
文摘A crystal plasticity finite element model was developed for the drawing deformation of pure copper micro wire,based on rate-dependent crystal plasticity theory.The impact of wire diameter compression ratio on the micro-mechanical deformation behavior during the wire drawing process was investigated.Results indicate that the internal deformation and slip of the drawn wire are unevenly distributed,forming distinct slip and non-slip zones.Additionally,horizontal strain concentration bands develop within the drawn wire.As the wire diameter compression ratio increases,the strength of the slip systems and the extent of slip zones inside the deformation zone also increase.However,the fluctuating stress state,induced by contact pressure and frictional stress,results in a rough and uneven wire surface and diminishes the stability of the drawing process.
基金funded by research projects (NSC97-2221-E-129-003) of the National Science Council
文摘Prandtl-Reuss flow rule and Hill’s yield criterion were adopted and combined with the concept of finite deformation theory, updated Lagrangian formulation, and a three-dimensional finite element analytical model was established by application of quadrilateral four-node degenerated shell elements coupling into a rigid matrix to deal with the sheet metal forming problems. The fractured thickness of a specimen obtained from a simple tension test was used to be the fracture criterion for the numerical analysis to explore the relationship between punch load and stroke, the thickness distribution, the deformation history and the forming limit of work-piece in the elliptical cup drawing process. The numerical analysis and experiment results show that the punch load increases with the increase of punch stroke, and when the load reaches its maximum, the blank continues to deform with the increase of the punch stroke, resulting in a reduced load until the extension is completed. The minimum thickness of the work-piece concentrates in the contact region of the work-piece and long axis of the punch due to the smaller radius of the curvature of the long axis than the short axis. So the blanks bore the maximum tensile stress in the long axis. Through the limit drawing ratio defined by perimeter of the elliptical punch, the limit drawing ratio of this elliptical cup drawing is defined to be 2.136.
基金Project (NCET-10-0278) supported by the Program for New Century Excellent Talents in University,China
文摘Electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM) were used to investigate effect of electropulsing on microstructure and texture evolution of Ti-6Al-4V during cold drawing. Research results demonstrate that the electropulsing treatment (EPT) can enhance the deformability of the grains with unfavorable orientations, which makes the compatibility of deformation among grains much better. A comparison in texture evolution between conventional cold drawing and EPT cold drawing indicates that the EPT promotes prismatic 〈a〉 slip moving, restricts pyramidal 〈c+a〉 slip occurring and accommodates the deformation with c-component by grain boundary sliding. The fraction decrease of low-angle grain boundaries for samples deformed with EPT reveals that the application of electropulsing restricts the formation of the incidental dislocation boundaries and the geometrically necessary boundaries.
基金Projects(51305385,51305386)supported by the National Natural Science Foundation of ChinaProject(QN20131080)supported by the Science Research Youth Foundation of Hebei Province Universities,China
文摘Combining solid granule medium forming technology with ultrasonic vibration plastic forming technology, ultrasonic vibration granule medium forming (UGMF) technology was proposed. To reveal the effect of ultrasonic vibration on flexible-die deep drawing, an ultrasonic vibration with a frequency of 20 kHz and a maximum output of 1.5 kW was on the solid granule medium deep drawing of AZ31B magnesium alloy sheet. The results revealed that ultrasonic vibration promotes the pressure transmission performance of the granule medium and the formability of the sheet. The forming load declines with the ultrasonic amplitude during the drawing process as a result of the combined influence of the "surface effect" and the "softening" of the "volume effect".
基金Projects(51375113,50805035)supported by the National Natural Science Foundation of China
文摘To decrease the size effects of friction in microforming, three kinds of surface coatings, such as diamond-like carbon(DLC), TiN and MoS2, were deposited on surfaces of dies with plasma based ion implantation and deposition(PBII D) method and magnetron sputtering technique, respectively. The tribological behavior of surface coatings was analyzed considering plastic deformation of specimen at contact interface. The analyses indicate that there is a lower coefficient of friction(COF) and a high wear resistance under the condition of large strain/stress when using the DLC film. The graphitization of DLC film occurs after 100 times of tests. The mechanism of graphitization was analyzed considering energy induced by friction work. The effects of DLC film properties on qualities of micro-deep drawn parts were investigated by analyzing the reduction of wall thickness, etc. The results indicate that DLC film is very helpful for improving the qualities of the micro-parts.
