The undeformed chip thickness and grinding force are key parameters for revealing the material removal mechanism in the grinding process.However,they are difficult to be well expressed due to the ununiformed protrusio...The undeformed chip thickness and grinding force are key parameters for revealing the material removal mechanism in the grinding process.However,they are difficult to be well expressed due to the ununiformed protrusion height and random position distribution of abrasive grains on the abrasive wheel surface.This study investigated the distribution of undeformed chip thickness and grinding force considering the non-uniform characteristics of abrasive wheel in the grinding of K4002 nickel-based superalloy.First,a novel grinding force model was established through a kinematic-geometric analysis and a grain-workpiece contact analysis.Then,a series of grinding experiments were conducted for verifying the model.The results indicate that the distribution of undeformed chip thickness is highly consistent with the Gaussian distribution formula.The increase in the grinding depth mainly leads to an increase in the average value of Gaussian distribution.On the contrary,the increase in the workpiece infeed speed or the decrease in the grinding speed mainly increases the standard deviation of Gaussian distribution.The average and maximum errors of the grinding force model are 4.9%and 14.6%respectively,indicating that the model is of high predication accuracy.展开更多
Cracks have consistently been a significant challenge limiting the development of additive manufactured nickel-based superalloys.It is essential to investigate the location of cracks and their forming mechanism.This s...Cracks have consistently been a significant challenge limiting the development of additive manufactured nickel-based superalloys.It is essential to investigate the location of cracks and their forming mechanism.This study extensively examines the impact of solidification process,microstructural evolution,and stress concentration on crack initiation during direct energy deposition(DED).The results emphasize that the crack formation is significantly related to large-angle grain boundaries,rapid cooling rates.Cracks caused by large-angle grain boundaries and a fast-cooling rate predominantly appear near the edge of the deposited samples.Liquation cracks are more likely to form near the top of the deposited sample,due to the presence ofγ/γ'eutectics.The secondary dendritic arm and the carbides in the interdendritic regions can obstruct liquid flow during the final stage of solidification,which results in the formation of solidification cracks and voids.This work paves the way to avoid cracks in nickel-based superalloys fabricated by DED,thereby enhancing the performance of superalloys.展开更多
A nickel-based superalloy with good corrosion resistance was fabricated by directional solidification, and its microstructure and tensile properties at elevated temperatures were investigated. Microstructure observati...A nickel-based superalloy with good corrosion resistance was fabricated by directional solidification, and its microstructure and tensile properties at elevated temperatures were investigated. Microstructure observations reveal that the γ' precipitates are arrayed in the y matrix regularly with some MC, Ni5Hf and M3B2 particles distributed along the grain boundary. The tensile tests exhibit that the tensile properties depend on temperature significantly and demonstrate obvious anomalous yield and intermediate-temperature brittleness (ITB) behavior. Below 650℃, the yield strength decreases slightly but the ultimate tensile strength almost has no change. When the temperature is between 650 ℃ and 750 ℃, the yield and ultimate tensile strengths rise rapidly, and after then they both decrease gradually with temperature increasing further. The elongation has its minimum value at about 700 ℃. The TEM examination exhibits that sharing of the γ' by dislocation is almost the main deformation mechanism at low temperatures, but the γ' by-pass dominates the deformation at high temperatures. The transition temperature from shearing to by-pass should be around 800 ℃. The anomalous yield and intermediate-temperature brittleness behaviors should be attributed to the high content of γ'. In addition, the carbides and eutectic structure also contribute some to the ITB behaviors of the alloy.展开更多
