期刊文献+
共找到110篇文章
< 1 2 6 >
每页显示 20 50 100
Pressure acid leaching of zinc sulfide concentrate 被引量:4
1
作者 古岩 张廷安 +4 位作者 刘燕 牟望重 张伟光 豆志河 蒋孝丽 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2010年第S1期136-140,共5页
Effects of particle size of the zinc sulfide concentrate,leaching temperature,solid-to-liquid ratio and additive amount on pressure acid leaching process of the zinc sulfide concentrate were studied.The results indica... Effects of particle size of the zinc sulfide concentrate,leaching temperature,solid-to-liquid ratio and additive amount on pressure acid leaching process of the zinc sulfide concentrate were studied.The results indicate that the additive can improve the reaction kinetics and the conversion rate.And sulfur can be successfully separated from the zinc sulfide concentrate as elemental sulfur.The reasonable experiment parameters are obtained as follows:the leaching temperature 150℃,oxygen partial pressure 1 MPa,additive amount 1%,solid-to-liquid ratio 1:4,leaching time 2 h,initial sulfuric acid concentration 15%,and particle size less than 44μm.Under the optimum conditions,the leaching rate of the zinc can reach 95%and the reduction rate of the sulfur can reach 90%. 展开更多
关键词 zinc sulfide concentrate pressure acid leaching zinc SULFUR
下载PDF
锌氧压酸浸硫精矿和硫尾矿的矿物学特征与环境活性
2
作者 孙朴 李兴彬 +4 位作者 魏昶 邓志敢 李旻廷 罗兴国 樊刚 《中南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2024年第1期32-42,共11页
采用电感耦合(ICP-OES)、X射线衍射(XRD)、扫面电镜-能谱(SEM-EDS)、红外光谱(FTIR)及差热差重(TG-DTA)等多种检测方法对锌氧压酸浸硫精矿和硫尾矿的化学组成、粒度分布、物相结构等进行研究,并采用毒性浸出程序(TCLP)法考察其短期环境... 采用电感耦合(ICP-OES)、X射线衍射(XRD)、扫面电镜-能谱(SEM-EDS)、红外光谱(FTIR)及差热差重(TG-DTA)等多种检测方法对锌氧压酸浸硫精矿和硫尾矿的化学组成、粒度分布、物相结构等进行研究,并采用毒性浸出程序(TCLP)法考察其短期环境活性。