期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
Outdoor Sports——The New Engine Driving Market Growth
1
作者 Zhao Fei 《China Textile》 2010年第9期42-44,共3页
Hot summer not only hampers the pace of people’s participation in outdoor sports,but also ignites the insiders’and more and more outdoor-sport lovers’enthusiasm.
关键词 engine The New engine Driving Market Growth Outdoor Sports
下载PDF
FATIGUE LIVES FOR INDUCTION HARDENED SHAFTS MATERIALS ACCORDING TO THE ENVIRONMENTAL TEMPERATURES 被引量:1
2
作者 D.G. Lee K.C. Jang +1 位作者 J.M. Kuk I.S. Kim 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2005年第5期585-593,共9页
Rotary bending fatigue tests were carried out with two kinds of materials, S43C and S50C, using the front engine and front drive shaft (FF shaft) of vehicle. The specimens were induction hardened about 1.0mm depth f... Rotary bending fatigue tests were carried out with two kinds of materials, S43C and S50C, using the front engine and front drive shaft (FF shaft) of vehicle. The specimens were induction hardened about 1.0mm depth from the specimen surface, and the hardness value on the surface was about HRC56-60. The tested environment temperatures were -30, 25 and 80℃ in order to look over effect of the induction hardening and the environmental temperatures on the fatigue characteristics. The fatigue limit of induction hardened specimens increased more about 45% than non-hardened specimens showing that the endurances of S43C and S50C were 98.1 and 107.9MPa in non-hardened samples, 147.1 and 156.9MPa in hardened samplesrespectably. The maximum tensile and compressive stress on the small circular defect was about +250 and -450MPa respectively when circular defect is situated on top and bottom. The fatigue life increased 80, 25 and -30℃ in order regardless of hardening. In comparison of the fatigue lives on the basis of tested result at 25℃, the fatigue lives of non-hardened specimens decreased about 35%, but that of hardened specimens decreased about only 5% at 80℃ more than at 25℃. And fatigue life of non-hardened and hardened specimens were about 110% and 120% higher at -30℃ than that of 25℃. Based on the result of stress distribution near the defect, the tensile and compressive stress repeatedly generated by load direction were the largest on the small circular defect due to the stress concentration. 展开更多
关键词 induction hardening fatigue test front engine and front drive shaft fatigue crack fatigue life fatigue life ratio