The effects of alloying elements in welding wires and submerged arc welding process on the microstructures and low-temperature impact toughness of weld metals have been investigated. The results indicate that the opti...The effects of alloying elements in welding wires and submerged arc welding process on the microstructures and low-temperature impact toughness of weld metals have been investigated. The results indicate that the optimal contents of alloying elements in welding wires can improve the low-temperature impact toughness of weld metals because the proeutectoid ferrite and bainite formations can be suppressed, and the fraction of acicular ferrite increases. However, the contents of alloying elements need to vary along with the welding heat input. With the increase in welding heat input, the contents of alloying elements in welding wires need to be increased accordingly. The microstructures mainly consisting of acicular ferrite can be obtained in weld metals after four-wire submerged arc welding using the wires with a low carbon content and appropriate contents of Mn, Mo, Ti-B, Cu, Ni, and RE, resulting in the high low-temperature impact toughness of weld metals.展开更多
The arc characteristics of submerged arc welding (SAW) with stainless steel wire were studied by using Analysator Hannover (AH). The tests were carded out under the same preset arc voltage combined with different ...The arc characteristics of submerged arc welding (SAW) with stainless steel wire were studied by using Analysator Hannover (AH). The tests were carded out under the same preset arc voltage combined with different welding currents. By comparing the probability density distribution (PDD) curves of arc voltage and welding current, the changes were analyzed, the metal transfer mode in SAW was deduced, and the characteristics of a stable arc were summarized. The analysis results show that, with an increase of welding parameters, the short-circuiting peak in the PDD curves of arc voltage decreases gradually until it disappears, and the dominant metal transfer mode changes from flux-wall guided transfer to projected transfer and then to streaming transfer. Moreover, when the PDD curves of arc voltage are both unimodal and generally symmetrical, the greater the peak probability and the smaller the peak span, the more stable the arc becomes.展开更多
In this study,the welding thermal cycle curve exhibited two temperature peaks in high heat-input twin-wire separate-pool submerged-arc welding and coarse-grained heat affected zone existed in the welded joint. The inc...In this study,the welding thermal cycle curve exhibited two temperature peaks in high heat-input twin-wire separate-pool submerged-arc welding and coarse-grained heat affected zone existed in the welded joint. The inclusions of primary weld metal and coarse-grained heat affected zone of Ce-added SAW should be Al_2O_3,MnO,SiO_2,TiO,Ce_2S_3,CeS,Ce_2O_2S and Ce_2O_3. Under the effect of welding thermal cycle,oxy-sulfides inclusions of Ce,the diameter of which was less than 2. 0 μm,slightly grew larger,but the composition and type of the inclusions didn't change. The microstructure of the large heat input weld metal had acicular ferrite that Ce oxide sulphide particles induced nucleation and proeutectoid ferrite. In the coarse-grained heat affected zone of weld metal,home-position precipitation of acicular ferrite and sympathetic acicular ferrite were both observed. It was supposed that previous crystal cells of acicular ferrite in austenite grain promoted home-position precipitation of acicular ferrite. Meanwhile,sympathetic acicular ferrite tended to nucleate at the primary acicular ferrite grain boundaries,where high dislocation density was located,and grew inside the neighboring carbon-depleted austenitic regions. The granular bainite nucleated in the austenitic zone with high carbon content close to acicular ferrite and sympathetic acicular ferrite.展开更多
According to the study of the microstructure and properties of X100 pipeline steel, the welding consumable-wire based on Mn-Ni-Mo-B-Ti alloy system was successfully designed and developed. The yield strength of the de...According to the study of the microstructure and properties of X100 pipeline steel, the welding consumable-wire based on Mn-Ni-Mo-B-Ti alloy system was successfully designed and developed. The yield strength of the deposited metal of the developed welding wire was 695 MPa, the tensile strength was 810 MPa, and Charpy impact energy was 92 J at negative 20 ℃ when matching with BSG-SJ101H1 sintered flux. The results of the weldability test for X100 pipeline steel which adopting this developed wire showed that the tensile strength of the weld was 827 MPa, 185 J of Charpy impact energy( -10 ℃ ) , 97% of section of shear and the weld had good strength and toughness matching when the welding speed got to 1.7 m/min. The microstructure and fracture appearance of the weld were analyzed by using metallographic microscope, scanning electron microscope (SEM) and laser confocal microscope, the results indicated that the microstructure was mainly granular bainite in the weld metal, and the fracture was dimple with 200 - 300 μm depth presenting a typical ductile fracture characteristics. The test of welding wire with different content of Ni and Cr element indicated that Ni was better than Cr in improving the strength and toughness of weld metal.展开更多