By means of microstructure observation and measurement of creep properties,the high temperature creep behaviors of a single crystal nickel-based superalloy containing Re were investigated.Results show that the single ...By means of microstructure observation and measurement of creep properties,the high temperature creep behaviors of a single crystal nickel-based superalloy containing Re were investigated.Results show that the single crystal nickel-based superalloy containing 4.2% Re possesses a better creep resistance at high temperature.After being crept up to fracture,the various morphologies are displayed in the different areas of the sample,and the γ' phase is transformed into the rafted structure along the direction vertical to the applied stress axis in the regions far from the fracture.But the coarsening and twisting extents of the rafted γ' phase increase in the regions near the fracture,which is attributed to the occurrence of the larger plastic deformation.In the later stage of creep,the deformation mechanism of the alloy is that the dislocations with [01^-1]and [011] trace features shear into the rafted γ' phase.The main/secondary slipping dislocations are alternately activated to twist the rafted γ' phase up to the occurrence of creep fracture,which is thought to be the fracture mechanism of the alloy during creep.展开更多
Nickel-based superalloys are easy to produce low cycle fatigue(LCF)damage when they are subjected to high temperature and mechanical stresses.Fatigue life prediction of nickel-based superalloys is of great importance ...Nickel-based superalloys are easy to produce low cycle fatigue(LCF)damage when they are subjected to high temperature and mechanical stresses.Fatigue life prediction of nickel-based superalloys is of great importance for their reliable practical application.To investigate the effects of total strain and grain size on LCF behavior,the high temperature LCF tests were carried out for a nickel-based superalloy.The results show that the fatigue lives decreased with the increase of strain amplitude and grain size.A new LCF life prediction model was established considering the effect of grain size on fatigue life.Error analyses indicate that the prediction accuracy of the new LCF life model is higher than those of Manson-Coffin relationship and Ostergren energy method.展开更多
Selective laser melting(SLM),an additive manufacturing process mostly applied in the metal material field,can fabricate complex-shaped metal objects with high precision.Nickel-based superalloy exhibits excellent mecha...Selective laser melting(SLM),an additive manufacturing process mostly applied in the metal material field,can fabricate complex-shaped metal objects with high precision.Nickel-based superalloy exhibits excellent mechanical properties at elevated temperatures and plays an important role in the aviation industry.This paper emphasizes the research of SLM processed Inconel 718,Inconel 625,CM247LC,and Hastelloy X,which are typical alloys with different strengthening mechanisms and operating temperatures.The strengthening mechanism and phase change evolution of different nickel-based superalloys under laser irradiation are discussed.The influence of laser parameters and the heat-treatment process on mechanical properties of SLM nickel-based superalloys are systematically introduced.Moreover,the attractive in-dustrial applications of SLM nickel-based superalloy and printed components are presented.Finally,the prospects for nickel-based superalloy materials for SLM technology are presented.展开更多
The morphological evolution of the γ' phase in nickel-based superalloy жc6y during various solution heat treatments was investigated. The significant changes of the γ' precipitates were observed in the solu...The morphological evolution of the γ' phase in nickel-based superalloy жc6y during various solution heat treatments was investigated. The significant changes of the γ' precipitates were observed in the solution-treated samples. The coarsening and dissolution of γ' phase simulta-neously occurred at intermediate temperatures. In some areas, the primary precipitates became blunt and the adjacent ones were intercon-nected with each other via a diffuse neck, indicating a coarsening process of the primary γ' population. The coarsening was dominated by the precipitate agglomeration mechanism (PAM) rather than by the well-known Ostwald ripening mechanism. In other areas, the partial dissolu-tion of the γ' precipitates began to occur, spreading gradually from dendrite cores to interdendritic regions. In addition, a flower-like γ' struc-ture was developed during the subsolvus solution treatments. The observable long filaments composed of erraticly shaped precipitates were caused by the heterogeneous nucleation of the cooling precipitates during water quenching.展开更多
