Treatment of hydrofluoric acid exposure to the eye 被引量:3
1
作者 Katherine Atley Edward Ridyard 《International Journal of Ophthalmology(English edition)》 SCIE CAS 2015年第1期157-161,共5页
AIM: To review the current evidence of the treatment of hydrofluoric acid(HF) exposure to the human cornea.METHODS: A comprehensive manual search of the literature was conducted through the Ovid interface to assess th... AIM: To review the current evidence of the treatment of hydrofluoric acid(HF) exposure to the human cornea.METHODS: A comprehensive manual search of the literature was conducted through the Ovid interface to assess the mechanism and efficacy of each irrigator through a variety of clinical cases and experimental studies.· RESULTS: Ocular exposure to HF is extremely damaging to the eye and swift recognition and decontamination with an appropriate agent forms the basis of treatment. Although there are various decontamination solutions that have efficacy against the corrosive action of HF, irrigation with Hexafluorine proved to be the most safe and effective treatment for the eye.CONCLUSION: In conclusion emergency departments could benefit from the availability of Hexafluorine for the treatment of HF ocular burns in patients. 展开更多
关键词 hydrofluoric acid CORNEA OCULAR INJURY
下载PDF
Kinetics of leaching lithium from lepidolite using mixture of hydrofluoric and sulfuric acid 被引量:15
2
作者 WANG Hai-dong ZHOU An-an +2 位作者 GUO Hui LÜMeng-hua YU Hai-zhao 《Journal of Central South University》 SCIE EI CAS CSCD 2020年第1期27-36,共10页
The fluorine-based chemical method shows great potential in leaching lithium(Li) from lepidolite. Leaching kinetics of Li in a mixture of sulfuric acid and hydrofluoric acid, which is a typical lixivant for the fluori... The fluorine-based chemical method shows great potential in leaching lithium(Li) from lepidolite. Leaching kinetics of Li in a mixture of sulfuric acid and hydrofluoric acid, which is a typical lixivant for the fluorine-based chemical method, was carried out under crucial factors such as different HF/ore ratios(1:1-3:1 g/mL) and leaching temperatures(50-85℃). The kinetics data fit well with the developed shrinking-core model, indicating that the leaching rate of Li was controlled by the chemical reaction and inner diffusion at the beginning of leaching(0-30 min) as a calculated apparent activation energy(Ea) of 20.62 kJ/mol. The inner diffusion became the rate-limiting step as the leaching continues(60-180 min). Moreover, effects of HF/ore ratio and leaching temperature on selective leaching behavior of Li, Al and Si were discussed. 90% of fluorine mainly existed as HF/F-in leaching solution, which can provide theoretical guidance for further removal or recovery of F. 展开更多
