Free-standing diamond films have been successfully deposited on stainless steel substrates using microwave plasma-assisted chemical vapor deposition. Although iron, which is the main element of stainless steel, is kno...Free-standing diamond films have been successfully deposited on stainless steel substrates using microwave plasma-assisted chemical vapor deposition. Although iron, which is the main element of stainless steel, is known to inhibit the nucleation of diamond and enhance the formation of graphite, we were able to grow relatively thick films (-1.2 mm). The films were easily detachable from the substrates. The poor adhesion made it possible to obtain free-standing diamond films without chemical etching. Raman spectroscopy showed the 1332 cm^-1 characteristic Raman peak of diamond and the 1580 cm^-1, 1350 cm^-1 bands of graphite on the growth surface and backside of the films, respectively. By energy dispersive X-ray spectroscopy it was only possible to detect iron on the back of the films, but not on the surface. The role of iron in the film growth is discussed.展开更多
Free-standing diamond films, deposited using DC Arc Plasma Jet CVD method onto graphite substrates with titanium interlayers, have been investigated. The Ti interlayers were deposited by arc ion plating equipments. Th...Free-standing diamond films, deposited using DC Arc Plasma Jet CVD method onto graphite substrates with titanium interlayers, have been investigated. The Ti interlayers were deposited by arc ion plating equipments. The thickness, morphology and composite phase of Ti interlayers were examined by scanning electron microscopy (SEM) and X-ray diffraction (XRD). The titanium carbide (TiC) was detected in both sides of the interlayers, which played an important role with respect to reasonable adhesion with film and diamond nucleation. The semi-translucent diamond films were characterized by SEM and Raman spectrum. The sharp diamond peak with low intensity of amorphous carbon shows that diamond films have very high quality. The overall results suggest that plating Ti interlayer on graphite substrate is an effective way to obtain optical grade free-standing diamond films.展开更多
Free-standing diamond films were prepared by hot filament chemical vapor deposition (HFCVD) method under different conditions. Inter-digital transducers (IDTs) were formed on the nucleation sides of free-standing diam...Free-standing diamond films were prepared by hot filament chemical vapor deposition (HFCVD) method under different conditions. Inter-digital transducers (IDTs) were formed on the nucleation sides of free-standing diamond films by photolithography technique. Then piezoelectric ZnO films were deposited by radio-frequency(RF) reactive magnetron sputtering to obtain the ZnO/diamond film structures. Surface morphologies of the nucleation sides and the IDTs were characterized by means of scanning electron microscopy (SEM), atomic force microscope (AFM) and optical microscopy. The results indicate that the surfaces of nucleation sides are very smooth and the IDTs are of high quality without discontinuity and short circuit phenomenon. Raman spectra show the sharp diamond feature peak at about 1 334 cm?1 and the small amount of non-diamond carbon in the nucleation side. X-ray diffraction (XRD) patterns of the structure of ZnO/diamond films show a strong diffraction peak of ZnO (002), which indicates that as-sputtered ZnO films are highly c-axis oriented.展开更多
This study focused on the investigation of the edge effect of diamond films deposited by microwave plasma chemical vapor de-position.Substrate bulge height△h is a factor that affects the edge effect,and it was used t...This study focused on the investigation of the edge effect of diamond films deposited by microwave plasma chemical vapor de-position.Substrate bulge height△h is a factor that affects the edge effect,and it was used to simulate plasma and guide the diamond-film deposition experiments.Finite-element software COMSOL Multiphysics was used to construct a multiphysics(electromagnetic,plasma,and fluid heat transfer fields)coupling model based on electron collision reaction.Raman spectroscopy and scanning electron microscopy were performed to characterize the experimental growth and validate the model.The simulation results reflected the experimental trends observed.Plasma discharge at the edge of the substrate accelerated due to the increase in△h(△h=0-3 mm),and the values of electron density(n_(c)),molar concentration of H(C_(H)),and molar concentration of CH_(3)(C_(CH_(3)))doubled at the edge(for the special concave sample with△h=−1 mm,the active chemical groups exhibited a decreased molar concentration at the edge of the substrate).At=0-3 mm,a high diamond growth rate and a large diamond grain size were observed at the edge of the substrate,and their values increased with.The uniformity of film thickness decreased with.The Raman spectra of all samples revealed the first-order characteristic peak of dia-mond near 1332 cm^(−1).When△h=−1 mm,tensile stress occurred in all regions of the film.When△h=1-3 mm,all areas in the film ex-hibited compressive stress.展开更多
Highly c-axis-oriented ZnO films were deposited successfully on the nucleation sides of free-standing diamond (FD) films by the direct current (DC) magnetron sputtering method. The effect of the sputtering paramet...Highly c-axis-oriented ZnO films were deposited successfully on the nucleation sides of free-standing diamond (FD) films by the direct current (DC) magnetron sputtering method. The effect of the sputtering parameters, such as power, gas pressure and sputtering plasma composition of Ar-to-O2, on the properties of ZnO thin films was investigated in detail. X-ray diffraction (XRD) measurements showed that, at a sputtering power of 200 W, gas pressure of 0.5 Pa and an Ar-to- O2 composition of 1:1, a higher intensity of the (002) diffraction peak and a narrower full width at half maximum (FWHM) were detected which meant high c-axis orientation and high quality of the ZnO films. To improve the quality of the ZnO film, a thin ZnO layer was pre-grown as a homo-buffer layer. XRD measurements showed that this buffer layer had a beneficial effect on the structural and morphological properties of the post-grown ZnO film.展开更多
