The friction behavior of the hot filament chemical vapor deposition(HFCVD) diamond film plays a critical role on its applications in mechanical fields and largely depends on the environment. Studies on the tribologi...The friction behavior of the hot filament chemical vapor deposition(HFCVD) diamond film plays a critical role on its applications in mechanical fields and largely depends on the environment. Studies on the tribological properties of HFCVD diamond films coated on Co-cemented tungsten carbide (WC-Co) substrates are rarely reported in available literatures, especially in the water lubricating conditions. In this paper, conventional microcrystalline diamond(MCD) and fine-grained diamond(FGD) films are deposited on WC-Co substrates and their friction properties are evaluated on a reciprocating ball-on-plate tribometer, where they are brought to slide against ball-bearing steel and copper balls in dry and water lubricating conditions. Scanning electron microscopy(SEM), atomic force microscopy(AFM), surface profilometer and Raman spectroscopy are adopted to characterize as-deposited diamond films; SEM and energy dispersive X-ray(EDX) are used to investigate the worn region on the surfaces of both counterface balls and diamond films. The research results show that the friction coefficient of HFCVD diamond films always starts with a high initial value, and then gradually transits to a relative stable state. For a given counterface and a sliding condition, the FGD film presents lower stable friction coefficients by 0.02-0.03 than MCD film. The transferred materials adhered on sliding interface are supposed to have predominate effect on the friction behaviors of HFCVD diamond films. Furthermore, the effect of water lubricating on reducing friction coefficient is significant. For a given counterpart, the stable friction coefficients of MCD or FGD films reduce by about 0.07-0.08 while sliding in the water lubricating condition, relative to in dry sliding condition. This study is beneficial for widespread applications of HFCVD diamond coated mechanical components and adopting water lubricating system, replacing ofoil lubricating, in a variety of mechanical processing fields to implement the green production process.展开更多
Atomic-layer MoS_2 ultrathin films are synthesized using a hot filament chemical vapor deposition method. A combination of atomic force microscopy(AFM), x-ray diffraction(XRD), high-resolution transition electron ...Atomic-layer MoS_2 ultrathin films are synthesized using a hot filament chemical vapor deposition method. A combination of atomic force microscopy(AFM), x-ray diffraction(XRD), high-resolution transition electron microscopy(HRTEM), photoluminescence(PL), and x-ray photoelectron spectroscopy(XPS) characterization methods is applied to investigate the crystal structures, valence states, and compositions of the ultrathin film areas. The nucleation particles show irregular morphology, while for a larger size somewhere, the films are granular and the grains have a triangle shape. The films grow in a preferred orientation(002). The HRTEM images present the graphene-like structure of stacked layers with low density of stacking fault, and the interlayer distance of plane is measured to be about 0.63 nm. It shows a clear quasihoneycomb-like structure and 6-fold coordination symmetry. Room-temperature PL spectra for the atomic layer MoS_2 under the condition of right and left circular light show that for both cases, the A1 and B1 direct excitonic transitions can be observed. In the meantime, valley polarization resolved PL spectra are obtained. XPS measurements provide high-purity samples aside from some contaminations from the air, and confirm the presence of pure MoS_2. The stoichiometric mole ratio of S/Mo is about 2.0–2.1, suggesting that sulfur is abundant rather than deficient in the atomic layer MoS_2 under our experimental conditions.展开更多
The <100> textured growth of diamond film on HF eroded silicon wafer has been studied by HFCVD. The evolution of grain size and sudece morphology vs deposition time is presented and the <100> textured thic...The <100> textured growth of diamond film on HF eroded silicon wafer has been studied by HFCVD. The evolution of grain size and sudece morphology vs deposition time is presented and the <100> textured thick diamond film (80μm) with smooth surface, desirable for practical application in many fields is obtained展开更多