TC4 titanium alloy was welded by double-sided gas tungsten arc welding(GTAW) process in comparison with conventional GTAW process, the microstructure and mechanical performance of weld were also studied. The results i...TC4 titanium alloy was welded by double-sided gas tungsten arc welding(GTAW) process in comparison with conventional GTAW process, the microstructure and mechanical performance of weld were also studied. The results indicate that double-sided GTAW is superior over regular single-sided GTAW on the aspects of increasing penetration, reducing welding deformation and improving welding efficiency. Good weld joint was obtained, which can reach 96.14% tensile strength and 70.85% elongation percentage of the base metal. The grains in heat-affected zone(HAZ) are thin and equiaxed and the degree of grain coarsening increases as one moves to the weld center line, and the interior of grains are α and α′ structures. The coarse columned and equiaxed grains, which interlace martensitic structures α′ and acicular α structures, are observed in weld zone. The fracture mode is ductile fracture.展开更多
In the double-sided arc welding system (DSAW) composing of PAW+TIG arcs, the PAW arc is guided by the TIG arc so that the current mostly flows through the direction of the workpiece thickness and the penetration is gr...In the double-sided arc welding system (DSAW) composing of PAW+TIG arcs, the PAW arc is guided by the TIG arc so that the current mostly flows through the direction of the workpiece thickness and the penetration is greatly improved. To analyze the current density distribution in DSAW is beneficial to understanding of this process. Considering all kinds of dynamic factors acting on the weldpool, this paper discusses firstly the surface deformation of the weldpool and the keyhole formation in PAW+TIG DSAW process on the basis of the magnetohydrodynamic theory and variation principles. Hence, a model of the current density distribution is developed. Through numerical simulation, the current density distribution in PAW+TIG DSAW process is quantitatively analyzed. It shows that the minimal radius of keyhole formed in PAW+TIG DSAW process is 0.5 mm and 89.5 percent of current flows through the keyhole.展开更多
Wire arc additive manufacturing(WAAM)has been investigated to deposit large-scale metal parts due to its high deposition efficiency and low material cost.However,in the process of automatically manufacturing the high-...Wire arc additive manufacturing(WAAM)has been investigated to deposit large-scale metal parts due to its high deposition efficiency and low material cost.However,in the process of automatically manufacturing the high-quality metal parts by WAAM,several problems about the heat build-up,the deposit-path optimization,and the stability of the process parameters need to be well addressed.To overcome these issues,a new WAAM method based on the double electrode micro plasma arc welding(DE-MPAW)was designed.The circuit principles of different metal-transfer models in the DE-MPAW deposition process were analyzed theoretically.The effects between the parameters,wire feed rate and torch stand-off distance,in the process of WAAM were investigated experimentally.In addition,a real-time DE-MPAW control system was developed to optimize and stabilize the deposition process by self-adaptively changing the wire feed rate and torch stand-off distance.Finally,a series of tests were performed to evaluate the control system’s performance.The results show that the capability against interferences in the process of WAAM has been enhanced by this self-adaptive adjustment system.Further,the deposition paths about the metal part’s layer heights in WAAM are simplified.Finally,the appearance of the WAAM-deposited metal layers is also improved with the use of the control system.展开更多
