Reduced graphene oxide aerogel decorated with Mo_(2)C nanoparticles toward multifunctional properties of hydrophobicity,thermal insulation and microwave absorption 被引量:3
1
作者 Yahui Wang Minghui Zhang +5 位作者 Xuesong Deng Zhigang Li Zongsheng Chen Jiaming Shi Xijiang Han Yunchen Du 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2023年第3期536-547,共12页
Reduced graphene oxide(rGO)aerogels are emerging as very attractive scaffolds for high-performance electromagnetic wave absorption materials(EWAMs)due to their intrinsic conductive networks and intricate interior micr... Reduced graphene oxide(rGO)aerogels are emerging as very attractive scaffolds for high-performance electromagnetic wave absorption materials(EWAMs)due to their intrinsic conductive networks and intricate interior microstructure,as well as good compatibility with other electromagnetic(EM)components.Herein,we realized the decoration of rGO aerogel with Mo_(2)C nanoparticles by sequential hydrothermal assembly,freeze-drying,and high-temperature pyrolysis.Results show that Mo_(2)C nanoparticle loading can be easily controlled by the ammonium molybdate to glucose molar ratio.The hydrophobicity and thermal insulation of the rGO aerogel are effectively improved upon the introduction of Mo_(2)C nanoparticles,and more importantly,these nanoparticles regulate the EM properties of the rGO aerogel to a large extent.Although more Mo_(2)C nanoparticles may decrease the overall attenuation ability of the rGO aerogel,they bring much better impedance matching.At a molar ratio of 1:1,a desirable balance between attenuation ability and impedance matching is observed.In this context,the Mo_(2)C/r GO aerogel displays strong reflection loss and broad response bandwidth,even with a small applied thickness(1.7 mm)and low filler loading(9.0wt%).The positive effects of Mo_(2)C nanoparticles on multifunctional properties may render Mo_(2)C/r GO aerogels promising candidates for high-performance EWAMs under harsh conditions. 展开更多
