Manganese was leached from a low-grade manganese ore(LGMO)using banana peel as the reductant in a dilute sulfuric acid medium.The effects of banana peel amount,H2SO4 concentration,reaction temperature,and time on Mn l...Manganese was leached from a low-grade manganese ore(LGMO)using banana peel as the reductant in a dilute sulfuric acid medium.The effects of banana peel amount,H2SO4 concentration,reaction temperature,and time on Mn leaching from the complex LGMO were studied.A leaching efficiency of~98%was achieved at a leaching time of 2 h,banana peel amount of 4 g,leaching temperature of 120°C,manganese ore amount of 5 g,and sulfuric acid concentration of 15vol%.The phase,microstructural,and chemical analyses of LGMO samples before and after the leaching process confirmed the successful leaching of manganese.Furthermore,the leaching process followed the shrinking core model and the leaching rate was controlled by a surface chemical reaction(1−(1−x)^1/3=kt)mechanism with an apparent activation energy of 40.19 kJ·mol^−1.展开更多
The recovery of zinc from low-grade zinc oxide ores with solvent extraction-electrowinning technique was investigated by using D2EHPA as extractant and 260 # kerosene as diluent. The results show that it is possible t...The recovery of zinc from low-grade zinc oxide ores with solvent extraction-electrowinning technique was investigated by using D2EHPA as extractant and 260 # kerosene as diluent. The results show that it is possible to selectively leach zinc from the ores by heap leaching. The zinc concentration of leach solution in the first leaching cycle is 32.57 g/L, and in the sixteenth cycle the zinc concentration is 8.27g/L after solvent extraction. The leaching solution is subjected to solvent extraction, scrubbing and selective stripping for enrichment of zinc and removal of impurities. The pregnant zinc sulfate solution produced from the stripping cycle is suitable for zinc electrowinning. Extra-pure zinc metal was obtained in the electrowinning test under conventional conditions.展开更多
This article reports the study on acid equilibrium during bioleaching of alkaline low-grade copper sulfide ore. Adding auxiliary agents 1# (sulfur) and 2# (pyrite) makes bacterial leaching of copper and acid produ...This article reports the study on acid equilibrium during bioleaching of alkaline low-grade copper sulfide ore. Adding auxiliary agents 1# (sulfur) and 2# (pyrite) makes bacterial leaching of copper and acid production carried out simultaneously because the auxiliary agents can be oxidized by bacteria and the oxidation products involve acid. The acid required for dissolving alkaline gangue during bacterial leaching is produced, and acid equilibrium is reached during the ore bio-leaching. The recovery of copper reaches more than 95%.展开更多
The hydrometallurgical strategy of extracting Mn from low-grade Mn ores has attracted attention for the production of electrolytic manganese metal(EMM). In this work, the reductive dissolution of low-grade Mn O2 ores ...The hydrometallurgical strategy of extracting Mn from low-grade Mn ores has attracted attention for the production of electrolytic manganese metal(EMM). In this work, the reductive dissolution of low-grade Mn O2 ores using toxic nitrocellulose acidic wastewater(NAW) as a reductant was investigated for the first time. Under the optimized conditions of an Mn O2 ore dosage of 100 g·L-1, an ore particle size of-200 mesh, concentrated H2 SO4-to-NAW volume ratio of 0.12, reaction temperature of 90°C, stirring speed at 160 r·min-1, and a contact time of 120 min, the reductive leaching efficiency of Mn and the total organic carbon(TOC) removal efficiency of NAW reached 97.4% and 98.5%, respectively. The residual TOC of 31.6 mg·L-1 did not adversely affect the preparation of EMM. The current process offers a feasible route for the concurrent realization of the reductive leaching of Mn and the treatment of toxic wastewater via a simple one-step process.展开更多
In order to economically recover the copper from the low grade copper ores, a bioleaching solvent extraction electrowinning plant with a design capacity of 2 000 t cathode copper per year in Dexing Copper Mine was ope...In order to economically recover the copper from the low grade copper ores, a bioleaching solvent extraction electrowinning plant with a design capacity of 2 000 t cathode copper per year in Dexing Copper Mine was operated in September, 1997. The results during the 10 month period of the industrial copper dump leaching have been obtained and the approaches have been carried out to enhance the copper dissolution from the waste rocks. The overall operation flowsheet is depicted. The problems confronted in the process and possible way for improving are discussed.展开更多