关键词 LEPIDOLITE lithium extraction fluorine-based chemical method hydrofluoric acid selective leaching leaching kinetics
下载PDF
Potentially fatal electrolyte imbalance caused by severe hydrofluoric acid burns combined with inhalation injury: A case report 被引量:3
3
作者 He Fang Guang-Yi Wang +2 位作者 Xun Wang Fang He Jian-Dong Su 《World Journal of Clinical Cases》 SCIE 2019年第20期3341-3346,共6页
BACKGROUND Hydrofluoric acid(HF)is one of the most common causes of chemical burns.HF burns can cause wounds that deepen and progress aggressively.As a result,HF burns are often severe even if they involve a small are... BACKGROUND Hydrofluoric acid(HF)is one of the most common causes of chemical burns.HF burns can cause wounds that deepen and progress aggressively.As a result,HF burns are often severe even if they involve a small area of the skin.Published cases of HF burns have mostly reported small HF burn areas.Few cases of HF inhalation injury have been reported to date.CASE SUMMARY A 24-year-old man suffered from extensive hydrofluoric acid burns covering 60%of the total body surface area(TBSA),including deep second degree burns on 47%and third degree burns on 13%of the TBSA,after he fell into a pickling pool containing 15%HF.Comprehensive treatments were carried out after the patient was admitted.Ventricular fibrillation occurred 9 times within the first 2 h,and the lowest serum Ca2+concentration was 0.192 mmol/L.A dose of calcium gluconate(37 g)was intravenously supplied during the first 24 h,and the total amount of calcium gluconate supplementation was 343 g.Extracorporeal membrane oxygenation(ECMO)was applied for 8 d to handle the acute respiratory distress syndrome(ARDS)induced by the HF inhalation injury.The patient was discharged after 99 d of comprehensive treatment,including skin grafting.CONCLUSION Extensive HF burns combined with an inhalation injury led to a potentially fatal electrolyte imbalance and ARDS.Adequate and timely calcium supplementation and ECMO application were the keys to successful treatment of the patient. 展开更多