Twin wire submerged arc welding (SAW) is widely used in oil or gas line pipe fabrication because of its high productivity. To investigate the strength and toughness of the heat-affected zone (HAZ) in twin wire SAW...Twin wire submerged arc welding (SAW) is widely used in oil or gas line pipe fabrication because of its high productivity. To investigate the strength and toughness of the heat-affected zone (HAZ) in twin wire SAW, the cooling time t8/5 of the coarse grained zone must be studied. The authors presented a method of predicting the cooling time in twin wire SAW of intermediate thickness plate. Based on Rosenthal analytical solutions, an energy factor was introduced to describe the energy contribution of the two wires, equations of thermal cycle and cooling time in twin wire SAW of both thick, and thin, plates were developed. Weighting factors determined by actual thickness and critical thickness were adopted to represent the thermal cycle and cooling time of intermediate thickness plate through linear interpolation with thick, and thin, plate solutions. The predicted cooling time for an intermediate thickness plate was verified experimentally, and the predicted results agreed therewith.展开更多
Aimed at plasma arc welding, a mathematic model was established according to the theory of magnetic fluid dyaamics. The model was numerically analyzed by ANSYS software. The temperature, current density and plasma vel...Aimed at plasma arc welding, a mathematic model was established according to the theory of magnetic fluid dyaamics. The model was numerically analyzed by ANSYS software. The temperature, current density and plasma velocity distributions of normal arc had been simulated and compared with those of double arc. The results show that the appearance of double arc has made the temperature of the nozzle rise up to 5 000 K. The appearance of side arc could make the current density of the main arc decrease, and also make the maximal temperature of the arc reduce.展开更多
A new high efficiency welding method, double-sided double arc welding with double powers (DSAW-D), is developed for thick plate of low alloy high strength steel in this study. It is well known that the thermal cycle...A new high efficiency welding method, double-sided double arc welding with double powers (DSAW-D), is developed for thick plate of low alloy high strength steel in this study. It is well known that the thermal cycles have an important influence on the microstructure, shape, stress, distortion and mechanical property. The DSA W-D method can control the temperature field on a wide range by regulating the distance between two arcs, improve the microstructure and prevent hot and cold cracking of high strength steel. But at present, the effect of arc distance on the temperature field and shape is not clear. Therefore, the paper researches the effect of arc distance on the temperature field and weld pool during DSAW-D using finite element method. The transient temperature field of different arc distance in DSAW-D is calculated. To verify the numerical results, the temperature is measured by the thermo-couple and the calculated results agree approximately with experimental data. Farther, the thermal property and mutual effect of double-sided arcs are investigated. The temperature distributions and weld pool profile at different arc distances are obtained. The results show that arc distance is a very important factor to affect the heat process.展开更多
The influence of laser parameters on are beharior of laser-TIC, dauble-side welding was investigated by utilizing CCD sensor and intage processing methods. It was found that are images had an obvious transformation fr...The influence of laser parameters on are beharior of laser-TIC, dauble-side welding was investigated by utilizing CCD sensor and intage processing methods. It was found that are images had an obvious transformation from laser preheating to laser plasma ejected from the keyhole bottom, resulting in the phenomena of arc column convergence and arc root constrictian. The attraction phenomenon of the laser and the arc is also found in laser-TIG double-side welding. More noteworthy is that the behavior of arc attraction or constriction became much obvious at a lower current or laser plasma ejected from the keyhole bottom. The decrease in arc voltage had a certain relation u'ith the improvement of arc stabilio.展开更多
Double-sided arc welding with a single power source can effectively increase the weld penetration, diminish distortion, improve welding speed and save energy. Compared to conventional arc welding processes, double-sid...Double-sided arc welding with a single power source can effectively increase the weld penetration, diminish distortion, improve welding speed and save energy. Compared to conventional arc welding processes, double-sided arc welding can generate a penetrating electromaguetic field to help to form fine dendritic microstrueture in the weld due to the symmetry of heating. Type 1Cr1SNi9Ti aastenitic stainless steel was bead-on-plate welded with double-sided arc welding and conventional plasma arc welding processes, respectively, and microstructure in the weld, heat-affected zone and base metal were examined. After analyzing the black carbon-enriched band in the weld during plasma arc welding with electron probe microanalyzer ( EPMA ) and X-ray diffraction (XRD) technology, it was found that the black band was shaped from the aggregation of ferrite in the fasion boundary. Hardness measurement showed that this black band does not apparently affect the microhardncss distribution in the weld.展开更多
