Diatomite-based porous ceramics were adopted as carriers to immobilize nano-TiO2 via a hydrolysis-deposition technique. The thermal degradation of as-prepared composites was investigated using thermogravimetric-differ...Diatomite-based porous ceramics were adopted as carriers to immobilize nano-TiO2 via a hydrolysis-deposition technique. The thermal degradation of as-prepared composites was investigated using thermogravimetric-differential thermal analysis, and the phase and microstructure were characterized by X-ray diffraction, Fourier transform infrared spectroscopy, and transmission electron microscopy. The results indicated that the carriers were encapsulated by nano-TiO2 with a thickness of 300-450 nm. The main crystalline phase of TiO2 calcined at 650~C was anatase, and the average grain size was 8.3 nm. The FT-IR absorption bands at 955.38 cm1 suggested that new chemical bonds among Ti, O, and Si had formed in the composites. The photocatalytic (PC) activity of the composites was investigated un- der UV irradiation. Furthermore, the photodegradation kinetics of formaldehyde was investigated using the composites as the cores of an air cleaner. A kinetics study showed that the reaction rate constants of the gas-phase PC reaction of formaldehyde were k = 0.576 mg'm3·min^-1 and K = 0.048 m3/mg.展开更多
Thermal insulation materials play an increasingly important role in protecting mechanical parts functioning at high temperatures.In this study,a new porous high-entropy(La_(1/6)Ce_(1/6)Pr_(1/6)Sm_(1/6)Eu_(1/6)Gd_(1/6)...Thermal insulation materials play an increasingly important role in protecting mechanical parts functioning at high temperatures.In this study,a new porous high-entropy(La_(1/6)Ce_(1/6)Pr_(1/6)Sm_(1/6)Eu_(1/6)Gd_(1/6))PO_(4)(HE(6RE_(1/6))PO_(4))ceramics was prepared by combining the high-entropy method with the pore-forming agent method and the effect of different starch contents(0–60vol%)on this ceramic properties was systematically investigated.The results show that the porous HE(6RE_(1/6))PO_(4)ceramics with 60vol%starch exhibit the lowest thermal conductivity of 0.061 W·m^(-1)·K^(-1)at room temperature and good pore structure stability with a linear shrinkage of approximately1.67%.Moreover,the effect of large regular spherical pores(>10μm)on its thermal insulation performance was discussed,and an optimal thermal conductivity prediction model was screened.The superior properties of the prepared porous HE(6RE_(1/6))PO_(4)ceramics allow them to be promising insulation materials in the future.展开更多
In this study,the effect of sintering temperature and the addition of kaolin,a sintering agent,on the microscopic,phase,and mechanical properties of ceramics were investigated using secondary aluminum dross(SAD)as the...In this study,the effect of sintering temperature and the addition of kaolin,a sintering agent,on the microscopic,phase,and mechanical properties of ceramics were investigated using secondary aluminum dross(SAD)as the main component in the manufacturing of ceramics.The basic phases of the ceramics were Al_(2)O_(3),MgAl_(2)O_(4),NaAl_(11)O_(17),and SiO_(2)without the addition of kaolin.The diffraction peaks of MgAl_(2)O_(4),NaAl_(11)O_(17),and SiO_(2)kept decreasing while those of Al_(2)O_(3)kept increasing with an increase in temperature.In addition,the increase in temperature promoted the growth of the grains.The grains were uniform in size and regular in distribution,with a shrinkage of 2.2%,porosity of 72.5%,bulk density of 1.076 g/cm^(3),and compressive strength of 1.12 MPa.When the sintering temperature was 1450°C,the basic phases of the ceramic after the addition of kaolin were Al_(2)O_(3),MgAl_(2)O_(4),NaAl_(11)O_(17),and SiO_(2).With the increase of kaolin,the diffraction peaks of NaAl_(11)O_(17)and SiO_(2)decreased until they disappeared,while the diffraction peaks of Al_(2)O_(3)increased significantly.When kaolin was added at 30 wt.%,the ceramics obtained had shrinkage of 18%,a porosity of 47.26%,a bulk density of 1.965 g/cm^(3),and compressive strength of 31.9 MPa.Cracks existed inside the ceramics without the addition of kaolin,while the addition of kaolin significantly changed this defect.It is shown that SAD can obtain porous ceramics with good properties at a sintering temperature of 1450°C and a kaolin addition of 30 wt.%.展开更多
A hybrid system combined with a non-contact membrane and bubbling absorption is proposed to capture CO_(2) from flue gas.The non-contact way of membrane and liquid absorbent effectively avoids the reduction of gas dif...A hybrid system combined with a non-contact membrane and bubbling absorption is proposed to capture CO_(2) from flue gas.The non-contact way of membrane and liquid absorbent effectively avoids the reduction of gas diffusion flux through the membrane.High-porosity ceramic membranes in hybrid systems are used for gas-solid separation in fuel gas treatment.Due to the high content of H_(2)O and cement dust in the flue gas of the cement plant,the membrane is hydrophobically modified by polytetrafluoroethylene(PTFE)to improve its anti-water,anti-fouling,and self-cleaning performances.The results show that the diffusion flux of CO_(2) through the membrane is still higher than 7.0×10^(−3) mol/m^(2)s(20%CO_(2) concentration)even under the influence of water and cement dust.In addition,slaked lime selected as the absorbent is cheap and the product after bubbling absorption is nano-scale light calcium carbonate.To sum up,the hybrid system combining non-contact membrane and bubbling absorption is expected to be used to capture carbon dioxide from the flue gas of the cement plant.展开更多