关键词 hydrofluoric acid burn INHALATION injury HYPOCALCEMIA Acute respiratory distress syndrome EXTRACORPOREAL membrane OXYGENATION Case report
下载PDF
Leaching kinetics of acid-soluble Cr(Ⅵ) from chromite ore processing residue with hydrofluoric acid 被引量:4
4
作者 李小斌 徐文彬 +2 位作者 周秋生 彭志宏 刘桂华 《Journal of Central South University》 SCIE EI CAS 2011年第2期399-405,共7页
Leaching kinetics of acid-soluble Cr(VI) in chromite ore processing residue (COPR) using hydrofluoric (HF) acid solution as a leaching agent was investigated for potential remediation of COPR with industrial was... Leaching kinetics of acid-soluble Cr(VI) in chromite ore processing residue (COPR) using hydrofluoric (HF) acid solution as a leaching agent was investigated for potential remediation of COPR with industrial waste water containing HF. The results show that HF can effectively destabilize the Cr(VI)-bearing minerals, resulting in the mobilization of Cr(VI) from COPR into the leachate. Particle size significantly influences the leaching of acid-soluble Cr(VI) from COPR, followed by leaching time, whereas the effects of HF concentration and leaching temperature are slight and the influence of stirring rate is negligible. The leaching process of acid-soluble Cr(VI) from COPR is controlled by the diffusion through the product layer. The apparent activation energy is 8.696 kJ/mol and the reaction orders with respect to HF concentration and particle size is 0.493 8 and -2.013 3, respectively. 展开更多
关键词 LEACHING KINETICS hydrofluoric acid hexavalent chromium chromite ore processing residue
下载PDF
Single amino acid substitution of VP1 N17D or VP2 H145Y confers acid-resistant phenotype of type Asia1 foot-and-mouth disease virus 被引量:2
5
作者 Haiwei Wang Shanshan Song +4 位作者 Jianxiong Zeng Guohui Zhou Decheng Yang Te Liang Li Yu 《Virologica Sinica》 SCIE CAS CSCD 2014年第2期103-111,共9页
Infection by foot-and-mouth disease virus(FMDV) is triggered by the acidic pH in endosomes after virus uptake by receptor-mediated endocytosis. However, dissociation of the FMDV 146S particle in mildly acidic conditio... Infection by foot-and-mouth disease virus(FMDV) is triggered by the acidic pH in endosomes after virus uptake by receptor-mediated endocytosis. However, dissociation of the FMDV 146S particle in mildly acidic conditions renders inactivated foot-and-mouth disease(FMD) vaccines much less