The interconnect materials La0.7Ca0.3Cr1-xZnxO3-δ(x=0,0.01,0.03,0.05,0.07) were prepared by a microwave assisted sol-gel auto-ignition process.The crystalline structures of the samples were characterized by X-ray dif...The interconnect materials La0.7Ca0.3Cr1-xZnxO3-δ(x=0,0.01,0.03,0.05,0.07) were prepared by a microwave assisted sol-gel auto-ignition process.The crystalline structures of the samples were characterized by X-ray diffraction(XRD) and the lattice parameters were evaluated with Rietveld method.For Ca-Zn co-doped LaCrO3 with x=0.03,the sintering activity was improved,and the relative density came up to 96.5% for the sample sintered at 1300 oC for 10 h.The electrical conductivity of the samples was increased fr...展开更多
基金supported by the Key Fund of Natural Science for Education Department of Anhui Province,China (KJ2008A150)
文摘The interconnect materials La0.7Ca0.3Cr1-xZnxO3-δ(x=0,0.01,0.03,0.05,0.07) were prepared by a microwave assisted sol-gel auto-ignition process.The crystalline structures of the samples were characterized by X-ray diffraction(XRD) and the lattice parameters were evaluated with Rietveld method.For Ca-Zn co-doped LaCrO3 with x=0.03,the sintering activity was improved,and the relative density came up to 96.5% for the sample sintered at 1300 oC for 10 h.The electrical conductivity of the samples was increased fr...