With the rapid industrialization and urbanization,the demand for air quality management is more and more urgent.High temperature dust filtration is one important environmental management technology.Porous ceramics are...With the rapid industrialization and urbanization,the demand for air quality management is more and more urgent.High temperature dust filtration is one important environmental management technology.Porous ceramics are used as filter materials in the field of high-temperature dust filtration because of their unique advantages such as high filtration efficiency,as well as high temperature stability,particle loss resistance,corrosion resistance and durability.This paper mainly introduced several common preparation techniques of porous ceramics,including the traditional organic foam impregnation method,foaming method,in-situ combustion method,pore-forming method and other new methods such as the template method,gel injection molding method,freeze-drying method,multi-component co-precipitation method and hydrogel method.The principle,advantages and disadvantages of these preparation technologies and their research status were described.The application of these technologies in the field of high temperature dust filtration was briefly reviewed.Finally,the application prospect of the porous ceramics in the field of high temperature dust filtration was prospected.展开更多
The core-shell structure silicon-resin precursor powders were synthesized through coat-mix process and addition of Al2O3-SiO2-Y2O3 composite additives.A series of porous silicon carbide ceramics were produced after mo...The core-shell structure silicon-resin precursor powders were synthesized through coat-mix process and addition of Al2O3-SiO2-Y2O3 composite additives.A series of porous silicon carbide ceramics were produced after molding,carbonization and sintering.The phase,morphology,porosity,thermal conductivity,thermal expansion coefficient,and thermal shock resistance were analyzed.The results show that porous silicon carbide ceramics can be produced at low temperature.The grain size of porous silicon carbide ceramic is small,and the thermal conductivity is enhanced significantly.Composite additives also improve the thermal shock resistance of porous ceramics.The bending strength loss rate after 30 times of thermal shock test of the porous ceramics which were added Al2O3-SiO2-Y2O3 and sintered at 1 650 ℃ is only 6.5%.Moreover,the pore inside of the sample is smooth,and the pore size distribution is uniform.Composite additives make little effect on the thermal expansion coefficient of the porous silicon carbide ceramics.展开更多
To improve the wall surface hydrophilicity of a tube type indirect evaporative cooler,a new method adopting porous ceramics is proposed.This method realizes the combination of porous ceramics and the evaporative cooli...To improve the wall surface hydrophilicity of a tube type indirect evaporative cooler,a new method adopting porous ceramics is proposed.This method realizes the combination of porous ceramics and the evaporative cooling technique.The design calculation of the porous ceramics tube type dew point indirect evaporative cooler are carried out from such aspects as the volumes and status parameters of the primary and secondary air,the cooler structure,the heat transfer of the solid porous ceramic tubes and the resistance of the cooler.The calculation results show that the design is reasonable.Finally,based on the design calculation,the porous ceramics tube type dew point indirect evaporative cooler is successfully manufactured.展开更多
Porous ceramics were prepared from kaolinite gangue and Al(OH)3 with double addition of MgCO3 and CaCO3 by the pore-forming in-situ technique.The characterizations of porous ceramics were investigated by X-ray diffr...Porous ceramics were prepared from kaolinite gangue and Al(OH)3 with double addition of MgCO3 and CaCO3 by the pore-forming in-situ technique.The characterizations of porous ceramics were investigated by X-ray diffractometry,scanning electron microscopy,and mercury porosimetry measurements,etc.It is found that although the decomposition of MgCO3 and CaCO3 has little contribution to the porosity,the double addition of MgCO3 and CaCO3 strongly affects the formation of liquid phase,and then changes the phase compositions,pore characterization,and strength.The appropriate mode is the sample containing 1.17wt% MgCO3 and 1.17wt% CaCO3,which has high apparent porosity(41.0%),high crushing strength(53.5 MPa),high mullite content(76wt%),and small average pore size(3.24 μm).展开更多