effective. Type Asia1 FMDV mutants with increased resistance to acid inactivation were selected to study the molecular basis of viral resistance to acid-induced disassembly and improve the acid stability of FMDV. Sequencing of capsid-coding regions revealed four amino acid replacements(VP1 N17D, VP2 H145Y, VP2 G192D, and VP3 K153E) in the viral population of the acid-selected 10th passage. We performed single or combined mutagenesis using a reverse genetic system, and our results provide direct experimental evidence that VP2 H145Y or VP1 N17D substitution confers an acid-resistant phenotype to type Asia1 FMDV. 展开更多
关键词 foot-and-mouth disease virus acid-resistant phenotype virus fitness
下载PDF
Surface Characterization of Titanium Implants Treated in Hydrofluoric Acid
6
作者 Danila M. Korotin Stefan Bartkowski +4 位作者 Ernst Z. Kurmaev Manfred Meumann Eugeniya B. Yakushina Ruslan Z. Valiev Seif O. Cholakh 《Journal of Biomaterials and Nanobiotechnology》 2012年第1期87-91,共5页
The results of XPS measurements of commercially pure titanium cp-Ti) before and after chemical treatment are presented. We have measured XPS spectra of core levels (Ti 2p, O 1s, C 1s, F 1s) and valence bands of coarse... The results of XPS measurements of commercially pure titanium cp-Ti) before and after chemical treatment are presented. We have measured XPS spectra of core levels (Ti 2p, O 1s, C 1s, F 1s) and valence bands of coarse-grained cp-Ti before and after standard acid treatment accepted in dentistry (in 1% HF and 40% HF for 1 min). It is found, that acid treatment of cp-Ti reduces the content of hydrocarbons increasing the surface energy and bio-compatibility of Ti-implants. On the other hand, it is fixed that oxygen concentration on the surface of the acid treated cp-Ti is much higher than for the untreated sample, because the acid treatment removes the contaminated surface layers, increases their reactivity, provides a better passivation and formation of thick protecting TiO2 layer. 展开更多
关键词 Commercially PURE TITANIUM SURFACE Composition hydrofluoric Acid SURFACE Characterization BIOCOMPATIBILITY
下载PDF
天然鳞片石墨提纯研究进展
7
作者 于倩 张晓臣 阚侃 《中国矿业》 北大核心 2024年第7期254-260,共7页