研究结果表明:硫精矿1和硫精矿2主要以球状的单质硫存在,其中,少量硫精矿1以小颗粒的闪锌矿、黄铁矿等附着于块状的铁矾颗粒上,平均粒径为22.1μm;少量硫精矿2以块状的闪锌矿、黄铁矿和小颗粒存在,平均粒径为59.2μm。2种硫精矿在185~340℃时会剧烈燃烧,热稳定性较差。2种硫尾矿主要以块状的铅黄铁矾和黄钠铁矾存在,其中,硫尾矿1平均粒径为21.1μm;硫尾矿2含一定的赤铁矿(16.86%),平均粒径为5.3μm。硫精矿和硫尾矿中锌和镉元素在弱酸条件下不稳定,硫尾矿1中锌和镉的浸出量分别超标1.93倍和2.50倍;硫精矿2的分别超标2.03倍和6.56倍,硫尾矿1的分别超标3.46倍和5.94倍,硫尾矿2的分别超标11.10倍和8.28倍。 展开更多
关键词 锌氧压酸浸 硫精矿 硫尾矿 微观结构 工艺矿物学 浸出毒性
下载PDF
硫化钠体系中异极矿表面的硫化特性及硫化产物解析
3
作者 张嘎 王美丽 +2 位作者 和永新 王涵 丰奇成 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2024年第2期629-642,共14页
通过多种分析检测方法揭示硫化钠体系中异极矿表面的硫化特性和机理,并对异极矿表面硫化产物进行分析测试。研究结果表明,硫化钠浓度对异极矿表面的硫化效果具有显著影响,即提高硫化钠浓度能促进矿浆溶液中硫组分与矿物表面反应,从而提... 通过多种分析检测方法揭示硫化钠体系中异极矿表面的硫化特性和机理,并对异极矿表面硫化产物进行分析测试。研究结果表明,硫化钠浓度对异极矿表面的硫化效果具有显著影响,即提高硫化钠浓度能促进矿浆溶液中硫组分与矿物表面反应,从而提高异极矿表面硫化产物的含量及矿物表面的疏水性。XPS和ToF-SIMS分析表明,异极矿表面的硫化产物并非单一的硫化物,而是由硫化物(S^(2−))和多硫化物(S_(n)^(2−))组成,且矿物表面多硫化物含量随硫化钠浓度的增加而增加,从而增强异极矿表面硫化产物的活性。 展开更多
关键词 硫化特性 异极矿 硫化钠浓度 硫化锌组分 多硫化物
下载PDF
高硅锌精矿焙烧过程中硅的控制及热平衡计算
4
作者 张恒星 陈杭 +4 位作者 陈芬 陈期生 应宗波 吴星琳 王俊娥 《有色金属工程》 CAS 北大核心 2024年第1期61-66,共6页
针对高硅锌精矿焙烧过程中焙砂可溶硅高、沸腾炉易结块、浸出固液分离困难等问题,以现场生产焙烧工艺参数为基础,研究了低温和高温焙烧对焙砂中可溶硅含量的影响,并基于MatCal软件对沸腾炉焙烧工艺进行热平衡计算。结果表明:在焙烧条件... 针对高硅锌精矿焙烧过程中焙砂可溶硅高、沸腾炉易结块、浸出固液分离困难等问题,以现场生产焙烧工艺参数为基础,研究了低温和高温焙烧对焙砂中可溶硅含量的影响,并基于MatCal软件对沸腾炉焙烧工艺进行热平衡计算。结果表明:在焙烧条件基本相同的情况下,随着硫化锌精矿焙烧温度的增加,焙砂中的可溶硅也增加。当焙砂中可溶硅高于3.18%会出现浓密机上清液跑混、低浸浓密底流矿浆过滤困难、净液中除杂钴偏高等问题。经MatCal模拟计算后,理论消耗空气50361.328 m 3/h,低温焙烧的平均风量47102.8 m 3/h,高温焙烧平均风量48005.7 m 3/h,实际的焙烧中平均风量偏低,需要增加沸腾炉的风料比。 展开更多
关键词 硫化锌精矿 沸腾炉 焙烧 热平衡
下载PDF
高浓度快速浮选技术在铅锌硫化矿浮选中的研究与应用
5
作者 张志 张飞超 +1 位作者 苟敏刚 杨宏波 《湖南有色金属》 CAS 2024年第1期18-21,共4页
采取高浓度快速浮选技术,解决了在不改变选矿工艺的情况下原矿处理量增大对生产指标的影响。技术改造后,铅、锌金属回收率分别提高了1.75%和1.61%,伴生银回收率提高了8.60%,药剂成本下降了1.36元/t,降低了选矿生产用水量,年创造经济效益... 采取高浓度快速浮选技术,解决了在不改变选矿工艺的情况下原矿处理量增大对生产指标的影响。技术改造后,铅、锌金属回收率分别提高了1.75%和1.61%,伴生银回收率提高了8.60%,药剂成本下降了1.36元/t,降低了选矿生产用水量,年创造经济效益约511.80万元,保护了生态环境。 展开更多