Oxidation characteristics of Alloy 617 and Haynes 230 at 900 oC in simulated helium environment,hot steam environment containing H2 as well as in air and pure helium conditions were investigated.Compared to air condit...Oxidation characteristics of Alloy 617 and Haynes 230 at 900 oC in simulated helium environment,hot steam environment containing H2 as well as in air and pure helium conditions were investigated.Compared to air condition,the oxidation rate of Alloy 617 was not significantly affected in helium and hot steam environments,while Haynes 230 showed lower oxidation rate in helium environment.On the other hand,the oxide morphology and structure of Alloy 617 were strongly affected by the environments,but those of Haynes 230 were less dependent on the environments.For Haynes 230,a Cr2O3 inner layer and a protective MnCr2O4 outer layer were formed in all environments,which contributed to the better oxidation resistance.As the mechanical properties,such as creep and tensile properties,were significantly affected by the oxidation behaviors,surface treatment methods to enhance oxidation resistance of these alloys should be developed.展开更多
Cylindrical samples of Ni-based GH4037 alloy were compressed at solid temperatures(1200,1250 and 1300℃) and semi-solid temperatures(1340,1350,1360,1370 and 1380℃) with different strain rates of 0.01,0.1 and 1 s-1.Hi...Cylindrical samples of Ni-based GH4037 alloy were compressed at solid temperatures(1200,1250 and 1300℃) and semi-solid temperatures(1340,1350,1360,1370 and 1380℃) with different strain rates of 0.01,0.1 and 1 s-1.High temperature deformation behavior and microstructure evolution of GH4037 alloy were investigated.The results indicated that flow stress decreased rapidly at semi-solid temperatures compared to that at solid temperatures.Besides,the flow stress continued to increase after reaching the initial peak stress at semi-solid temperatures when the strain rate was 1 s-1.With increasing the deformation temperature,the size of initial solid grains and recrystallized grains increased.At semi-solid temperatures,the grains were equiaxed,and liquid phase existed at the grain boundaries and inside the grains.Discontinuous dynamic recrystallization(DDRX) characterized by grain boundary bulging was the main nucleation mechanism for GH4037 alloy.展开更多
To study the hot deformation behavior of a new powder metallurgy nickel-based superalloy,hot compression tests were conducted in the temperature range of 1020−1110℃ with the strain rates of 0.001−1 s^−1.It is found t...To study the hot deformation behavior of a new powder metallurgy nickel-based superalloy,hot compression tests were conducted in the temperature range of 1020−1110℃ with the strain rates of 0.001−1 s^−1.It is found that the flow stress of the superalloy decreases with increasing temperature and decreasing strain rate.An accurate constitutive equation is established using a hyperbolic-sine type expression.Moreover,processing map of the alloy is constructed to optimize its hot forging parameters.Three domains of dynamic recrystallization stability and instability regions are identified from the processing map at a strain of 0.7,respectively.The adiabatic shear band,intergranular crack and a combination of intergranular crack and wedge crack are demonstrated to be responsible for the instabilities.Comprehensively analyzing the processing map and microstructure,the optimal isothermal forging conditions for the superalloy is determined to be t=1075−1105℃ andε&=10^−3−10−2.8 s^−1.展开更多
The surface microstructure and the surface segregation of FGH 95 nickel-basedsuperalloy powders prepared through plasma rotating electrode processing (PREP) have beeninvestigated by using SEM and AES. The results indi...The surface microstructure and the surface segregation of FGH 95 nickel-basedsuperalloy powders prepared through plasma rotating electrode processing (PREP) have beeninvestigated by using SEM and AES. The results indicate that the surface microstructure of powderschanges from dendrite into cellular stricture as the particle size of powders decrease, and thepredominant precipitates solidified on the particle surfaces were identified as MC' type carbidesenriched with Nb and Ti. It was also indicated that along with the depth of particle surfaces, thesegregation layer of S, C and O elements are thick, and that of Ti, Cr elements are thin for largesire powders while they are in reverse for median size particles.展开更多