Heterogeneous catalysts with ultrafine or nano particle size have currently attracted considerable attentions in the chemical and petrochemical production processes, but their large-scale applications remain challengi...Heterogeneous catalysts with ultrafine or nano particle size have currently attracted considerable attentions in the chemical and petrochemical production processes, but their large-scale applications remain challenging because of difficulties associated with their efficient separation from the reaction slurry. A porous ceramic membrane reactor has emerged as a promising method to solve the problem concerning catalysts separation in situ from the reaction mixture and make the production process continuous in heterogeneous catalysis. This article presents a review of the present progress on porous ceramic membrane reactors for heterogeneous catalysis, which covers classification of configurations of porous ceramic membrane reactor, major considerations and some important industrial applications. A special emphasis is paid to major considerations in term of application-oriented ceramic membrane design, optimization of ceramic membrane reactor performance and membrane fouling mechanism. Finally, brief concluding remarks on porous ceramic membrane reactors are given and possible future research interests are also outlined.展开更多
A new approach in combination of the effective medium theory with the equivalent unit in numerical simulation was developed to study the effective thermal conductivity of porous ceramics. The finite element method was...A new approach in combination of the effective medium theory with the equivalent unit in numerical simulation was developed to study the effective thermal conductivity of porous ceramics. The finite element method was used to simulate the heat transfer process which enables to acquire accurate results through highly complicated modeling and intensive computation. An alternative approach to mesh the material into small cells was also presented. The effective medium theory accounts for the effective thermal conductivity of cells while the equivalent unit is subsequently applied in numerical simulation to analyze the effective thermal conductivity of the porous ceramics. A new expression for the effective thermal conductivity, allowing for some structure factors such as volume fraction of pores and thermal conductivity, was put forward, and the results of its application was proved to be close to those of the mathematical simulation.展开更多
Medical stone-based porous ceramics as a carrier were prepared by ultra-fine grinding and low-temperature sintering method. Nano-TiO~ thin films were loaded on the carrier by chemical liquid deposition method using ti...Medical stone-based porous ceramics as a carrier were prepared by ultra-fine grinding and low-temperature sintering method. Nano-TiO~ thin films were loaded on the carrier by chemical liquid deposition method using titanium tetrachloride as a precursor. The micro-morphology and microstructure of the synthesized samples were characterized using X-ray diffraction, scanning electron microscopy with energy dispersive spectrometry, and mercury injection method. The photo-catalytic activity of the TiO2 thin films was investigated by degrading formaldehyde. The main crystalline phase in the TiO2 thin films calcined at 550~C is anatase with the average particle size about 10 nm. The specific surface area of the carrier-coated nano-TiO2 increases from 3.68 to 5.32 m2/g. The formaldehyde removal rate of the TiO2/medical stone-based porous ceramics irradiated under an ultraviolet lamp for 120 min reaches 85.6%.展开更多
By employing sintering additives of Li2CO3 and Y2O3,porous Si3N4 ceramics are prepared after experiencing the processes of sintering and post-vacuum heat treatment at 1680 and 1550°C,respectively.The experimental...By employing sintering additives of Li2CO3 and Y2O3,porous Si3N4 ceramics are prepared after experiencing the processes of sintering and post-vacuum heat treatment at 1680 and 1550°C,respectively.The experimental results demonstrate the completed phase transformation fromαtoβ-Si3N4 in Si3N4 ceramic samples with a amount of 1.60 wt%Li2CO3(0.65 wt%Li2O)and 0.33 wt%Y2O3 additives.The as-synthesized porous Si3N4 ceramics exhibit high flexural strength((126.7±2.7)MPa)and high open porosity of 50.4%at elevated temperature(1200°C).These results are attributed to the significant role of added Li2CO3 as sintering additive,where the volatilization of intergranular glassy phase occurs during sintering process.Therefore,porous Si3N4 ceramics with desired mechanical property prepared by altering the addition of sintering additives demonstrate their great potential as a promising candidate for high temperature applications.展开更多
The large-scale accumulation and pollution of solid mining waste is an urgent issue.Coal gangue is a prominent type of solid waste,and shows promise for use in high value-added products due to its content of many impo...The large-scale accumulation and pollution of solid mining waste is an urgent issue.Coal gangue is a prominent type of solid waste,and shows promise for use in high value-added products due to its content of many important compounds,including SiO_(2) and Al2O3.This study proposed the preparation of highly porous ceramics from coal gangue,coal slime,and coconut palm fibers.The ceramics were produced at a sintering temperature of 950℃ with a fiber content of 6 wt%,which led to the formation of porous ceramics with a porosity of 66.93%,volume density of 1.0329 g/cm^(3),compressive strength of 1.1025 MPa,and thermal conductivity is 0.3919 K(W/mk).A finite element model of the porous ceramics was established using the Abaqus module in ANSYS software,where the stress distribution and compressive strength were simulated.Further,the relationship between porosity and compressive strength was analyzed.The thermal properties of the porous ceramics were analyzed using the Fluent module,where the simulated changes in porosity under various sintering temperatures were consistent with the experimental data.The preparation of this highly porous ceramic from solid waste coal gangue shows promise for the minimizing the impact of waste gas and wastewater pollution in the future.展开更多