文摘Although line drawings consist of only line segments on a plane, they convey much information about the three-dimensional object structures. For a computer interpreting line drawings, some intelligent mechanism is required to extract three-dimensional information from the two-dimensional line drawings. In this paper, a new labeling theory and method are proposed for the two-dimensional line drawing with hidden-part-draw of a three-dimensional planar object with trihedral vertices. Some rules for labeling line drawing are established. There are 24 kinds of possible junctions for line drawing with hidden-part-draw, in which there are 8 possible Y and 16 W junctions. The three problems are solved that Sugihara's line drawing labeling technique exists. By analyzing the projections of the holes in manifold planar object, we have put forward a labeling method for the line drawing. Our labeling theory and method can discriminate between correct and incorrect hidden-part-draw natural line drawings. The hidden-part-draw natural line drawings can be labeled correctly by our labeling theory and method, whereas the labeling theory of Sugihara can only label the hidden-part-draw unnatural line drawings in which some visible lines must be drawn as hidden lines, and some invisible lines must be drawn as continuous lines.
文摘Simulating the traditional painting art by computer graphics is a challenging and attractive subject. Basing on the experience in the ink wash drawing, in this paper, we expound the artistic characters of ink wash painting and particularly analyze the characteristics of the materials used in the ink wash drawing and the relationships between them. A simulation model is presented and some typical visual effects of the ink wash painting are realized.
基金Project(2009ZX04014-074)supported by the National Science and Technology Major Project of ChinaProject(P2014-15)supported by the State Key Laboratory of Materials Processing and Die&Mould Technology,Huazhong University of Science and Technology,ChinaProject(20120006110017)supported by the Specialized Research Fund for the Doctoral Program of Higher Education of China
文摘The effect of friction coefficient on the deep drawing of aluminum alloy AA6111 at elevated temperatures was analyzed based on the three conditions using the finite element analysis and the experimental approach.Results indicate that the friction coefficient and lubrication position significantly influence the minimum thickness,the thickness deviation and the failure mode of the formed parts.During the hot forming process,the failure modes are draw mode,stretch mode and equi-biaxial stretch mode induced by different lubrication conditions.In terms of formability,the optimal value of friction coefficient determined in this work is 0.15.At the same time,the good agreement is performed between the experimental and simulated results.Fracture often occurs at the center of cup bottom or near the cup corner in a ductile mode or ductile-brittle mixed mode,respectively.
基金Project(U0834002)supported by the Joint Funds of NSFC-Guangdong of ChinaProject(2009ZM0121)supported by the Fundamental Research Funds for the Central Universities,ChinaProjects(LYM09024)supported by Training Program for Excellent Young Teachers with Innovation of Guangdong University,China
文摘Using high-speed oil-filled spinning method,high quality micro copper tube with straight grooves(MCTSG) with an outer diameter of 6 mm was obtained.Then,MCTSG with an outer diameter of 3-6 mm was fabricated successfully by multi-pass drawing processing method.The influence of drawing parameters on the forming of micro straight grooves was investigated based on the forming mechanism.The results show that the values of groove depth and width decrease,while the wall thickness increases as the drawing diameter decreases.At the same time,the groove depth and width increase,while the wall thickness decreases as the die angle increases.The drawing force increases as the reduction increases.Excessive copper tube reduction may results in groove folding and segmental teeth.The drawing force decreases firstly and then increases with the increases in die angle.When the die angle α is 16°,the drawing force is the smallest,indicating 16° is the optimal angle.
文摘In this paper, the forming features of tapered rectangular box during hydrodynamic deep drawing are studied by means of FEM.The effect rules of square blank corner corner amount on body wrinkling are recognized and corresponding methods are discussed. At last, the results of FEM are verified by experi- ment.