关键词 Mo_(2)C/reduced graphene oxide aerogel microwave absorption dielectric loss HYDROPHOBICITY thermal insulation
下载PDF
AMPS/DMAEMA/AM三元共聚物钻井液降滤失剂的研制
2
作者 薛丹 张笑 +2 位作者 李善建 陈亚联 史俊 《应用化工》 CAS CSCD 北大核心 2024年第3期600-603,607,共5页
以丙烯酰胺、2-丙烯酰胺-2-甲基丙磺酸和甲基丙烯酸二甲氨基乙酯为单体,过硫酸铵为引发剂,采用水溶液聚合法制备了PAAD降滤失剂,通过单因素实验对其制备工艺进行了优化,并对降滤失剂的耐温耐盐性能进行了探究。结果表明,在丙烯酰胺、2-... 以丙烯酰胺、2-丙烯酰胺-2-甲基丙磺酸和甲基丙烯酸二甲氨基乙酯为单体,过硫酸铵为引发剂,采用水溶液聚合法制备了PAAD降滤失剂,通过单因素实验对其制备工艺进行了优化,并对降滤失剂的耐温耐盐性能进行了探究。结果表明,在丙烯酰胺、2-丙烯酰胺-2-甲基丙磺酸和甲基丙烯酸二甲氨基乙酯质量比为4∶2∶0.02、反应温度为60℃、反应时间4 h、过硫酸铵用量为混合单体质量的0.15%的最佳条件下,所制备的降滤失剂的降滤失效果最佳,抗温达210℃。 展开更多
关键词 降滤失剂 抗温抗盐性能 钻井液
下载PDF
环保型改性纳米碳酸钙降滤失剂的合成与性能评价
3
作者 黄维安 李国真 +4 位作者 贾江鸿 张金昭 江琳 余婷 苏锐 《中国石油大学学报(自然科学版)》 EI CAS CSCD 北大核心 2024年第2期126-134,共9页
纳米碳酸钙在钻井液中具有降滤失及封堵作用、且环保,但分散性差、易团聚,导致效果不理想。使用硅烷偶联剂对纳米碳酸钙进行表面改性,再通过自由基共聚法将抗温、抗盐单体接枝到改性纳米碳酸钙表面,得到改性纳米碳酸钙降滤失剂SDNPJ-2,... 纳米碳酸钙在钻井液中具有降滤失及封堵作用、且环保,但分散性差、易团聚,导致效果不理想。使用硅烷偶联剂对纳米碳酸钙进行表面改性,再通过自由基共聚法将抗温、抗盐单体接枝到改性纳米碳酸钙表面,得到改性纳米碳酸钙降滤失剂SDNPJ-2,采用红外光谱(FTIR)、热重分析进行表征,同时对比评价其综合性能,通过对膨润土基浆粒径、zeta电位分析,滤饼扫描电镜(SEM)分析,考察SDNPJ-2在黏土颗粒上的吸附特征,研究改性纳米碳酸钙降滤失剂在水基钻井液中的降滤失机制。结果表明:SDNPJ-2可抗230℃高温;1%SDNPJ-2可分别使4%膨润土基浆、25%盐水基浆、10%CaCl_(2)基浆150℃/(16 h)老化后的API滤失量降低70%、89%和85%,可抗氯化钠250000 mg/L、抗氯化钙100000 mg/L,降滤失效果优于国外同类目前最优产品Driscal D;生化需氧量(BOD_(5))为558 mg/L、BOD_(5)/COD(化学需氧量)达22.6%,可生物降解;SDNPJ-2通过酰胺基团吸附于黏土表面、改善其分散性,优化体系粒径级配、通过物理堆积有效封堵滤饼和地层孔隙,两方面协同达到优良的降滤失效果。 展开更多
关键词 纳米碳酸钙 降滤失剂 钻井液 耐温耐盐
下载PDF
基于缩尺模型的高铁桥梁预应力损失试验研究
4
作者 许开成 黄凌娟 +3 位作者 李鹏清 张立卿 邱日旭 陈梦成 《华东交通大学学报》 2024年第2期48-55,共8页
