期刊文献+
共找到233篇文章
< 1 2 12 >
每页显示 20 50 100
Effects of Potassium Ferrate and Low-Temperature Thermal Hydrolysis Co-Pretreatment on the Hydrolysis and Anaerobic Digestion Process of Waste Activated Sludge
1
作者 MA Yingpeng HAO Di +3 位作者 YAO Shuo ZHANG Dahai LI Xianguo FENG Lijuan 《Journal of Ocean University of China》 SCIE CAS CSCD 2023年第6期1583-1591,共9页
This study evaluated the effect of potassium ferrate(PF)and low-temperature thermal hydrolysis co-pretreatment on the promotion of sludge hydrolysis process and the impact on acid production in the subsequent anaerobi... This study evaluated the effect of potassium ferrate(PF)and low-temperature thermal hydrolysis co-pretreatment on the promotion of sludge hydrolysis process and the impact on acid production in the subsequent anaerobic digestion process.The analytical investigations showed that co-pretreatment significantly facilitated the hydrolysis process of the sludge and contributed to the accumulation of short-chain fatty acids(SCFAs).The pretreatment conditions under the optimal leaching of organic matter from sludge were hydrothermal temperature of 75℃,hydrothermal treatment time of 12 h,and PF dosage of 0.25 g g^(−1)TSS(total suspended solids),according to the results of orthogonal experiments.By pretreatment under proper conditions,the removal rate of soluble chemical oxygen demand(SCOD)achieved 71.8%at the end of fermentation and the removal rate of total phosphorus(TP)was 69.1%.The maximum yield of SCFAs was 750.3 mg L^(−1),7.45 times greater than that of the blank group.Based on the analysis of the anaerobic digestion mechanism,it was indicated that the co-pretreatment could destroy the floc structure on the sludge surface and improve organic matter dissolving,resulting in more soluble organic substances for the acidification process.Furthermore,microbial community research revealed that the main cause of enhanced SCFAs generation was an increase in acidogenic bacteria and a reduction of methanogenic bacteria. 展开更多
关键词 waste activated sludge potassium ferrate low-temperature thermal hydrolysis anaerobic digestion short-chain fatty acids
下载PDF
Low-temperature Denitration Mechanism of NH_(3)-SCR over Fe/AC Catalyst
2
作者 杨征宇 黄帮福 +3 位作者 ZHANG Guifang DAI Meng WEN Zhenjing LI Wanjun 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS CSCD 2023年第3期475-484,共10页