Blue-green electroluminescence has been observed in free-standing diamond films which were deposited by microwave plasma assisted CVD on silicon substrates.The electroluminescence device is driven by a 60 Hz power sup...Blue-green electroluminescence has been observed in free-standing diamond films which were deposited by microwave plasma assisted CVD on silicon substrates.The electroluminescence device is driven by a 60 Hz power supply.The threshold voltage was about 112 V peak-to-peak.The electroluminescence spectrum at room temperature,showed a blue-green band with the peak centered at 485nm suggesting band A type emission.Electroluminescence was also observed at 77K.展开更多
Recently,with the rapid development of chemical vapor deposition(CVD)technology,large area free-standing CVD diamond films have been produced successfully.However,the coarse grain size on the surface and the non-unifo...Recently,with the rapid development of chemical vapor deposition(CVD)technology,large area free-standing CVD diamond films have been produced successfully.However,the coarse grain size on the surface and the non-uniform thickness of unprocessed CVD diamond films make it difficult to meet the application requirement.The current study evaluates several existing polishing methods for CVD diamond films,including mechanical polishing,chemical mechanical polishing and tribochemical polishing technology.展开更多
Thermal stress in large area free-standing diamond films was remarkable during the post-deposition cooling of direct current (DC) arc plasma jet chemical vapor deposition (CVD) process.In this research,the stress ...Thermal stress in large area free-standing diamond films was remarkable during the post-deposition cooling of direct current (DC) arc plasma jet chemical vapor deposition (CVD) process.In this research,the stress release caused by delamination of Cr interlayer was of great importance to ensure the integrity of free-standing diamond film.The effects of Cr interlayer on Mo substrate,namely composite substrate,on thermal stress were investigated.Thermo-mechanical coupling analysis of the thermal stress was applied by finite element analysis (FEA) using ANSYS code.It was found that the interlayer could be destroyed first by the large thermal stress,and then the stress could be released and the probability of diamond film crack initiation would be reduced.The stress concentration at the bent edge of diamond film was also discussed.In addition,diamond films deposited on Mo substrates with and without Cr interlayer were prepared by DC arc plasma jet CVD system and experimental measurements were used to characterize these films.It was found that composite substrate could be an effective method of growing free-standing crack-free diamond films by DC arc plasma jet CVD system when there is no special requirement to the film strength.展开更多
Electrophoretic deposition in conjunction with electrochemical reduction was used to make flexible free-standing graphene-like films. Firstly, graphene oxide (GO) film was deposited on graphite substrate by electrop...Electrophoretic deposition in conjunction with electrochemical reduction was used to make flexible free-standing graphene-like films. Firstly, graphene oxide (GO) film was deposited on graphite substrate by electrophoretic deposition method, and then reduced by subsequent electrochemical reduction of GO to obtain reduced GO (ERGO) film with high electrochemical performance. The morphology, structure and electrochemical performance of the prepared graphene-like film were confirmed by SEM, XRD and FT-IR. These unique materials were found to provide high specific capacitance and good cycling stability. The high specific capacitance of 254 F/g was obtained from cyclic voltammetry measurement at a scan rate of 10 mV/s. When the current density increased to 83.3 A/g, the specific capacitance values still remained 132 F/g. Meanwhile, the high powder density of 39.1 kW/kg was measured at energy density of 11.8 W-h/kg in 1 mol/L H2SO4 solution. Furthermore, at a constant scan rate of 50 mV/s, 97.02% of its capacitance was retained for 1000 cycles. These promising results were attributed to the unique assembly structure of graphene film and low contact resistance, which indicated their potential application to electrochemical capacitors.展开更多
The structure characteristic and electric performance of ZnO film deposited on nucleation side of free-standing diamond substrates under different heating temperatures (Th) of substrate and working pressures (p) were ...The structure characteristic and electric performance of ZnO film deposited on nucleation side of free-standing diamond substrates under different heating temperatures (Th) of substrate and working pressures (p) were studied. The structure of the ZnO films tested by X-ray diffraction shows that ZnO film of high c-axis orientation is deposited on the nucleation side of free-standing diamond substrate which is extremely smooth when Th=250 ℃ and p=0.4 Pa. After annealing at 480 ℃ in N2 atmosphere, the SEM and the AFM analyses demonstrate that the c-axis orientation of ZnO film is obviously enhanced. The resistivity of ZnO films also increases up to 8×105 ■·cm which is observed by I?V test.展开更多
Flexible electronic devices have attracted much attention due to their practical and commercial value. Integration of thin films with soft substrate is an effective way to fabricate flexible electronic devices. Ga_2O_...Flexible electronic devices have attracted much attention due to their practical and commercial value. Integration of thin films with soft substrate is an effective way to fabricate flexible electronic devices. Ga_2O_3 thin films deposited directly on soft substrates would be amorphous mostly. However, the thickness of the thin film obtained by mechanical exfoliation method is difficult to control and the edge of the film is fragile and easy to be damaged. In this work, we fabricated free-standing Ga_2O_3 thin films using the water-soluble perovskite Sr_3Al_2O_6 as a sacrificial buffer layer. The obtained Ga_2O_3 thin films were polycrystalline. The thickness and dimension of the films were controllable. A flexible Ga_2O_3solar-blind UV photodetector was fabricated by transferring the free-standing Ga_2O_3 film on a flexible polyethylene terephthalate substrate. The results displayed that the photoelectric performances of the flexible Ga_2O_3 photodetector were not sensitive to bending of the device. The free-standing Ga_2O_3 thin films synthesized through the method described here can be transferred to any substrates or integrated with other thin films to fabricate electronic devices.展开更多
