The weldability of two Fe3Al-based intermetallic alloys and one Fe-16%Al-based (atom fraction) alloy has been investigated for gas tungsten are (GTA) welding on sheets with a thickness of 2 mm. The results indicated t...The weldability of two Fe3Al-based intermetallic alloys and one Fe-16%Al-based (atom fraction) alloy has been investigated for gas tungsten are (GTA) welding on sheets with a thickness of 2 mm. The results indicated that pre-heating and post-annealing treatment were important procedures for retarding cold crack initiation and the propel selection of filler could effectively improve the weldability. For the same alloys with the same welding filler, it is better to choose lower welding current, in another word, lower heat input.展开更多
基金the Ford ChinaResearch & Development Fund Program tinder contract 9715 1016. The effort is also supported by the fundofAdv
文摘The weldability of two Fe3Al-based intermetallic alloys and one Fe-16%Al-based (atom fraction) alloy has been investigated for gas tungsten are (GTA) welding on sheets with a thickness of 2 mm. The results indicated that pre-heating and post-annealing treatment were important procedures for retarding cold crack initiation and the propel selection of filler could effectively improve the weldability. For the same alloys with the same welding filler, it is better to choose lower welding current, in another word, lower heat input.