In this study, the temperature and gas velocity distributions in hot filament chemical vapor deposition(HFCVD) diamond film growth on the end surfaces of seals are simulated by the finite volume method. The influence ...In this study, the temperature and gas velocity distributions in hot filament chemical vapor deposition(HFCVD) diamond film growth on the end surfaces of seals are simulated by the finite volume method. The influence of filament diameter, filament separation and rotational speed of the substrates is considered. Firstly,the simulation model is established by simplifying operating conditions to simulate the temperature and gas velocity distributions. Thereafter, the deposition parameters are optimized as 0.6 mm filament diameter, 18 mm filament separation and 5 r/min rotational speed to get the uniform temperature distribution. Under the influence of the rotational speed, the difference between temperature gradients along the directions perpendicular to the filament and parallel to the filament becomes narrow, it is consistent with the actual condition, and the maximum temperature difference on the substrates decreases to 7.4?C. Furthermore, the effect of the rotational speed on the gas velocity distribution is studied. Finally, diamond films are deposited on the end surfaces of Si C seals with the optimized deposition parameters. The characterizations by scanning electron microscopy(SEM) and Raman spectroscopy exhibit a layer of homogeneous diamond films with fine-faceted crystals and uniform thickness. The results validate the simulation model.展开更多
Boron doped diamond(BDD)performs well in electrochemical oxidation for organic pollutants thanks to its wide electrochemical window and superior chemical stability.We presented a method to obtain well-adherent large-s...Boron doped diamond(BDD)performs well in electrochemical oxidation for organic pollutants thanks to its wide electrochemical window and superior chemical stability.We presented a method to obtain well-adherent large-scale BDD/Nb electrode by the modified hot filament chemical vapor deposition system(HFCVD).SiC particles were sand blasted to enhance the adhesion of BDD coating.The BDD coating was then deposited on both sides of Nb which was placed vertically and closely with filament grids on both sides.The BDD/Nb electrodes had no deformation because the thermal deformations of the BDD films on both sides of the Nb substrate conteracted each other during cooling process after deposition.The surface morphology and purity of the BDD/Nb electrode were analyzed by Raman and scanning elestron microscope(SEM)techniques.Scratch test was used to investigate the adhesion of BDD films.The electrochemical performances were measured by cyclic voltammetry test.The BDD electrode at the B/C ratio of 2 000×10^(-6) held a higher oxygen evolution potential thanks to its high sp3 carbon content.Accelerated life test illustrated that the sandblasting pretreatment obviously enhanced the adhesion of BDD coating which resulted in a longer service duration than the un-sandblasted one.展开更多
基金supported by National Natural Science Foundation of China (Grant No. 50575135)Program for New Century Excellent Talents of Ministry of Education of China (Grant No. NCET-06-0399)Tribology Science Fund of the State Key Laboratory of Tribology, China
文摘The friction behavior of the hot filament chemical vapor deposition(HFCVD) diamond film plays a critical role on its applications in mechanical fields and largely depends on the environment. Studies on the tribological properties of HFCVD diamond films coated on Co-cemented tungsten carbide (WC-Co) substrates are rarely reported in available literatures, especially in the water lubricating conditions. In this paper, conventional microcrystalline diamond(MCD) and fine-grained diamond(FGD) films are deposited on WC-Co substrates and their friction properties are evaluated on a reciprocating ball-on-plate tribometer, where they are brought to slide against ball-bearing steel and copper balls in dry and water lubricating conditions. Scanning electron microscopy(SEM), atomic force microscopy(AFM), surface profilometer and Raman spectroscopy are adopted to characterize as-deposited diamond films; SEM and energy dispersive X-ray(EDX) are used to investigate the worn region on the surfaces of both counterface balls and diamond films. The research results show that the friction coefficient of HFCVD diamond films always starts with a high initial value, and then gradually transits to a relative stable state. For a given counterface and a sliding condition, the FGD film presents lower stable friction coefficients by 0.02-0.03 than MCD film. The transferred materials adhered on sliding interface are supposed to have predominate effect on the friction behaviors of HFCVD diamond films. Furthermore, the effect of water lubricating on reducing friction coefficient is significant. For a given counterpart, the stable friction coefficients of MCD or FGD films reduce by about 0.07-0.08 while sliding in the water lubricating condition, relative to in dry sliding condition. This study is beneficial for widespread applications of HFCVD diamond coated mechanical components and adopting water lubricating system, replacing ofoil lubricating, in a variety of mechanical processing fields to implement the green production process.
