期刊文献+
共找到3篇文章
< 1 >
每页显示 20 50 100
Short-term results of incremental penile girth enhancement using liquid injectable silicone: words of praise for a change 被引量:2
1
作者 YacovYacobi Alexander Tsivian +1 位作者 Roman Grinberg Oded Kessler 《Asian Journal of Andrology》 SCIE CAS CSCD 2007年第3期408-413,共6页
Aim: To report our experience with penile girth augmentation using liquid injectable silicone. Methods: Between August 2003 and July 2006, 324 men (mean age 35 years, range 19-65 years) received a series of liquid... Aim: To report our experience with penile girth augmentation using liquid injectable silicone. Methods: Between August 2003 and July 2006, 324 men (mean age 35 years, range 19-65 years) received a series of liquid silicone subcutaneous injections between the penile skin and the corpora cavernosa on the dorsal and lateral aspects of the penile shaft, under local anesthesia. Digital photographs taken pre- and post-procedure (n = 324), and penile contour measurements (n = 30) yielded objective results. Subjective results were derived from patient and partner testimony of satisfaction. Follow-up averaged 20 months (range 1-36 months). Results: Three hundred and twenty-four procedures were primary augmentations. Most men (61%) were married, 7% were accompanied by their partners, and 93% were circumcised. The mean measured penile circumference was 9.5 cm (7.5-11.5 cm) pretreatment and 12.1 cm (10.3-15.3 cm) post-treatment (mean increase of 27% in circumference and 0.84 cm in diameter). Patient and partner satisfaction was already expressed after the first two treatments. Sexual activity could be resumed after 8 h. Complications (mild bruising) were easily resolved. Conclusion: Penile girth augmentation using liquid injectable silicone yields very satisfactory short-term results with no immediate or short-term complications. 展开更多
关键词 injectable silicone penile girth augmentation penile contouring
下载PDF
Goniosynechialysis for secondary angle closure glaucoma in a pseudophakic patient after vitrectomy and silicone oil injection 被引量:4
2
作者 Jonghoon Shin Hyeshin Jeon +1 位作者 Ik Soo Byon Ji-Woong Lee 《International Journal of Ophthalmology(English edition)》 SCIE CAS 2014年第5期914-916,共3页
Dear Sir,Iam Jonghoon Shin,from the Department of Ophthalmology of Pusan National University Hospital,Busan,Korea.I write to present a patient with secondary angle closure glaucoma(SACG)after vitrectomy and silicone o... Dear Sir,Iam Jonghoon Shin,from the Department of Ophthalmology of Pusan National University Hospital,Busan,Korea.I write to present a patient with secondary angle closure glaucoma(SACG)after vitrectomy and silicone oil(SO)injection who was successfully treated by 展开更多
关键词 SO IOP Goniosynechialysis for secondary angle closure glaucoma in a pseudophakic patient after vitrectomy and silicone oil injection UBM
下载PDF
Injection molding of ultra-fine Si_3N_4 powder for gas-pressure sintering 被引量:5
3
作者 Xian-feng Yang Jiang-hong Yang +3 位作者 Xie-wen Xu Qi-cheng Liu Zhi-peng Xie Wei Liu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2015年第6期654-659,共6页
The ceramic injection molding technique was used in the gas-pressure sintering of ultra-fine Si3N4 powder. The feedstock's flowability, debinding rate, defect evolution, and microstructural evolution during productio... The ceramic injection molding technique was used in the gas-pressure sintering of ultra-fine Si3N4 powder. The feedstock's flowability, debinding rate, defect evolution, and microstructural evolution during production were explored. The results show that the solid volume loading of less than 50vol% and the surfactant mass fraction of 6wt% result in a perfect flowability of feedstock; this feedstock is suitable for injection molding. When the debinding time is 8 h at 40°C, approximately 50% of the wax can be solvent debinded. Defects detected during the preparation are traced to improper injection parameters, mold design, debinding parameters, residual stress, or inhomogeneous composition distribution in the green body. The bulk density, Vickers hardness, and fracture toughness of the gas-pressure-sintered Si3N4 ceramic reach 3.2 g/cm^3, 16.5 GPa, and 7.2 MPa·m^1/2, respectively. 展开更多
关键词 ceramic materials silicon nitride injection molding sintering near net shaping