Three novel poly(ether imide)s were synthesized by one-step solution polymerization from 2-(3, 4-dicarboxyl-N-phenyl)-4-(3, 4-dicarboxyl-phenoxyl-4-(2-methyl)-phenyl)-2, 3- phthal-azin-1-one dianhydride and three amin...Three novel poly(ether imide)s were synthesized by one-step solution polymerization from 2-(3, 4-dicarboxyl-N-phenyl)-4-(3, 4-dicarboxyl-phenoxyl-4-(2-methyl)-phenyl)-2, 3- phthal-azin-1-one dianhydride and three amines, and characterized. The polymers show good solubility and thermal properties.展开更多
The direct polymerization of an unsymmetrical kink non-coplanar heterocyclic diamine (1) with various aromatic bis(trimellitimide)s (2a-e) using triphenyl phosphite and pyridine as condensing agents could generate a s...The direct polymerization of an unsymmetrical kink non-coplanar heterocyclic diamine (1) with various aromatic bis(trimellitimide)s (2a-e) using triphenyl phosphite and pyridine as condensing agents could generate a series of new aromatic poly(amide imide)s (3a-e) containing the kink non-coplanar phthalazinone heterocyclic units in the polymer main chains with inherent viscosities of 0.58-0.66 dL/g. The polymers are readily soluble in a variety of solvents such as N,N- dimethylformamide, N,N-dimethylacetamide, dimethyl sulfoxide, N-methyl-2-pyrrolidinone, pyridine and m-cresol and can be cast to form flexible and tough films. The glass transition temperatures of polymers (Tg) are in the range of 301-327°C, and the temperatures for 5% weight loss in nitrogen are in the range of 498-521 'C.展开更多
A novel poly(ether imide)s containing phthalazinone and isopropyl moieties derived from 2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl]-phthalazin-1-one and bisphenol-A diphthalic anhydride was synthesized by one-step ...A novel poly(ether imide)s containing phthalazinone and isopropyl moieties derived from 2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl]-phthalazin-1-one and bisphenol-A diphthalic anhydride was synthesized by one-step solution condensation polymerization in nr-cresol. The polymer was characterized by FTIR, NMR, molecular weights, glass transition temperature, thermal degradation temperature and WAXD.展开更多
The synthesis and characterization of a series of novel poly(aryl amide imide)s based on o diphenyltrimellitic anhydride are described.The poly(aryl amide imide)s having inherent viscosities of 0.39-1.43dL/g in N m...The synthesis and characterization of a series of novel poly(aryl amide imide)s based on o diphenyltrimellitic anhydride are described.The poly(aryl amide imide)s having inherent viscosities of 0.39-1.43dL/g in N methyl 2 pyrrolidinone at 30℃,were prepared by polymerization with aromatic diamines in N,N-dimethylacetamide and subsequent chemical imidization.All the polymers were amorphous,readily soluble in aprotic polar solvents such as DMAC,NMP,DMF,DMSO,and m cresol,and could be cast to form flexible and tough films.The glass trsanition temperatures were in the range of 284-336℃,and the temperatures for 5% weight loss in nitrogen were above 468℃.展开更多
基金This work was sponsored by the National Natural Science Foundation of China (No. 59473901).
文摘Three novel poly(ether imide)s were synthesized by one-step solution polymerization from 2-(3, 4-dicarboxyl-N-phenyl)-4-(3, 4-dicarboxyl-phenoxyl-4-(2-methyl)-phenyl)-2, 3- phthal-azin-1-one dianhydride and three amines, and characterized. The polymers show good solubility and thermal properties.
基金This work was supported by the Key Natural Science Foundation of Fujian Province (E0320003).
文摘The direct polymerization of an unsymmetrical kink non-coplanar heterocyclic diamine (1) with various aromatic bis(trimellitimide)s (2a-e) using triphenyl phosphite and pyridine as condensing agents could generate a series of new aromatic poly(amide imide)s (3a-e) containing the kink non-coplanar phthalazinone heterocyclic units in the polymer main chains with inherent viscosities of 0.58-0.66 dL/g. The polymers are readily soluble in a variety of solvents such as N,N- dimethylformamide, N,N-dimethylacetamide, dimethyl sulfoxide, N-methyl-2-pyrrolidinone, pyridine and m-cresol and can be cast to form flexible and tough films. The glass transition temperatures of polymers (Tg) are in the range of 301-327°C, and the temperatures for 5% weight loss in nitrogen are in the range of 498-521 'C.
文摘A novel poly(ether imide)s containing phthalazinone and isopropyl moieties derived from 2-(4-aminophenyl)-4-[4-(4-aminophenoxy)phenyl]-phthalazin-1-one and bisphenol-A diphthalic anhydride was synthesized by one-step solution condensation polymerization in nr-cresol. The polymer was characterized by FTIR, NMR, molecular weights, glass transition temperature, thermal degradation temperature and WAXD.
文摘The synthesis and characterization of a series of novel poly(aryl amide imide)s based on o diphenyltrimellitic anhydride are described.The poly(aryl amide imide)s having inherent viscosities of 0.39-1.43dL/g in N methyl 2 pyrrolidinone at 30℃,were prepared by polymerization with aromatic diamines in N,N-dimethylacetamide and subsequent chemical imidization.All the polymers were amorphous,readily soluble in aprotic polar solvents such as DMAC,NMP,DMF,DMSO,and m cresol,and could be cast to form flexible and tough films.The glass trsanition temperatures were in the range of 284-336℃,and the temperatures for 5% weight loss in nitrogen were above 468℃.