A free-standing diamond film with millimeter thickness prepared by DC arc plasma jet was thinned successively by mechanical grinding. The orientation and quality of the diamond films with different thicknesses were ch...A free-standing diamond film with millimeter thickness prepared by DC arc plasma jet was thinned successively by mechanical grinding. The orientation and quality of the diamond films with different thicknesses were characterized by X-ray diffraction and Raman spectroscopy, respectively. The results show a random grain-orientatinn distribution during the initial growth stage. As the film thickness increases, the preferred orientation of the diamond film changes from (111) to (220), due to the competitive growth mechanism. Twinning generated during the nucleation stage appears to stabilize the preferential growth along the 〈110〉 direction. The interplanar spacing of the (220) plane is enlarged as the film thickness increases, which is caused by the increase of non-diamond-phase carbon and impurities under the cyclic gas. In addition, the quality of the diamond film is barely degraded during the growth process. Furthermore, the peak shift demonstrates a significant inhomogeneity of stress along the film growth direction, which results from competitive growth.展开更多
An insulate to metal transition was investigated based on the measurements of the dependence of the conductivity, activation energy on the protonation state of polyaniline (PANI). An isotropy in conductivity for stret...An insulate to metal transition was investigated based on the measurements of the dependence of the conductivity, activation energy on the protonation state of polyaniline (PANI). An isotropy in conductivity for stretched salt form of PANI was observed.For salt film of PANI, the Ⅰ-Ⅴ curve obeys Ohm's law, which shows a typical metal behavior, however, for base film or film with low protonation state, it can be explained by Space Charge Limited Current (SCLC). It is also found that the Ⅰ-Ⅴ curve of base film of PANI is independent of the work function of electrodes and the polymerization temperature.展开更多
The effect of silicon doping on the residual stress of CVD diamond films is examined using both X-ray diffraction (XRD) analysis and Raman spectroscopy measurements. The examined Si-doped diamond films are deposited o...The effect of silicon doping on the residual stress of CVD diamond films is examined using both X-ray diffraction (XRD) analysis and Raman spectroscopy measurements. The examined Si-doped diamond films are deposited on WC-Co substrates in a home-made bias-enhanced HFCVD apparatus. Ethyl silicate (Si(OC2H5)4) is dissolved in acetone to obtain various Si/C mole ratio ranging from 0.1% to 1.4% in the reaction gas. Characterizations with SEM and XRD indicate increasing silicon concentration may result in grain size decreasing and diamond [110] texture becoming dominant. The residual stress values of as-deposited Si-doped diamond films are evaluated by both sin2ψ method, which measures the (220) diamond Bragg diffraction peaks using XRD, with ψ-values ranging from 0° to 45°, and Raman spectroscopy, which detects the diamond Raman peak shift from the natural diamond line at 1332 cm-1. The residual stress evolution on the silicon doping level estimated from the above two methods presents rather good agreements, exhibiting that all deposited Si-doped diamond films present compressive stress and the sample with Si/C mole ratio of 0.1% possesses the largest residual stress of ~1.75 GPa (Raman) or ~2.3 GPa (XRD). As the silicon doping level is up further, the residual stress reduces to a relative stable value around 1.3 GPa.展开更多
The characteristics of hot filament chemical vapor deposition(HFCVD) diamond films are significantly influenced by the deposition parameters, such as the substrate temperature, total pressure and carbon concentratio...The characteristics of hot filament chemical vapor deposition(HFCVD) diamond films are significantly influenced by the deposition parameters, such as the substrate temperature, total pressure and carbon concentration. Orthogonal experiments were introduced to study the comprehensive effects of such three parameters on diamond films deposited on WC-Co substrates. Field emission scanning electron microscopy, atomic force microscopy and Raman spectrum were employed to analyze the morphology, growth rate and composition of as-deposited diamond films. The morphology varies from pyramidal to cluster features with temperature decreasing. It is found that the low total pressure is suitable for nano-crystalline diamond films growth. Moreover, the substrate temperature and total pressure have combined influence on the growth rate of the diamond films.展开更多
A Ni layer with a thickness of about 100 nm was sputtered on Cu substrates,followed by an ultrasonic seeding with nanodiamond suspension.High-quality diamond film with its crystalline grains close to thermal equilibri...A Ni layer with a thickness of about 100 nm was sputtered on Cu substrates,followed by an ultrasonic seeding with nanodiamond suspension.High-quality diamond film with its crystalline grains close to thermal equilibrium shape was deposited on Cu substrates by hot-filament chemical vapor deposition(HF-CVD),and the sp2 carbon content was less than 5.56%.The nucleation and growth of diamond film were investigated by micro-Raman spectroscopy,scanning electron microscopy,and X-ray diffraction.The results show that the nucleation density of diamond on the Ni-modified Cu substrates is 10 times higher than that on blank Cu substrates.The enhancement mechanism of the nucleation kinetics by Ni modification layer results from two effects:namely,the nanometer rough Ni-modified surface shows an improved absorption of nanodiamond particles that act as starting points for the diamond nucleation during HF-CVD process;the strong catalytic effect of the Ni-modified surface causes the formation of graphite layer that acts as an intermediate to facilitate diamond nucleation quickly.展开更多