This paper presents the microwave dielectric properties of reaction bonded porous silicon nitride ceramics with variant porosity and pore size, which were prepared by adding pore-forming agent grains into the silicon ...This paper presents the microwave dielectric properties of reaction bonded porous silicon nitride ceramics with variant porosity and pore size, which were prepared by adding pore-forming agent grains into the silicon powders. The experimental results show that the dielectric constant and the dielectric loss of the samples reduce evidently with increasing porosity in the sample. When the porosity is constant, the dielectric constant and the dielectric loss of the ceramics decrease visibly as the pore size increases. Among all the obtained samples, the minimum dielectric constant is about 2.4.展开更多
Porous ceramics were prepared with spodumene flotation talings(SFT),kaolin and low-melting point glass(LPG)powder,whose pores were formed by the chemical reaction of hydrogen peroxide(H_(2)O_(2)).LPG was used to reduc...Porous ceramics were prepared with spodumene flotation talings(SFT),kaolin and low-melting point glass(LPG)powder,whose pores were formed by the chemical reaction of hydrogen peroxide(H_(2)O_(2)).LPG was used to reduce the sintering temperature of porous ceramics and kaolin was used to realize the adsorption to methylene blue(MB)of porous ceramics.The average flexural strength,compressive strength,apparent porosity,water absorption and maximum MB adsorption capacity were 5.60 MPa,4.66 MPa,52.27%,44.32%and 0.7 mg/g,respectively.Moreover,the results of orthogonal experiments present that the sintering temperature and the dosage of H_(2)O_(2)had great influence on the mechanical properties and apparent porosity of porous ceramics,respectively.The main reason for the improvement of mechanical properties of porous ceramics was that LPG gradually became soft with increasing the sintering temperature,which made the mineral particles adhere to each other closely.Kaolinite was not completely converted into metakaolin at 550℃,which might be the main reason why porous ceramics had adsorption properties.展开更多
To obtain porous alumina ceramic with high strength,a novel gelcasting system based on 2-hydroxyethyl methacrylate(HEMA)dissolved in tert-butyl alcohol(TBA)was developed.The polymerization of the HEMA-TBA gelcasting s...To obtain porous alumina ceramic with high strength,a novel gelcasting system based on 2-hydroxyethyl methacrylate(HEMA)dissolved in tert-butyl alcohol(TBA)was developed.The polymerization of the HEMA-TBA gelcasting system,the thermal behavior of obtained green body,and the microstructures and mechanical properties of the sintered bodies were investigated by rheometer,TG-DSC,SEM and bending strength testing,respectively.The results show that,(1)10 mg/mL of the initiator(benzoyl peroxide)is the optimal amount for polymerization of this gelscasting system at 25 ℃;(2)The alumina suspension of the HEMA-TBA gelcasting system showing shear-thinning behavior is sufficiently low for gelcasting process;(3)The bending strength of porous alumina ceramic samples,whose porosities range from 42% to 56%,is from(8±0.5)to(91±4.5)MPa.展开更多
Porous ceramics was made from coal fly ash, and the microstructure and other properties were characterized as a function of the amount of the pore-forming agent and firing temperature. The results indicated that the p...Porous ceramics was made from coal fly ash, and the microstructure and other properties were characterized as a function of the amount of the pore-forming agent and firing temperature. The results indicated that the proper sintering temperature for the useful ceramic materials is 1 250℃, and a liquid-phase was involved in the densification process.展开更多
The general behavior of micron-particles in the inner domain of porous ceramic vessel was simulated by computational fluid dynamics software in terms of sampling experimental data.The results show that there is an opt...The general behavior of micron-particles in the inner domain of porous ceramic vessel was simulated by computational fluid dynamics software in terms of sampling experimental data.The results show that there is an optimum porosity of 0.32 to get a higher efficiency and lower pressure drop during filtration.According to the results of simulation and experiment,it is evident that lower inlet velocity can maintain lower pressure drop and obtain higher collection efficiency and inlet concentration also has a crucial influence on the collection efficiency.The collection efficiency of equipment increases significantly with the increase of inlet concentration when the inlet concentration is less than 6.3 g/m3,but it gradually tends to be stable in the range of 97.3%-99.7%when the inlet concentration is over this concentration.展开更多
