In areas where hot mix asphalt(HMA)is likely to be exposed by any form of mineral oil the layer has to withstand the attack of these substances in order not to damage the construction.The European Standard EN 12697-43...In areas where hot mix asphalt(HMA)is likely to be exposed by any form of mineral oil the layer has to withstand the attack of these substances in order not to damage the construction.The European Standard EN 12697-43 provides a test procedure to determine the resistance of HMA to fuel.The paper reviews this method thoroughly.A completely revised and simplified test device for the brush test was developed meeting the requirements of the standard and creating results with a high repeatability at the same time.The test conditions given by the standard such as the exposure to fuel,cleaning of the specimen after exposure or the contact pressure of the brush were varied to isolate those test conditions with a substantial influence on the result.The research revealed that in the standard some conditions with a rather small influence are set quite strictly while other conditions with a distinct influence on the result are not defined with the required accuracy to obtain comparable and repeatable results.The paper presents suggestions for the improvement of the test method and the standard itself in respect to the layout of the test device and the definition of important test conditions to enhance the outcome of the EN 12697-43.展开更多
The fatigue behavior, indirect tensile strength (ITS) and resilient modulus test results for warm mix asphalt (WMA) as well as hot mix asphalt (HMA) at different ageing levels were evaluated. Laboratory-prepared...The fatigue behavior, indirect tensile strength (ITS) and resilient modulus test results for warm mix asphalt (WMA) as well as hot mix asphalt (HMA) at different ageing levels were evaluated. Laboratory-prepared samples were aged artificially in the oven to simulate short-term and long term ageing in accordance with AASHTO R30 and then compared with unaged specimens. Beam fatigue testing was performed using beam specimens at 25 ℃ based on AASHTO T321 standard. Fatigue life, bending stiffness and dissipated energy for both unaged and aged mixtures were calculated using four-point beam fatigue test results. Three-point bending tests were performed using semi-circular bend (SCB) specimens at -10 ℃ and the critical mode I stress intensity factor K1 was then calculated using the peak load obtained from the load-displacement curve. It is observed that Sasobit and Rheofalt warm mix asphalt additives have a significant effect on indirect tensile strength, resilient modulus, fatigue behavior and stress intensity factor of aged and unaged mixtures.展开更多
This paper presented the methods of reducing the compaction segregation of asphalt layer by improving the operating characteristics of roller and paver. The fit formula, which expresses the compaction rule of the pavi...This paper presented the methods of reducing the compaction segregation of asphalt layer by improving the operating characteristics of roller and paver. The fit formula, which expresses the compaction rule of the paving layer after passing different rolling passes of the steel wheel roller, was also put forward. The measured results of test road show that when some technical methods are adopted, the compaction segregation can be controlled.展开更多
The quality of compaction is important to the performance of hot mixed asphalt (HMA) pavement. Most premature failures of asphalt pavement are concerned with poor compaction. Compaction characteristic of lIMA mixtur...The quality of compaction is important to the performance of hot mixed asphalt (HMA) pavement. Most premature failures of asphalt pavement are concerned with poor compaction. Compaction characteristic of lIMA mixtures were studied. Compaction tests were done with typical widely used HMA mixtures, including dense gradation asphalt mixtures with different nominal maximum aggregate size (AC13,AC20,AC25), and mixtures with different gradation (AC13, SMA13,Supl3 and OGFC13). HMA mixtures were sampled at different compaction temperature and Marshall blow numbers, varying between 60 and 175 ~C and between 15 and 75 lows, respectively. The compaction characteristics of these mixtures were evaluated. The results showed that the Marshall stability and volumetric properties were significantly affected by the compaction temperature. Mixtures with the same NMAS but different type of gradation need different compaction energy to get the designed density.展开更多
Nano silica due to its spherical shape, tiny size and higher density compared to bitumen, may have an inherent potential to improve hot mix asphalt(HMA) self-healing. In this research scanning electron microscopy(SEM)...Nano silica due to its spherical shape, tiny size and higher density compared to bitumen, may have an inherent potential to improve hot mix asphalt(HMA) self-healing. In this research scanning electron microscopy(SEM) images were used to investigate size, morphology and dispersion of nano silica particles. Additionally, HMA self-healing mechanism was also examined by SEM. Furthermore, dynamic indirect tensile test(IDT) was used to evaluate HMA self-healing index. The SEM results indicated that bitumen mortar flowing into micro cracks may be one of the most important mechanisms of HMA self-healing. The experiment results also showed that modification of bitumen by nano silica promotes the ability of the HMA self-healing.展开更多
The primary goal of this study is the design and construction of semi-flexible pavement(SFP)mixture in accordance with the engineering and mechanical criteria.This study involves the use of a range of gradation curves...The primary goal of this study is the design and construction of semi-flexible pavement(SFP)mixture in accordance with the engineering and mechanical criteria.This study involves the use of a range of gradation curves,air void contents,cellulose and synthesized fibers,and neat and modified asphalt binders to prepare the open-graded asphalt(OGA)mixtures.To analyze the characteristics of these mixtures,a variety of test,namely binder drainage,semi-circular bending(SCB),Cantabro,wheel tracking,indirect tensile strength(ITS),and permeability tests were conducted.Additionally,to analyze the prepared grouting material,flexural strength,compressive strength,and fluidity tests were conducted.In the final stage,SFP was compared to HMA in terms of engineering characteristics and performance.According to the results,SFP was more resistant to skid,rutting,fire,and moisture damage,while HMA had a better performance in fracture tests,including SCB test.According to the results of the mechanical performance tests conducted on OGA mixtures,the highest and lowest values for air void content to achieve the highest mechanical performance level were 30%-35%and 25%,respectively.Also,based on the laboratory results,it was determined that the required void ratio for constructing OGA mixtures was 24%-26%based on the bitumen type and fibers amount in the mixture.Finally,SFP mixture can be regarded as a viable alternative to common pavements thanks to its high resistance to rutting and moisture damage,long freezing-thawing fatigue life,and adequate fire and skid resistance.展开更多
文摘In areas where hot mix asphalt(HMA)is likely to be exposed by any form of mineral oil the layer has to withstand the attack of these substances in order not to damage the construction.The European Standard EN 12697-43 provides a test procedure to determine the resistance of HMA to fuel.The paper reviews this method thoroughly.A completely revised and simplified test device for the brush test was developed meeting the requirements of the standard and creating results with a high repeatability at the same time.The test conditions given by the standard such as the exposure to fuel,cleaning of the specimen after exposure or the contact pressure of the brush were varied to isolate those test conditions with a substantial influence on the result.The research revealed that in the standard some conditions with a rather small influence are set quite strictly while other conditions with a distinct influence on the result are not defined with the required accuracy to obtain comparable and repeatable results.The paper presents suggestions for the improvement of the test method and the standard itself in respect to the layout of the test device and the definition of important test conditions to enhance the outcome of the EN 12697-43.