Deposition parameters that have great influences on hot filament chemical vapor deposition (HFCVD) diamond films growth on inner hole surfaces of WC?Co substrates mainly include the substrate temperature (t), carbon c...Deposition parameters that have great influences on hot filament chemical vapor deposition (HFCVD) diamond films growth on inner hole surfaces of WC?Co substrates mainly include the substrate temperature (t), carbon content (φ), total pressure (p) and total mass flow (F). Taguchi method was used for the experimental design in order to study the combined effects of the four parameters on the properties of as-deposited diamond films. A new figure-of-merit (FOM) was defined to assess their comprehensive performance. It is clarified thatt,φandp all have significant and complicated effects on the performance of the diamond film and the FOM, which also present some differences as compared with the previous studies on CVD diamond films growth on plane or external surfaces. Aiming to deposit HFCVD diamond films with the best comprehensive performance, the key deposition parameters were finally optimized as:t=830 °C,φ=4.5%,p=4000 Pa,F=800 mL/min.展开更多
A specific revised HFCVD apparatus and a novel process combining HFCVD and polishing technique were presented to deposit the micro-and nano-crystalline multilayered ultra-smooth diamond(USCD) film on the interior-ho...A specific revised HFCVD apparatus and a novel process combining HFCVD and polishing technique were presented to deposit the micro-and nano-crystalline multilayered ultra-smooth diamond(USCD) film on the interior-hole surface of WC-Co drawing dies with aperture ranging from d1.0 mm to 60 mm.Characterization results indicate that the surface roughness values(Ra) in the entry zone,drawing zone and bearing zone of as-fabricated USCD coated drawing die were measured as low as 25.7,23.3 and 25.5 nm,respectively.Furthermore,the friction properties of USCD films were examined in both dry sliding and water-lubricating conditions,and the results show that the USCD film presents much superior friction properties.Its friction coefficients against ball-bearing steel,copper and silicon nitride balls(d4 mm),is always lower than that of microcrystalline diamond(MCD) or WC-Co sample,regardless of the lubricating condition.Meanwhile,it still presents competitive wear resistance with the MCD films.Finally,the working lifetime and performance of as-fabricated USCD coated drawing dies were examined under producing low-carbon steel pipes in dry-sliding and water-lubricating conditions.Under the water-lubricating drawing condition,its production significantly increases by about 20 times compared with the conventional WC-Co drawing dies.展开更多
Large area diamond films were fabricated on copper substrates by a multi-step process comprised of electroplating Cu-diamond composite layer on Cu substrate, plating a Cu layer to fix the protruding diamond particles,...Large area diamond films were fabricated on copper substrates by a multi-step process comprised of electroplating Cu-diamond composite layer on Cu substrate, plating a Cu layer to fix the protruding diamond particles, and depositing continuous diamond film on composite interlayer by hot-filament chemical vapor deposition (HFCVD). The interface characteristics, internal stress and adhesion strength were investigated by scanning electron microscopy, Raman analysis and indentation test. The results show that the continuous film without cracks is successfully obtained. The microstructure of the film is a mixture of large cubo-octahedron grains grown from homo-epitaxial growth and small grains with (111) apparent facets grown from lateral second nuclei. The improved adhesion between diamond film and substrate results from the deep anchoring of the diamond particles in the Cu matrix and the low residual stress in the film.展开更多
Polycrystalline diamond thin films are deposited on an n-type Si substrates by hot filament chemical vapor deposition,and then are implanted with boron ions in a 200keV ion implanter.In order to achieve a better distr...Polycrystalline diamond thin films are deposited on an n-type Si substrates by hot filament chemical vapor deposition,and then are implanted with boron ions in a 200keV ion implanter.In order to achieve a better distribution of the implanted element,boron ions are implanted by two steps:implanting boron ions with the energy of 70keV first,and then with the energy of 100keV.The homogeneous distribution of the B ion is gained.The current-voltage characteristics of the samples are studied.It is found that the p-n heterojunction effect is achieved in these samples.展开更多
文摘Free-standing diamond films have been successfully deposited on stainless steel substrates using microwave plasma-assisted chemical vapor deposition. Although iron, which is the main element of stainless steel, is known to inhibit the nucleation of diamond and enhance the formation of graphite, we were able to grow relatively thick films (-1.2 mm). The films were easily detachable from the substrates. The poor adhesion made it possible to obtain free-standing diamond films without chemical etching. Raman spectroscopy showed the 1332 cm^-1 characteristic Raman peak of diamond and the 1580 cm^-1, 1350 cm^-1 bands of graphite on the growth surface and backside of the films, respectively. By energy dispersive X-ray spectroscopy it was only possible to detect iron on the back of the films, but not on the surface. The role of iron in the film growth is discussed.