天然鳞片石墨是一种战略资源,对国民经济发展及现代化建设具有重要作用。石墨材料因其具有导电、耐热、抗腐蚀、韧性好、润滑性能好等优异性能,被广泛应用于密封、铸造、防火材料、导电材料等传统工业领域,在新能源、电子信息技术、高... 天然鳞片石墨是一种战略资源,对国民经济发展及现代化建设具有重要作用。石墨材料因其具有导电、耐热、抗腐蚀、韧性好、润滑性能好等优异性能,被广泛应用于密封、铸造、防火材料、导电材料等传统工业领域,在新能源、电子信息技术、高端装备技术等新兴领域也具有潜在的应用价值,被誉为“工业黑金”。虽然我国有着丰富的石墨资源,但由于石墨提纯技术落后,石墨深加工产品与国外仍有一定差距。石墨材料纯度越高其应用价值越高,因此,研究高效、节能的石墨提纯技术对我国石墨产业的发展具有十分重要的意义。目前,常用的石墨提纯方法可分为物理提纯法和化学提纯法,其中,物理提纯法包括浮选法、高温法,化学提纯法包括氢氟酸法、酸碱法和氯化焙烧法。分析对比了这几种提纯方法的原理、优点及存在的问题。未来的研究方向主要集中在对单一提纯方法的工艺流程、提纯设备的优化,多种方法联合使用,以及新方法的开发及应用等方面。 展开更多
关键词 石墨 提纯 碱酸法 氢氟酸法 氯化焙烧法
下载PDF
高压密闭酸溶-电感耦合等离子体发射光谱法测定硼矿石中的硼
8
作者 王蕾 于汀汀 +1 位作者 孙红宾 张保科 《岩矿测试》 CAS CSCD 北大核心 2024年第3期468-475,共8页
应用电感耦合等离子体发射光谱法(ICP-OES)分析硼矿石中的硼含量,样品分解方法多采用酸溶法和熔融法,硼酸在浓酸溶液中加热蒸发时形成易挥发的BF_(3)或BCl_(3),造成硼的损失。熔融法可分解难溶于酸的硅硼钙石、电气石等样品,但将大量钠... 应用电感耦合等离子体发射光谱法(ICP-OES)分析硼矿石中的硼含量,样品分解方法多采用酸溶法和熔融法,硼酸在浓酸溶液中加热蒸发时形成易挥发的BF_(3)或BCl_(3),造成硼的损失。熔融法可分解难溶于酸的硅硼钙石、电气石等样品,但将大量钠盐引入了样品中,基体较大,检出限高。本文建立了高压密闭酸溶、ICP-OES测定硼矿石中硼含量的方法。样品经硝酸和氢氟酸在高压密闭溶样罐中分解完全、定容稀释后,样品溶液用配备耐氢氟酸进样系统的ICP-OES测定。在ICP-OES中,硼有三条常用分析谱线,选取249.677nm为硼的分析谱线,标准曲线的线性相关系数大于0.9995。采用本方法对硼镁矿、锰方硼石和盐湖型固体硼矿三种类型5个不同含量范围的实际样品进行测定,相对标准偏差(RSD,n=11)为0.39%~2.66%,方法检出限为1.76μg/g,硼含量定量范围为5.87μg/g~10.8%。经标准物质验证,硼含量测定值与标准值一致,与容量法和微波消解法测定结果吻合。本方法试剂用量少,无需蒸干样品溶液,有效地避免了硼酸易挥发和试剂用量大的问题。 展开更多
关键词 硼矿石 高压密闭酸溶 电感耦合等离子体发射光谱法 耐氢氟酸进样系统
下载PDF
萤石与浓硫酸反应制备氢氟酸动力学研究
9
作者 杨旭 袁鑫 +3 位作者 李育彪 谢顺昕 陈鹏 宋少先 《非金属矿》 2024年第4期1-5,共5页
为解决采用伴生型萤石代替单一型萤石生产氢氟酸的技术难题,揭示了伴生型萤石与浓硫酸的反应机制及动力学规律。研究在不同液固摩尔比和温度条件下单一型萤石和伴生型萤石与浓硫酸反应生成氟化氢的转化率。结果表明,单一型萤石产酸的最... 为解决采用伴生型萤石代替单一型萤石生产氢氟酸的技术难题,揭示了伴生型萤石与浓硫酸的反应机制及动力学规律。研究在不同液固摩尔比和温度条件下单一型萤石和伴生型萤石与浓硫酸反应生成氟化氢的转化率。结果表明,单一型萤石产酸的最佳液固摩尔比和温度分别为1.25∶1和200℃,转化率为97.5%;伴生型萤石为1.50∶1和200℃,转化率为84.5%。单一型萤石产酸反应符合界面化学反应控制模型,而伴生型萤石产酸反应符合固相产物层内扩散控制模型。扫描电镜(SEM)结果表明,伴生型萤石与浓硫酸反应时存在严重的团聚现象并形成致密的硫酸钙钝化层,阻碍了浓硫酸与未反应萤石内核的接触。本试验为伴生型萤石与浓硫酸反应生产无水氢氟酸提供了科学依据。 展开更多
关键词 萤石 浓硫酸 氢氟酸 转化率 动力学
下载PDF
某冶金级萤石精矿提质降杂试验研究
10
作者 冯青舒 缪亚兵 +5 位作者 陈文胜 刘旭 王舰 李文风 赵文坡 陆泽雍 《矿冶工程》 CAS 北大核心 2024年第3期73-76,共4页
针对某CaF_(2)品位70.34%的冶金级萤石精矿进行了提质降杂试验研究。结果表明,采用“强磁选降硅-非磁性产品浮选降钙”工艺,实验室全流程试验获得了精矿产率58.30%、CaF2品位91.95%、回收率76.52%的萤石产品,萤石产品质量达到了制备无... 针对某CaF_(2)品位70.34%的冶金级萤石精矿进行了提质降杂试验研究。结果表明,采用“强磁选降硅-非磁性产品浮选降钙”工艺,实验室全流程试验获得了精矿产率58.30%、CaF2品位91.95%、回收率76.52%的萤石产品,萤石产品质量达到了制备无水氢氟酸的原料要求。 展开更多
关键词 萤石 强磁选 浮选 提质降杂 氢氟酸
下载PDF
含氟废液资源化制备氟化钠的工艺研究 被引量:1
11
作者 邓国平 伍勇 +2 位作者 段利中 任至 吴莉鑫 《无机盐工业》 CAS CSCD 北大核心 2024年第6期133-138,共6页
萤石资源的短缺导致氟类资源紧张,为缓解氟资源的压力,需充分提高氟资源的有效利用率。以含氟化铵或氢氟酸废水为原料,采用沉淀法将含氟废液中的游离氟资源化制备氟化钠,研究了制备过程中反应时间、温度、p H和钠盐对氟化钠产品品质的影... 萤石资源的短缺导致氟类资源紧张,为缓解氟资源的压力,需充分提高氟资源的有效利用率。以含氟化铵或氢氟酸废水为原料,采用沉淀法将含氟废液中的游离氟资源化制备氟化钠,研究了制备过程中反应时间、温度、p H和钠盐对氟化钠产品品质的影响,探究了反应后滤液的回用次数及效果。研究结果表明:氟化铵废液在反应时间为120 min、反应温度为85℃的条件下,氟离子与氯化钠中钠离子的物质的量比为1∶1反应时,制备的氟化钠品质最佳(98.30%),产率为67.92%,反应后滤液除氟后蒸发,氯化铵的含氮质量分数为24.47%,达到农业用氯化铵合格品要求;含氢氟酸废液通过中和法加氢氧化钠调节pH至6,制备的氟化钠的质量分数为98.15%,且滤液至少能回用5次。该研究实现了不同成分的含氟废液均可资源化制备氟化钠的工艺流程,极大程度减少了氟资源的浪费,使氟资源得到充分有效的利用。 展开更多