In this paper,calcium hexaaluminate(CA6)porous ceramics were prepared by a foaming method combined with cement solidification molding.The effects of the foaming agent addition on the microstructure and the properties ...In this paper,calcium hexaaluminate(CA6)porous ceramics were prepared by a foaming method combined with cement solidification molding.The effects of the foaming agent addition on the microstructure and the properties of the ceramics were studied.The results show that the microstructure and the porosity of the ceramics can be controlled by adjusting the addition of the foaming agent.As the addition of the foaming agent increased,the bulk density reduced from 1 g·cm^-3 to 0.35 g·cm^-3,the porosity increased from 70.4%to 89.6%,the compressive strength reduced from 18.46 MPa to 1.66 MPa,and the thermal conductivity at 1000°C decreased from 0.382 W·m^-1·K^-1 to 0.144 W·m^-1·K^-1.It is indicated that calcium hexaaluminate porous ceramics with low density,high strength and low thermal conductivity can be obtained by the foaming method.As the lining material of high temperature electric furnaces,the ceramic has excellent energy saving effect.展开更多
基金financially supported by the National Natural Science Foundation of China (No. 50708037)the National Science Fund for Excellent Young Scholars of China (No. 51522402)+1 种基金the Science and Technology Research Projects in Zhengzhou (No. 141PPTGG388)the National Innovation and Entrepreneurship Training Program of the Undergraduate (No. 201610078034)
文摘Diatomite-based porous ceramics were adopted as carriers to immobilize nano-TiO2 via a hydrolysis-deposition technique. The thermal degradation of as-prepared composites was investigated using thermogravimetric-differential thermal analysis, and the phase and microstructure were characterized by X-ray diffraction, Fourier transform infrared spectroscopy, and transmission electron microscopy. The results indicated that the carriers were encapsulated by nano-TiO2 with a thickness of 300-450 nm. The main crystalline phase of TiO2 calcined at 650~C was anatase, and the average grain size was 8.3 nm. The FT-IR absorption bands at 955.38 cm1 suggested that new chemical bonds among Ti, O, and Si had formed in the composites. The photocatalytic (PC) activity of the composites was investigated un- der UV irradiation. Furthermore, the photodegradation kinetics of formaldehyde was investigated using the composites as the cores of an air cleaner. A kinetics study showed that the reaction rate constants of the gas-phase PC reaction of formaldehyde were k = 0.576 mg'm3·min^-1 and K = 0.048 m3/mg.
基金the National Key R&D Program of China(No.2021YFB3701404)the National Natural Science Fund for Distinguished Young Scholars(No.52025041)+1 种基金the National Natural Science Foundation of China(Nos.52250091,51904021,and 52174294)the Fundamental Research Funds for the Central Universities(Nos.FRF-TP-20-02C2 and FRF-BD-22-05).
文摘Thermal insulation materials play an increasingly important role in protecting mechanical parts functioning at high temperatures.In this study,a new porous high-entropy(La_(1/6)Ce_(1/6)Pr_(1/6)Sm_(1/6)Eu_(1/6)Gd_(1/6))PO_(4)(HE(6RE_(1/6))PO_(4))ceramics was prepared by combining the high-entropy method with the pore-forming agent method and the effect of different starch contents(0–60vol%)on this ceramic properties was systematically investigated.The results show that the porous HE(6RE_(1/6))PO_(4)ceramics with 60vol%starch exhibit the lowest thermal conductivity of 0.061 W·m^(-1)·K^(-1)at room temperature and good pore structure stability with a linear shrinkage of approximately1.67%.Moreover,the effect of large regular spherical pores(>10μm)on its thermal insulation performance was discussed,and an optimal thermal conductivity prediction model was screened.The superior properties of the prepared porous HE(6RE_(1/6))PO_(4)ceramics allow them to be promising insulation materials in the future.
基金Funding Statement:The work was supported by the National Natural Science Foundation of China(51465014)Guangxi Innovation Driven Development Project(Grant No.AA17204021)+1 种基金the Foundation of Guangxi Key Laboratory of Optical and Electronic Materials and Devices(No.20KF-4)Foundation of Introduction of Senior Talents in Hebei Province(H192003015).
文摘In this study,the effect of sintering temperature and the addition of kaolin,a sintering agent,on the microscopic,phase,and mechanical properties of ceramics were investigated using secondary aluminum dross(SAD)as the main component in the manufacturing of ceramics.The basic phases of the ceramics were Al_(2)O_(3),MgAl_(2)O_(4),NaAl_(11)O_(17),and SiO_(2)without the addition of kaolin.The diffraction peaks of MgAl_(2)O_(4),NaAl_(11)O_(17),and SiO_(2)kept decreasing while those of Al_(2)O_(3)kept increasing with an increase in temperature.In addition,the increase in temperature promoted the growth of the grains.The grains were uniform in size and regular in distribution,with a shrinkage of 2.2%,porosity of 72.5%,bulk density of 1.076 g/cm^(3),and compressive strength of 1.12 MPa.When the sintering temperature was 1450°C,the basic phases of the ceramic after the addition of kaolin were Al_(2)O_(3),MgAl_(2)O_(4),NaAl_(11)O_(17),and SiO_(2).With the increase of kaolin,the diffraction peaks of NaAl_(11)O_(17)and SiO_(2)decreased until they disappeared,while the diffraction peaks of Al_(2)O_(3)increased significantly.When kaolin was added at 30 wt.%,the ceramics obtained had shrinkage of 18%,a porosity of 47.26%,a bulk density of 1.965 g/cm^(3),and compressive strength of 31.9 MPa.Cracks existed inside the ceramics without the addition of kaolin,while the addition of kaolin significantly changed this defect.It is shown that SAD can obtain porous ceramics with good properties at a sintering temperature of 1450°C and a kaolin addition of 30 wt.%.