High strength steel thick plate is widely used in shipbuilding, pressure vessels, etc. , the balance between weld quality and welding efficiency is becoming a research focus. In this paper, double-sided double arc fia...High strength steel thick plate is widely used in shipbuilding, pressure vessels, etc. , the balance between weld quality and welding efficiency is becoming a research focus. In this paper, double-sided double arc fiat-overhead welding experiments for high strength steel thick plate were conducted. Microstructures of weld have been observed through optical microscope (OM) and scanning electron microscope (SEM). Transformation of microstructures under thermal cycles of multi peaks was analyzed. Macro and micro hardness were also tested. The results show that the heat-affected zone (HAZ) near the fusion line experiences thermal cycles up to three times. The microstructures there are the most complex, including coarse lath martensite in original coarse-grained zone, and net-like structure along grain boundaries in critical reheat coarse-grained zone. After several times of tempering for bucking welding, the features of acicula and lath are weakened. Its microstructure approaches to the microstructure of base metal which is tempering sorbite. The hardness test shows that the maximum hardness occurs at critical reheat coarse-grained zone, the hardness of reticulation structure at grain boundary can be up to 450 HV.展开更多
The effect of laser power on metal transfer is studied under conditions of alternating combustion of double arcs in order to develop the welding process of the laser-double arcs pulsed metal active gas (P-MAG) hybri...The effect of laser power on metal transfer is studied under conditions of alternating combustion of double arcs in order to develop the welding process of the laser-double arcs pulsed metal active gas (P-MAG) hybrid welding with single power. Different laser power corresponds to different interactive mechanisms of laser and arc and to different methods of metal transfer in the hybrid welding. When the laser power ascends from 500 W to 1 500 W, the methods of metal transfer change from the complex transfer of one droplet per pulse, one droplet two pulses and one droplet much more pulses during the mixture of globular and projected transfer of the lead wire, and from one droplet two pulses and one droplet three pulses during globular transfer of the follow wire to the methods of the metal transfer of both lead wire and follow wire are stable one droplet two pulses and one droplet three pulses when the metal transfer is mainly globular. The arc sharps and pressure of droplet are altered with the laser power changing. The compression of the arcs is strengthened by the laser and the offset of the center of droplet mass is much more obvious with the increasing of the laser power.展开更多
The tenacity of heat-affected zone (HAZ) will decline and the size of grains will increase, because of the overheating on HAZ when submerged are welding (SAW) is ased to thick plate with high heat input. The shapi...The tenacity of heat-affected zone (HAZ) will decline and the size of grains will increase, because of the overheating on HAZ when submerged are welding (SAW) is ased to thick plate with high heat input. The shaping will worsen when SAW is used to thin plate with high current at high speed. A new SAW technology, the pulsed direct current (DC) automatic SAW, will be put forward in this paper in order to overcome the above shortcomings. And a pulsed controller with micro-controller unit (MCU) as the core, nixie tube (NT) and keyboard as the man-machine conversation interface is developed. The main functions of the pulsed controller include the output of pulsed welding current and the working with twinwire. The research has widely prospects in application with significant meanings in theory and practical engineering.展开更多
A series of laser-TIG double-side welding experiments for aluminum alloys were carried out to investigate the heat efficiency of the process. The melting efficiency was introduced to evaluate quantitatively the degree...A series of laser-TIG double-side welding experiments for aluminum alloys were carried out to investigate the heat efficiency of the process. The melting efficiency was introduced to evaluate quantitatively the degree of the mutual effect of the laser and the arc. The results showed that the melting efficiency of laser-TIG double-side welding exceeded the sum of the laser and the arc taken separately. With the increase of heat input, the weld depth and melting efficiency of the laser and the arc were increased signifwantly. This, in fact, implies the strong mutual effect of the laser and the arc as heat sources joined simultaneously in the process. Comparatively, the higher efficiency of the laser constituent of heat sources plays the main role in the increase of the process efficiency. The phenomena of arc column convergence, increased laser absorptivity and the formation of heat accumulation region are the causes of the improvement of heat efficiency.展开更多