关键词 铅锌硫化矿 高浓度浮选 浮选速率 回收率 药剂成本 效益
下载PDF
铟的还原浸出动力学及分步沉淀选择性分离 被引量:2
6
作者 李存兄 张兆闫 +3 位作者 张耀阳 邓志敢 吉文斌 林晓坦 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2023年第1期315-324,共10页
开展硫化锌精矿还原浸出高铁锌浸出渣高效浸铟及浸出液中铟选择性分离的研究。结果表明:在固体物料粒度74~105μm、反应温度90℃、浸出时间300 min、硫酸浓度1.4 mol/L的条件下,铟的浸出率达95%以上。采用收缩核模型对还原浸出动力学进... 开展硫化锌精矿还原浸出高铁锌浸出渣高效浸铟及浸出液中铟选择性分离的研究。结果表明:在固体物料粒度74~105μm、反应温度90℃、浸出时间300 min、硫酸浓度1.4 mol/L的条件下,铟的浸出率达95%以上。采用收缩核模型对还原浸出动力学进行分析,不同条件下的浸出实验结果表明反应受穿过固体产物层的扩散控制,活化能为17.96 k J/mol,相对于硫酸浓度的反应级数为2.41。铁粉置换沉铜过程铜和砷的沉淀率均达99%以上。98%以上的铟从含高亚铁离子浓度的硫酸锌溶液中选择性分离,获得铟含量约为2.4%的富铟渣,经酸浸-萃取-电积工艺流程进一步处理后可得到纯铟。 展开更多
关键词 还原浸出 高铁锌浸出渣 硫化锌精矿 动力学 铟沉淀
下载PDF
某铜铅锌硫化矿浮选分离试验研究 被引量:4
7
作者 段胜红 姜亚雄 周光浪 《矿冶工程》 CAS 北大核心 2023年第1期72-76,共5页
以云南某铜铅锌硫化矿为研究对象,采用铜-铅-锌全优先浮选工艺,通过原矿细磨和铅粗精矿选择性再磨强化矿物单体解离,充分利用组合抑制剂亚硫酸钠+硫酸锌的协调效应和选择性,捕收剂Z-200、乙硫氮及BK906的高选择性,在适宜工艺参数下,获... 以云南某铜铅锌硫化矿为研究对象,采用铜-铅-锌全优先浮选工艺,通过原矿细磨和铅粗精矿选择性再磨强化矿物单体解离,充分利用组合抑制剂亚硫酸钠+硫酸锌的协调效应和选择性,捕收剂Z-200、乙硫氮及BK906的高选择性,在适宜工艺参数下,获得了铜品位22.78%、铜回收率83.28%、含铅3.01%、含锌4.23%的铜精矿,铅品位75.86%、铅回收率82.75%、含铜0.17%、含锌1.64%的铅精矿和锌品位51.87%、锌回收率93.16%、含铜0.24%、含铅0.31%的锌精矿。 展开更多
关键词 铜铅锌硫化矿 优先浮选 铜精矿 铅精矿 锌精矿
下载PDF
某地区磁黄铁矿型铅锌硫化矿浮选试验研究
8
作者 耿亮 钟志刚 +2 位作者 曾建红 宁江峰 杨备 《矿冶工程》 CAS 北大核心 2023年第2期69-73,共5页
对某地区难选磁黄铁矿型铅锌硫化矿开展了铅、锌综合回收工艺试验研究。以新型酯类铅矿物捕收剂ZQ⁃11与25#黑药组合作铅捕收剂浮选铅矿物,铅浮选尾矿进行磁选脱硫,脱硫尾矿以丁基黄药作捕收剂浮选锌矿物,在原矿铅品位1.84%、锌品位4.53... 对某地区难选磁黄铁矿型铅锌硫化矿开展了铅、锌综合回收工艺试验研究。以新型酯类铅矿物捕收剂ZQ⁃11与25#黑药组合作铅捕收剂浮选铅矿物,铅浮选尾矿进行磁选脱硫,脱硫尾矿以丁基黄药作捕收剂浮选锌矿物,在原矿铅品位1.84%、锌品位4.53%情况下,闭路试验获得了铅品位62.57%、含锌3.30%、铅回收率89.49%的铅精矿和锌品位43.37%、含铅1.01%、锌回收率85.79%的锌精矿,实现了难选磁黄铁矿型铅锌硫化矿的有效回收。 展开更多
关键词 浮选 捕收剂 铅锌硫化矿 ZQ⁃11 锌精矿 铅精矿 磁选
