The decomposed characteristic of nanometer ZnO precursor compound was studied. From the research, the decomposed temperature of nanometer precursor compound of ZnO is about 230 ℃ and it may be completely decompounded...The decomposed characteristic of nanometer ZnO precursor compound was studied. From the research, the decomposed temperature of nanometer precursor compound of ZnO is about 230 ℃ and it may be completely decompounded at 350 ℃. By means of the kinetics theory, the dynamics equation of precursor compound of nanometer ZnO was obtained. Activation energy is approximately 789.83±40 J·mol -1, reaction order is about 3, and pre-exponential factor is 0.0696 mg·s -1.展开更多
文摘The decomposed characteristic of nanometer ZnO precursor compound was studied. From the research, the decomposed temperature of nanometer precursor compound of ZnO is about 230 ℃ and it may be completely decompounded at 350 ℃. By means of the kinetics theory, the dynamics equation of precursor compound of nanometer ZnO was obtained. Activation energy is approximately 789.83±40 J·mol -1, reaction order is about 3, and pre-exponential factor is 0.0696 mg·s -1.