The castables for ladle nozzle were developed using brown corundum as the main raw material and the right amounts of complex additives . The influence of several additives on the properties such as strength and perman...The castables for ladle nozzle were developed using brown corundum as the main raw material and the right amounts of complex additives . The influence of several additives on the properties such as strength and permanent linear change of the samples was studied . The results showed that applying complex additives improved the strength and the volume stability of the castables greatly. The campaign of the castables for ladle nozzle has increased from about 40 heats to 70 heats.展开更多
Fine bubbles will create when the inert gas is introduced to the high rapidsteel stream within the shroud nozzle between ladle and tundish. The collision and attachment amongthe bubbles and fine inclusions will promot...Fine bubbles will create when the inert gas is introduced to the high rapidsteel stream within the shroud nozzle between ladle and tundish. The collision and attachment amongthe bubbles and fine inclusions will promote the floatation efficiency of inclusions in the tundish.The behaviors of the bubbles, such as the dispersion in shroud, coalescence and floatation intundish, are studied. The results show that the maximum sizes of the bubbles in the water and steelflow within the shroud in the length of 1.2 m are 0.70-1.44 mm and 1.53-3.16 mm respectively whenthe flow rates are 0.006-0.016 m^3/s; the terminal velocities of fine bubbles in the water andmolten steel within the tundish are 0.02-0.2 and 0.05-0.6 m/s.展开更多
文摘The castables for ladle nozzle were developed using brown corundum as the main raw material and the right amounts of complex additives . The influence of several additives on the properties such as strength and permanent linear change of the samples was studied . The results showed that applying complex additives improved the strength and the volume stability of the castables greatly. The campaign of the castables for ladle nozzle has increased from about 40 heats to 70 heats.
基金The project is sponsored by the National Natural Science Foundation of China (No.50274007).
文摘Fine bubbles will create when the inert gas is introduced to the high rapidsteel stream within the shroud nozzle between ladle and tundish. The collision and attachment amongthe bubbles and fine inclusions will promote the floatation efficiency of inclusions in the tundish.The behaviors of the bubbles, such as the dispersion in shroud, coalescence and floatation intundish, are studied. The results show that the maximum sizes of the bubbles in the water and steelflow within the shroud in the length of 1.2 m are 0.70-1.44 mm and 1.53-3.16 mm respectively whenthe flow rates are 0.006-0.016 m^3/s; the terminal velocities of fine bubbles in the water andmolten steel within the tundish are 0.02-0.2 and 0.05-0.6 m/s.