In view of the unstable welding process of Tri-Arc DE,surfacing test with Q235 steel plate was completed with the help of the self-built high-speed camera and waveform synchronous acquisition system using the Tri-Arc ...In view of the unstable welding process of Tri-Arc DE,surfacing test with Q235 steel plate was completed with the help of the self-built high-speed camera and waveform synchronous acquisition system using the Tri-Arc DE technology. The effects of pulsed M-Arc frequency on Tri-Arc DE droplet transfer and weld formation were analyzed. The results show that while the gradual increase of pulse frequency,the droplet transfer frequency gradually decreases,which is followed by several drops per pulse,one drop per pulse,and one drop within several pulses. The most ideal transfer form is one drop per pulse,of which the welding process is the most stable,and the quality of weld formation is the most satisfied.展开更多
基金supported by the Research and Development Project of Science and Technology of Hebei Province, China (No.03212211D and No.002121186D)
文摘The effects of alloying elements in welding wires and submerged arc welding process on the microstructures and low-temperature impact toughness of weld metals have been investigated. The results indicate that the optimal contents of alloying elements in welding wires can improve the low-temperature impact toughness of weld metals because the proeutectoid ferrite and bainite formations can be suppressed, and the fraction of acicular ferrite increases. However, the contents of alloying elements need to vary along with the welding heat input. With the increase in welding heat input, the contents of alloying elements in welding wires need to be increased accordingly. The microstructures mainly consisting of acicular ferrite can be obtained in weld metals after four-wire submerged arc welding using the wires with a low carbon content and appropriate contents of Mn, Mo, Ti-B, Cu, Ni, and RE, resulting in the high low-temperature impact toughness of weld metals.
基金financially supported by the Shanxi Provincial Key Programs for Science and Technology Development (No. 20100321084)Taiyuan Special Foundation for Excellent Talents (No. 20111075)
文摘The arc characteristics of submerged arc welding (SAW) with stainless steel wire were studied by using Analysator Hannover (AH). The tests were carded out under the same preset arc voltage combined with different welding currents. By comparing the probability density distribution (PDD) curves of arc voltage and welding current, the changes were analyzed, the metal transfer mode in SAW was deduced, and the characteristics of a stable arc were summarized. The analysis results show that, with an increase of welding parameters, the short-circuiting peak in the PDD curves of arc voltage decreases gradually until it disappears, and the dominant metal transfer mode changes from flux-wall guided transfer to projected transfer and then to streaming transfer. Moreover, when the PDD curves of arc voltage are both unimodal and generally symmetrical, the greater the peak probability and the smaller the peak span, the more stable the arc becomes.
基金supported by the National Natural Science Foundation of China,the Baoshan Iron&Steel Co.,Ltd(No.U1260103)
文摘In this study,the welding thermal cycle curve exhibited two temperature peaks in high heat-input twin-wire separate-pool submerged-arc welding and coarse-grained heat affected zone existed in the welded joint. The inclusions of primary weld metal and coarse-grained heat affected zone of Ce-added SAW should be Al_2O_3,MnO,SiO_2,TiO,Ce_2S_3,CeS,Ce_2O_2S and Ce_2O_3. Under the effect of welding thermal cycle,oxy-sulfides inclusions of Ce,the diameter of which was less than 2. 0 μm,slightly grew larger,but the composition and type of the inclusions didn't change. The microstructure of the large heat input weld metal had acicular ferrite that Ce oxide sulphide particles induced nucleation and proeutectoid ferrite. In the coarse-grained heat affected zone of weld metal,home-position precipitation of acicular ferrite and sympathetic acicular ferrite were both observed. It was supposed that previous crystal cells of acicular ferrite in austenite grain promoted home-position precipitation of acicular ferrite. Meanwhile,sympathetic acicular ferrite tended to nucleate at the primary acicular ferrite grain boundaries,where high dislocation density was located,and grew inside the neighboring carbon-depleted austenitic regions. The granular bainite nucleated in the austenitic zone with high carbon content close to acicular ferrite and sympathetic acicular ferrite.
