期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
Low temperature hydrogen production from water and methanol over Pt/α-MoC catalysts 被引量:1
1
作者 Ma Ding (马丁) Zhou Wu (周武) +1 位作者 Wen Xiaodong (温晓东) Shi Chuan (石川) 《Science Foundation in China》 CAS 2017年第2期5-5,共1页
Subject Code:B03 With the support by the National Natural Science Foundation of China,a collaborative study by the research groups led by Prof.Ma Ding(马丁)from Peking University,Prof.Zhou Wu(周武)from the University ... Subject Code:B03 With the support by the National Natural Science Foundation of China,a collaborative study by the research groups led by Prof.Ma Ding(马丁)from Peking University,Prof.Zhou Wu(周武)from the University of Chinese Academy of Sciences,Prof.Wen Xiaodong(温晓东)from the Institute of 展开更多
关键词 OVER low temperature hydrogen production from water and methanol over Pt MoC catalysts
原文传递
Sintered Ore Sprayed by Acid and Alkaline Waste Water Resulted From Cold Rolling
2
作者 YANG Da-zheng QI Dian-wei +3 位作者 XU Peng-fei ZHANG Da-kui MA Guang-yu LI Jing 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2013年第3期36-38,共3页
In order to prevent the powdering of a sintered ore from influencing the smooth operation of a blast furnace,the conventional way to deal with it is that the CaCl2 solution is prepared by tap water,and then the soluti... In order to prevent the powdering of a sintered ore from influencing the smooth operation of a blast furnace,the conventional way to deal with it is that the CaCl2 solution is prepared by tap water,and then the solution is sprayed onto the sintered ore for improving its RDI(low temperature reduction degradation index).The CaCl2 solution prepared by adding acid and alkaline waste water resulted from cold rolling is sprayed onto the sintered ore to improve its RDI.The values of RDI+6.3 and RDI+3.15 of the sintered ore which is sprayed by the CaCl2 solution with the CaCl2 concentration of 3.5%(mass percent) are increased by 17.5% and 11.63%,but the index of RDI-0.5 is decreased by 3.1% when the spraying amount of the solution is making up 0.5% of the total sintered ore sprayed in comparison with those of the sintered ore which is not sprayed by using the CaCl2 solution.Experimental results show that after the CaCl2 solutions prepared by adding the acid and alkaline waste water are sprayed on the sintered ore,RDI of the ore can be remarkably improved and therefore another way for recycling acid and alkaline waste water can be available,by which both cost for treating waste water and cost for producing a sintered ore can be decreased and environment is free of pollution by harmful substances in the waste water. 展开更多
关键词 waste water sintered ore low temperature reduction degradation index(RDI)
原文传递