基金financially supported by the Graduate Student Foundation of University of Science and Technology BeijingNational Natural Science Foundation of China
文摘Free-standing diamond films, deposited using DC Arc Plasma Jet CVD method onto graphite substrates with titanium interlayers, have been investigated. The Ti interlayers were deposited by arc ion plating equipments. The thickness, morphology and composite phase of Ti interlayers were examined by scanning electron microscopy (SEM) and X-ray diffraction (XRD). The titanium carbide (TiC) was detected in both sides of the interlayers, which played an important role with respect to reasonable adhesion with film and diamond nucleation. The semi-translucent diamond films were characterized by SEM and Raman spectrum. The sharp diamond peak with low intensity of amorphous carbon shows that diamond films have very high quality. The overall results suggest that plating Ti interlayer on graphite substrate is an effective way to obtain optical grade free-standing diamond films.
基金Projects(60577040) supported by the National Natural Science Foundation of China Project(0404) supported by the Shanghai Foundation of Applied Materials Research and Development+1 种基金 Projects(0452nm051, 05nm05046) supported by the Nano-technology Project of Shanghai Project(T0101) supported by the Shanghai Leading Academic Disciplines
文摘Free-standing diamond films were prepared by hot filament chemical vapor deposition (HFCVD) method under different conditions. Inter-digital transducers (IDTs) were formed on the nucleation sides of free-standing diamond films by photolithography technique. Then piezoelectric ZnO films were deposited by radio-frequency(RF) reactive magnetron sputtering to obtain the ZnO/diamond film structures. Surface morphologies of the nucleation sides and the IDTs were characterized by means of scanning electron microscopy (SEM), atomic force microscope (AFM) and optical microscopy. The results indicate that the surfaces of nucleation sides are very smooth and the IDTs are of high quality without discontinuity and short circuit phenomenon. Raman spectra show the sharp diamond feature peak at about 1 334 cm?1 and the small amount of non-diamond carbon in the nucleation side. X-ray diffraction (XRD) patterns of the structure of ZnO/diamond films show a strong diffraction peak of ZnO (002), which indicates that as-sputtered ZnO films are highly c-axis oriented.
基金supported by the National Key Research and Development Program(No.2019YFE03100200)the State Key Lab for Advanced Metals and Materials,the Fund of National Key Laboratory of Solid-State Microwave Devices and Circuits,the National Natural Science Foundation of China(No.52102034)the Or-ganized Research Fund of North China University of Tech-nology(No.2023YZZKY12).The authors are very grateful for the financial support of these institutions.
文摘This study focused on the investigation of the edge effect of diamond films deposited by microwave plasma chemical vapor de-position.Substrate bulge height△h is a factor that affects the edge effect,and it was used to simulate plasma and guide the diamond-film deposition experiments.Finite-element software COMSOL Multiphysics was used to construct a multiphysics(electromagnetic,plasma,and fluid heat transfer fields)coupling model based on electron collision reaction.Raman spectroscopy and scanning electron microscopy were performed to characterize the experimental growth and validate the model.The simulation results reflected the experimental trends observed.Plasma discharge at the edge of the substrate accelerated due to the increase in△h(△h=0-3 mm),and the values of electron density(n_(c)),molar concentration of H(C_(H)),and molar concentration of CH_(3)(C_(CH_(3)))doubled at the edge(for the special concave sample with△h=−1 mm,the active chemical groups exhibited a decreased molar concentration at the edge of the substrate).At=0-3 mm,a high diamond growth rate and a large diamond grain size were observed at the edge of the substrate,and their values increased with.The uniformity of film thickness decreased with.The Raman spectra of all samples revealed the first-order characteristic peak of dia-mond near 1332 cm^(−1).When△h=−1 mm,tensile stress occurred in all regions of the film.When△h=1-3 mm,all areas in the film ex-hibited compressive stress.