文摘According to the study of the microstructure and properties of X100 pipeline steel, the welding consumable-wire based on Mn-Ni-Mo-B-Ti alloy system was successfully designed and developed. The yield strength of the deposited metal of the developed welding wire was 695 MPa, the tensile strength was 810 MPa, and Charpy impact energy was 92 J at negative 20 ℃ when matching with BSG-SJ101H1 sintered flux. The results of the weldability test for X100 pipeline steel which adopting this developed wire showed that the tensile strength of the weld was 827 MPa, 185 J of Charpy impact energy( -10 ℃ ) , 97% of section of shear and the weld had good strength and toughness matching when the welding speed got to 1.7 m/min. The microstructure and fracture appearance of the weld were analyzed by using metallographic microscope, scanning electron microscope (SEM) and laser confocal microscope, the results indicated that the microstructure was mainly granular bainite in the weld metal, and the fracture was dimple with 200 - 300 μm depth presenting a typical ductile fracture characteristics. The test of welding wire with different content of Ni and Cr element indicated that Ni was better than Cr in improving the strength and toughness of weld metal.
文摘TC4 titanium alloy was welded by double-sided gas tungsten arc welding(GTAW) process in comparison with conventional GTAW process, the microstructure and mechanical performance of weld were also studied. The results indicate that double-sided GTAW is superior over regular single-sided GTAW on the aspects of increasing penetration, reducing welding deformation and improving welding efficiency. Good weld joint was obtained, which can reach 96.14% tensile strength and 70.85% elongation percentage of the base metal. The grains in heat-affected zone(HAZ) are thin and equiaxed and the degree of grain coarsening increases as one moves to the weld center line, and the interior of grains are α and α′ structures. The coarse columned and equiaxed grains, which interlace martensitic structures α′ and acicular α structures, are observed in weld zone. The fracture mode is ductile fracture.
基金The authors wish to express their gratitude to the financial support to this project from the project foundation of the National Key Laboratory of Advanced Welding Production Technology of Harbin Institute of Technology and the US National Science Foundation under grant No.DMI 9812981
文摘In the double-sided arc welding system (DSAW) composing of PAW+TIG arcs, the PAW arc is guided by the TIG arc so that the current mostly flows through the direction of the workpiece thickness and the penetration is greatly improved. To analyze the current density distribution in DSAW is beneficial to understanding of this process. Considering all kinds of dynamic factors acting on the weldpool, this paper discusses firstly the surface deformation of the weldpool and the keyhole formation in PAW+TIG DSAW process on the basis of the magnetohydrodynamic theory and variation principles. Hence, a model of the current density distribution is developed. Through numerical simulation, the current density distribution in PAW+TIG DSAW process is quantitatively analyzed. It shows that the minimal radius of keyhole formed in PAW+TIG DSAW process is 0.5 mm and 89.5 percent of current flows through the keyhole.
基金Supported by National Natural Science Foundation of China(Grant No.51665034).
文摘Wire arc additive manufacturing(WAAM)has been investigated to deposit large-scale metal parts due to its high deposition efficiency and low material cost.However,in the process of automatically manufacturing the high-quality metal parts by WAAM,several problems about the heat build-up,the deposit-path optimization,and the stability of the process parameters need to be well addressed.To overcome these issues,a new WAAM method based on the double electrode micro plasma arc welding(DE-MPAW)was designed.The circuit principles of different metal-transfer models in the DE-MPAW deposition process were analyzed theoretically.The effects between the parameters,wire feed rate and torch stand-off distance,in the process of WAAM were investigated experimentally.In addition,a real-time DE-MPAW control system was developed to optimize and stabilize the deposition process by self-adaptively changing the wire feed rate and torch stand-off distance.Finally,a series of tests were performed to evaluate the control system’s performance.The results show that the capability against interferences in the process of WAAM has been enhanced by this self-adaptive adjustment system.Further,the deposition paths about the metal part’s layer heights in WAAM are simplified.Finally,the appearance of the WAAM-deposited metal layers is also improved with the use of the control system.