关键词 氟化钠 氟化铵废液 氢氟酸废液 资源化
下载PDF
某高钙钨尾矿反—正浮选工艺回收铷的研究
12
作者 冯章标 阳华玲 王长福 《矿产保护与利用》 2024年第1期89-94,共6页
某钨尾矿含铷0.098%,脉石矿物主要为石英、石榴石、萤石、方解石,铷主要赋存在白云母、黑云母及钾长石中,其与脉石矿物嵌布关系极为复杂,属伴生高钙低品位铷矿。为确定铷回收工艺,采用反浮选脱钙—铷正浮选原则流程,详细开展了反浮选脱... 某钨尾矿含铷0.098%,脉石矿物主要为石英、石榴石、萤石、方解石,铷主要赋存在白云母、黑云母及钾长石中,其与脉石矿物嵌布关系极为复杂,属伴生高钙低品位铷矿。为确定铷回收工艺,采用反浮选脱钙—铷正浮选原则流程,详细开展了反浮选脱钙粗选捕收剂、抑制剂和铷浮选粗选活化剂、矿浆pH、十二胺用量、精选抑制剂六偏磷酸钠用量等条件实验。结果表明,反浮选脱钙采用捕收剂CYP+抑制剂SN-1,铷正浮选采用硫酸+十二胺,最终通过反浮选脱钙(两粗三精)—无氟少酸铷正浮选(一粗一扫一精)闭路流程,获得了铷精矿Rb2O品位0.214%、Rb2O回收率71.04%的指标,较好地实现了铷资源的回收。 展开更多
关键词 铷矿 云母 长石 反浮选 脱钙 无氟少酸
下载PDF
用氢氟酸从白云鄂博矿中浸出铌及动力学研究
13
作者 孙盘石 赵增武 +4 位作者 贾艳 贺宇龙 崔久龙 张文迪 汪文清 《湿法冶金》 CAS 北大核心 2024年第3期236-241,共6页
针对白云鄂博尾矿中含铌矿物综合回收利用中存在的问题,研究了用氢氟酸浸出含铌矿物中的铌,确定了最佳工艺条件,并探讨了浸出动力学。结果表明:在反应温度90℃、液固体积质量比7/1、氢氟酸浓度20 mol/L、反应时间2 h、搅拌速率300 r/mi... 针对白云鄂博尾矿中含铌矿物综合回收利用中存在的问题,研究了用氢氟酸浸出含铌矿物中的铌,确定了最佳工艺条件,并探讨了浸出动力学。结果表明:在反应温度90℃、液固体积质量比7/1、氢氟酸浓度20 mol/L、反应时间2 h、搅拌速率300 r/min条件下,铌浸出率达90.91%;铌的浸出过程符合核收缩模型,浸出过程由化学反应和扩散混合控制,表观活化能为35.459 kJ/mol。该法能有效提取尾矿中的铌,有利于后续分离提纯。 展开更多
关键词 白云鄂博尾矿 含铌矿物 氢氟酸 浸出 动力学
下载PDF
电感耦合等离子体发射光谱法同时测定土壤样品中的硼、磷、钠、钾的方法研究 被引量:3
14
作者 黄浩 武明丽 《分析测试技术与仪器》 CAS 2024年第1期47-52,共6页
土壤样品中的硼元素在酸溶体系中易挥发,采用碱熔法则无法同时测定钾、钠,并且大量的盐类也不利于检测.而在盐酸-氢氟酸-硝酸三酸体系中,通过加入甘露醇可以保护硼在密闭消解条件下不易挥发损失.以电感耦合等离子体发射光谱法(ICP-OES)... 土壤样品中的硼元素在酸溶体系中易挥发,采用碱熔法则无法同时测定钾、钠,并且大量的盐类也不利于检测.而在盐酸-氢氟酸-硝酸三酸体系中,通过加入甘露醇可以保护硼在密闭消解条件下不易挥发损失.以电感耦合等离子体发射光谱法(ICP-OES)为测试手段,使用耐氢氟酸进样系统,可以有效避免待测元素受到污染,通过预加内标的方法来纠正体积偏差后,可以实现对土壤样品中硼、磷、钠、钾元素的同时测定.试验结果表明,在没有加稳定剂时,硼在消解过程中会因挥发而损失严重,但在有稳定剂的存在下,即使在160℃以上,硼也没有检测到挥发损失,证明采用甘露醇作为稳定剂是可行的.通过有证土壤和水系沉积物标准样品的测试验证,对于硼质量分数高于10mg/kg的土壤样品,其测试结果与认定值相对偏差小于10%,具有很好的灵敏度且操作简单,易用于大批量的检测任务. 展开更多
关键词 甘露醇稳定剂 ICP-OES 耐氢氟酸进样系统 预加内标
下载PDF
Fe_(3)O_(4)@TiO_(2)纳米催化剂的制备及其催化氧化CO的性能研究
15
作者 张尚文 张康毅 +1 位作者 田甜 王磊 《广州化工》 CAS 2024年第13期51-54,共4页
采用过渡金属铁(Fe)掺杂经过氢氟酸(HF)蚀刻的TiO_(2)载体制备出Fe_(2)O_(3)/TiO_(2)催化剂,可以解决将过渡金属(Fe)直接掺杂到TiO_(2)载体形成的催化剂催化活性低等问题。探究不同浓度的HF对TiO_(2)蚀刻后其表征情况和对CO的催化转化... 采用过渡金属铁(Fe)掺杂经过氢氟酸(HF)蚀刻的TiO_(2)载体制备出Fe_(2)O_(3)/TiO_(2)催化剂,可以解决将过渡金属(Fe)直接掺杂到TiO_(2)载体形成的催化剂催化活性低等问题。探究不同浓度的HF对TiO_(2)蚀刻后其表征情况和对CO的催化转化效率。结果表明,在4.16 mol/L浓度的HF溶液中加入TiOSO_(4),并利用水热法制备出的暴露高指数晶面TiO_(2)载体去负载过渡金属(Fe)做出来的催化剂在对CO吸附转化的测试中表现出最高的活性,在180℃时对CO的转化率可以达到90%,而且该类催化剂对CO催化转化效率高,在废气的光催化转化方面有着广阔的发展前景。 展开更多
关键词 二氧化钛 过渡金属催化剂 氢氟酸表面处理