下载PDF
Re-Os Dating of Galena and Sphalerite from Lead-Zinc Sulfide Deposits in Yunnan Province, SW China 被引量:17
9
作者 Yingying Liu Liang Qi +3 位作者 Jianfeng Gao Lin Ye Zhilong Huang Jiaxi Zhou 《Journal of Earth Science》 SCIE CAS CSCD 2015年第3期343-351,共9页
Dating of lead-zinc deposits is of critical importance for better understanding of ore genesis, but has long been a big challenge due to the lack of suitable minerals that can be unequivocally linked to the ore genesi... Dating of lead-zinc deposits is of critical importance for better understanding of ore genesis, but has long been a big challenge due to the lack of suitable minerals that can be unequivocally linked to the ore genesis and that can be used for tradition radiometric methods. This kind of deposits have simple mineralogy dominated by galena and sphalerite commonly associated with calcite and other gangue minerals. Both galena and sphalerite have low and high variable Re concentrations and thus Re-Os dating of these minerals have been less promising. In addition, the recovery of Re is extremely low for galena when conventional method was applied, lending additional difficulty in precisely dating galena. In this study, we investigate the recovery of Re using different media for anion exchange separation and reporte a revised preparation method for Re-Os dating of galena and sphalerite. By using the new protocol, two reliable Re-Os isochron ages of galena and sphalerite from the Fule(20.4±3.2 Ma) and Laochang(308±25 Ma) Pb-Zn deposits in Yunnan Province, SW China, are achieved. 展开更多
关键词 lead-zinc sulfide deposits Re-Os isotope dating separation and concentration of Re GALENA SPHALERITE YUNNAN
原文传递