文摘The fatigue behavior, indirect tensile strength (ITS) and resilient modulus test results for warm mix asphalt (WMA) as well as hot mix asphalt (HMA) at different ageing levels were evaluated. Laboratory-prepared samples were aged artificially in the oven to simulate short-term and long term ageing in accordance with AASHTO R30 and then compared with unaged specimens. Beam fatigue testing was performed using beam specimens at 25 ℃ based on AASHTO T321 standard. Fatigue life, bending stiffness and dissipated energy for both unaged and aged mixtures were calculated using four-point beam fatigue test results. Three-point bending tests were performed using semi-circular bend (SCB) specimens at -10 ℃ and the critical mode I stress intensity factor K1 was then calculated using the peak load obtained from the load-displacement curve. It is observed that Sasobit and Rheofalt warm mix asphalt additives have a significant effect on indirect tensile strength, resilient modulus, fatigue behavior and stress intensity factor of aged and unaged mixtures.
文摘This paper presented the methods of reducing the compaction segregation of asphalt layer by improving the operating characteristics of roller and paver. The fit formula, which expresses the compaction rule of the paving layer after passing different rolling passes of the steel wheel roller, was also put forward. The measured results of test road show that when some technical methods are adopted, the compaction segregation can be controlled.
基金Funded by the National Natural Science Foundation of China(No.51108081)SRF for ROCS,SEM,and Xuzhou Science Bureau(No.1016)
文摘The quality of compaction is important to the performance of hot mixed asphalt (HMA) pavement. Most premature failures of asphalt pavement are concerned with poor compaction. Compaction characteristic of lIMA mixtures were studied. Compaction tests were done with typical widely used HMA mixtures, including dense gradation asphalt mixtures with different nominal maximum aggregate size (AC13,AC20,AC25), and mixtures with different gradation (AC13, SMA13,Supl3 and OGFC13). HMA mixtures were sampled at different compaction temperature and Marshall blow numbers, varying between 60 and 175 ~C and between 15 and 75 lows, respectively. The compaction characteristics of these mixtures were evaluated. The results showed that the Marshall stability and volumetric properties were significantly affected by the compaction temperature. Mixtures with the same NMAS but different type of gradation need different compaction energy to get the designed density.
文摘Nano silica due to its spherical shape, tiny size and higher density compared to bitumen, may have an inherent potential to improve hot mix asphalt(HMA) self-healing. In this research scanning electron microscopy(SEM) images were used to investigate size, morphology and dispersion of nano silica particles. Additionally, HMA self-healing mechanism was also examined by SEM. Furthermore, dynamic indirect tensile test(IDT) was used to evaluate HMA self-healing index. The SEM results indicated that bitumen mortar flowing into micro cracks may be one of the most important mechanisms of HMA self-healing. The experiment results also showed that modification of bitumen by nano silica promotes the ability of the HMA self-healing.
文摘The primary goal of this study is the design and construction of semi-flexible pavement(SFP)mixture in accordance with the engineering and mechanical criteria.This study involves the use of a range of gradation curves,air void contents,cellulose and synthesized fibers,and neat and modified asphalt binders to prepare the open-graded asphalt(OGA)mixtures.To analyze the characteristics of these mixtures,a variety of test,namely binder drainage,semi-circular bending(SCB),Cantabro,wheel tracking,indirect tensile strength(ITS),and permeability tests were conducted.Additionally,to analyze the prepared grouting material,flexural strength,compressive strength,and fluidity tests were conducted.In the final stage,SFP was compared to HMA in terms of engineering characteristics and performance.According to the results,SFP was more resistant to skid,rutting,fire,and moisture damage,while HMA had a better performance in fracture tests,including SCB test.According to the results of the mechanical performance tests conducted on OGA mixtures,the highest and lowest values for air void content to achieve the highest mechanical performance level were 30%-35%and 25%,respectively.Also,based on the laboratory results,it was determined that the required void ratio for constructing OGA mixtures was 24%-26%based on the bitumen type and fibers amount in the mixture.Finally,SFP mixture can be regarded as a viable alternative to common pavements thanks to its high resistance to rutting and moisture damage,long freezing-thawing fatigue life,and adequate fire and skid resistance.