Rare earth resources are relatively scarce worldwide, but their global consumption is increasing year-by-year. At present, China has about 36% of the global rare earth reserves, but provides 90% of the world's supply...Rare earth resources are relatively scarce worldwide, but their global consumption is increasing year-by-year. At present, China has about 36% of the global rare earth reserves, but provides 90% of the world's supply, which has generally met world demand and promoted the development of the world economy. In order to continuously and stably supply rare earths to international markets, the Chinese Government has financially supported the Institute of Multipurpose Utilization of Mineral Resources within the China Geological Survey to study the utilization of low-grade rare earth ores. Following many years of experimental research, the project has developed a new technology entitled "Flotation to Form Agglomerates and then Magnetic Separation", which will bring a technological revolution to the world's light rare earth ore dressing.展开更多
Bacterial community dynamics and copper leaching with applied forced aeration were investigated during low-grade copper sulphide bioleaching to obtain better bioleaching efficiency.Results illustrated that appropriate...Bacterial community dynamics and copper leaching with applied forced aeration were investigated during low-grade copper sulphide bioleaching to obtain better bioleaching efficiency.Results illustrated that appropriate aeration improved bacterial concentrations and leaching efficiencies.The highest bacterial concentration and Cu^(2+)concentration after 14-d leaching were 7.61×10^(7) cells·mL^(−1) and 704.9 mg·L^(−1),respectively,at aeration duration of 4 h·d^(−1).The attached bacteria played a significant role during bioleaching from 1 to 7 d.However,free bacteria dominated the bioleaching processes from 8 to 14 d.This phenomenon was mainly caused by the formation of passivation layer through Fe3+hydrolysis along with bioleaching,which inhibited the contact between the attached bacteria and ore.Meanwhile,16S rDNA analysis verified the effect of Acidithiobacillus ferrooxidans and Acidithiobacillus thiooxidans on the bioleaching process.The results demonstrate the importance of free and attached bacteria in bioleaching.展开更多
A low-grade ore containing ~0.3% Cu, remains unutilized for want of a viable process at Malanjkhand Copper Project (MCP), India in which copper is present as chalcopyrite associated with pyrite in quartz veins and gra...A low-grade ore containing ~0.3% Cu, remains unutilized for want of a viable process at Malanjkhand Copper Project (MCP), India in which copper is present as chalcopyrite associated with pyrite in quartz veins and granitic rocks. In order to extract copper from this material, bioleaching has been attempted on bench scale using Acidithiobacillus fer-rooxidans (A. ferrooxidans) isolated from the native mine water. The enriched culture containing A. ferrooxidans when adapted to the ore and employed for the bioleaching at 5% (w/v) pulp density, pH 2.0 and 25°C with three particle sizes viz.150 -76 μm, 76 - 50 μm and SCE) from 530 to 654 mV in 35 days. Under similar conditions, the unadapted strains gave a recovery of 44.0% for SCE from 525 to 650 mV. On using unadapted bacte-rial culture directly in shake flask at pH 2.0 and 35°C temperature and 5% (w/v) pulp density (PD) for 9 cells/mL in 35 days. The higher bio-recovery of copper with the adapted bacterial culture may be attributed to the improved iron oxidation (Fe2+ to Fe3+) exhibiting higher ESCE as compared to that of unadapted strains.展开更多