To study the modification mechanism of activated carbon(AC)by Fe and the low-temperature NH_(3)-selective catalytic reduction(SCR)denitration mechanism of Fe/AC catalysts,Fe/AC catalysts were prepared using coconut sh... To study the modification mechanism of activated carbon(AC)by Fe and the low-temperature NH_(3)-selective catalytic reduction(SCR)denitration mechanism of Fe/AC catalysts,Fe/AC catalysts were prepared using coconut shell AC activated by nitric acid as the support and iron oxide as the active component.The crystal structure,surface morphology,pore structure,functional groups and valence states of the active components of Fe/AC catalysts were characterised by X-ray diffraction,scanning electron microscopy,nitrogen adsorption and desorption,Fourier transform infrared spectroscopy and X-ray photoelectron spectroscopy,respectively.The effect of Fe loading and calcination temperature on the low-temperature denitration of NH_(3)-SCR over Fe/AC catalysts was studied using NH_(3)as the reducing gas at low temperature(150℃).The results show that the iron oxide on the Fe/AC catalyst is spherical and uniformly dispersed on the surface of AC,thereby improving the crystallisation performance and increasing the number of active sites and specific surface area on AC in contact with the reaction gas.Hence,a rapid NH_(3)-SCR reaction was realised.When the roasting temperature remains constant,the iron oxide crystals formed by increasing the amount of loading can enter the AC pore structure and accumulate to form more micropores.When the roasting temperature is raised from 400 to 500℃,the iron oxide is mainly transformed fromα-Fe_(2)O_(3)toγ-Fe_(2)O_(3),which improves the iron oxide dispersion and increases its denitration active site,allowing gas adsorption.When the Fe loading amount is 10%,and the roasting temperature is 500℃,the NO removal rate of the Fe/AC catalyst can reach 95%.According to the study,the low-temperature NH_(3)-SCR mechanism of Fe/AC catalyst is proposed,in which the redox reaction between Fe~(2+)and Fe~(3+)will facilitate the formation of reactive oxygen vacancies,which increases the amount of oxygen adsorption on the surface,especially the increase in surface acid sites,and promotes and adsorbs more reaction gases(NH_(3),O_(2),NO).The transformation from the standard SCR reaction to the fast SCR reaction is accelerated. 展开更多
关键词 nitric acid activation method coconut shell activated carbon Fe/AC catalyst NH_(3)-scr low-temperature denitrification mechanism
下载PDF
NH_(3)SO_(3)改性稀土尾矿催化剂NH_(3)-SCR脱硝活性及SO_(2)/H_(2)O耐受性能研究
3