文摘Twin wire submerged arc welding (SAW) is widely used in oil or gas line pipe fabrication because of its high productivity. To investigate the strength and toughness of the heat-affected zone (HAZ) in twin wire SAW, the cooling time t8/5 of the coarse grained zone must be studied. The authors presented a method of predicting the cooling time in twin wire SAW of intermediate thickness plate. Based on Rosenthal analytical solutions, an energy factor was introduced to describe the energy contribution of the two wires, equations of thermal cycle and cooling time in twin wire SAW of both thick, and thin, plates were developed. Weighting factors determined by actual thickness and critical thickness were adopted to represent the thermal cycle and cooling time of intermediate thickness plate through linear interpolation with thick, and thin, plate solutions. The predicted cooling time for an intermediate thickness plate was verified experimentally, and the predicted results agreed therewith.
文摘Aimed at plasma arc welding, a mathematic model was established according to the theory of magnetic fluid dyaamics. The model was numerically analyzed by ANSYS software. The temperature, current density and plasma velocity distributions of normal arc had been simulated and compared with those of double arc. The results show that the appearance of double arc has made the temperature of the nozzle rise up to 5 000 K. The appearance of side arc could make the current density of the main arc decrease, and also make the maximal temperature of the arc reduce.
基金This work was supported by National Natural Science Foundation of China, No 50675046, 50775053.
文摘A new high efficiency welding method, double-sided double arc welding with double powers (DSAW-D), is developed for thick plate of low alloy high strength steel in this study. It is well known that the thermal cycles have an important influence on the microstructure, shape, stress, distortion and mechanical property. The DSA W-D method can control the temperature field on a wide range by regulating the distance between two arcs, improve the microstructure and prevent hot and cold cracking of high strength steel. But at present, the effect of arc distance on the temperature field and shape is not clear. Therefore, the paper researches the effect of arc distance on the temperature field and weld pool during DSAW-D using finite element method. The transient temperature field of different arc distance in DSAW-D is calculated. To verify the numerical results, the temperature is measured by the thermo-couple and the calculated results agree approximately with experimental data. Farther, the thermal property and mutual effect of double-sided arcs are investigated. The temperature distributions and weld pool profile at different arc distances are obtained. The results show that arc distance is a very important factor to affect the heat process.
文摘The influence of laser parameters on are beharior of laser-TIC, dauble-side welding was investigated by utilizing CCD sensor and intage processing methods. It was found that are images had an obvious transformation from laser preheating to laser plasma ejected from the keyhole bottom, resulting in the phenomena of arc column convergence and arc root constrictian. The attraction phenomenon of the laser and the arc is also found in laser-TIG double-side welding. More noteworthy is that the behavior of arc attraction or constriction became much obvious at a lower current or laser plasma ejected from the keyhole bottom. The decrease in arc voltage had a certain relation u'ith the improvement of arc stabilio.
文摘Double-sided arc welding with a single power source can effectively increase the weld penetration, diminish distortion, improve welding speed and save energy. Compared to conventional arc welding processes, double-sided arc welding can generate a penetrating electromaguetic field to help to form fine dendritic microstrueture in the weld due to the symmetry of heating. Type 1Cr1SNi9Ti aastenitic stainless steel was bead-on-plate welded with double-sided arc welding and conventional plasma arc welding processes, respectively, and microstructure in the weld, heat-affected zone and base metal were examined. After analyzing the black carbon-enriched band in the weld during plasma arc welding with electron probe microanalyzer ( EPMA ) and X-ray diffraction (XRD) technology, it was found that the black band was shaped from the aggregation of ferrite in the fasion boundary. Hardness measurement showed that this black band does not apparently affect the microhardncss distribution in the weld.
基金Acknowledgments The authors gratefully acknowledge the financial support provided by the National Natural Science Foundation of China under grant No. 51175119.
