Degradation of ethyl xanthate in flotation residues by hydrogen peroxide 被引量:3
1
作者 陈兴华 胡岳华 +1 位作者 彭宏 曹学锋 《Journal of Central South University》 SCIE EI CAS CSCD 2015年第2期495-501,共7页
The degradation behavior of ethyl xanthate(EX) salt was the most widely used collector in sulfide mineral flotation and emission of flotation tailings with residual EX was harmful to environment. In this work, hydroge... The degradation behavior of ethyl xanthate(EX) salt was the most widely used collector in sulfide mineral flotation and emission of flotation tailings with residual EX was harmful to environment. In this work, hydrogen peroxide(H2O2) was investigated by UV-visible spectroscopy(UV/Vis) at different p H values from 3 to 12. For p H value from 5 to 12, EX was oxidized into ethyl per xanthate(EPX) by H2O2. Then EPX was further oxidized into thiosulfate(TS) salt rather than ethyl thiocarbonate(ETC) and this step was the reaction-limited step. Then depending on p H values, TS was degraded into sulphate and carbonate salts(p H>7) or elemental sulfur(p H<7). The kinetics data show that the degradation rate of EX increases with increasing the H2O2 concentration and is independent on the p H values. Without H2O2, EX is hydrolyzed to carbon disulfide fast at p H value <3.0, but the reaction of hydrolysis is undetectable at p H value >3.0 during test time. 展开更多
关键词 ethyl-xanthate THIOSULFATE hydrogen peroxide UV-visible spectroscopy
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部