作者 焦坤灵 焦晓云 +3 位作者 刘佳杰 汪思瀛 李娜 武文斐 《稀有金属与硬质合金》 CAS CSCD 北大核心 2024年第2期32-37,75,共7页
采用球磨、微波焙烧方法制备了不同质量分数NH_(3)SO_(3)改性稀土尾矿NH_(3)-SCR脱硝催化剂。通过BET、SEM-EDS、XRD、NH_(3)-TPD、H_(2)-TPR分析了催化剂脱硝活性及SO_(2)/H_(2)O耐受性能。结果表明:NH_(3)SO_(3)改性使催化剂脱硝活性... 采用球磨、微波焙烧方法制备了不同质量分数NH_(3)SO_(3)改性稀土尾矿NH_(3)-SCR脱硝催化剂。通过BET、SEM-EDS、XRD、NH_(3)-TPD、H_(2)-TPR分析了催化剂脱硝活性及SO_(2)/H_(2)O耐受性能。结果表明:NH_(3)SO_(3)改性使催化剂脱硝活性得到了显著提高,10%NH_(3)SO_(3)改性催化剂在300~350℃脱硝活性可达90%左右。SO_(2)/H_(2)O共同作用可将10%NH_(3)SO_(3)改性催化剂脱硝活性提高至97%,其促进作用保持了良好的稳定性,且具有可逆性。NH_(3)SO_(3)改性稀土尾矿后,催化剂比表面积、酸性位点及强度增加,表面活性物质分散度更高,弱化了尾矿矿物晶型,提高了催化剂吸附能力和氧化还原能力,从而提高催化脱硝活性,同时具备优良的SO_(2)/H_(2)O耐受性。 展开更多
关键词 NH_(3)SO_(3)改性 稀土尾矿 催化剂 NH_(3)-scr脱硝 SO_(2)/H_(2)O耐受性能 脱硝活性
下载PDF
Low-Temperature SCR of NO with NH_3 on Mn-Based Catalysts Modified with Cerium 被引量:5
4
作者 唐晓龙 郝吉明 +1 位作者 易红宏 宁平 《Journal of Rare Earths》 SCIE EI CAS CSCD 2007年第S1期240-243,共4页
A series of Mn-based catalysts, MnOx, MnOx-CeO, Pd-Mn-Ce, MnOx/AC were prepared. And their performances for NO low-temperature SCR were investigated in this study. The NO conversion is about 90% at 100 ℃ on MnOx-CeOa... A series of Mn-based catalysts, MnOx, MnOx-CeO, Pd-Mn-Ce, MnOx/AC were prepared. And their performances for NO low-temperature SCR were investigated in this study. The NO conversion is about 90% at 100 ℃ on MnOx-CeOand almost all NO can be converted at 120 ℃. Similar results are also observed in the tests on MnOx-CeO/AC. The excellent low-temperature catalytic activity of modified Mn-based catalysts, which may be mainly due to the oxygen storage function of CeO, can improve the oxygen flow on the catalysts surface. Then the oxidation of NO to NO2 is accelerated, which is the key step of NO SCR. 展开更多
关键词 low-temperature selective catalytic reduction (scr) NO CERIUM rare earths
下载PDF
V-MoO_(x)对FeTiO_(x)/TiO_(2)催化剂上NH_(3)-SCR反应活性的影响
5
作者 刘淑珍 边春艺 +2 位作者 于浩 訾学红 宋丽云 《化学研究与应用》 CAS 北大核心 2024年第4期868-875,共8页
氮氧化物(NO_(x))是当前重要的大气污染物之一,其主要治理技术有选择性催化还原(SCR)、吸附法等,其中前者应用最为广泛。随着中低温SCR脱硝技术在钢铁、水泥、垃圾焚烧等行业的应用,NO_(x)排放得到有效控制。催化剂是SCR技术的核心,以Fe... 氮氧化物(NO_(x))是当前重要的大气污染物之一,其主要治理技术有选择性催化还原(SCR)、吸附法等,其中前者应用最为广泛。随着中低温SCR脱硝技术在钢铁、水泥、垃圾焚烧等行业的应用,NO_(x)排放得到有效控制。催化剂是SCR技术的核心,以FeTiO_(x)/TiO_(2)催化材料为主要研究对象,考察该催化剂及负载V_(2)O_(5)和MoO_(3)后的V-Mo/FeTiO_(x)/TiO_(2)催化剂的SCR性能,通过多项表征技术研究催化剂结构与性能的关系,为脱硝催化剂性能优化提供参考。结果表明:V-Mo/FeTiO_(x)/TiO_(2)催化剂因其较好的氧化还原性能、较多的弱酸性位点,在200-400℃范围内具有较高的催化活性;催化剂吸附NH_(3)前后的IR结果表明,负载钒钼后的催化剂L酸位点和B酸位点强度均高于负载前的催化剂,吸附NO_(2)前后的IR结果表明FeTiO_(x)/TiO_(2)催化剂表面的活性位点被大量硝酸盐物种覆盖。 展开更多
关键词 NO_(x) scr 催化活性 酸性位点 催化剂
下载PDF