文摘High strength steel thick plate is widely used in shipbuilding, pressure vessels, etc. , the balance between weld quality and welding efficiency is becoming a research focus. In this paper, double-sided double arc fiat-overhead welding experiments for high strength steel thick plate were conducted. Microstructures of weld have been observed through optical microscope (OM) and scanning electron microscope (SEM). Transformation of microstructures under thermal cycles of multi peaks was analyzed. Macro and micro hardness were also tested. The results show that the heat-affected zone (HAZ) near the fusion line experiences thermal cycles up to three times. The microstructures there are the most complex, including coarse lath martensite in original coarse-grained zone, and net-like structure along grain boundaries in critical reheat coarse-grained zone. After several times of tempering for bucking welding, the features of acicula and lath are weakened. Its microstructure approaches to the microstructure of base metal which is tempering sorbite. The hardness test shows that the maximum hardness occurs at critical reheat coarse-grained zone, the hardness of reticulation structure at grain boundary can be up to 450 HV.
基金This paper is supported by National Natural Science Foundation of China (Grant No. 51175374) , the Application of Basic & Frontier Technology Program of Tianjin (Grant No. OgJCYBJC05000) and the Science & Technology Pillar Program of Tianjin (Grant No. 10ZCKFSF00200).
文摘The effect of laser power on metal transfer is studied under conditions of alternating combustion of double arcs in order to develop the welding process of the laser-double arcs pulsed metal active gas (P-MAG) hybrid welding with single power. Different laser power corresponds to different interactive mechanisms of laser and arc and to different methods of metal transfer in the hybrid welding. When the laser power ascends from 500 W to 1 500 W, the methods of metal transfer change from the complex transfer of one droplet per pulse, one droplet two pulses and one droplet much more pulses during the mixture of globular and projected transfer of the lead wire, and from one droplet two pulses and one droplet three pulses during globular transfer of the follow wire to the methods of the metal transfer of both lead wire and follow wire are stable one droplet two pulses and one droplet three pulses when the metal transfer is mainly globular. The arc sharps and pressure of droplet are altered with the laser power changing. The compression of the arcs is strengthened by the laser and the offset of the center of droplet mass is much more obvious with the increasing of the laser power.
文摘The tenacity of heat-affected zone (HAZ) will decline and the size of grains will increase, because of the overheating on HAZ when submerged are welding (SAW) is ased to thick plate with high heat input. The shaping will worsen when SAW is used to thin plate with high current at high speed. A new SAW technology, the pulsed direct current (DC) automatic SAW, will be put forward in this paper in order to overcome the above shortcomings. And a pulsed controller with micro-controller unit (MCU) as the core, nixie tube (NT) and keyboard as the man-machine conversation interface is developed. The main functions of the pulsed controller include the output of pulsed welding current and the working with twinwire. The research has widely prospects in application with significant meanings in theory and practical engineering.
文摘A series of laser-TIG double-side welding experiments for aluminum alloys were carried out to investigate the heat efficiency of the process. The melting efficiency was introduced to evaluate quantitatively the degree of the mutual effect of the laser and the arc. The results showed that the melting efficiency of laser-TIG double-side welding exceeded the sum of the laser and the arc taken separately. With the increase of heat input, the weld depth and melting efficiency of the laser and the arc were increased signifwantly. This, in fact, implies the strong mutual effect of the laser and the arc as heat sources joined simultaneously in the process. Comparatively, the higher efficiency of the laser constituent of heat sources plays the main role in the increase of the process efficiency. The phenomena of arc column convergence, increased laser absorptivity and the formation of heat accumulation region are the causes of the improvement of heat efficiency.
基金Project was supported by the National Natural Science Foundation of China(Grant No.U1733125)Natural Science Foundation of Tianjin(Grant No.18JCYBJC19100,18JCYJC18700)
文摘In view of the unstable welding process of Tri-Arc DE,surfacing test with Q235 steel plate was completed with the help of the self-built high-speed camera and waveform synchronous acquisition system using the Tri-Arc DE technology. The effects of pulsed M-Arc frequency on Tri-Arc DE droplet transfer and weld formation were analyzed. The results show that while the gradual increase of pulse frequency,the droplet transfer frequency gradually decreases,which is followed by several drops per pulse,one drop per pulse,and one drop within several pulses. The most ideal transfer form is one drop per pulse,of which the welding process is the most stable,and the quality of weld formation is the most satisfied.