SiCp/Al2O3-Al composites were synthesized by means of direct metal oxidation method. The composition and microstructures of the composites were investigated using X-ray diffraction (XRD), scanning electron microsco...SiCp/Al2O3-Al composites were synthesized by means of direct metal oxidation method. The composition and microstructures of the composites were investigated using X-ray diffraction (XRD), scanning electron microscopy (SEM) and metallurgical microscope. The effects of technical parameters on the properties of the product were analyzed. The results indicate that the composite possesses a dense microstructure, composed of three interpenetrated phases. Of them, SiO2 layer prohibits the powdering of the composites; Mg promotes the wetting and infiltration of the system and Si restricts the interfacial reaction while improving the wetting ability between reinforcement and matrix.展开更多
To explain the growth mechanism of Al 2O 3/Al Lanxide composites,the dynamics of the directed oxidation of Al-Mg-Si alloys are analyzed.The experimental methods to produce Lanxide composites by directed oxidation of...To explain the growth mechanism of Al 2O 3/Al Lanxide composites,the dynamics of the directed oxidation of Al-Mg-Si alloys are analyzed.The experimental methods to produce Lanxide composites by directed oxidation of metal melts at high temperatures are presented.The effect of the processing factors on the microstructures and properties of Al 2O 3/Al composites and enforced Al 2O 3/Al composites is also analyzed.Compared with sintering ceramic composites,the advantages of Lanxide process and Lanxide materials are as following:it is a near net shaped process;the process is very simple;the microstructures and properties of Lanxide materials can be adjusted;and this process can be used to infiltrate ceramic fiber or particle preforms.展开更多
基金National Natural Science Foundation of China (50372037)Scientific Research Foundations of Shaanxi University of Science and Technology (SUST-B14)
文摘SiCp/Al2O3-Al composites were synthesized by means of direct metal oxidation method. The composition and microstructures of the composites were investigated using X-ray diffraction (XRD), scanning electron microscopy (SEM) and metallurgical microscope. The effects of technical parameters on the properties of the product were analyzed. The results indicate that the composite possesses a dense microstructure, composed of three interpenetrated phases. Of them, SiO2 layer prohibits the powdering of the composites; Mg promotes the wetting and infiltration of the system and Si restricts the interfacial reaction while improving the wetting ability between reinforcement and matrix.
文摘To explain the growth mechanism of Al 2O 3/Al Lanxide composites,the dynamics of the directed oxidation of Al-Mg-Si alloys are analyzed.The experimental methods to produce Lanxide composites by directed oxidation of metal melts at high temperatures are presented.The effect of the processing factors on the microstructures and properties of Al 2O 3/Al composites and enforced Al 2O 3/Al composites is also analyzed.Compared with sintering ceramic composites,the advantages of Lanxide process and Lanxide materials are as following:it is a near net shaped process;the process is very simple;the microstructures and properties of Lanxide materials can be adjusted;and this process can be used to infiltrate ceramic fiber or particle preforms.