The low-cycle fatigue (LCF) behavior of a nickel-based single crystal superalloy with [001] orientation was studied at an intermediate temperature of T0℃ and a higher temperature of To + 250℃ under a constant low...The low-cycle fatigue (LCF) behavior of a nickel-based single crystal superalloy with [001] orientation was studied at an intermediate temperature of T0℃ and a higher temperature of To + 250℃ under a constant low strain rate of 10^-3 s^-1 in ambient atmosphere. The superalloy exhibited cyclic tension-compression asymmetry which is dependent on the temperature and applied strain amplitude. Analysis on the fracture surfaces showed that the surface and subsurface casting micropores were the major crack initiation sites. Interior Ta-rich carbides were frequently observed in all specimens. Two distinct types of fracture were suggested by fractogaphy. One type was characterized by Mode-I cracking with a microscopically rough surface at To + 250℃. Whereas the other type at lower temperature T0℃ favored either one or several of the octahedral {111} planes, in contrast to the normal Mode-I growth mode typically observed at low loading frequencies (several Hz). The failure mechanisms for two cracking modes are shearing of γ' precipitates together with the matrix at T0℃ and cracking confined in the matrix and the γ/γ'interface at To - 250℃.展开更多
A series of directional solidification experiments have been performed to study the effect of cooling rate on the precipitation behavior of MC carbide in nickel-based superalloy under the temperature gradient of 500 K...A series of directional solidification experiments have been performed to study the effect of cooling rate on the precipitation behavior of MC carbide in nickel-based superalloy under the temperature gradient of 500 K-s^-1. Results reveal that the morphology of MC carbide changes from coarse block to fine strip, then to Chinese-script, and their sizes reduce gradually with the increasing of cooling rate from 2.53 K.s^-1 to 36.4 K.s^-1. At low cooling rates, most of these carbides are found to be located at the grain boundary and interdendritic regions, while the coupled growth of some carbides and 7 matrix in the center of 7 grains is occurred at high cooling rate. The main elements forming MC carbide are Ta, W, and Hf.展开更多
Evaluating the recyclability of powders in additive manufacturing has been a long-term challenge.In this study,the microstructure and mechanical properties of a nickel-based superalloy fabricated by laser powder-bed f...Evaluating the recyclability of powders in additive manufacturing has been a long-term challenge.In this study,the microstructure and mechanical properties of a nickel-based superalloy fabricated by laser powder-bed fusion(LPBF)using recycled powders were investigated.Re-melted powder surfaces,satellite particles,and deformed powders were found in the recycled powders,combined with a high-oxygencontent surface layer.The increasing oxygen content led to the formation of high-density oxide inclusions;moreover,printing-induced cracks widely occurred and mainly formed along the grain boundaries in the as-built LPBF nickel-based superalloys fabricated using recycled powders.A little change in the Si or Mn content did not increase the hot cracking susceptibility(HCS)of the printed parts.The changing aspect ratio and the surface damage of the recycled powders might contribute to increasing the crack density.Moreover,the configuration of cracks in the as-built parts led to anisotropic mechanical properties,mainly resulting in extremely low ductility vertical to the building direction,and the cracks mainly propagated along the cellular boundary owing to the existence of a brittle precipitation phase.展开更多