基金National Natural Science Foundation of China (Nos.60577040,60877017)Program for Changjiang Scholars,Innovative Research Team in University of China (No.IRT0739)+1 种基金Innovation Program of Shanghai Municipal Education Commission of China (08YZ04)Shanghai Leading Academic Disciplines of China (S30107)
文摘Highly c-axis-oriented ZnO films were deposited successfully on the nucleation sides of free-standing diamond (FD) films by the direct current (DC) magnetron sputtering method. The effect of the sputtering parameters, such as power, gas pressure and sputtering plasma composition of Ar-to-O2, on the properties of ZnO thin films was investigated in detail. X-ray diffraction (XRD) measurements showed that, at a sputtering power of 200 W, gas pressure of 0.5 Pa and an Ar-to- O2 composition of 1:1, a higher intensity of the (002) diffraction peak and a narrower full width at half maximum (FWHM) were detected which meant high c-axis orientation and high quality of the ZnO films. To improve the quality of the ZnO film, a thin ZnO layer was pre-grown as a homo-buffer layer. XRD measurements showed that this buffer layer had a beneficial effect on the structural and morphological properties of the post-grown ZnO film.
基金the National Natural Science Foundation of China,and the Natural Science Foundation of He'nan province.
文摘Blue-green electroluminescence has been observed in free-standing diamond films which were deposited by microwave plasma assisted CVD on silicon substrates.The electroluminescence device is driven by a 60 Hz power supply.The threshold voltage was about 112 V peak-to-peak.The electroluminescence spectrum at room temperature,showed a blue-green band with the peak centered at 485nm suggesting band A type emission.Electroluminescence was also observed at 77K.
基金Science and technology plan project of Hebei Academy of Sciences(No.191408)Natural Science Foundation of Hebei Province(E2019302005)
文摘Recently,with the rapid development of chemical vapor deposition(CVD)technology,large area free-standing CVD diamond films have been produced successfully.However,the coarse grain size on the surface and the non-uniform thickness of unprocessed CVD diamond films make it difficult to meet the application requirement.The current study evaluates several existing polishing methods for CVD diamond films,including mechanical polishing,chemical mechanical polishing and tribochemical polishing technology.
基金supported by the National Natural Science Foundation of China (Grant No. 50471090)
文摘Thermal stress in large area free-standing diamond films was remarkable during the post-deposition cooling of direct current (DC) arc plasma jet chemical vapor deposition (CVD) process.In this research,the stress release caused by delamination of Cr interlayer was of great importance to ensure the integrity of free-standing diamond film.The effects of Cr interlayer on Mo substrate,namely composite substrate,on thermal stress were investigated.Thermo-mechanical coupling analysis of the thermal stress was applied by finite element analysis (FEA) using ANSYS code.It was found that the interlayer could be destroyed first by the large thermal stress,and then the stress could be released and the probability of diamond film crack initiation would be reduced.The stress concentration at the bent edge of diamond film was also discussed.In addition,diamond films deposited on Mo substrates with and without Cr interlayer were prepared by DC arc plasma jet CVD system and experimental measurements were used to characterize these films.It was found that composite substrate could be an effective method of growing free-standing crack-free diamond films by DC arc plasma jet CVD system when there is no special requirement to the film strength.
基金Projects(21361020,21061012)supported by the National Natural Science Foundation of ChinaProject(NZ12156)supported by the Natural Science Foundation of Ningxia,ChinaProject(N-09-13)supported by Project of State Key Laboratory of Catalysis,Dalian Institute of Chemical Physics of the Chinese Academy of Sciences
文摘Electrophoretic deposition in conjunction with electrochemical reduction was used to make flexible free-standing graphene-like films. Firstly, graphene oxide (GO) film was deposited on graphite substrate by electrophoretic deposition method, and then reduced by subsequent electrochemical reduction of GO to obtain reduced GO (ERGO) film with high electrochemical performance. The morphology, structure and electrochemical performance of the prepared graphene-like film were confirmed by SEM, XRD and FT-IR. These unique materials were found to provide high specific capacitance and good cycling stability. The high specific capacitance of 254 F/g was obtained from cyclic voltammetry measurement at a scan rate of 10 mV/s. When the current density increased to 83.3 A/g, the specific capacitance values still remained 132 F/g. Meanwhile, the high powder density of 39.1 kW/kg was measured at energy density of 11.8 W-h/kg in 1 mol/L H2SO4 solution. Furthermore, at a constant scan rate of 50 mV/s, 97.02% of its capacitance was retained for 1000 cycles. These promising results were attributed to the unique assembly structure of graphene film and low contact resistance, which indicated their potential application to electrochemical capacitors.
基金Project (60577040) supported by the National Natural Science Foundation of China Project (0404) supported by the Shanghai Foundation of Applied Materials Research and Development+1 种基金 Projects(0452nm051, 05nm05046) supported by the Nano-technology Project of Shanghai Project (T0101) supported by the Shanghai Leading Academic Disciplines
文摘The structure characteristic and electric performance of ZnO film deposited on nucleation side of free-standing diamond substrates under different heating temperatures (Th) of substrate and working pressures (p) were studied. The structure of the ZnO films tested by X-ray diffraction shows that ZnO film of high c-axis orientation is deposited on the nucleation side of free-standing diamond substrate which is extremely smooth when Th=250 ℃ and p=0.4 Pa. After annealing at 480 ℃ in N2 atmosphere, the SEM and the AFM analyses demonstrate that the c-axis orientation of ZnO film is obviously enhanced. The resistivity of ZnO films also increases up to 8×105 ■·cm which is observed by I?V test.