The development and utilization of low-grade polymetallic deposits with strategic mineral resources is one of the important measures to alleviate the current high dependence on strategic mineral resources in China. Ho...The development and utilization of low-grade polymetallic deposits with strategic mineral resources is one of the important measures to alleviate the current high dependence on strategic mineral resources in China. However, domestic mining enterprises and most mining consulting and design institutes usually use general industrial indicators to carry out reserve estimation and technical and economic feasibility studies on low-grade polymetallic deposits, which cannot truly reflect the economic value of such deposits. The article expounds on the definitions of net return value (NSR) and on-site total maintenance cost (AISC) of common ore smelters in the evaluation of overseas mineral resources. Taking a low-grade polymetallic copper-molybdenum mine in Guangdong Province as an example, comparing the research results showed the NSR-AISC method and the general industrial index method in low-grade polymetallic deposit. There are huge differences in the results of reserve estimation;through the further introduction of Taylor’s formula and the research results on the relationship between investment intensity and production scale, a more reasonable mine life and investment scale are recommended, and a more in-depth comparative study has been carried out in the dimension of technical and economic indicators. Based on the comparative study of the above two methods in reserve estimation and the evaluation results of technical and economic indicators, the author believes that the NSR-AISC method can better reflect the true value of low-grade polymetallic ore projects, and should be popularized and applied in resource evaluation and development practice. This article further describes the application status of the NSR-AISC method for reserve estimation and the evaluation of technical economic indicators, and suggests the main points that should be paid attention to in the use of the NSR-AISC method.展开更多
Stainless steel crude alloy recovery from direct smelting of low-grade chromite, nickel laterite and manganese ores was investigated. The mixed low-grade ores were directly smelted in an elevator furnace at smelting t...Stainless steel crude alloy recovery from direct smelting of low-grade chromite, nickel laterite and manganese ores was investigated. The mixed low-grade ores were directly smelted in an elevator furnace at smelting temperatures ranging from 1550 to 1600 ℃. Smelting experiments were conducted in a laboratory elevator furnace equipped with 8 U-shaped high- quality molybdenum disilicide heating elements. A low-grade coal was used as the reductant. Experimental results showed that the recovery of Fe, Cr, Ni, Mn and Si within the alloy increased from 34.22, 60.27, 57.14, 25.42 and 13.02% to 69.91, 99.26, 86.02, 60.8 and 34.21%, respectively, when the temperature was increased from 1550 to 1600 ℃. There was a general increase in the total recoveries of Fe, Cr, and Ni in the alloy with CaO addition increasing from 0.4 g up to 1.2 g. However, the recoveries of Mn and Si vividly decreased as the CaO contents were increased. In general, the recoveries of the metal contents of the crude alloy increase with the increase in the amount of manganese ore. Compared to the recoveries of Fe, Cr, and Ni when CaO was added, the recoveries of Fe, Cr and Ni were lower when manganese ore was used as an additive.展开更多
文摘Manganese was leached from a low-grade manganese ore(LGMO)using banana peel as the reductant in a dilute sulfuric acid medium.The effects of banana peel amount,H2SO4 concentration,reaction temperature,and time on Mn leaching from the complex LGMO were studied.A leaching efficiency of~98%was achieved at a leaching time of 2 h,banana peel amount of 4 g,leaching temperature of 120°C,manganese ore amount of 5 g,and sulfuric acid concentration of 15vol%.The phase,microstructural,and chemical analyses of LGMO samples before and after the leaching process confirmed the successful leaching of manganese.Furthermore,the leaching process followed the shrinking core model and the leaching rate was controlled by a surface chemical reaction(1−(1−x)^1/3=kt)mechanism with an apparent activation energy of 40.19 kJ·mol^−1.
文摘The recovery of zinc from low-grade zinc oxide ores with solvent extraction-electrowinning technique was investigated by using D2EHPA as extractant and 260 # kerosene as diluent. The results show that it is possible to selectively leach zinc from the ores by heap leaching. The zinc concentration of leach solution in the first leaching cycle is 32.57 g/L, and in the sixteenth cycle the zinc concentration is 8.27g/L after solvent extraction. The leaching solution is subjected to solvent extraction, scrubbing and selective stripping for enrichment of zinc and removal of impurities. The pregnant zinc sulfate solution produced from the stripping cycle is suitable for zinc electrowinning. Extra-pure zinc metal was obtained in the electrowinning test under conventional conditions.