硫化锌精矿氧压酸浸渣中综合回收硫的工艺研究
10
作者 刘贵清 解雪 +1 位作者 张帆 王芳 《中国资源综合利用》 2023年第9期1-4,共4页
氧压酸浸渣是硫化锌精矿冶炼过程的副产物,其中硫仍具有回收利用价值。某硫化锌精矿氧压酸浸渣中,粒度小于0.038 mm的占比为67.65%,硫含量为36.27%。本文采用絮凝-浮选工艺,高效回收硫化锌精矿氧压酸浸渣中的硫。其间以O-异丙基-N-乙基... 氧压酸浸渣是硫化锌精矿冶炼过程的副产物,其中硫仍具有回收利用价值。某硫化锌精矿氧压酸浸渣中,粒度小于0.038 mm的占比为67.65%,硫含量为36.27%。本文采用絮凝-浮选工艺,高效回收硫化锌精矿氧压酸浸渣中的硫。其间以O-异丙基-N-乙基氨基甲酸酯(Z-200)为捕收剂,以聚丙烯酰胺为絮凝剂,进行闭路浮选试验。试验结果表明,经一次空白浮选、两次加药和两次空白清洗,硫的回收率可达94.59%,硫精矿品位可达87.92%。作为浮选尾渣,滤饼含有硫化物,返回浸出工序进行锌回收。 展开更多
关键词 硫化锌精矿 氧压酸浸渣 单质硫 综合回收 絮凝 浮选
下载PDF
中浸渣配入硫化锌精矿氧压酸浸的工艺研究及应用
11
作者 李雨耕 雷华志 +4 位作者 李玉章 孙彦华 张永平 梁智 包稚群 《云南冶金》 2023年第S01期210-214,共5页
利用加压釜高温、高压和富氧条件,在处理硫化锌精矿的同时,对中性浸出渣进行浸出研究,取消原中浸渣处理所需的高浸、沉矾等高能耗工艺。研究结果表明:确保硫化锌精矿处理量的同时,中浸渣按一定比例入釜,锌的浸出率达到97%,渣含难溶锌小... 利用加压釜高温、高压和富氧条件,在处理硫化锌精矿的同时,对中性浸出渣进行浸出研究,取消原中浸渣处理所需的高浸、沉矾等高能耗工艺。研究结果表明:确保硫化锌精矿处理量的同时,中浸渣按一定比例入釜,锌的浸出率达到97%,渣含难溶锌小于1.5%。 展开更多
关键词 硫化锌精矿 中浸渣 加压浸出
下载PDF
某难选硫化钼铅锌矿石选矿试验研究
12
作者 梁晓 王三海 刘涛 《现代矿业》 CAS 2023年第6期260-264,共5页
我国东北某钼铅锌硫化矿石中主要有回收价值的成分为钼,可综合回收成分为铅、锌、硫,伴生回收成分为铼、金、银;钼、铅、锌主要以辉钼矿、方铅矿与闪锌矿的形式产出;这些硫化矿物的嵌连关系不密切,但嵌布粒度较细,通过细磨也难以充分解... 我国东北某钼铅锌硫化矿石中主要有回收价值的成分为钼,可综合回收成分为铅、锌、硫,伴生回收成分为铼、金、银;钼、铅、锌主要以辉钼矿、方铅矿与闪锌矿的形式产出;这些硫化矿物的嵌连关系不密切,但嵌布粒度较细,通过细磨也难以充分解离。为确定矿石的合理开发利用工艺进行了选矿试验研究。结果表明,矿石采用钼铅锌混浮—混合精矿抑铅锌浮钼—混合浮选尾矿强化锌硫混浮再分离流程处理,最终获得钼品位46.51%、回收率77.74%的钼精矿,铅锌品位分别为21.52%和16.21%、回收率分别为39.97%和6.80%的铅锌混合精矿,锌品位41.25%、回收率55.89%的锌精矿,硫品位49.46%、回收率51.98%的硫精矿。 展开更多
关键词 硫化钼铅锌矿石 混合浮选 优先浮选 混合精矿分离
下载PDF
硫化锌精矿富氧浸出的动力学研究 被引量:7
13
作者 吕国志 赵爱春 +5 位作者 张廷安 古岩 谢刚 张莹 张国权 刘燕 《中南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2014年第12期4116-4122,共7页
以硫化锌精矿为研究对象,采用富氧-硫酸浸出的方式提取矿物中的锌元素并使硫元素以单质的形态进入浸出渣中,考察浸出粒度、温度、初酸浓度、氧分压对酸浸过程动力学的影响。研究结果表明:硫化锌精矿的浸出过程由表面化学反应控制,反应遵... 以硫化锌精矿为研究对象,采用富氧-硫酸浸出的方式提取矿物中的锌元素并使硫元素以单质的形态进入浸出渣中,考察浸出粒度、温度、初酸浓度、氧分压对酸浸过程动力学的影响。研究结果表明:硫化锌精矿的浸出过程由表面化学反应控制,反应遵循"未反应核收缩模型"的表面化学反应控制的动力学规律,其反应活化能E=73.58 k J/mol。 展开更多