基金Project supported by the National Natural Science Foundation of China(Grant Nos.51572033,51572241,61774019,61704153,and 11404029)the Fund of State Key Laboratory of IPOC(BUPT)+1 种基金the Open Fund of IPOC(BUPT)Beijing Municipal Commission of Science and Technology,China(Grant No.SX2018-04)
文摘Flexible electronic devices have attracted much attention due to their practical and commercial value. Integration of thin films with soft substrate is an effective way to fabricate flexible electronic devices. Ga_2O_3 thin films deposited directly on soft substrates would be amorphous mostly. However, the thickness of the thin film obtained by mechanical exfoliation method is difficult to control and the edge of the film is fragile and easy to be damaged. In this work, we fabricated free-standing Ga_2O_3 thin films using the water-soluble perovskite Sr_3Al_2O_6 as a sacrificial buffer layer. The obtained Ga_2O_3 thin films were polycrystalline. The thickness and dimension of the films were controllable. A flexible Ga_2O_3solar-blind UV photodetector was fabricated by transferring the free-standing Ga_2O_3 film on a flexible polyethylene terephthalate substrate. The results displayed that the photoelectric performances of the flexible Ga_2O_3 photodetector were not sensitive to bending of the device. The free-standing Ga_2O_3 thin films synthesized through the method described here can be transferred to any substrates or integrated with other thin films to fabricate electronic devices.
基金financially supported by the National Natural Science Foundation of China (No. 51272024)the Ph.D. Programs Foundation of the Ministry of Education of China (No. 20110006110011)the Fundamental Research Funds for Central Universities of China (No. FRF-TP-13-035A)
文摘A free-standing diamond film with millimeter thickness prepared by DC arc plasma jet was thinned successively by mechanical grinding. The orientation and quality of the diamond films with different thicknesses were characterized by X-ray diffraction and Raman spectroscopy, respectively. The results show a random grain-orientatinn distribution during the initial growth stage. As the film thickness increases, the preferred orientation of the diamond film changes from (111) to (220), due to the competitive growth mechanism. Twinning generated during the nucleation stage appears to stabilize the preferential growth along the 〈110〉 direction. The interplanar spacing of the (220) plane is enlarged as the film thickness increases, which is caused by the increase of non-diamond-phase carbon and impurities under the cyclic gas. In addition, the quality of the diamond film is barely degraded during the growth process. Furthermore, the peak shift demonstrates a significant inhomogeneity of stress along the film growth direction, which results from competitive growth.
文摘An insulate to metal transition was investigated based on the measurements of the dependence of the conductivity, activation energy on the protonation state of polyaniline (PANI). An isotropy in conductivity for stretched salt form of PANI was observed.For salt film of PANI, the Ⅰ-Ⅴ curve obeys Ohm's law, which shows a typical metal behavior, however, for base film or film with low protonation state, it can be explained by Space Charge Limited Current (SCLC). It is also found that the Ⅰ-Ⅴ curve of base film of PANI is independent of the work function of electrodes and the polymerization temperature.
基金Project (51005154) supported by the National Natural Science Foundation of ChinaProject (12CG11) supported by the Chenguang Program of Shanghai Municipal Education Commission, ChinaProject (201104271) supported by the China Postdoctoral Science Foundation
文摘The effect of silicon doping on the residual stress of CVD diamond films is examined using both X-ray diffraction (XRD) analysis and Raman spectroscopy measurements. The examined Si-doped diamond films are deposited on WC-Co substrates in a home-made bias-enhanced HFCVD apparatus. Ethyl silicate (Si(OC2H5)4) is dissolved in acetone to obtain various Si/C mole ratio ranging from 0.1% to 1.4% in the reaction gas. Characterizations with SEM and XRD indicate increasing silicon concentration may result in grain size decreasing and diamond [110] texture becoming dominant. The residual stress values of as-deposited Si-doped diamond films are evaluated by both sin2ψ method, which measures the (220) diamond Bragg diffraction peaks using XRD, with ψ-values ranging from 0° to 45°, and Raman spectroscopy, which detects the diamond Raman peak shift from the natural diamond line at 1332 cm-1. The residual stress evolution on the silicon doping level estimated from the above two methods presents rather good agreements, exhibiting that all deposited Si-doped diamond films present compressive stress and the sample with Si/C mole ratio of 0.1% possesses the largest residual stress of ~1.75 GPa (Raman) or ~2.3 GPa (XRD). As the silicon doping level is up further, the residual stress reduces to a relative stable value around 1.3 GPa.
基金Project(2012ZX04003-031)supported by the National Science and Technology Major Project,China
文摘The characteristics of hot filament chemical vapor deposition(HFCVD) diamond films are significantly influenced by the deposition parameters, such as the substrate temperature, total pressure and carbon concentration. Orthogonal experiments were introduced to study the comprehensive effects of such three parameters on diamond films deposited on WC-Co substrates. Field emission scanning electron microscopy, atomic force microscopy and Raman spectrum were employed to analyze the morphology, growth rate and composition of as-deposited diamond films. The morphology varies from pyramidal to cluster features with temperature decreasing. It is found that the low total pressure is suitable for nano-crystalline diamond films growth. Moreover, the substrate temperature and total pressure have combined influence on the growth rate of the diamond films.