【目的】为更好的评估在役预应力混凝土桥梁结构预应力损失状况。【方法】选用国内高铁中应用最广的32 m预应力混凝土箱梁作为研究对象,按照1:16的缩尺比例将箱梁转化为T形截面制作了26根C50混凝土试验模型梁。通过对试验梁预应力钢绞... 【目的】为更好的评估在役预应力混凝土桥梁结构预应力损失状况。【方法】选用国内高铁中应用最广的32 m预应力混凝土箱梁作为研究对象,按照1:16的缩尺比例将箱梁转化为T形截面制作了26根C50混凝土试验模型梁。通过对试验梁预应力钢绞线应变、伸长量的瞬时和长期监测得到预应力损失的实际值,并将此实际值与目前国内外常用预应力损失规范计算所得值进行对比分析。【结果】预应力损失主要发生在前期即瞬时损失,约占总损失的70%;84.6%的试验梁锚固损失占瞬时损失总和的70%以上,最高达80.57%;试验梁的长期损失在锚固后的前10 d内变化较快,后期逐渐趋于稳定;将5种规范的计算结果与试验实测值进行对比,对于长期损失,数据显示实测数据与《铁路桥涵设计规范》(TB 10002—2017)计算结果最为吻合。【结论】研究结果可为实际工程中预应力梁的预应力损失计算提供参考。 展开更多
关键词 预应力混凝土梁 预应力损失 缩尺模型 规范对比 应变监测
下载PDF
摆线针轮减速机参数对传动效率的影响与参数优化
5
作者 张跃明 李天宇 纪姝婷 《华南理工大学学报(自然科学版)》 EI CAS CSCD 北大核心 2024年第4期77-87,共11页
为进一步提高摆线针轮减速机的传动效率,对减速机传动效率的影响规律进行了深入研究,提出了考虑设计参数与工况参数变化的摆线针轮减速机传动效率计算模型,并对参数进行了优化。首先,考虑摩擦力和啮合齿隙,建立了摆线针轮传动机构的多... 为进一步提高摆线针轮减速机的传动效率,对减速机传动效率的影响规律进行了深入研究,提出了考虑设计参数与工况参数变化的摆线针轮减速机传动效率计算模型,并对参数进行了优化。首先,考虑摩擦力和啮合齿隙,建立了摆线针轮传动机构的多齿承载接触分析模型,计算了摆线针齿啮合力与载荷分布规律;然后,考虑摆线针轮减速机的啮合损耗、输出损耗、轴承损耗、润滑损耗和密封损耗,提出了摆线针轮减速机传动效率计算模型,并分析了设计参数和工况参数对摆线针轮减速机传动效率的影响规律。研究表明,在考虑摩擦受力的情况下,转速、负载、针齿销半径、针齿分布圆半径、偏心距、针齿套半径是影响传动效率的主要参数,针齿销数、柱销分布圆半径、柱销半径和摆线轮齿宽次之。最后,以齿轮强度、齿轮宽度、齿廓形状、齿间间隙和承载能力作为参数优化范围,将效率和体积作为目标对设计参数进行多目标优化分析,得到最优参数解,进而获得了更小体积、更高传动效率的摆线针轮减速机。 展开更多
关键词 减速机 摆线针轮传动 摩擦损耗 传动效率 多目标优化
下载PDF
北方防沙带大型露天煤矿区生态保护与修复技术 被引量:2
6
作者 李全生 李淋 +4 位作者 方杰 周伟 雷少刚 包玉英 崔明 《煤炭科学技术》 EI CAS CSCD 北大核心 2024年第1期323-333,共11页
北方防沙带是我国防治沙化和荒漠化的关键地带,是“三北”工程的核心区,区内土壤贫瘠、风速大、干旱缺水、植被稀少、生态恢复力低,而大型露天煤矿开采与生态保护矛盾突出,直接影响区域生态安全和国家能源保供,迫切需要开展大型露天矿... 北方防沙带是我国防治沙化和荒漠化的关键地带,是“三北”工程的核心区,区内土壤贫瘠、风速大、干旱缺水、植被稀少、生态恢复力低,而大型露天煤矿开采与生态保护矛盾突出,直接影响区域生态安全和国家能源保供,迫切需要开展大型露天矿区生态保护修复研究。针对北方防沙带大型露天煤矿区开采引起的土地破坏、扬尘起沙、水位下降、土壤沙化、植被退化等问题。以北方防沙带面积和露天煤炭产量占比均最大的内蒙古的大型露天煤矿区为研究区,秉承“减损开采-立体保水-造土活土-系统修复-集成监管”的研究思路,揭示大型露天矿岩土损伤-生态退化传导机理、生态减损开采机制、重建生态自维持机制,研发生态保护型减损开采、生态化设计、水资源保护与综合利用、抗侵蚀地貌重塑、排土场活土层精细重构、土壤改良与提质增容、菌-藻-草联合修复、生态系统退化监管等关键技术,形成适合北方防沙带露天煤矿区生态保护与修复技术体系,建成大型露天矿区生态保护修复集成示范区。创建低成本、高效率、可持续、可复制的大型露天矿区生态保护修复模式,为保障我国北方防沙带大型露天矿区科学开采与生态安全提供支撑,实现煤炭开发能源保供与生态保护相协调、“开发金山银山,再造绿水青山”的目标。 展开更多
关键词 北方防沙带 露天矿 生态保护 减损开采 系统修复
下载PDF
生态保护型煤炭开采技术与实践
7
作者 李全生 李淋 +4 位作者 方杰 郭俊廷 李军 徐祝贺 李晓斌 《煤炭科学技术》 EI CAS CSCD 北大核心 2024年第4期28-37,共10页