关键词 硫化锌精矿 富氧浸出 动力学
下载PDF
内蒙古某复杂多金属硫化矿选矿技术研究 被引量:16
14
作者 简胜 孙伟 胡岳华 《矿冶工程》 CAS CSCD 北大核心 2019年第4期50-53,62,共5页
对内蒙古某铜铅锌多金属硫化矿石进行了浮选试验研究。采用"铜铅混合浮选-铜铅分离-尾矿再选锌"的工艺流程,在磨矿细度-0.074 mm粒级占80%条件下,优化药剂制度,获得了铜精矿铜品位20.14%、铜回收率40.27%,铅精矿铅品位62.46%... 对内蒙古某铜铅锌多金属硫化矿石进行了浮选试验研究。采用"铜铅混合浮选-铜铅分离-尾矿再选锌"的工艺流程,在磨矿细度-0.074 mm粒级占80%条件下,优化药剂制度,获得了铜精矿铜品位20.14%、铜回收率40.27%,铅精矿铅品位62.46%、铅回收率93.56%,锌精矿锌品位48.84%、锌回收率89.27%的选别指标,银总回收率达到了88.01%。 展开更多
关键词 多金属硫化矿 浮选 铜铅分离 铅抑制剂 铜精矿 铅精矿 锌精矿
下载PDF
富氧硫酸体系中硫化锌精矿的常压直接浸出动力学 被引量:10
15
作者 徐志峰 朱辉 王成彦 《中国有色金属学报》 EI CAS CSCD 北大核心 2013年第12期3440-3447,共8页
采用常压浸出与加压浸出相结合的方法,研究硫化锌精矿在富氧硫酸体系中的常压直接浸出动力学。结果表明:锌浸出受界面化学反应控制,浸出反应表观活化能为(44.28±4.28)kJ/mol。浸出槽底部锌的浸出速率远高于浸出槽上部锌的浸出速率... 采用常压浸出与加压浸出相结合的方法,研究硫化锌精矿在富氧硫酸体系中的常压直接浸出动力学。结果表明:锌浸出受界面化学反应控制,浸出反应表观活化能为(44.28±4.28)kJ/mol。浸出槽底部锌的浸出速率远高于浸出槽上部锌的浸出速率,且随槽底矿浆压力的增大,锌的浸出速率明显提高。进一步基于收缩核模型,通过二次回归方法,建立浸出槽底部锌的浸出动力学方程。在硫化锌精矿常压富氧直接浸出中,对于位于浸出槽底部的锌浸出,温度的影响明显大于矿浆压力的影响。 展开更多
关键词 硫化锌精矿 硫酸 常压直接浸出 富氧 动力学
下载PDF
西藏某铜铅锌硫化矿浮选工艺研究 被引量:11
16
作者 刘安荣 唐云 陈福林 《矿冶工程》 CAS CSCD 北大核心 2009年第2期36-39,共4页
根据西藏某铜铅锌硫化矿矿石的性质,分别研究了磨矿粒度、捕收剂及工艺流程对浮选的影响。在磨矿粒度为-0.074mm占67.00%条件下,以乙黄药和乙硫氮的混合物为捕收剂,采用一粗一精两扫闭路浮选工艺流程,获得混合精矿中铜、铅、锌的品位分... 根据西藏某铜铅锌硫化矿矿石的性质,分别研究了磨矿粒度、捕收剂及工艺流程对浮选的影响。在磨矿粒度为-0.074mm占67.00%条件下,以乙黄药和乙硫氮的混合物为捕收剂,采用一粗一精两扫闭路浮选工艺流程,获得混合精矿中铜、铅、锌的品位分别为13.81%、16.74%、22.41%,回收率分别为95.47%、93.85%、94.04%。 展开更多
关键词 铜铅锌硫化矿 磨矿粒度 浮选 混合精矿
下载PDF
锌铅混合精矿加压浸出过程研究 被引量:6
17
作者 陈永强 张寅生 +1 位作者 尹飞 王飞 《有色金属》 CSCD 2003年第4期57-60,共4页
研究锌铅混合精矿加压浸出过程。结果表明,在100℃、0.6MPa氧分压下加压浸出,锌浸出率达95%,原料中的铁闪锌矿、黄铜矿、硫镉矿、磁黄铁矿和砷黄铁矿在此条件下属于易浸矿物,而黄铁矿、砷黝铜矿和银黝铜矿属于难浸矿物,方铅矿表面形成... 研究锌铅混合精矿加压浸出过程。结果表明,在100℃、0.6MPa氧分压下加压浸出,锌浸出率达95%,原料中的铁闪锌矿、黄铜矿、硫镉矿、磁黄铁矿和砷黄铁矿在此条件下属于易浸矿物,而黄铁矿、砷黝铜矿和银黝铜矿属于难浸矿物,方铅矿表面形成一层硫酸铅和铅铁矾阻碍其氧化。生成的元素硫在100℃时为疏松的硫膜,150℃时在添加剂作用下聚集成硫珠。 展开更多