文摘A hybrid system combined with a non-contact membrane and bubbling absorption is proposed to capture CO_(2) from flue gas.The non-contact way of membrane and liquid absorbent effectively avoids the reduction of gas diffusion flux through the membrane.High-porosity ceramic membranes in hybrid systems are used for gas-solid separation in fuel gas treatment.Due to the high content of H_(2)O and cement dust in the flue gas of the cement plant,the membrane is hydrophobically modified by polytetrafluoroethylene(PTFE)to improve its anti-water,anti-fouling,and self-cleaning performances.The results show that the diffusion flux of CO_(2) through the membrane is still higher than 7.0×10^(−3) mol/m^(2)s(20%CO_(2) concentration)even under the influence of water and cement dust.In addition,slaked lime selected as the absorbent is cheap and the product after bubbling absorption is nano-scale light calcium carbonate.To sum up,the hybrid system combining non-contact membrane and bubbling absorption is expected to be used to capture carbon dioxide from the flue gas of the cement plant.
文摘With the rapid industrialization and urbanization,the demand for air quality management is more and more urgent.High temperature dust filtration is one important environmental management technology.Porous ceramics are used as filter materials in the field of high-temperature dust filtration because of their unique advantages such as high filtration efficiency,as well as high temperature stability,particle loss resistance,corrosion resistance and durability.This paper mainly introduced several common preparation techniques of porous ceramics,including the traditional organic foam impregnation method,foaming method,in-situ combustion method,pore-forming method and other new methods such as the template method,gel injection molding method,freeze-drying method,multi-component co-precipitation method and hydrogel method.The principle,advantages and disadvantages of these preparation technologies and their research status were described.The application of these technologies in the field of high temperature dust filtration was briefly reviewed.Finally,the application prospect of the porous ceramics in the field of high temperature dust filtration was prospected.
基金Project(50802052)supported by the National Natural Science Foundation of China
文摘The core-shell structure silicon-resin precursor powders were synthesized through coat-mix process and addition of Al2O3-SiO2-Y2O3 composite additives.A series of porous silicon carbide ceramics were produced after molding,carbonization and sintering.The phase,morphology,porosity,thermal conductivity,thermal expansion coefficient,and thermal shock resistance were analyzed.The results show that porous silicon carbide ceramics can be produced at low temperature.The grain size of porous silicon carbide ceramic is small,and the thermal conductivity is enhanced significantly.Composite additives also improve the thermal shock resistance of porous ceramics.The bending strength loss rate after 30 times of thermal shock test of the porous ceramics which were added Al2O3-SiO2-Y2O3 and sintered at 1 650 ℃ is only 6.5%.Moreover,the pore inside of the sample is smooth,and the pore size distribution is uniform.Composite additives make little effect on the thermal expansion coefficient of the porous silicon carbide ceramics.
基金The National Natural Science Foundation of China(No.50846056)
文摘To improve the wall surface hydrophilicity of a tube type indirect evaporative cooler,a new method adopting porous ceramics is proposed.This method realizes the combination of porous ceramics and the evaporative cooling technique.The design calculation of the porous ceramics tube type dew point indirect evaporative cooler are carried out from such aspects as the volumes and status parameters of the primary and secondary air,the cooler structure,the heat transfer of the solid porous ceramic tubes and the resistance of the cooler.The calculation results show that the design is reasonable.Finally,based on the design calculation,the porous ceramics tube type dew point indirect evaporative cooler is successfully manufactured.
基金Puyang Re-fractories Co. Ltd. for financially supporting
文摘Porous ceramics were prepared from kaolinite gangue and Al(OH)3 with double addition of MgCO3 and CaCO3 by the pore-forming in-situ technique.The characterizations of porous ceramics were investigated by X-ray diffractometry,scanning electron microscopy,and mercury porosimetry measurements,etc.It is found that although the decomposition of MgCO3 and CaCO3 has little contribution to the porosity,the double addition of MgCO3 and CaCO3 strongly affects the formation of liquid phase,and then changes the phase compositions,pore characterization,and strength.The appropriate mode is the sample containing 1.17wt% MgCO3 and 1.17wt% CaCO3,which has high apparent porosity(41.0%),high crushing strength(53.5 MPa),high mullite content(76wt%),and small average pore size(3.24 μm).
基金Supported by the National Natural Science Foundation of China (20990222, 21106061), the National Basic Research Program of China (2009CB623406), the National Key Science and Technology Program of China (2011BAE07B05) and the Natural Science Foundation of Jiangsu Province, China (BK2010549, BK2009021).