The Shima yield criterion used in finite element analysis for nickel-based superalloy powder compact during hot isostatic pressing(HIP) was modified through uniaxial compression experiments. The influence of cylindric...The Shima yield criterion used in finite element analysis for nickel-based superalloy powder compact during hot isostatic pressing(HIP) was modified through uniaxial compression experiments. The influence of cylindrical capsule characteristics on FGH4096M superalloy powder compact deformation and densification behavior during HIP was investigated through simulations and experiments. Results revealed the simulation shrinkage prediction fitted well with the experimental shrinkage including a maximum shrinkage error of 1.5%. It was shown that the axial shrinkage was 1.7% higher than radial shrinkage for a cylindrical capsule with the size of ∮50 mm × 100 mm due to the force arm difference along the axial and radial direction of the capsule. The stress deviated from the isostatic state in the capsule led to the uneven shrinkage and non-uniform densification of the powder compact. The ratio of the maximum radial displacement to axial displacement increased from0.47 to 0.75 with the capsule thickness increasing from 2 to 4 mm. The pressure transmission is related to the capsule thickness, the capsule material performance, and physical parameters in the HIP process.展开更多
The service performance of the turbine blade root of an aero-engine depends on the microstructures in its superficial layer.This work investigated the surface deformation structures of turbine blade root of single cry...The service performance of the turbine blade root of an aero-engine depends on the microstructures in its superficial layer.This work investigated the surface deformation structures of turbine blade root of single crystal nickel-based superalloy produced under different creep feed grinding conditions.Gradient microstructures in the superficial layer were clarified and composed of a severely deformed layer(DFL)with nano-sized grains(48–67 nm)at the topmost surface,a DFL with submicron-sized grains(66–158 nm)and micron-sized laminated structures at the subsurface,and a dislocation accumulated layer extending to the bulk material.The formation of such gradient microstructures was found to be related to the graded variations in the plastic strain and strain rate induced in the creep feed grinding process,which were as high as 6.67 and 8.17×10^(7)s^(−1),respectively.In the current study,the evolution of surface gradient microstructures was essentially a transition process from a coarse single crystal to nano-sized grains and,simultaneously,from one orientation of a single crystal to random orientations of polycrystals,during which the dislocation slips dominated the creep feed grinding induced microstructure deformation of single crystal nickel-based superalloy.展开更多
The cyclic deformation behavior and microstructure evolution of the 55Ni−23Cr−13Co nickel-based superalloy were studied at 750℃ under the strain amplitudes from 0.35%to 0.6%.Coffin−Manson−Basquin and Smith−Watson−Top...The cyclic deformation behavior and microstructure evolution of the 55Ni−23Cr−13Co nickel-based superalloy were studied at 750℃ under the strain amplitudes from 0.35%to 0.6%.Coffin−Manson−Basquin and Smith−Watson−Topper relationships were employed,which satisfactorily predicted the fatigue life of the alloy under various strain amplitudes.The superalloy showed an initial cyclic hardening as a result of the interaction between the dislocations and the precipitates,and following cyclic softening behavior mainly due to the shearing of theγ′phase by dislocations and dislocations recovery under all strain amplitudes.Microstructure analyses showed that the M_(23)C_(6) carbides exhibited a continuous-chain distribution at lower strain amplitudes,while they showed a discontinuous distribution at higher strain amplitudes.As the strain amplitude increased,the size of theγ′phase decreased as the consequence of repeated shearing by dislocations.Fracture mechanisms were analyzed.Under higher strain amplitudes,cavities preferred to form around grain boundaries.展开更多
The present research aims to establish a quantitative relation between microstructure and chemical composition (i.e., Ti, Al, and Nb) of newly designed nickel-based superalloys. This research attempts to identify an...The present research aims to establish a quantitative relation between microstructure and chemical composition (i.e., Ti, Al, and Nb) of newly designed nickel-based superalloys. This research attempts to identify an optimum microstructure at which the minimum quanti- fies of γ/γ' and γ/γ" compounds are achieved and the best castability is predicted. The results demonstrate that the highest quantity of inter- metallic eutectics (i.e., 41.5wt%) is formed at 9.8wt% (Ti + A1). A significant quantity of intermetallics formed in superalloy 1 (with a com- position of7 - 9.8wt% (Ti + A1)), which can deteriorate its castability. The type and morphology of the eutectics changed and the amount considerably decreased with decreasing Ti + A1 content in superalloy 2 (with a composition ofy - 7.6wt% (Ti + A1), 1.Swt% Nb). Thus, it is predicted that the castability would improve for superalloy 2. The same trend was observed for superalloy 4 (with a composition of 7 - 3.7wt% (Ti + A1), 4.4wt% Nb). This means that the amount of Laves increases with increasing Nb (to 4.4wt%) and decreasing Ti + A1 (to 3.7wt%) in su- peralloy 4. The best castability was predicted for superalloy 3 (with a composition ofy - 5.7wt% (Ti + A1), 2.8wt% Nb).展开更多