关键词 锌铅混合精矿 加压浸出 硫化矿 浸出率 氧化 添加剂
下载PDF
闪锌矿与中性浸出渣合并氧压酸浸(英文) 被引量:10
18
作者 梁铎强 王吉坤 +1 位作者 周廷熙 张怀伟 《有色金属》 CAS CSCD 北大核心 2009年第4期72-76,共5页
硫化锌精矿和由传统流程得到的中浸渣混在一块,对其进行了浸出的小型试验。试验在不同的条件下进行,以考察影响浸出的各种因素,包括浸出温度、浸出时间、氧分压和搅拌速度。试验在一个两升的高压釜内进行。试验结果表明了硫化锌精矿和... 硫化锌精矿和由传统流程得到的中浸渣混在一块,对其进行了浸出的小型试验。试验在不同的条件下进行,以考察影响浸出的各种因素,包括浸出温度、浸出时间、氧分压和搅拌速度。试验在一个两升的高压釜内进行。试验结果表明了硫化锌精矿和中浸渣能相互促进浸出,但只有在一定的浸出条件下这种耦合作用才表现得比较明显。研究过程中一些机理也得到了证实。最后为了后面的扩大试验提供了关键的浸出条件:浸出温度135℃;浸出时间2h;氧分压0.8MPa;初始酸度120g/L。 展开更多
关键词 冶金技术 加压酸浸 闪锌矿 中性浸出渣
下载PDF
郴州某复杂硫化铅锌矿阶段磨浮试验研究 被引量:7
19
作者 曾维伟 阳俊 《矿冶工程》 CAS CSCD 北大核心 2020年第4期53-56,共4页
针对郴州某复杂硫化铅锌矿资源的性质特点,采用铅快速浮选后尾矿再磨再选的阶磨阶选工艺,较好地实现了铅锌的高效浮选回收。研究了磨矿方式、捕收剂和调整剂种类及用量等因素对该矿石浮选的影响,确定了最佳浮选条件,通过小型闭路浮选试... 针对郴州某复杂硫化铅锌矿资源的性质特点,采用铅快速浮选后尾矿再磨再选的阶磨阶选工艺,较好地实现了铅锌的高效浮选回收。研究了磨矿方式、捕收剂和调整剂种类及用量等因素对该矿石浮选的影响,确定了最佳浮选条件,通过小型闭路浮选试验,得到了铅品位60.05%、回收率89.63%的铅精矿和锌品位47.01%、回收率88.14%的锌精矿。 展开更多
关键词 硫化铅锌矿 阶磨阶选 硫化钠 浮选 快速浮选 铅精矿 锌精矿
下载PDF
铜-锌-硫混合粗精矿的选择性浮选分离 被引量:8
20
作者 谢海云 吴继宗 +4 位作者 田小松 肖炜 刘榕鑫 高利坤 童雄 《矿物学报》 CAS CSCD 北大核心 2019年第1期1-6,共6页
细粒嵌布型铜锌硫化矿采用粗磨后混合浮选工艺,具有回收率高和成本低的优势,但对所产出的混合精矿,亟需解决铜、锌、硫之间的高效彻底分离。云南玉溪地区铜锌硫混合粗精矿,其细度为-74μm 75%,含Cu 2.45%、Zn 4.93%、S 31.21%,笔者采用... 细粒嵌布型铜锌硫化矿采用粗磨后混合浮选工艺,具有回收率高和成本低的优势,但对所产出的混合精矿,亟需解决铜、锌、硫之间的高效彻底分离。云南玉溪地区铜锌硫混合粗精矿,其细度为-74μm 75%,含Cu 2.45%、Zn 4.93%、S 31.21%,笔者采用粗精矿再磨-铜、锌、硫选择性浮选分离工艺,研究了再磨细度、药剂种类、用量等因素对各矿物分离效果的影响。当粗精矿再磨细度为-38μm90%时,闭路试验获得品位和回收率均较高的铜、锌和硫精矿产品,铜精矿含Cu 21.00%,Cu回收率84.27%,锌精矿含Zn 48.37%,Zn回收率85.94%,硫精矿含S37.90%,S回收率82.85%,混合精矿中的铜矿物、锌矿物、硫矿物均实现了较彻底的分离。本研究为铜多金属混合精矿的有效分离提供了一种可资借鉴的方法。 展开更多
关键词 铜锌硫化矿 选矿 混合粗精矿 浮选分离
下载PDF
上一页 1 2 6 下一页 到第