文摘This article reports the study on acid equilibrium during bioleaching of alkaline low-grade copper sulfide ore. Adding auxiliary agents 1# (sulfur) and 2# (pyrite) makes bacterial leaching of copper and acid production carried out simultaneously because the auxiliary agents can be oxidized by bacteria and the oxidation products involve acid. The acid required for dissolving alkaline gangue during bacterial leaching is produced, and acid equilibrium is reached during the ore bio-leaching. The recovery of copper reaches more than 95%.
基金financially supported by the National Natural Science Foundation of China (No. 21277012)the Nature Scientific Research Foundation of Shaanxi Provincial Education Office of China (No. 17JK0864)the Scientific Research Foundation for Ph D of Yan'an University(No. YDBK2018-10)
文摘The hydrometallurgical strategy of extracting Mn from low-grade Mn ores has attracted attention for the production of electrolytic manganese metal(EMM). In this work, the reductive dissolution of low-grade Mn O2 ores using toxic nitrocellulose acidic wastewater(NAW) as a reductant was investigated for the first time. Under the optimized conditions of an Mn O2 ore dosage of 100 g·L-1, an ore particle size of-200 mesh, concentrated H2 SO4-to-NAW volume ratio of 0.12, reaction temperature of 90°C, stirring speed at 160 r·min-1, and a contact time of 120 min, the reductive leaching efficiency of Mn and the total organic carbon(TOC) removal efficiency of NAW reached 97.4% and 98.5%, respectively. The residual TOC of 31.6 mg·L-1 did not adversely affect the preparation of EMM. The current process offers a feasible route for the concurrent realization of the reductive leaching of Mn and the treatment of toxic wastewater via a simple one-step process.
文摘In order to economically recover the copper from the low grade copper ores, a bioleaching solvent extraction electrowinning plant with a design capacity of 2 000 t cathode copper per year in Dexing Copper Mine was operated in September, 1997. The results during the 10 month period of the industrial copper dump leaching have been obtained and the approaches have been carried out to enhance the copper dissolution from the waste rocks. The overall operation flowsheet is depicted. The problems confronted in the process and possible way for improving are discussed.
文摘Rare earth resources are relatively scarce worldwide, but their global consumption is increasing year-by-year. At present, China has about 36% of the global rare earth reserves, but provides 90% of the world's supply, which has generally met world demand and promoted the development of the world economy. In order to continuously and stably supply rare earths to international markets, the Chinese Government has financially supported the Institute of Multipurpose Utilization of Mineral Resources within the China Geological Survey to study the utilization of low-grade rare earth ores. Following many years of experimental research, the project has developed a new technology entitled "Flotation to Form Agglomerates and then Magnetic Separation", which will bring a technological revolution to the world's light rare earth ore dressing.
基金This work was supported by National Science Foundation for Excellent Young Scholars,China(No.51722401)Key Project of National Natural Science Foundation,China(No.51734001)Fundamental Research Funds for the Central Universities(No.FRF-TP-18-003C1).
文摘Bacterial community dynamics and copper leaching with applied forced aeration were investigated during low-grade copper sulphide bioleaching to obtain better bioleaching efficiency.Results illustrated that appropriate aeration improved bacterial concentrations and leaching efficiencies.The highest bacterial concentration and Cu^(2+)concentration after 14-d leaching were 7.61×10^(7) cells·mL^(−1) and 704.9 mg·L^(−1),respectively,at aeration duration of 4 h·d^(−1).The attached bacteria played a significant role during bioleaching from 1 to 7 d.However,free bacteria dominated the bioleaching processes from 8 to 14 d.This phenomenon was mainly caused by the formation of passivation layer through Fe3+hydrolysis along with bioleaching,which inhibited the contact between the attached bacteria and ore.Meanwhile,16S rDNA analysis verified the effect of Acidithiobacillus ferrooxidans and Acidithiobacillus thiooxidans on the bioleaching process.The results demonstrate the importance of free and attached bacteria in bioleaching.