The oxidation behavior of a nickel-based superalloy at 1000°C in air was investigated through X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy analysis. A series of oxides, incl...The oxidation behavior of a nickel-based superalloy at 1000°C in air was investigated through X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy analysis. A series of oxides, including external oxide scales(Cr_2O_3,(TiO_2 + Mn Cr_2O_4)) and internal oxides(Al_2O_3,Ti N), were formed on the surface or sub-surface of the substrate at 1000°C in experimental still air. The oxidation resistance of the alloy was dependent on the stability of the surface oxide layer. The continuity and density of the protective Cr_2O_3 scale were affected by minor alloying elements such as Ti and Mn. The outermost oxide scale was composed of TiO_2 rutile and Mn Cr_2O_4 spinel, and the growth of TiO_2 particles was controlled by the outer diffusion of Ti ions through the pre-existing oxide layer. Severe internal oxidation occurred beneath the external oxide scale, consuming Al and Ti of the strength phase γ′(Ni_3(Al,Ti)) and thereby severely deteriorating the surface mechanical properties. The depth of the internal oxidation region was approximately 35 μm after exposure to experimental air at 1000°C for 80 h.展开更多
Grain growth, mechanical properties, and fracture mechanism of nickel-based GH4099 superalloy are investigated using heat treatments, tensile tests, optical microscopy (OM), and scanning electron microscopy (SEM) with...Grain growth, mechanical properties, and fracture mechanism of nickel-based GH4099 superalloy are investigated using heat treatments, tensile tests, optical microscopy (OM), and scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDS). The OM observation shows that the matrix grains (γ-grains) undergo an apparent growth during the solution treatment. The grain size diameter increases from 100 to 174 μm when the solution temperature rises from 1100℃ to 1160℃ for 30 min. When the holding time increases from 15 to 60 min at 1140℃, the grain size diameter increases from 140 to 176 μm, indicating that the γ-grain growth is more sensitive to temperature than time. Standard deviation, <em>S</em><sub>v</sub>, and the grain size distribution are utilized to characterize the microstructural uniformity. To predict the grain size more accurately, we develop the grain growth kinetics and find that the growth index is close to 5. The yield strength (<em>R</em><sub>p0.2</sub>), tensile strength (<em>R</em><sub>m</sub>), and ductility (<em>A</em><sub>f</sub>) are also measured. It is found that the effect decreases in the order cooling rate, solution temperature, time. <em>R</em><sub>p0.2</sub> reduces by 47% with the increase in the cooling rate from 1℃ to 8000℃/min, while both strength and ductility exhibit little changes with time. The SEM results show that the fracture surfaces have typical mixed brittle and ductile characteristics when specimens are subjected to water quenching and air cooling. However, a complete brittle fracture occurs under furnace cooling conditions. The EDS analysis indicates that the brittle γ' (Ni<sub>3</sub>Ti) phase precipitates around the γ-grain boundary during the slow cooling process, which is the main factor yielding the complete brittle fracture. Finally, the optimal solution treatment scheme for the GH4099 superalloy is proposed—a temperature of 1140℃ for 30 min followed by air cooling.展开更多
基金financially supported by the National Natural Science Foundation of China(Nos.92160301,92060203,52175415 and 52205475)the Science Center for Gas Turbine Project(Nos.P2022-AB-Ⅳ-002-001 and P2023-B-Ⅳ-003-001)+3 种基金the Jiangsu Key Laboratory of Precision and Micro-Manufacturing Technology(No.JSKL2223K01)the Natural Science Foundation of Jiangsu Province(No.BK20210295)the Superior Postdoctoral Project of Jiangsu Province(No.2022ZB215)the Henan Science and Technology Public Relations Project(No.212102210445).
