Synthetic goethite(α-FeOOH) was prepared in the laboratory using a modified version of Brauer's method.The process of steam-crystallization was prolonged and impurities were removed by dialysis.The products have ...Synthetic goethite(α-FeOOH) was prepared in the laboratory using a modified version of Brauer's method.The process of steam-crystallization was prolonged and impurities were removed by dialysis.The products have been characterised by Surface Area Analyser and Scanning Electron Microscope, and proved to have larger Specific Surface Area than that in literature.展开更多
The preparation method of H_4MoO_(26)-polyaniline film modified electrode and its voltammetric behaviour are described. The modified electrode has high electrocatalytic activity on chlorate ions.
文摘Synthetic goethite(α-FeOOH) was prepared in the laboratory using a modified version of Brauer's method.The process of steam-crystallization was prolonged and impurities were removed by dialysis.The products have been characterised by Surface Area Analyser and Scanning Electron Microscope, and proved to have larger Specific Surface Area than that in literature.
文摘The preparation method of H_4MoO_(26)-polyaniline film modified electrode and its voltammetric behaviour are described. The modified electrode has high electrocatalytic activity on chlorate ions.