Due to creep characteristics of wood,long-term loading can cause a significant stress loss of steel bars in rein-forced glulam beams and high long-term deflection of the beam midspan.In this study,15 glulam beams were...Due to creep characteristics of wood,long-term loading can cause a significant stress loss of steel bars in rein-forced glulam beams and high long-term deflection of the beam midspan.In this study,15 glulam beams were subjected to a 90-day long-term loading test,and the effects of long-term loading value,reinforcement ratio and prestress level on the stress of steel bars,midspan long-term deflection,and other parameters were compared and analyzed.The main conclusions drawn from this study were that the long-term deflection of the reinforced glulam beams accounted for 22.5%,20.6%,and 18.2%of the total deflection respectively when the loading value was 20%,30%,and 40%of the estimated ultimate load under the long-term loading.The higher the loading level was,the smaller the proportion of the long-term deflection in the total deflection was.Compared with ordinary glulam beams,the long-term deflection of the reinforced glulam beam was even smaller.Under the condition of the constant loading level,the total stress value of the steel bars decreased by 17.5%,13.6%,and 9.1%,and the proportion of the long-term deflection of the beam midspan in the total deflection was 26.9%,24.2%,and 20.6%respectively when the reinforcement ratio was 2.05%,2.68%,and 3.39%.With the increase of the reinfor-cement ratio,the stress loss of the steel bars decreased,and the proportion of the long-term deflection decreased as well.When other conditions remained constant and the prestress level of the steel bars was 0 MPa,30 MPa,and 60 MPa,the total stress value of the steel bars decreased by 9.1%,9.4%,and 10.2%,respectively,and the propor-tion of the long-term deflection in the total deflection was 20.6%,26.1%,and 64.9%,respectively.With the increase of the prestress value,the stress loss of the steel bars increased,and the proportion of the long-term deflection increased as well.展开更多
This paper presents the method of reinforcing main girder of reinforced concrete cable-stayed bridge with prestressed steel strands.To verify the effectiveness of external prestressed strand reinforcement method.Stati...This paper presents the method of reinforcing main girder of reinforced concrete cable-stayed bridge with prestressed steel strands.To verify the effectiveness of external prestressed strand reinforcement method.Static load tests and health monitoring-based assessment were carried out before and after reinforcement.Field load test shows that the deflection and stress values of the main girder are reduced by 10%~20%after reinforcement,and the flexural strength and stiffness of the strengthened beam are improved.The deflection and strain data of health monitoring of the specified section are collected.The deflection of the second span is 4 mm~10 mm,the strain range of the upper edge of the second span is-10με~-40με,and the strain range of the lower edge is 30με~75με.These values show the deflection and strain values fluctuate within a prescribed range,verifying the safety of the bridge.The reinforcement method of prestressed steel strand is feasible and effective.It can provide reference basis for the application of external prestressed strand reinforcement technology in similar projects.展开更多
基金This research work was supported by the Fundamental Research Funds for the Central Universities(2572017DB02)the natural science foundation of Heilongjiang Province(LH2019E005)the natural science of Heilongjiang Province(LH2020E009).
文摘Due to creep characteristics of wood,long-term loading can cause a significant stress loss of steel bars in rein-forced glulam beams and high long-term deflection of the beam midspan.In this study,15 glulam beams were subjected to a 90-day long-term loading test,and the effects of long-term loading value,reinforcement ratio and prestress level on the stress of steel bars,midspan long-term deflection,and other parameters were compared and analyzed.The main conclusions drawn from this study were that the long-term deflection of the reinforced glulam beams accounted for 22.5%,20.6%,and 18.2%of the total deflection respectively when the loading value was 20%,30%,and 40%of the estimated ultimate load under the long-term loading.The higher the loading level was,the smaller the proportion of the long-term deflection in the total deflection was.Compared with ordinary glulam beams,the long-term deflection of the reinforced glulam beam was even smaller.Under the condition of the constant loading level,the total stress value of the steel bars decreased by 17.5%,13.6%,and 9.1%,and the proportion of the long-term deflection of the beam midspan in the total deflection was 26.9%,24.2%,and 20.6%respectively when the reinforcement ratio was 2.05%,2.68%,and 3.39%.With the increase of the reinfor-cement ratio,the stress loss of the steel bars decreased,and the proportion of the long-term deflection decreased as well.When other conditions remained constant and the prestress level of the steel bars was 0 MPa,30 MPa,and 60 MPa,the total stress value of the steel bars decreased by 9.1%,9.4%,and 10.2%,respectively,and the propor-tion of the long-term deflection in the total deflection was 20.6%,26.1%,and 64.9%,respectively.With the increase of the prestress value,the stress loss of the steel bars increased,and the proportion of the long-term deflection increased as well.
文摘This paper presents the method of reinforcing main girder of reinforced concrete cable-stayed bridge with prestressed steel strands.To verify the effectiveness of external prestressed strand reinforcement method.Static load tests and health monitoring-based assessment were carried out before and after reinforcement.Field load test shows that the deflection and stress values of the main girder are reduced by 10%~20%after reinforcement,and the flexural strength and stiffness of the strengthened beam are improved.The deflection and strain data of health monitoring of the specified section are collected.The deflection of the second span is 4 mm~10 mm,the strain range of the upper edge of the second span is-10με~-40με,and the strain range of the lower edge is 30με~75με.These values show the deflection and strain values fluctuate within a prescribed range,verifying the safety of the bridge.The reinforcement method of prestressed steel strand is feasible and effective.It can provide reference basis for the application of external prestressed strand reinforcement technology in similar projects.