文摘The undeformed chip thickness and grinding force are key parameters for revealing the material removal mechanism in the grinding process.However,they are difficult to be well expressed due to the ununiformed protrusion height and random position distribution of abrasive grains on the abrasive wheel surface.This study investigated the distribution of undeformed chip thickness and grinding force considering the non-uniform characteristics of abrasive wheel in the grinding of K4002 nickel-based superalloy.First,a novel grinding force model was established through a kinematic-geometric analysis and a grain-workpiece contact analysis.Then,a series of grinding experiments were conducted for verifying the model.The results indicate that the distribution of undeformed chip thickness is highly consistent with the Gaussian distribution formula.The increase in the grinding depth mainly leads to an increase in the average value of Gaussian distribution.On the contrary,the increase in the workpiece infeed speed or the decrease in the grinding speed mainly increases the standard deviation of Gaussian distribution.The average and maximum errors of the grinding force model are 4.9%and 14.6%respectively,indicating that the model is of high predication accuracy.
基金the financial support by the Defense Industrial Technology Development Program(No.JCKY2020130C024)the National Science and Technology Major Project,China(No.Y2019-Ⅶ-0011-0151)the Science Center for Gas Turbine Project(No.P2022-C-Ⅳ-002-001)。
文摘Cracks have consistently been a significant challenge limiting the development of additive manufactured nickel-based superalloys.It is essential to investigate the location of cracks and their forming mechanism.This study extensively examines the impact of solidification process,microstructural evolution,and stress concentration on crack initiation during direct energy deposition(DED).The results emphasize that the crack formation is significantly related to large-angle grain boundaries,rapid cooling rates.Cracks caused by large-angle grain boundaries and a fast-cooling rate predominantly appear near the edge of the deposited samples.Liquation cracks are more likely to form near the top of the deposited sample,due to the presence ofγ/γ'eutectics.The secondary dendritic arm and the carbides in the interdendritic regions can obstruct liquid flow during the final stage of solidification,which results in the formation of solidification cracks and voids.This work paves the way to avoid cracks in nickel-based superalloys fabricated by DED,thereby enhancing the performance of superalloys.
基金Projects(2012BAI18B05,2012BAI18B01)supported by the Twelfth Five-Year National Science&Technology Support Program of ChinaProject(2009CB93004)supported by the National Basic Researh Program of China
文摘A nickel-based superalloy with good corrosion resistance was fabricated by directional solidification, and its microstructure and tensile properties at elevated temperatures were investigated. Microstructure observations reveal that the γ' precipitates are arrayed in the y matrix regularly with some MC, Ni5Hf and M3B2 particles distributed along the grain boundary. The tensile tests exhibit that the tensile properties depend on temperature significantly and demonstrate obvious anomalous yield and intermediate-temperature brittleness (ITB) behavior. Below 650℃, the yield strength decreases slightly but the ultimate tensile strength almost has no change. When the temperature is between 650 ℃ and 750 ℃, the yield and ultimate tensile strengths rise rapidly, and after then they both decrease gradually with temperature increasing further. The elongation has its minimum value at about 700 ℃. The TEM examination exhibits that sharing of the γ' by dislocation is almost the main deformation mechanism at low temperatures, but the γ' by-pass dominates the deformation at high temperatures. The transition temperature from shearing to by-pass should be around 800 ℃. The anomalous yield and intermediate-temperature brittleness behaviors should be attributed to the high content of γ'. In addition, the carbides and eutectic structure also contribute some to the ITB behaviors of the alloy.
基金Project(50571070) supported by the National Natural Science Foundation of China
文摘By means of microstructure observation and measurement of creep properties,the high temperature creep behaviors of a single crystal nickel-based superalloy containing Re were investigated.Results show that the single crystal nickel-based superalloy containing 4.2% Re possesses a better creep resistance at high temperature.After being crept up to fracture,the various morphologies are displayed in the different areas of the sample,and the γ' phase is transformed into the rafted structure along the direction vertical to the applied stress axis in the regions far from the fracture.But the coarsening and twisting extents of the rafted γ' phase increase in the regions near the fracture,which is attributed to the occurrence of the larger plastic deformation.In the later stage of creep,the deformation mechanism of the alloy is that the dislocations with [01^-1]and [011] trace features shear into the rafted γ' phase.The main/secondary slipping dislocations are alternately activated to twist the rafted γ' phase up to the occurrence of creep fracture,which is thought to be the fracture mechanism of the alloy during creep.