基金Project(20110933K) supported by the State Key Laboratory of Powder Metallurgy,ChinaProject(2012QNZT002) supported by the Freedom Explore Program of Central South University,ChinaProject(CSUZC2012024) supported by the Open-End Fund for the Valuable and Precision Instruments of Central South University,China
文摘A Ni layer with a thickness of about 100 nm was sputtered on Cu substrates,followed by an ultrasonic seeding with nanodiamond suspension.High-quality diamond film with its crystalline grains close to thermal equilibrium shape was deposited on Cu substrates by hot-filament chemical vapor deposition(HF-CVD),and the sp2 carbon content was less than 5.56%.The nucleation and growth of diamond film were investigated by micro-Raman spectroscopy,scanning electron microscopy,and X-ray diffraction.The results show that the nucleation density of diamond on the Ni-modified Cu substrates is 10 times higher than that on blank Cu substrates.The enhancement mechanism of the nucleation kinetics by Ni modification layer results from two effects:namely,the nanometer rough Ni-modified surface shows an improved absorption of nanodiamond particles that act as starting points for the diamond nucleation during HF-CVD process;the strong catalytic effect of the Ni-modified surface causes the formation of graphite layer that acts as an intermediate to facilitate diamond nucleation quickly.
基金Projects(51275302,51005154)supported by the National Natural Science Foundation of China
文摘Deposition parameters that have great influences on hot filament chemical vapor deposition (HFCVD) diamond films growth on inner hole surfaces of WC?Co substrates mainly include the substrate temperature (t), carbon content (φ), total pressure (p) and total mass flow (F). Taguchi method was used for the experimental design in order to study the combined effects of the four parameters on the properties of as-deposited diamond films. A new figure-of-merit (FOM) was defined to assess their comprehensive performance. It is clarified thatt,φandp all have significant and complicated effects on the performance of the diamond film and the FOM, which also present some differences as compared with the previous studies on CVD diamond films growth on plane or external surfaces. Aiming to deposit HFCVD diamond films with the best comprehensive performance, the key deposition parameters were finally optimized as:t=830 °C,φ=4.5%,p=4000 Pa,F=800 mL/min.
基金Project(51005154) supported by the National Natural Science Foundation of ChinaProject(12CG11) supported by the Chenguang Program of Shanghai Municipal Education Commission,ChinaProject(201104271) supported by the China Postdoctoral Science Foundation Special Funded Project
文摘A specific revised HFCVD apparatus and a novel process combining HFCVD and polishing technique were presented to deposit the micro-and nano-crystalline multilayered ultra-smooth diamond(USCD) film on the interior-hole surface of WC-Co drawing dies with aperture ranging from d1.0 mm to 60 mm.Characterization results indicate that the surface roughness values(Ra) in the entry zone,drawing zone and bearing zone of as-fabricated USCD coated drawing die were measured as low as 25.7,23.3 and 25.5 nm,respectively.Furthermore,the friction properties of USCD films were examined in both dry sliding and water-lubricating conditions,and the results show that the USCD film presents much superior friction properties.Its friction coefficients against ball-bearing steel,copper and silicon nitride balls(d4 mm),is always lower than that of microcrystalline diamond(MCD) or WC-Co sample,regardless of the lubricating condition.Meanwhile,it still presents competitive wear resistance with the MCD films.Finally,the working lifetime and performance of as-fabricated USCD coated drawing dies were examined under producing low-carbon steel pipes in dry-sliding and water-lubricating conditions.Under the water-lubricating drawing condition,its production significantly increases by about 20 times compared with the conventional WC-Co drawing dies.
基金Projects(51071070,51271079)supported by the National Natural Science Foundation of ChinaProject(NCET-11-0156)supported by New Century Excellent Talents in University,China
文摘Large area diamond films were fabricated on copper substrates by a multi-step process comprised of electroplating Cu-diamond composite layer on Cu substrate, plating a Cu layer to fix the protruding diamond particles, and depositing continuous diamond film on composite interlayer by hot-filament chemical vapor deposition (HFCVD). The interface characteristics, internal stress and adhesion strength were investigated by scanning electron microscopy, Raman analysis and indentation test. The results show that the continuous film without cracks is successfully obtained. The microstructure of the film is a mixture of large cubo-octahedron grains grown from homo-epitaxial growth and small grains with (111) apparent facets grown from lateral second nuclei. The improved adhesion between diamond film and substrate results from the deep anchoring of the diamond particles in the Cu matrix and the low residual stress in the film.
文摘Polycrystalline diamond thin films are deposited on an n-type Si substrates by hot filament chemical vapor deposition,and then are implanted with boron ions in a 200keV ion implanter.In order to achieve a better distribution of the implanted element,boron ions are implanted by two steps:implanting boron ions with the energy of 70keV first,and then with the energy of 100keV.The homogeneous distribution of the B ion is gained.The current-voltage characteristics of the samples are studied.It is found that the p-n heterojunction effect is achieved in these samples.