下载PDF
萤石生产高纯氢氟酸工艺研究进展
16
作者 刘禹博 郭其景 +2 位作者 杨华春 易浩 宋少先 《当代化工研究》 CAS 2024年第6期9-11,共3页
伴随着我国半导体、集成电路、太阳能光伏等行业的快速发展,高纯氢氟酸作为重要的湿电子材料具有重要地位。萤石中的氟含量高达49%且杂质相对易去除,便于低成本、高品质的高纯氢氟酸生产,故目前工业上主要利用萤石生产氢氟酸。本文主要... 伴随着我国半导体、集成电路、太阳能光伏等行业的快速发展,高纯氢氟酸作为重要的湿电子材料具有重要地位。萤石中的氟含量高达49%且杂质相对易去除,便于低成本、高品质的高纯氢氟酸生产,故目前工业上主要利用萤石生产氢氟酸。本文主要阐述和分析萤石选矿工艺及萤石生产高纯氢氟酸的工艺流程、氢氟酸产品的杂质去除方法与杂质检测技术等,并提出了氢氟酸生产工艺未来发展方向,以促进氢氟酸行业及氢氟酸生产工艺未来的蓬勃发展。 展开更多
关键词 萤石 高纯氢氟酸 非金属矿 工艺分析
下载PDF
基于我国战略性矿产萤石及磷矿的氟资源供应形势研究及建议
17
作者 高永璋 《中国矿业》 北大核心 2024年第10期44-53,共10页
氟在现代工业中用途广泛,重要的含氟矿物有萤石、氟磷灰石等,以往研究多关注单一萤石,缺乏对氟资源的综合讨论。本文从氟产业链角度梳理了近十年来我国在资源勘查、提取、供应等方面取得的重要新进展。研究结果表明,作为传统的全球最大... 氟在现代工业中用途广泛,重要的含氟矿物有萤石、氟磷灰石等,以往研究多关注单一萤石,缺乏对氟资源的综合讨论。本文从氟产业链角度梳理了近十年来我国在资源勘查、提取、供应等方面取得的重要新进展。研究结果表明,作为传统的全球最大萤石生产国和消费国,我国氟资源开发格局已经发生较大变化,近十年通过勘查萤石及磷矿,新增了数亿吨氟资源;与多金属矿、稀土矿、非金属矿等共伴生萤石分选技术取得突破,盘活萤石资源1亿t以上;实现了磷矿伴生低品位氟资源的利用,已建氟硅酸法生产氟化氢产能全球最大;我国是世界上最主要的萤石原材料和初级产品供应国,2018年起已转变为萤石净进口国,氟化氢出口量是进口量的16~25倍。综合我国氟资源供应形势认为:①我国的氟资源供应格局已由单一萤石为主逐步变为由单一萤石、共伴生萤石及磷矿共同供应;②我国单一萤石矿开采规模稳步提升,共伴生萤石矿回收技术及规模世界领先;③我国共伴生氟资源开发利用以延伸产业链为特征,技术门槛较高;④我国氟资源的供应特征为进口初级矿产品、加工出口初级化工产品,仍为氟资源净出口国;⑤建议积极调整氟资源开发结构,向产业链下游转移。本文研究为我国氟资源及战略性矿产萤石和磷矿的开发和保护提供了新的思路与方向。 展开更多
关键词 氟资源 萤石 共伴生矿 磷矿 氢氟酸
下载PDF
氢氟酸沉淀法制备松装密度适度的大颗粒无水氟化镨钕的研究
18
作者 郑艳玲 蓝桥发 +3 位作者 邱小英 兰剑波 肖莉 葛刘生 《稀有金属与硬质合金》 CAS CSCD 北大核心 2024年第4期34-39,共6页
采用氢氟酸沉淀法制备无水氟化镨钕粉体,考察了草酸加入量、底水酸度、上清液循环利用次数、氢氟酸用量等条件对水合氟化镨钕晶体的形成和无水氟化镨钕粉体的形貌、粒度、松装密度、杂质等的影响。结果表明,优化的工艺条件为:草酸投入... 采用氢氟酸沉淀法制备无水氟化镨钕粉体,考察了草酸加入量、底水酸度、上清液循环利用次数、氢氟酸用量等条件对水合氟化镨钕晶体的形成和无水氟化镨钕粉体的形貌、粒度、松装密度、杂质等的影响。结果表明,优化的工艺条件为:草酸投入量为理论用量(RE^(3+)物质的量的1.5倍)的6%~10%,底水的酸度为1.6~2.0 mol/L,上清液循环利用次数≤3次,氢氟酸投入量为100%理论用量(RE^(3+)物质的量的3倍)。采用优化工艺条件制备的无水氟化镨钕中位粒径D_(50)可达到10~30μm,松装密度为0.7~0.8 g/cm^(3),非稀土杂质含量低,稀土收率达到99.81%。 展开更多
关键词 无水氟化镨钕 氢氟酸 沉淀 松装密度 粒度
下载PDF
氢氟酸废液协同含铅飞灰无害化处理研究
19
作者 钟琦 李行德 +1 位作者 张千帆 任雪娇 《云南化工》 CAS 2024年第4期82-84,共3页
为了使碱性含铅飞灰达到危险废物填埋限值,使用氢氟酸废液作为含铅飞灰的稳定化药剂,在探究出氢氟酸废液的最佳用量后,以石灰作为pH调节剂,水泥做固化剂,可使总铅、无机氟化物的浸出毒性低于《危险废物填埋污染控制标准》(GB19598-2019... 为了使碱性含铅飞灰达到危险废物填埋限值,使用氢氟酸废液作为含铅飞灰的稳定化药剂,在探究出氢氟酸废液的最佳用量后,以石灰作为pH调节剂,水泥做固化剂,可使总铅、无机氟化物的浸出毒性低于《危险废物填埋污染控制标准》(GB19598-2019)要求。结果表明,氢氟酸废液的加入量为10%(质量分数),石灰的加入量为4%(质量分数)调节pH在7.10~7.15之间时稳定化效果显著,最优结果为pH=7.15,总铅质量浓度0.145 mg/L,无机氟化物质量浓度3.7 mg/L。 展开更多
关键词 含铅飞灰 氢氟酸 石灰 浸出毒性
下载PDF
浅谈电子级氢氟酸技术及发展
20
作者 苏宁 曾明辉 杨宏 《有机氟工业》 CAS 2024年第2期54-57,共4页
电子级氢氟酸是湿电子化学品中的一种,主要应用于集成电路、液晶显示器、太阳能光伏、LED制造等工艺中。综述了电子级氢氟酸的常用提纯技术、关键技术和质量指标等,并对制备方法、关键技术等进行对比分析,最后对技术及行业发展进行了展望。
关键词 电子级氢氟酸 制备 工艺
下载PDF