针对生态脆弱区煤炭规模化高效开采造成生态影响范围大、周期长和强度高,缺乏统筹开采全周期源头减损与生态全要素系统技术,导致矿区生态修复成本高、效率低和效果差的问题,提出了生态保护型煤炭开采理念,露天开采损伤传导途径和井工开... 针对生态脆弱区煤炭规模化高效开采造成生态影响范围大、周期长和强度高,缺乏统筹开采全周期源头减损与生态全要素系统技术,导致矿区生态修复成本高、效率低和效果差的问题,提出了生态保护型煤炭开采理念,露天开采损伤传导途径和井工开采损伤传导模型、生态损伤定量分析方法和矿区生态修复决策方法,研发了露天矿节地减损开采、生态型地层重构、分布式水资源集−储−用、基于“生态修复窗口期”协同修复技术;研发了井工开采损伤传导控制、含水层生态功能恢复、装配式楔形地下水库坝体构筑、沉陷区分时分区生态修复技术。建成蒙东矿区生态保护型露天开采示范工程,宝日希勒露天矿示范区植被盖度由开发前30%提高到59%,胜利露天矿示范区植被盖度由开发前5%提高到39%;建成神东井工生态保护型煤炭开采示范工程,植被盖度由开发前不足10%提高到70%。研究成果为生态保护型煤炭开采提供了科技支撑,具有广泛的应用和推广价值。 展开更多
关键词 露天开采 井工开采 生态保护 减损开采 生态修复 绿色开采
下载PDF
高性能密胺降滤失剂的研究
8
作者 刘海波 薛丹 史俊 《化工技术与开发》 CAS 2024年第1期31-34,71,共5页
用多聚甲醛与三聚氰胺合成了密胺树脂,对经黏土改性后的丙烯酰胺类聚合物进行包覆,制备了一种抗温抗盐的钻井液降滤失剂。采用单因素实验对样品的加量及耐温耐盐性能进行了评价,实验结果表明,2号样品的性能最佳。在盐浓度为8%的钻井液中... 用多聚甲醛与三聚氰胺合成了密胺树脂,对经黏土改性后的丙烯酰胺类聚合物进行包覆,制备了一种抗温抗盐的钻井液降滤失剂。采用单因素实验对样品的加量及耐温耐盐性能进行了评价,实验结果表明,2号样品的性能最佳。在盐浓度为8%的钻井液中,加量为1.5%时,经100℃老化后,2号样品的加量比对照样品减少3%,滤失率为77.7%,性能更优良。 展开更多
关键词 密胺树脂 降滤失剂 泥浆工作液
下载PDF
复合功能型聚羧酸减水剂的制备及其性能研究
9
作者 王海 莫祥银 林军 《应用化工》 CAS CSCD 北大核心 2024年第3期511-515,共5页
以改性聚醚异戊烯醇聚氧乙烯醚(TPEG-2400)为功能大单体,甲基丙烯酰氧乙基三甲基氯化铵(DMC)、丙烯酸(AA)和顺丁烯二酸酐(MA)为功能小单体,以过氧化氢(H_(2)O_(2))-抗坏血酸(Vc)氧化还原体系为引发剂,以巯基丙酸(MPA)为链转移剂,通过水... 以改性聚醚异戊烯醇聚氧乙烯醚(TPEG-2400)为功能大单体,甲基丙烯酰氧乙基三甲基氯化铵(DMC)、丙烯酸(AA)和顺丁烯二酸酐(MA)为功能小单体,以过氧化氢(H_(2)O_(2))-抗坏血酸(Vc)氧化还原体系为引发剂,以巯基丙酸(MPA)为链转移剂,通过水溶液自由基聚合法,制备一种兼具抗泥、保坍性能的复合功能型聚羧酸减水剂。通过正交实验设计得出最佳合成条件,并通过单因素实验优化合成条件。通过FTIR、TGA、TOC进行性能表征。结果表明,最佳合成工艺条件:反应温度为45℃,n(AA)∶n(TPEG)=4.0∶1,n(DMC)∶n(TPEG)=0.75∶1,n(MA)∶n(TPEG)=0.6∶1,巯基丙酸(MPA)用量为大单体聚醚的0.65%,引发剂用量为大单体聚醚的1.27%,且m(H_(2)O_(2))∶m(Vc)=3.5∶1,A液、B液滴加时间为3.0,3.5 h。此合成工艺条件下,得到的复合功能型聚羧酸减水剂分散性能较好,对蒙脱土的敏感性较低且经时坍落度损失较小。 展开更多
关键词 复合功能型聚羧酸减水剂 顺丁烯二酸酐 抗泥 坍落度损失
下载PDF
抗高温抗盐水基降滤失剂的合成与性能评价
10
作者 李保陆 白杨 +4 位作者 王瑞芳 陈新 李道雄 吴凌风 王海波 《广东化工》 CAS 2024年第5期9-13,共5页