Fe Promotion Effect in Mn/USY for Low-temperature Selective Catalytic Reduction of NO with NH_(3) 被引量:7
6
作者 Qi Chun LIN Ji Ming HAO Jun Hua LI 《Chinese Chemical Letters》 SCIE CAS CSCD 2006年第7期991-994,共4页
A series of catalysts of Mn/USY and Mn-Fe/USY prepared by impregnation were studied for low-temperature selective catalytic reduction (SCR) of NO with NH3 in the presence of excess of oxygen. It was found that the a... A series of catalysts of Mn/USY and Mn-Fe/USY prepared by impregnation were studied for low-temperature selective catalytic reduction (SCR) of NO with NH3 in the presence of excess of oxygen. It was found that the addition of Fe enhanced the catalytic performance at low-temperature. Mn-Fe/USY catalyst yielded nearly 100% NO conversion in a range of temperature from 423 to 573 K at a space velocity of 36 000 cm3g^-1·h^-1. Coexistence of manganese and iron oxides enhanced the dispersion of the supported oxides, no visible phase of the oxides can be observed on catalyst. The addition of Fe enhanced the number and strength of the Bronsted and Lewis acid sites on the surface of the catalyst, which might promote the absorption of NH3 to form active intermediate and enhance the catalytic performance at low-temperature. 展开更多
关键词 low-temperature scr Mn/USY Mn-Fe/USY scr of NO with NH3.
下载PDF
Surface chemical properties and pore structure of the activated coke and their effects on the denitrification activity of selective catalytic reduction 被引量:8
7
作者 Wei Xie Daming Liang +2 位作者 Lanting Li Sijian Qu Wu Tao 《International Journal of Coal Science & Technology》 EI 2019年第4期595-602,共8页
In order to study the mechanism of selective catalytic reduction of activated coke to remove NO in low-temperature flue gas and provide some theoretical basis for the development of related technologies.The pore sized... In order to study the mechanism of selective catalytic reduction of activated coke to remove NO in low-temperature flue gas and provide some theoretical basis for the development of related technologies.The pore sizedistribution and BET specific surface area of AC were obtain by data analyzing of N2 adsorption/desorption isotherm at -196 ℃ and carbon matrix and surface chemistry of virgin activated coke samples were characterized by acid-base titration and XPS.The process of selective catalytic reduction of activated coke (AC) samples with NH3 as reducing agent was studied in a fixed bed reactor at 150 ℃.The result shows that pore size