Development of Thermal Shock Resistant and Low Creep Bricks for Hot Blast Stove
1
作者 LIN Binyin LIU Jiehua +1 位作者 ZHOU Ningsheng ZHANG Jianwu 《China's Refractories》 CAS 2005年第4期8-12,共5页
The paper describes the ries with high thermal shock development of brick seresistance and low creep rate for hot blast stove, including research target and research plan on the basis of analysis on how to enhance the... The paper describes the ries with high thermal shock development of brick seresistance and low creep rate for hot blast stove, including research target and research plan on the basis of analysis on how to enhance the thermal shock resistance and to lower creep rate of the bricks. Efforts have been made on the selection of starting materials such as corundum, mullite, andalusite and sillimanite etc., together with some measures taken on multi-grade formulation, homogenizing of the matrix of bricks and addition of some special additives. The results indicated that the bricks were with characteristics such as higher thermal shock resistance of 〉 30 cycles under quenching in water from 1000℃, and creep rate of 0. 2 under 1400℃ for 20 -50hrs with load of 0.2 MPa. Now a series of products of this kind have been developed and produced. The application of the products in Wuhan Iron and Steel Co. showed very prospective results. Now most of domestic large sized blast furnaces say ≥- 1000m^3, including those of Baoshan Iron and Steel Co. , have selected the series products made by Gongyi No. 5 Refractories Head Factory(GYWN) for their hot blast stoves. 展开更多
关键词 Refractory bricks Hot blast stove low creep Thermal shock resistance Andalusite Mullite CORUNDUM SILLIMANITE
下载PDF
Development of Andalusite Bricks for Hot Blast Stove
2
作者 KANG Huarong LI Xianming +3 位作者 DONG Shengying XUE Wendong LI Yong SONG Wen 《China's Refractories》 CAS 2008年第2期25-28,共4页
Low-creep andalusite bricks are characterized by high refractoriness under load, good anti-creep property, high mechanical strength, low porosity, good thermal shock resistance, etc. In this study, low-creep andalusit... Low-creep andalusite bricks are characterized by high refractoriness under load, good anti-creep property, high mechanical strength, low porosity, good thermal shock resistance, etc. In this study, low-creep andalusite brick specimens were investigated in the lab using mullite, bauxite and andalusite. Andalusite with the different particle sizes were used in the experiment and the specimen with the best property was selected us the production standard. In addition, the industrial produced low-creep andalusite bricks were compared with other low-creep bricks. The results show that the developed low-creep andalusite bricks is an excellent material for hot blast stove. 展开更多
关键词 ANDALUSITE low-creep bricks Hot blast stove
下载PDF
热风炉低蠕变粘土砖的研制 被引量:1
3
作者 吴永涛 《四川冶金》 CAS 2008年第2期35-38,共4页
分别从焦宝石骨料级配、兰晶石加入量、兰晶石粒度、粉料加入方式以及烧成温度等方面较为详细的分析了对低蠕变粘土砖性能的影响。另外适当的加入α-A l2O3或莫来石微粉作为添加剂,可以进一步改善制品的各项性能。
关键词 热风炉 低蠕变 粘土砖
下载PDF
热风炉用低蠕变硅砖的研制 被引量:1
4
作者 肖伟 曹梅 陈艳 《耐火材料》 CAS 北大核心 2012年第5期361-362,共2页
为了满足热风炉生产的要求,通过选择硅石原料、确定试样配方和烧成制度研制了一种热风炉用低蠕变硅砖。结果表明,采用混合硅石配料制砖,以65%~75%(w)的硅石A颗粒和25%~30%(w)的硅石B细粉配料,在隧道窑中于1 450℃48 h烧成制备的硅砖,... 为了满足热风炉生产的要求,通过选择硅石原料、确定试样配方和烧成制度研制了一种热风炉用低蠕变硅砖。结果表明,采用混合硅石配料制砖,以65%~75%(w)的硅石A颗粒和25%~30%(w)的硅石B细粉配料,在隧道窑中于1 450℃48 h烧成制备的硅砖,无裂纹,其w(鳞石英)=65%,w(残余石英)=0.66%,高温蠕变率(0.2 MPa,1 500℃,25 h)为-0.03%。 展开更多
关键词 低蠕变 硅砖 热风炉