针对现有水基钻井液用降滤失剂抗高温和抗盐能力不足的问题,提出以腐植酸钠(Na Hm)、N,N-二甲基丙烯酰胺(NNDMA)、二甲基二烯丙基氯化铵(DMAAC)、对苯乙烯磺酸钠(SSS)为单体,过硫酸铵为引发剂,通过水溶液自由基聚合制备了一种抗高温抗... 针对现有水基钻井液用降滤失剂抗高温和抗盐能力不足的问题,提出以腐植酸钠(Na Hm)、N,N-二甲基丙烯酰胺(NNDMA)、二甲基二烯丙基氯化铵(DMAAC)、对苯乙烯磺酸钠(SSS)为单体,过硫酸铵为引发剂,通过水溶液自由基聚合制备了一种抗高温抗盐降滤失剂。采用正交实验确定最佳反应条件:m(Na Hm∶NNDMA∶DMDAAC∶SSS)=2∶6∶2∶2,单体浓度30%,引发剂加量1.0%,反应温度65℃。利用红外光谱、热失重、核磁共振氢谱及环境扫描电镜对产物进行了结构表征和分析,证明四元聚合物制备成功,并通过抗高温、抗盐性能评价以及和市面常用产品对比,实验发现所合成的降滤失剂具有良好的抗高温抗盐性能,230℃老化16 h后,中压滤失量为5 m L,高温高压滤失量为22 m L,抗Na Cl 25%,抗Ca Cl21.5%,在高温高盐水基钻井液中具有广阔的应用前景。 展开更多
关键词 水基钻井液 降滤失剂 抗高温 抗盐 聚合物
下载PDF
Tracking Regulatory Mechanism of Trace Fe on Graphene Electromagnetic Wave Absorption
11
作者 Kaili Zhang Yuhao Liu +5 位作者 Yanan Liu Yuefeng Yan Guansheng Ma Bo Zhong Renchao Che Xiaoxiao Huang 《Nano-Micro Letters》 SCIE EI CAS CSCD 2024年第4期79-96,共18页
Polarization and conductance losses are the fundamental dielectric attenuation mechanisms for graphene-based absorbers, but it is not fully understood in revealing the loss mechanism of affect graphene itself. For the... Polarization and conductance losses are the fundamental dielectric attenuation mechanisms for graphene-based absorbers, but it is not fully understood in revealing the loss mechanism of affect graphene itself. For the first time, the reduced graphene oxide(RGO) based absorbers are developed with regulatory absorption properties and the absorption mechanism of RGO is mainly originated from the carrier injection behavior of trace metal Fe nanosheets on graphene. Accordingly, the minimum reflection loss(RLmin) of Fe/RGO-2composite reaches-53.38 dB(2.45 mm), and the effective absorption bandwidth achieves 7.52 GHz(2.62 mm) with lower filling loading of 2 wt%. Using off-axis electron hologram testing combined with simulation calculation and carrier transport property experiments, we demonstrate here the carrier injection behavior from Fe to graphene at the interface and the induced charge