distribution or BET specific surface of activated cokes have not correlation with denitrification activity for SCR.The NO reduction activities of the activated cokes are apparent to increase with their surface oxygen element content and total amount of acidic sites.Obviously there is good linear relationship between the NH3 adsorption capacity and activity for SCR with linear correlation coefficient 0.943.It has been presented that adsorption of NH3 on acidic functional groups in the edge of large polycyclic aromatic ring of activated coke is key rate controlling step in the SCR heterogeneous catalytic reaction. 展开更多
关键词 activATED COKE scr PORE structure Surface chemical properties DENITRIFICATION
下载PDF
Cu-ZSM-5分子筛催化剂对NH_(3)-SCR催化性能的影响
8
作者 裴婕 刘明康 《化学工程师》 CAS 2023年第8期97-100,105,共5页
本文以H-ZSM-5分子筛为基础,考察了制备方法、铜源类型以及铜含量对Cu-ZSM-5分子筛催化剂的NH_(3)选择性催化还原NO(NH_(3)-SCR)的性能影响。结果表明,采用离子交换法制备的Cu改性ZSM-5分子筛的NH_(3)-SCR活性最好;以Cu(NO3)2·3H2... 本文以H-ZSM-5分子筛为基础,考察了制备方法、铜源类型以及铜含量对Cu-ZSM-5分子筛催化剂的NH_(3)选择性催化还原NO(NH_(3)-SCR)的性能影响。结果表明,采用离子交换法制备的Cu改性ZSM-5分子筛的NH_(3)-SCR活性最好;以Cu(NO3)2·3H2O为前驱体的Cu-ZSM-5催化剂具有最佳的低温NH_(3)-SCR催化活性,并且获得了最宽的活性温度窗口;制备所得4种不同铜含量样品中,铜含量负载为2.84%的Cu-ZSM-5分子筛催化剂的活性温度窗口范围最大,在200~600℃范围内NO转化率在90%以上。由此可以说明,引入Cu2+后能够明显提高ZSM-5分子筛的催化活性。此外,XRD分析结果显示,Cu-ZSM-5催化剂的晶相结构并未改变,SEM扫描发现分子筛的形貌并未改变,但粒径变小。本文通过考察Cu-ZSM-5分子筛催化剂的NH_(3)-SCR催化性能,为进一步制备高性能脱硝分子筛催化剂研究提供了实验依据。 展开更多
关键词 Cu-ZSM-5分子筛催化剂 NO转化率 活性温度 NH_(3)-scr
下载PDF
Enhancement in Activity of a Vanadium Catalyst for the Oxidation of Sulfur Dioxide by Radio Frequency Plasma During the Preparation Process 被引量:2
9
作者 Zhenxing Chen, Honggui Li, Lingsen WangState Key Laboratory for Powder Metallurgy, College of Chemistry and Chemical Engineering, Central South University, Changsha 410083, China 《Journal of Natural Gas Chemistry》 EI CAS CSCD 2003年第3期195-200,共6页
Radio frequency plasma was used to prepare a vanadium catalyst. The resultsshowed that activating time of the catalyst could be shortened quickly and the catalytic activitywas improved to some extent with the use of p... Radio frequency plasma was used to prepare a vanadium catalyst. The resultsshowed that activating time of the catalyst could be shortened quickly and the catalytic activitywas improved to some extent with the use of plasma. Catalyst Ls-9 was prepared under an optimalcondition of 40 W discharge power, 10 min discharge time and 8 Pa gas pressure. The catalyticactivity was up to 54.7% at 410℃, which was 2.2% higher than that of the Ls-8 catalyst. Only 