基金Project supported by the Natural Science Foundation of Zhejiang Province,China(Grant Nos.LY16F040003 and LY16A040007)the National Natural Science Foundation of China(Grant Nos.51401069 and 11574067)
文摘Atomic-layer MoS_2 ultrathin films are synthesized using a hot filament chemical vapor deposition method. A combination of atomic force microscopy(AFM), x-ray diffraction(XRD), high-resolution transition electron microscopy(HRTEM), photoluminescence(PL), and x-ray photoelectron spectroscopy(XPS) characterization methods is applied to investigate the crystal structures, valence states, and compositions of the ultrathin film areas. The nucleation particles show irregular morphology, while for a larger size somewhere, the films are granular and the grains have a triangle shape. The films grow in a preferred orientation(002). The HRTEM images present the graphene-like structure of stacked layers with low density of stacking fault, and the interlayer distance of plane is measured to be about 0.63 nm. It shows a clear quasihoneycomb-like structure and 6-fold coordination symmetry. Room-temperature PL spectra for the atomic layer MoS_2 under the condition of right and left circular light show that for both cases, the A1 and B1 direct excitonic transitions can be observed. In the meantime, valley polarization resolved PL spectra are obtained. XPS measurements provide high-purity samples aside from some contaminations from the air, and confirm the presence of pure MoS_2. The stoichiometric mole ratio of S/Mo is about 2.0–2.1, suggesting that sulfur is abundant rather than deficient in the atomic layer MoS_2 under our experimental conditions.
文摘The <100> textured growth of diamond film on HF eroded silicon wafer has been studied by HFCVD. The evolution of grain size and sudece morphology vs deposition time is presented and the <100> textured thick diamond film (80μm) with smooth surface, desirable for practical application in many fields is obtained
基金the Important National Science and Technology Specific Projects(No.2012ZX04003-031)
文摘In this study, the temperature and gas velocity distributions in hot filament chemical vapor deposition(HFCVD) diamond film growth on the end surfaces of seals are simulated by the finite volume method. The influence of filament diameter, filament separation and rotational speed of the substrates is considered. Firstly,the simulation model is established by simplifying operating conditions to simulate the temperature and gas velocity distributions. Thereafter, the deposition parameters are optimized as 0.6 mm filament diameter, 18 mm filament separation and 5 r/min rotational speed to get the uniform temperature distribution. Under the influence of the rotational speed, the difference between temperature gradients along the directions perpendicular to the filament and parallel to the filament becomes narrow, it is consistent with the actual condition, and the maximum temperature difference on the substrates decreases to 7.4?C. Furthermore, the effect of the rotational speed on the gas velocity distribution is studied. Finally, diamond films are deposited on the end surfaces of Si C seals with the optimized deposition parameters. The characterizations by scanning electron microscopy(SEM) and Raman spectroscopy exhibit a layer of homogeneous diamond films with fine-faceted crystals and uniform thickness. The results validate the simulation model.
基金supported by the National Natural Science Foundation of China(Nos.51575269,51275232)the Six Talent Peaks Project in Jiangsu Province(No.ZBZZ005)the Zhejiang Provincial Key Laboratory for Cutting Tools(No.ZD201305)
文摘Boron doped diamond(BDD)performs well in electrochemical oxidation for organic pollutants thanks to its wide electrochemical window and superior chemical stability.We presented a method to obtain well-adherent large-scale BDD/Nb electrode by the modified hot filament chemical vapor deposition system(HFCVD).SiC particles were sand blasted to enhance the adhesion of BDD coating.The BDD coating was then deposited on both sides of Nb which was placed vertically and closely with filament grids on both sides.The BDD/Nb electrodes had no deformation because the thermal deformations of the BDD films on both sides of the Nb substrate conteracted each other during cooling process after deposition.The surface morphology and purity of the BDD/Nb electrode were analyzed by Raman and scanning elestron microscope(SEM)techniques.Scratch test was used to investigate the adhesion of BDD films.The electrochemical performances were measured by cyclic voltammetry test.The BDD electrode at the B/C ratio of 2 000×10^(-6) held a higher oxygen evolution potential thanks to its high sp3 carbon content.Accelerated life test illustrated that the sandblasting pretreatment obviously enhanced the adhesion of BDD coating which resulted in a longer service duration than the un-sandblasted one.