accumulation and rearrangement, resulting in the increased interfacial and dipole polarization and the conductance loss. This work has confirmed that regulating the dielectric property of graphene itself by adding trace metals can not only ensure good impedance matching, but also fully exploit the dielectric loss ability of graphene at low filler content,which opens up an efficient way for designing lightweight absorbers and may be extended to other types materials. 展开更多
关键词 reduced graphene oxide Fe nanosheets Dielectric loss Electromagnetic wave absorption
下载PDF
不同粒径淀粉对水基钻井液性能的影响
12
作者 黄磊 《山东化工》 CAS 2024年第4期52-54,61,共4页
淀粉具有来源广、无毒易降解的特点,可有效降低钻井液泥饼厚度,常被作为降滤失剂应用于水基钻井液中。为了探讨不同粒径淀粉对钻井液增粘、降滤失效果的影响,通过球磨方法制备微细淀粉,使其评价粒径从38.87μm降低至10.32μm,增大了淀... 淀粉具有来源广、无毒易降解的特点,可有效降低钻井液泥饼厚度,常被作为降滤失剂应用于水基钻井液中。为了探讨不同粒径淀粉对钻井液增粘、降滤失效果的影响,通过球磨方法制备微细淀粉,使其评价粒径从38.87μm降低至10.32μm,增大了淀粉的比表面积,可在钻井液中与更多的水分子接触,提高淀粉分子上的氢键与水分子之间的水化作用和黏土颗粒的吸附能力,其降滤失效果优于玉米淀粉、羧甲基纤维素(CMC),羟乙基纤维素(HEC)。淀粉粒径分布的改变影响了水基钻井液的流变性以及降滤失性能,这一发现以期为钻井现场优选淀粉降滤失剂提供技术指导。 展开更多
关键词 玉米淀粉 水基钻井液 降滤失剂 糊化温度 滤失量
下载PDF
硼砂交联PVA降失水剂的合成及滤失性能研究
13
作者 答欣宇 李万东 +4 位作者 董志明 谢杨杰 吴艺旋 赵媛君 高国新 《广州化工》 CAS 2024年第2期93-96,共4页
以聚乙烯醇(PVA1788)为水泥浆降失水剂基础原料,考察了交联剂种类和用量、反应温度、溶液pH值等对PVA胶液粘度和水泥浆滤失性能的影响规律,发现硼砂水解后对PVA的交联效果最显著,而且随着硼砂与PVA配比、反应温度和pH值升高,PVA胶液粘... 以聚乙烯醇(PVA1788)为水泥浆降失水剂基础原料,考察了交联剂种类和用量、反应温度、溶液pH值等对PVA胶液粘度和水泥浆滤失性能的影响规律,发现硼砂水解后对PVA的交联效果最显著,而且随着硼砂与PVA配比、反应温度和pH值升高,PVA胶液粘度及水泥浆滤失性能呈现显著增高趋势,所形成的滤饼更加致密,保水能力更好。但一旦超过最佳配比时,水泥颗粒表面降滤失剂膜层变厚,滤饼致密性变差,反而不利于水泥浆保水,滤失性能下降。 展开更多
关键词 硼砂 聚乙烯醇 降滤失剂 交联
下载PDF
一种复杂多金属硫化矿中硫精矿再选优化工艺
14
作者 郝泽飞 鲁雯 +2 位作者 何永利 景世妍 杨丹琪 《世界有色金属》 2024年第8期104-106,共3页
由于某多金属铅锌矿选厂脱硫一步扫尾(硫精矿)金属损失严重,脱硫二步作业流程产出的铅锌精矿2品位较低,与分离产出的铅锌精矿1混合拉低了总铅锌精矿品位。为解决这一问题,提高混合铅锌品位,脱硫一步扫尾再浮选,实验室以脱硫粗一扫尾为原... 由于某多金属铅锌矿选厂脱硫一步扫尾(硫精矿)金属损失严重,脱硫二步作业流程产出的铅锌精矿2品位较低,与分离产出的铅锌精矿1混合拉低了总铅锌精矿品位。为解决这一问题,提高混合铅锌品位,脱硫一步扫尾再浮选,实验室以脱硫粗一扫尾为原矿,脱硫二步开展氧化钙、硫酸铜药剂用量试验,进一步优化脱硫二步粗、扫选工艺。铅锌2改造为活流程的方案(高原矿时铅锌2直接进入铅锌精矿,低原矿时返回脱硫一步精选作业),降低硫精矿中Cu、Pb、Zn的品位,减少金属损失,提高回收率。 展开更多