10 minwas needed to activate the catalyst with plasma, which was 1/9 of the traditional calcination time.For Ls-9, both the endothermic as well as the exothermic peaks detected by differential thermalanalysis shifted to higher temperatures obviously, indicating that its crystal phase could melteasily. There existed an apparent endothermic peak at 283℃. SEM photographs showed a uniform sizedistribution. It is inferred that the quadrivalent vanadium compound may exist mainly in the form ofVOSO_4. 展开更多
关键词 PLASMA activATION DISPERSION vanadium catalyst low-temperature activity
下载PDF
SCR脱硝系统的改进线性自抗扰优化控制研究 被引量:1
10
作者 杨超杰 刘长良 +1 位作者 王梓齐 韩超 《动力工程学报》 CAS CSCD 北大核心 2023年第7期893-900,共8页
针对SCR脱硝系统大惯性、大迟延、多扰动问题,提出一种模型辅助迟延线性自抗扰控制(MDLADRC)。首先,利用模型信息,将高阶纯迟延系统补偿为一阶惯性环节;然后,根据闭环系统二自由度表达式,推导最优参数量化公式,简化参数调节,并通过参数... 针对SCR脱硝系统大惯性、大迟延、多扰动问题,提出一种模型辅助迟延线性自抗扰控制(MDLADRC)。首先,利用模型信息,将高阶纯迟延系统补偿为一阶惯性环节;然后,根据闭环系统二自由度表达式,推导最优参数量化公式,简化参数调节,并通过参数遍历实验验证控制器参数与响应指标的关系;最后,将MDLADRC应用于选择性催化还原(SCR)脱硝控制系统,并与多种控制器性能进行比较。结果表明:对于SCR脱硝系统这类高阶大惯性大迟延系统,MDLADRC的定值跟随以及抗干扰能力更优;蒙特卡洛实验和多工况实验进一步说明MDLADRC的鲁棒性较优;此外,MDLADRC参数调节简单,更适用于工程实际。 展开更多
关键词 scr脱硝 自抗扰控制 史密斯预估 二自由度 蒙特卡洛实验
下载PDF
Ce改性对活化稀土尾矿催化剂NH3-SCR脱硝性能的影响
11
作者 侯丽敏 许杰 +4 位作者 王甜甜 乔超越 陈翰 付善聪 武文斐 《稀有金属与硬质合金》 CAS CSCD 北大核心 2023年第2期60-67,共8页
白云鄂博稀土尾矿主要成分为赤铁矿、氟碳铈矿、萤石、石英和磁铁矿,其中稀土元素Ce和过渡金属Fe、Mn等是催化剂所需活性元素。本文利用浸渍法对活化稀土尾矿进行Ce改性,借助SEM-EDS、XRD、BET、NH_(3)-TPD、H_(2)-TPR、XPS等表征手段探... 白云鄂博稀土尾矿主要成分为赤铁矿、氟碳铈矿、萤石、石英和磁铁矿,其中稀土元素Ce和过渡金属Fe、Mn等是催化剂所需活性元素。本文利用浸渍法对活化稀土尾矿进行Ce改性,借助SEM-EDS、XRD、BET、NH_(3)-TPD、H_(2)-TPR、XPS等表征手段探究Ce改性对活化稀土尾矿催化剂性能的影响。结果表明,Ce改性活化稀土尾矿催化剂以介孔结构为主,Ce元素在催化剂表面高度分散;Ce元素与Fe元素之间存在协同作用,两者之间存在氧化还原电子对,促进了不同价态Ce、Fe离子之间的转化,增强了催化剂的氧化还原能力,提高了催化剂的酸性位点数量和酸性能,有利于NH_(3)的吸附与活化,从而使催化剂的脱硝效率提高。活化稀土尾矿经15%Ce改性后,脱硝效率由70%提升至82%,N_(2)选择性在90%以上,反应温度窗口拓宽至275~450℃。 展开更多
关键词 稀土尾矿 脱硝催化剂 活化 Ce改性 浸渍 NH_(3)-scr
下载PDF
某火电厂SCR催化剂不同服役阶段脱硝性能试验及研究
12
作者 刘智湘 肖芝 聂辉文 《河南科技》 2023年第14期91-94,共4页
【目的】某1 000 WM燃煤火力发电厂SCR脱硝系统采用蜂窝状催化剂。为把握随着催化剂服役时间增加相关脱硝性能参数的变化规律,对脱硝系统多次进行现场试验。【方法】试验采用专业仪器设备对脱硝系统烟气流速、脱硝效率、氨逃逸率、SO_(2... 【目的】某1 000 WM燃煤火力发电厂SCR脱硝系统采用蜂窝状催化剂。为把握随着催化剂服役时间增加相关脱硝性能参数的变化规律,对脱硝系统多次进行现场试验。【方法】试验采用专业仪器设备对脱硝系统烟气流速、脱硝效率、氨逃逸率、SO_(2)/SO_(3)转化率等性能参数进行测量分析。【结果】随着催化剂服役时间的增加,脱硝效率会明显降低,氨逃逸率有一定程度的增大,空气预热器处会生成硫酸氢铵等有害物质,造成堵塞。【结论】随着服役时间的增加,催化剂会因为飞灰冲刷、堆积及重金属中毒等导致活性下降,催化剂局部区域积灰较多,空气预热器堵塞情况严重,需要及时对催化剂进行更新或者再生处理,提高催化剂活性,保证脱硝系统安全经济运行。 展开更多
关键词 scr脱硝系统 脱硝效率 催化剂活性
下载PDF
基于性能检测的SCR脱硝催化剂寿命管理分析 被引量:1
13
作者 张志中 孙强 +7 位作者 姜肇中 齐佶 陈琦 刘现伟 江建平 唐郭安 张杨 郭栋 《电力科技与环保》 2023年第1期59-70,共12页