文摘A low-grade ore containing ~0.3% Cu, remains unutilized for want of a viable process at Malanjkhand Copper Project (MCP), India in which copper is present as chalcopyrite associated with pyrite in quartz veins and granitic rocks. In order to extract copper from this material, bioleaching has been attempted on bench scale using Acidithiobacillus fer-rooxidans (A. ferrooxidans) isolated from the native mine water. The enriched culture containing A. ferrooxidans when adapted to the ore and employed for the bioleaching at 5% (w/v) pulp density, pH 2.0 and 25°C with three particle sizes viz.150 -76 μm, 76 - 50 μm and SCE) from 530 to 654 mV in 35 days. Under similar conditions, the unadapted strains gave a recovery of 44.0% for SCE from 525 to 650 mV. On using unadapted bacte-rial culture directly in shake flask at pH 2.0 and 35°C temperature and 5% (w/v) pulp density (PD) for 9 cells/mL in 35 days. The higher bio-recovery of copper with the adapted bacterial culture may be attributed to the improved iron oxidation (Fe2+ to Fe3+) exhibiting higher ESCE as compared to that of unadapted strains.
文摘The development and utilization of low-grade polymetallic deposits with strategic mineral resources is one of the important measures to alleviate the current high dependence on strategic mineral resources in China. However, domestic mining enterprises and most mining consulting and design institutes usually use general industrial indicators to carry out reserve estimation and technical and economic feasibility studies on low-grade polymetallic deposits, which cannot truly reflect the economic value of such deposits. The article expounds on the definitions of net return value (NSR) and on-site total maintenance cost (AISC) of common ore smelters in the evaluation of overseas mineral resources. Taking a low-grade polymetallic copper-molybdenum mine in Guangdong Province as an example, comparing the research results showed the NSR-AISC method and the general industrial index method in low-grade polymetallic deposit. There are huge differences in the results of reserve estimation;through the further introduction of Taylor’s formula and the research results on the relationship between investment intensity and production scale, a more reasonable mine life and investment scale are recommended, and a more in-depth comparative study has been carried out in the dimension of technical and economic indicators. Based on the comparative study of the above two methods in reserve estimation and the evaluation results of technical and economic indicators, the author believes that the NSR-AISC method can better reflect the true value of low-grade polymetallic ore projects, and should be popularized and applied in resource evaluation and development practice. This article further describes the application status of the NSR-AISC method for reserve estimation and the evaluation of technical economic indicators, and suggests the main points that should be paid attention to in the use of the NSR-AISC method.
文摘Stainless steel crude alloy recovery from direct smelting of low-grade chromite, nickel laterite and manganese ores was investigated. The mixed low-grade ores were directly smelted in an elevator furnace at smelting temperatures ranging from 1550 to 1600 ℃. Smelting experiments were conducted in a laboratory elevator furnace equipped with 8 U-shaped high- quality molybdenum disilicide heating elements. A low-grade coal was used as the reductant. Experimental results showed that the recovery of Fe, Cr, Ni, Mn and Si within the alloy increased from 34.22, 60.27, 57.14, 25.42 and 13.02% to 69.91, 99.26, 86.02, 60.8 and 34.21%, respectively, when the temperature was increased from 1550 to 1600 ℃. There was a general increase in the total recoveries of Fe, Cr, and Ni in the alloy with CaO addition increasing from 0.4 g up to 1.2 g. However, the recoveries of Mn and Si vividly decreased as the CaO contents were increased. In general, the recoveries of the metal contents of the crude alloy increase with the increase in the amount of manganese ore. Compared to the recoveries of Fe, Cr, and Ni when CaO was added, the recoveries of Fe, Cr and Ni were lower when manganese ore was used as an additive.