文摘Heterogeneous catalysts with ultrafine or nano particle size have currently attracted considerable attentions in the chemical and petrochemical production processes, but their large-scale applications remain challenging because of difficulties associated with their efficient separation from the reaction slurry. A porous ceramic membrane reactor has emerged as a promising method to solve the problem concerning catalysts separation in situ from the reaction mixture and make the production process continuous in heterogeneous catalysis. This article presents a review of the present progress on porous ceramic membrane reactors for heterogeneous catalysis, which covers classification of configurations of porous ceramic membrane reactor, major considerations and some important industrial applications. A special emphasis is paid to major considerations in term of application-oriented ceramic membrane design, optimization of ceramic membrane reactor performance and membrane fouling mechanism. Finally, brief concluding remarks on porous ceramic membrane reactors are given and possible future research interests are also outlined.
文摘A new approach in combination of the effective medium theory with the equivalent unit in numerical simulation was developed to study the effective thermal conductivity of porous ceramics. The finite element method was used to simulate the heat transfer process which enables to acquire accurate results through highly complicated modeling and intensive computation. An alternative approach to mesh the material into small cells was also presented. The effective medium theory accounts for the effective thermal conductivity of cells while the equivalent unit is subsequently applied in numerical simulation to analyze the effective thermal conductivity of the porous ceramics. A new expression for the effective thermal conductivity, allowing for some structure factors such as volume fraction of pores and thermal conductivity, was put forward, and the results of its application was proved to be close to those of the mathematical simulation.
基金supported by the Natural Science Research Projects of the Education Department of Henan Province,China(No.2011B610005)
文摘Medical stone-based porous ceramics as a carrier were prepared by ultra-fine grinding and low-temperature sintering method. Nano-TiO~ thin films were loaded on the carrier by chemical liquid deposition method using titanium tetrachloride as a precursor. The micro-morphology and microstructure of the synthesized samples were characterized using X-ray diffraction, scanning electron microscopy with energy dispersive spectrometry, and mercury injection method. The photo-catalytic activity of the TiO2 thin films was investigated by degrading formaldehyde. The main crystalline phase in the TiO2 thin films calcined at 550~C is anatase with the average particle size about 10 nm. The specific surface area of the carrier-coated nano-TiO2 increases from 3.68 to 5.32 m2/g. The formaldehyde removal rate of the TiO2/medical stone-based porous ceramics irradiated under an ultraviolet lamp for 120 min reaches 85.6%.
基金Project(202045007)supported by the Start-up Funds for Outstanding Talents in Central South University,China。
文摘By employing sintering additives of Li2CO3 and Y2O3,porous Si3N4 ceramics are prepared after experiencing the processes of sintering and post-vacuum heat treatment at 1680 and 1550°C,respectively.The experimental results demonstrate the completed phase transformation fromαtoβ-Si3N4 in Si3N4 ceramic samples with a amount of 1.60 wt%Li2CO3(0.65 wt%Li2O)and 0.33 wt%Y2O3 additives.The as-synthesized porous Si3N4 ceramics exhibit high flexural strength((126.7±2.7)MPa)and high open porosity of 50.4%at elevated temperature(1200°C).These results are attributed to the significant role of added Li2CO3 as sintering additive,where the volatilization of intergranular glassy phase occurs during sintering process.Therefore,porous Si3N4 ceramics with desired mechanical property prepared by altering the addition of sintering additives demonstrate their great potential as a promising candidate for high temperature applications.
基金financially supported by the Project of the Science and Technology Creative Team of Universities in Jiangxi Province,China(No.00008713)the Open Foundation of Jiangxi Key Laboratory for Advanced Copper and Tungsten Materials(No.2013-KLP-04)
基金National Natural Science Foundation of China under Grant No.(51372197)Key Innovation Team of Shaanxi Province under Grant No.(2014KCT-04)Provincial Joint Fund of Shaanxi(2021JLM-28).
文摘The large-scale accumulation and pollution of solid mining waste is an urgent issue.Coal gangue is a prominent type of solid waste,and shows promise for use in high value-added products due to its content of many important compounds,including SiO_(2) and Al2O3.This study proposed the preparation of highly porous ceramics from coal gangue,coal slime,and coconut palm fibers.The ceramics were produced at a sintering temperature of 950℃ with a fiber content of 6 wt%,which led to the formation of porous ceramics with a porosity of 66.93%,volume density of 1.0329 g/cm^(3),compressive strength of 1.1025 MPa,and thermal conductivity is 0.3919 K(W/mk).A finite element model of the porous ceramics was established using the Abaqus module in ANSYS software,where the stress distribution and compressive strength were simulated.Further,the relationship between porosity and compressive strength was analyzed.The thermal properties of the porous ceramics were analyzed using the Fluent module,where the simulated changes in porosity under various sintering temperatures were consistent with the experimental data.The preparation of this highly porous ceramic from solid waste coal gangue shows promise for the minimizing the impact of waste gas and wastewater pollution in the future.