燃煤电厂在完成烟气超低排放改造后,对SCR脱硝催化剂的质量、性能指标和寿命管理水平提出了更高的要求。基于某机组历年的催化剂性能检测结果,首先分析了催化剂的几何参数、机械性能参数、主要化学成分、微量元素、微观结构参数的变化... 燃煤电厂在完成烟气超低排放改造后,对SCR脱硝催化剂的质量、性能指标和寿命管理水平提出了更高的要求。基于某机组历年的催化剂性能检测结果,首先分析了催化剂的几何参数、机械性能参数、主要化学成分、微量元素、微观结构参数的变化趋势及催化剂运行中存在的问题和产生的原因,其次根据工艺特性检测结果分析催化剂不同运行阶段的活性衰减情况。结果表明,上层催化剂的As含量年平均增幅为166μg/g,中、下层催化剂的平均As含量年平均增幅为661μg/g,As增加使催化剂的比较面积和酸位点数量减少;上层催化剂平均比表面积降幅为17.5%,中、下层催化剂平均比表面积降幅为27.0%,比表面积的下降减少活性位点的数量;三层催化剂的整体活性由2016年的20.5 m/h下降至2019年的17.7 m/h,活性衰减导致喷氨量加大和氨逃逸增加。总结得出催化剂寿命管理的关键点:根据相关标准规范和技术要求正确选用催化剂;优化脱硝装置运行条件;采用合理的运行控制手段;密切跟踪催化剂的活性。结合催化剂性能检测结果的分析和对催化剂寿命管理关键点的总结,能够为火电厂脱硝催化剂的寿命管理提供有效借鉴。 展开更多
关键词 燃煤电厂 scr脱硝催化剂 性能检测 活性衰减 寿命管理
下载PDF
商用SCR催化剂催化生成SO_(3)特性
14
作者 张雪伟 黄亚继 +7 位作者 程好强 王圣 朱志成 李金壘 丁雪宇 李雨欣 魏泽坤 张荣初 《化工进展》 EI CAS CSCD 北大核心 2023年第12期6354-6362,共9页
选择性催化还原(SCR)设备可以有效脱除烟气污染物NO_(x),但也会催化生成SO_(3),从而危害设备安全和大气环境。本研究在模拟SCR实验台基础上考察了温度、烟气气氛和催化剂组分对SCR催化剂催化生成SO_(3)的影响,并采用X射线荧光光谱(XRF)... 选择性催化还原(SCR)设备可以有效脱除烟气污染物NO_(x),但也会催化生成SO_(3),从而危害设备安全和大气环境。本研究在模拟SCR实验台基础上考察了温度、烟气气氛和催化剂组分对SCR催化剂催化生成SO_(3)的影响,并采用X射线荧光光谱(XRF)和X射线光电子能谱(XPS)分析了催化剂在反应前后的变化。结果表明:温度升高会提高SO_(3)的生成率;O_(2)含量对SO_(3)的生成产生影响,但是O_(2)含量超过2%后影响微小;增大SO_(2)浓度会降低SO_(3)生成率,但SO_(3)总量仍不断提升;一定浓度的NH3显著抑制了SO_(3)的生成,同时产生大量硫铵盐沉积物,而NO_(x)中的氧化性气体NO_(2)会提高催化剂中V5+的比例,促进SO_(3)生成;实际反应过程中脱硝与SO_(2)氧化存在竞争,降低烟气中NO_(2)浓度会提升脱硝效率且减少SO_(3)生成;催化剂中的钒和钛会提高SO_(3)生成率,而硅对SO_(3)的生成有抑制作用。本研究为SCR的实际运行优化提供了一定的理论基础和参考。 展开更多
关键词 选择性催化还原催化剂 催化氧化 SO_(3)生成 烟气气氛 活性组分
下载PDF
高阶时滞系统的改进线性自抗扰控制及参数整定方法
15
作者 刘长良 杨超杰 +2 位作者 刘卫亮 刘帅 王梓齐 《动力工程学报》 CAS CSCD 北大核心 2024年第4期599-606,640,共9页
针对高阶时滞系统采用传统线性自抗扰控制调节效果不佳、参数整定困难的问题,提出一种高阶时滞线性自抗扰控制。在一阶线性自抗扰控制的基础上,串联高阶前馈补偿器,从而解决了线性扩张状态观测器前馈信号和反馈信号不同步的问题,提高了... 针对高阶时滞系统采用传统线性自抗扰控制调节效果不佳、参数整定困难的问题,提出一种高阶时滞线性自抗扰控制。在一阶线性自抗扰控制的基础上,串联高阶前馈补偿器,从而解决了线性扩张状态观测器前馈信号和反馈信号不同步的问题,提高了系统的状态观测精度;在此基础上,采用目标逼近法定量化参数整定公式,并推导出参数可调节区间,实现利用单参数λ调节控制器参数,简化参数整定;进一步采用频域分析法验证该整定方法的有效性,并确定参数和系统鲁棒性的关系。最后,在选择性催化还原(SCR)脱硝控制系统的仿真实验中将所提出的控制器与其他类型控制器进行了对比,验证了该控制器的优越性。结果表明:所提出的高阶时滞线性自抗扰控制在定值跟随、抗扰动和鲁棒性上均具有明显优势,具有很大的工程应用潜力。 展开更多
关键词 高阶时滞系统 线性自抗扰控制 定量化参数整定 scr脱硝控制
下载PDF
V2O5-WO3/TiO2基SCR催化剂的研究进展 被引量:15
16
作者 赵毅 朱振峰 +2 位作者 贺瑞华 胡峻涛 李军奇 《材料导报》 EI CAS CSCD 北大核心 2009年第1期28-31,共4页
SCR是一种新型的脱硝催化技术。概述了选择性催化还原法的反应机理、载体掺杂V2O5-WO3对催化性能的影响,介绍了各种因素对催化剂成型性能的影响,提出了催化剂需要满足的一些条件,分析了技术方面需要解决的一些问题,总结了国内外SCR催化... SCR是一种新型的脱硝催化技术。概述了选择性催化还原法的反应机理、载体掺杂V2O5-WO3对催化性能的影响,介绍了各种因素对催化剂成型性能的影响,提出了催化剂需要满足的一些条件,分析了技术方面需要解决的一些问题,总结了国内外SCR催化剂的研究现状和发展前景。 展开更多
关键词 scr 催化剂 氮氧化物
下载PDF
三聚氰胺浸渍活性炭用于低温NH_3-SCR脱硝的研究 被引量:12
17
作者 李巧艳 侯亚芹 +4 位作者 韩小金 黄张根 郭倩倩 孙德魁 刘建东 《燃料化学学报》 EI CAS CSCD 北大核心 2014年第4期487-493,共7页