关键词 多金属硫化矿 减少金属流失 脱硫硫精矿
下载PDF
膨润土种类及黄原胶含量对减阻泥浆性能的影响
15
作者 高增奎 张睿钦 +2 位作者 王先甲 胡家新 王丹生 《土木工程与管理学报》 2024年第1期19-24,共6页
减阻触变泥浆在地下综合管廊顶管施工中具有支撑、填充、润滑等重要作用。本文对减阻触变泥浆中主要原材料—膨润土的种类及含量对泥浆性能的影响进行了实验研究。结果表明:减阻泥浆的漏斗粘度、失水量和析水率等性能指标随钠基、有机... 减阻触变泥浆在地下综合管廊顶管施工中具有支撑、填充、润滑等重要作用。本文对减阻触变泥浆中主要原材料—膨润土的种类及含量对泥浆性能的影响进行了实验研究。结果表明:减阻泥浆的漏斗粘度、失水量和析水率等性能指标随钠基、有机和钙基3种膨润土含量的变化规律基本相同。由钠基或有机膨润土配制的泥浆失水量性能优于钙基膨润土,但钙基膨润土在泥浆漏斗粘度性能上表现更好;由上述3种类型膨润土分别配制的泥浆析水率性能相当。另外,本文还研究了黄原胶含量对减阻泥浆性能的影响,实验结果表明添加黄原胶能显著降低减阻触变泥浆的失水量,并在一定程度上提高泥浆的漏斗粘度。 展开更多
关键词 顶管施工 减阻触变泥浆 膨润土种类 黄原胶 漏斗粘度 失水量 析水率
下载PDF
基于能量损耗比的驱动轮减振结构ANSYS一阶优化分析
16
作者 满仲鹏 赵章达 王瑶 《机械设计与制造工程》 2024年第4期11-15,共5页
针对应用于履带式工程车辆驱动轮的“阻尼层+过渡层”复合减振结构,通过建立能量损耗比模型,分析了其应力、应变特性。此外,在四层管状过渡阻尼减振结构厚度值恒定的情况下,基于ANSYS一阶优化方法,探究并优化了不同设计变量(基层、约束... 针对应用于履带式工程车辆驱动轮的“阻尼层+过渡层”复合减振结构,通过建立能量损耗比模型,分析了其应力、应变特性。此外,在四层管状过渡阻尼减振结构厚度值恒定的情况下,基于ANSYS一阶优化方法,探究并优化了不同设计变量(基层、约束层、过渡层、阻尼层的厚度值和过渡层、阻尼层材料的弹性模量以及损耗因子)对结构优化目标函数能量损耗比的影响规律。研究结果表明,相比于优化前结构的能耗比参数,优化后结构的耗能值增加了56.8%,增长值为0.1654。所提分析方法可为中国高端大型履带式工程车辆的减振设计以及绿色化提供参考,同时对于遗传算法优化在各种车辆结构设计中的运用具有一定的借鉴价值。 展开更多
关键词 驱动轮 减振结构 能量损耗比 一阶优化方法
下载PDF
改性柚子皮降滤失剂的合成与评价研究
17
作者 王梦园 薛曼 +3 位作者 梁梦佳 金纯正 杨现禹 蔡记华 《钻探工程》 2024年第3期84-93,共10页
天然材料因其易降解、环境友好、来源丰富和价格低廉等优势,成为环保型钻井液处理剂研发的重要方向。在天然柚子皮的基础上,通过化学合成引入酰胺基和磺酸基,形成了一种可满足高温地层绿色、安全、高效钻进的改性柚子皮降滤失剂,并对其... 天然材料因其易降解、环境友好、来源丰富和价格低廉等优势,成为环保型钻井液处理剂研发的重要方向。在天然柚子皮的基础上,通过化学合成引入酰胺基和磺酸基,形成了一种可满足高温地层绿色、安全、高效钻进的改性柚子皮降滤失剂,并对其抗温性、抑制性和抗盐抗钙性能进行了评价。柚子皮富含植物酚和聚糖等活性成分,改性后的柚子皮抗温能力强,在150℃的滤失量降低率超过70%;滚动回收实验结果表明,在加量为0.3%的情况下,其抑制效果优于KCl;抗污染实验表明,改性柚子皮降滤失剂抗盐抗钙效果好,0.3%的加量下,在淡水基浆、盐水基浆、饱和盐水基浆中均能使滤失量保持在10 mL以下,在CaCl2含量为3%时,滤失量降低率达到82.22%。改性后的柚子皮具有良好的降滤失性能,为环境友好型钻井液处理剂的开发提供了新的技术思路。 展开更多
关键词 改性柚子皮 环保型钻井液 降滤失剂 抗高温 抗盐抗钙
下载PDF
不同金属离子条件下微生物对聚合物溶液黏度的影响及作用机制
18
作者 卞立红 曲丽娜 +4 位作者 高清河 任国领 胡敏 张奕婷 王超 《大庆石油地质与开发》 CAS 北大核心 2024年第2期108-114,共7页