基金supported by the National Natural Science Foundation of China under grant No.90305016.
文摘This paper presents the microwave dielectric properties of reaction bonded porous silicon nitride ceramics with variant porosity and pore size, which were prepared by adding pore-forming agent grains into the silicon powders. The experimental results show that the dielectric constant and the dielectric loss of the samples reduce evidently with increasing porosity in the sample. When the porosity is constant, the dielectric constant and the dielectric loss of the ceramics decrease visibly as the pore size increases. Among all the obtained samples, the minimum dielectric constant is about 2.4.
基金The authors are grateful for the financial supports from the National Natural Science Foundation of China(Nos.51674207,51922091)the Young Elite Scientists Sponsorship Program by CAST,China(No.2018QNRC001)the Sichuan Science and Technology Program,China(Nos.2019YFS0453,2018JY0148).
文摘Porous ceramics were prepared with spodumene flotation talings(SFT),kaolin and low-melting point glass(LPG)powder,whose pores were formed by the chemical reaction of hydrogen peroxide(H_(2)O_(2)).LPG was used to reduce the sintering temperature of porous ceramics and kaolin was used to realize the adsorption to methylene blue(MB)of porous ceramics.The average flexural strength,compressive strength,apparent porosity,water absorption and maximum MB adsorption capacity were 5.60 MPa,4.66 MPa,52.27%,44.32%and 0.7 mg/g,respectively.Moreover,the results of orthogonal experiments present that the sintering temperature and the dosage of H_(2)O_(2)had great influence on the mechanical properties and apparent porosity of porous ceramics,respectively.The main reason for the improvement of mechanical properties of porous ceramics was that LPG gradually became soft with increasing the sintering temperature,which made the mineral particles adhere to each other closely.Kaolinite was not completely converted into metakaolin at 550℃,which might be the main reason why porous ceramics had adsorption properties.
基金Project(51202296) supported by the National Natural Science Foundation of China
文摘To obtain porous alumina ceramic with high strength,a novel gelcasting system based on 2-hydroxyethyl methacrylate(HEMA)dissolved in tert-butyl alcohol(TBA)was developed.The polymerization of the HEMA-TBA gelcasting system,the thermal behavior of obtained green body,and the microstructures and mechanical properties of the sintered bodies were investigated by rheometer,TG-DSC,SEM and bending strength testing,respectively.The results show that,(1)10 mg/mL of the initiator(benzoyl peroxide)is the optimal amount for polymerization of this gelscasting system at 25 ℃;(2)The alumina suspension of the HEMA-TBA gelcasting system showing shear-thinning behavior is sufficiently low for gelcasting process;(3)The bending strength of porous alumina ceramic samples,whose porosities range from 42% to 56%,is from(8±0.5)to(91±4.5)MPa.
文摘Porous ceramics was made from coal fly ash, and the microstructure and other properties were characterized as a function of the amount of the pore-forming agent and firing temperature. The results indicated that the proper sintering temperature for the useful ceramic materials is 1 250℃, and a liquid-phase was involved in the densification process.
基金Project(50878080)supported by the National Natural Science Foundation of ChinaProject(K0902006-31)supported by the Key Scientific and Technological Special of Changsha City in China
文摘The general behavior of micron-particles in the inner domain of porous ceramic vessel was simulated by computational fluid dynamics software in terms of sampling experimental data.The results show that there is an optimum porosity of 0.32 to get a higher efficiency and lower pressure drop during filtration.According to the results of simulation and experiment,it is evident that lower inlet velocity can maintain lower pressure drop and obtain higher collection efficiency and inlet concentration also has a crucial influence on the collection efficiency.The collection efficiency of equipment increases significantly with the increase of inlet concentration when the inlet concentration is less than 6.3 g/m3,but it gradually tends to be stable in the range of 97.3%-99.7%when the inlet concentration is over this concentration.
基金supported by grants from the National Natural Science Foundation of China (NSFC-No. 51672256)Project of Outstanding Talents of Henan Province (No.184200510024).
文摘In this paper,calcium hexaaluminate(CA6)porous ceramics were prepared by a foaming method combined with cement solidification molding.The effects of the foaming agent addition on the microstructure and the properties of the ceramics were studied.The results show that the microstructure and the porosity of the ceramics can be controlled by adjusting the addition of the foaming agent.As the addition of the foaming agent increased,the bulk density reduced from 1 g·cm^-3 to 0.35 g·cm^-3,the porosity increased from 70.4%to 89.6%,the compressive strength reduced from 18.46 MPa to 1.66 MPa,and the thermal conductivity at 1000°C decreased from 0.382 W·m^-1·K^-1 to 0.144 W·m^-1·K^-1.It is indicated that calcium hexaaluminate porous ceramics with low density,high strength and low thermal conductivity can be obtained by the foaming method.As the lining material of high temperature electric furnaces,the ceramic has excellent energy saving effect.