通过将三聚氰胺(M)浸渍在活性炭(AC)上制备了渗氮活性炭(ACM),研究了浸渍时间、煅烧温度等因素对ACM含氮量以及低温NH3-SCR脱硝活性的影响。结果表明,三聚氰胺浸渍后可以提高活性炭的低温脱硝活性,在80℃下ACM-5-900的NO转化率达到51.6... 通过将三聚氰胺(M)浸渍在活性炭(AC)上制备了渗氮活性炭(ACM),研究了浸渍时间、煅烧温度等因素对ACM含氮量以及低温NH3-SCR脱硝活性的影响。结果表明,三聚氰胺浸渍后可以提高活性炭的低温脱硝活性,在80℃下ACM-5-900的NO转化率达到51.67%,而AC只有21.92%。采用BET、元素分析及XPS等分别对渗氮活性炭ACM的结构、表面含氮量以及含氮官能团分布进行分析,表明含氮官能团的存在形式而不是含氮量影响渗氮活性炭的低温脱硝活性。同时NO+O2-TPD结果表明,渗氮改性后脱硝活性提高主要是由于表面含氮官能团提高了活性炭对NO的吸附和氧化。另外,SO2的存在会抑制渗氮活性炭的低温脱硝活性。 展开更多
关键词 脱硝 活性炭 选择性催化还原 含氮官能团
下载PDF
Ce掺杂对Mn/ACN催化剂低温NH_3-SCR脱硝活性的影响 被引量:9
18
作者 楚英豪 盖志谱 +4 位作者 王天泽 刘正 姚远 尹华强 郭家秀 《四川大学学报(工程科学版)》 EI CAS CSCD 北大核心 2015年第3期180-186,共7页
采用浸渍法将活性组分Mn、Ce负载到酸处理后的椰壳活性炭(ACN)上,制备出Mn/CAN和Mn-Ce/ACN脱硝催化剂,在固定床上对所制备的催化剂进行了脱硝性能评价,着重探讨了2种活性组分的负载顺序、负载量对催化剂活性的影响,并对催化剂进行了BET... 采用浸渍法将活性组分Mn、Ce负载到酸处理后的椰壳活性炭(ACN)上,制备出Mn/CAN和Mn-Ce/ACN脱硝催化剂,在固定床上对所制备的催化剂进行了脱硝性能评价,着重探讨了2种活性组分的负载顺序、负载量对催化剂活性的影响,并对催化剂进行了BET、SEM、XRD、XPS表征。结果表明,通过比较Mn/CAN和Mn-Ce/ACN催化剂的脱硝活性,发现Ce的添加能明显提高催化剂的脱硝活性,在温度高于90℃时能达到90%以上的NO去除率,在120~250℃之间,NO转化率维持在100%。活性组分的负载顺序及负载量是影响催化剂活性的重要因素。同时负载活性组分,Ce、Mn负载量均为5%时,催化剂表现出最好的脱硝性能。Mn负载在活性炭上,降低了活性炭的比表面积和孔容,而Mn、Ce负载量均为5%的Mn-Ce/ACN的比表面积和微孔孔容降到695.0 m2/g和0.130cm3/g,随着Mn、Ce负载量的增加,比表面积和孔容进一步降低;当Ce、Mn负载量均增加到10%时,其比表面积和微孔孔容只有539.8 m2/g和0.106 cm3/g。Mn3+和Mn4+共存于两种催化剂上,而Ce4+和Ce3+共存并使Mn-Ce/CAN上Mn4+比例略微增加,导致催化剂表现出最好的脱硝性能。 展开更多
关键词 低温 scr 活性炭 MN CE
下载PDF
稻壳基活性炭催化剂的低温NH3-SCR抗硫性能 被引量:9
19
作者 束韫 张凡 +2 位作者 王洪昌 石应杰 朱金伟 《中国环境科学》 EI CAS CSCD 北大核心 2019年第11期4620-4627,共8页
以稻壳基活性炭(DAC)为载体,利用等体积浸渍法制备了DAC负载Mn、Ce氧化物的Mn-Ce/DAC脱硝催化剂,并用于氨法SCR反应.采用N2吸附、X射线衍射(XRD)、X射线光电子能谱(XPS)和程序升温吸附脱附(TPR/TPD)等手段对催化剂的物理化学性能进行了... 以稻壳基活性炭(DAC)为载体,利用等体积浸渍法制备了DAC负载Mn、Ce氧化物的Mn-Ce/DAC脱硝催化剂,并用于氨法SCR反应.采用N2吸附、X射线衍射(XRD)、X射线光电子能谱(XPS)和程序升温吸附脱附(TPR/TPD)等手段对催化剂的物理化学性能进行了表征.结果发现与商业木屑基活性炭负载Mn、Ce氧化物催化剂(Mn-Ce/MAC)相比,Mn-Ce/DAC具有更高的Ce^3+/Ce^4+比率、表面化学吸附氧含量以及表面Brφnsted酸性位点,这与其优良的低温SCR活性及抗硫抗水性能直接相关.原位红外光谱结果显示在含硫气氛中Mn-Ce/DAC表面的硫酸盐含量明显低于Mn-Ce/MAC,表明前者具有优良抗硫性能. 展开更多
关键词 低温选择催化还原 生物质 活性炭 抗硫
下载PDF
以活性炭为载体的负载型催化剂的SCR脱硝性能 被引量:25
20
作者 吴海苗 王晓波 归柯庭 《东南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2013年第4期814-818,共5页
通过浸渍法负载Fe,Cr,Cu,Mn等过渡金属组分,制备以活性炭为载体的低温、廉价、高效的负载型催化剂,用于SCR脱硝.实验研究了活性组分、负载量、反应温度、氧气含量、表观流速等不同参数对催化剂脱硝效率的影响.结果表明,Mn的活性比Cu,Cr... 通过浸渍法负载Fe,Cr,Cu,Mn等过渡金属组分,制备以活性炭为载体的低温、廉价、高效的负载型催化剂,用于SCR脱硝.实验研究了活性组分、负载量、反应温度、氧气含量、表观流速等不同参数对催化剂脱硝效率的影响.结果表明,Mn的活性比Cu,Cr以及Fe的活性大,能更好地促进催化剂的催化脱硝;多组分催化剂催化脱硝效率要比单组分的脱硝效率高;活性炭载体上负载8%的Mn,Cu,Cr,Fe时,催化剂脱硝效率最佳;在一定氧气含量下,催化剂脱硝效率要比无氧时的脱硝效率高;在所制备的以活性炭为载体的负载型催化剂中,8Mn-8Fe/AC催化剂性能最稳定,催化脱硝效率最佳. 展开更多
关键词 活性炭 负载型催化剂 选择性催化还原(scr) 脱硝效率