为了减少采油过程中因为金属离子导致的聚合物黏损,从而提高原油采收率,利用从大庆油田腐蚀管道筛选出的降黏菌S,通过向聚合物培养基中添加不同种类及浓度的金属离子,将降黏菌S对聚合物黏度的影响及作用机制进行了研究。结果表明:在2 00... 为了减少采油过程中因为金属离子导致的聚合物黏损,从而提高原油采收率,利用从大庆油田腐蚀管道筛选出的降黏菌S,通过向聚合物培养基中添加不同种类及浓度的金属离子,将降黏菌S对聚合物黏度的影响及作用机制进行了研究。结果表明:在2 000 mg/L的聚合物质量浓度下,向基础降黏培养基中加入10~50 mg/L的金属离子,Mn^(2+)、Fe^(2+)和Fe^(3+)的加入可以很大程度地提高降黏菌S的降黏率,最高黏损率分别为38.3%、35.6%、34.7%;K~+的加入对降黏菌S的降黏率影响不大;Cu^(2+)、Zn^(2+)的加入会降低菌S所引起的黏损;因此要控制采油体系中Mn^(2+)、Fe^(2+)和Fe^(3+)的含量,从而降低聚合物黏损;K~+离子含量也不宜太多。适当增加采油体系中Zn^(2+)、Cu^(2+),减少聚合物黏损,或者将6种离子均以质量浓度30 mg/L混合加入会降低聚合物黏损。研究成果对油田减少聚合物黏损,提高原油采收率提供了一定的方法和理论支撑。 展开更多
关键词 聚合物溶液 降黏菌 金属离子 黏损 作用机制
下载PDF
聚合物型钻井液降滤失剂的合成及其性能研究
19
作者 王金树 张玉平 +2 位作者 高树峰 周芳芳 郭光范 《精细石油化工进展》 CAS 2024年第2期1-4,共4页
以N,N-二甲基丙烯酰胺(DMAM)、顺丁烯二酸酐(MA)和二甲基二烯丙基氯化铵(DMDAAC)为改性单体,与丙烯酰胺(AM)聚合,采用水溶液聚合法合成了P(AM/DMAM/DMDAAC/MA)四元共聚物钻井液降滤失剂,研究了pH、单体用量、聚合时间等因素对聚合物降... 以N,N-二甲基丙烯酰胺(DMAM)、顺丁烯二酸酐(MA)和二甲基二烯丙基氯化铵(DMDAAC)为改性单体,与丙烯酰胺(AM)聚合,采用水溶液聚合法合成了P(AM/DMAM/DMDAAC/MA)四元共聚物钻井液降滤失剂,研究了pH、单体用量、聚合时间等因素对聚合物降滤失性能的影响。结果表明:聚合反应温度为55℃、反应时间为3 h、AM/DMAM/DMDAAC/MA单体质量比为7∶2∶2∶0.5、引发剂质量分数为0.5%时,得到的四元共聚物黏均分子量为3.98×10^(6);当温度达到180℃、四元共聚物在基浆中的加量为0.5%时,滤失量保持在7.8 mL,符合SY/T 5621—93的API滤失量标准。 展开更多
关键词 N N-二甲基丙烯酰胺(DMAM) 顺丁烯二酸酐(MA) 二甲基二烯丙基氯化铵(DMDAAC) 降滤失性能 钻井液降滤失剂
下载PDF
热引发聚合方法制备抗240℃水泥浆降失水剂
20
作者 林鑫 刘硕琼 +1 位作者 夏修建 孟仁洲 《钻井液与完井液》 CAS 北大核心 2024年第1期98-104,共7页
针对现有水泥浆降失水剂耐高温性能不足的问题,以高温热引发聚合方法替代传统水溶液引发剂聚合方法,设计并合成了抗温为240℃的三元水泥浆降失水剂HTFLA-A。通过实验确定了HTFLA-A的最佳合成条件:水与单体总质量比1∶1,控制温度为150℃... 针对现有水泥浆降失水剂耐高温性能不足的问题,以高温热引发聚合方法替代传统水溶液引发剂聚合方法,设计并合成了抗温为240℃的三元水泥浆降失水剂HTFLA-A。通过实验确定了HTFLA-A的最佳合成条件:水与单体总质量比1∶1,控制温度为150℃,体系pH值为9,反应时间为32 h。并采用红外光谱(FT-IR)、热重分析(DSC/TGA)及核磁共振谱对HTFLA-A进行了表征。结果表明,HTFLA-A为目标预期产物,在439℃时的热失重仅为23.80%,这是由于高温合成过程中去除了单体中不稳定结构和有机合成过程中副反应产物,提升了高分子材料的抗温性能。对HTFLA-A的性能评价结果表明,当HTFLA-A加量为1.2%,可将水泥浆在180~240℃、6.9 MPa时API失水量控制在50 mL以内。 展开更多
关键词 水泥浆 降失水剂 热引发聚合 耐高温
下载PDF