基金Project(2010CB731701) supported by the National Basic Research Program of ChinaProjects(50805121,51175428) supported by the National Natural Science Foundation of China+3 种基金Project(50935007) supported by the National Natural Science Foundation of China for Key ProgramProject(NPU-FFR-JC20100229) supported by the Foundation for Fundamental Research of Northwestern Polytechnical University in ChinaProject(2011-P06) supported by the Foundation of the State Key Laboratory of Materials Processing and Die & Mould Technology,Huazhong University of Science and TechnologyProject(B08040) supported by Program of Introducing Talents of Discipline to Universities("111"),China
文摘Three different stress states of the combination of tensile(t) stress and compressive(c) stress,t t,t c and t c c,exist in the deformed commercially pure titanium(CP-Ti) sheet during cold drawing-bulging.The textures and microstructures in the different stress state regions were investigated by means of XRD and TEM analysis.Similar development of texture and microstructure is achieved with less thickness strain under multiaxial stresses in drawing-bulging than in cold rolling.The results show that texture and microstructure are much sensitive to multiaxial stresses.Twinning is more easily activated under compressive stress than tensile stress.Prism a slip is heavily affected by tensile stress,resulting in a remarkable change of the intensity of(0°,35°,0°) texture,while pyramidal c+a slip,forming(20°,35°,30°) texture,weakens with the increase of thickness strain in spite of stress state.
文摘In sheet metal forming, drawbeads are often used to control uneven material flow which may cause defects such as wrinkles, fracture, surface distortion and springback. Appropriate setting and adjusting the drawbead force is one of the most important pa- rameters in sheet metal forming process control. This paper derives the model of loop drawbead restraining force (DBRF) using plastic forming theory, and gives the min imum blankholding force. Experiments are carried out to verify the proposed DBRF model. The good agreement between the calculated values and experiments data justi- fies the proposed loop drawbead restraining force model.
文摘The deformation characteristic of bland in deep drawing is discussed. It is pointed out that the friction and lubrication conditions in for drawing are different from that in mechanical motion or machine work or other plastic process. The common test methods in laboratories are analyzed. It shows that though all those test methods can test the friction coefficient, the probe test method is most suitable for the research of friction and lubrication and the process in deep drawing, for this method is identical with the actual work condition either from the test principle or deformation status of the blank. Last the successful application in the deep drawing simulator newly developed the the probe method are intro- duced in detail.
基金supported by the National Basic Research Program(2011CB933300)of Chinathe National Natural Science Foundation of China(11204093,11374110)‘the Fundamental Research Funds for the Central Universities’,HUST:2012QN114,2013TS033
文摘A solid-state powerful supercapacitor(SC) is fabricated with a substrate of Xerox paper. Its current collector based on a foldable electronic circuit is developed by simply pencil drawing. Thin graphite sheets on paper provide effective channels for electron transmission with a low resistance of 95 X sq-1. The conductive organic material of polypyrrole coated on thin graphite sheets acts as the electrode material of the device. The as-fabricated SC exhibits a high specific capacitance of 52.9 F cm-3at a scan rate of 1 m V s-1. An energy storage unit fabricated by three full-charged series SCs can drive a commercial light-emitting diode robustly. This work demonstrated a simple, versatile and costeffective method for paper-based devices.
文摘Basing on warm mechanical property of SUS304 stainless steel and hydro-mechanical deep drawing process, warm hydro-mechanical deep drawing process is proposed and discussed with experiments in this paper. The experiments are performed at four different temperatures. The results show that the formability of stainless steel is improved under the condition of warm temperature. Warm hydro-mechanical deep drawing raises limiting drawing ratio of SUS304 effectively, and limiting drawing ratio 3.3 is obtained, which is beyond 2.0 with conventional deep drawing. The temperature of 90℃ is beneficial to the forming of SUS304 stainless steel, the strain-induced martensite is controlled effectively, and the thickness distribution is more uniform.