基金Project(51575129) supported by the National Natural Science Foundation of ChinaProject(J15LA51) supported by Shandong Province Higher Educational Science and Technology Program,ChinaProject(2017T100238) supported by China Postdoctoral Science Foundation
文摘Nickel-based superalloys are easy to produce low cycle fatigue(LCF)damage when they are subjected to high temperature and mechanical stresses.Fatigue life prediction of nickel-based superalloys is of great importance for their reliable practical application.To investigate the effects of total strain and grain size on LCF behavior,the high temperature LCF tests were carried out for a nickel-based superalloy.The results show that the fatigue lives decreased with the increase of strain amplitude and grain size.A new LCF life prediction model was established considering the effect of grain size on fatigue life.Error analyses indicate that the prediction accuracy of the new LCF life model is higher than those of Manson-Coffin relationship and Ostergren energy method.
基金the National Nat-ural Science Foundation of China(No.51901020)Shan-dong Key Research and Development Plan Project(No.2019JZZY010327)+1 种基金Aeronautical Science Foundation of China(No.201942074001)the Fundamental Research Funds for the Central Universities,University of Science and Technology Beijing(No.FRF-IP-20-05).
文摘Selective laser melting(SLM),an additive manufacturing process mostly applied in the metal material field,can fabricate complex-shaped metal objects with high precision.Nickel-based superalloy exhibits excellent mechanical properties at elevated temperatures and plays an important role in the aviation industry.This paper emphasizes the research of SLM processed Inconel 718,Inconel 625,CM247LC,and Hastelloy X,which are typical alloys with different strengthening mechanisms and operating temperatures.The strengthening mechanism and phase change evolution of different nickel-based superalloys under laser irradiation are discussed.The influence of laser parameters and the heat-treatment process on mechanical properties of SLM nickel-based superalloys are systematically introduced.Moreover,the attractive in-dustrial applications of SLM nickel-based superalloy and printed components are presented.Finally,the prospects for nickel-based superalloy materials for SLM technology are presented.
基金supported by the Aviation Industry Corporation of China (No. 201110026-01)
文摘The morphological evolution of the γ' phase in nickel-based superalloy жc6y during various solution heat treatments was investigated. The significant changes of the γ' precipitates were observed in the solution-treated samples. The coarsening and dissolution of γ' phase simulta-neously occurred at intermediate temperatures. In some areas, the primary precipitates became blunt and the adjacent ones were intercon-nected with each other via a diffuse neck, indicating a coarsening process of the primary γ' population. The coarsening was dominated by the precipitate agglomeration mechanism (PAM) rather than by the well-known Ostwald ripening mechanism. In other areas, the partial dissolu-tion of the γ' precipitates began to occur, spreading gradually from dendrite cores to interdendritic regions. In addition, a flower-like γ' struc-ture was developed during the subsolvus solution treatments. The observable long filaments composed of erraticly shaped precipitates were caused by the heterogeneous nucleation of the cooling precipitates during water quenching.
基金supported by the MEST/NRF (Nuclear R&D Program,2005-2004718 and 2009 0083392) of Korea
文摘Oxidation characteristics of Alloy 617 and Haynes 230 at 900 oC in simulated helium environment,hot steam environment containing H2 as well as in air and pure helium conditions were investigated.Compared to air condition,the oxidation rate of Alloy 617 was not significantly affected in helium and hot steam environments,while Haynes 230 showed lower oxidation rate in helium environment.On the other hand,the oxide morphology and structure of Alloy 617 were strongly affected by the environments,but those of Haynes 230 were less dependent on the environments.For Haynes 230,a Cr2O3 inner layer and a protective MnCr2O4 outer layer were formed in all environments,which contributed to the better oxidation resistance.As the mechanical properties,such as creep and tensile properties,were significantly affected by the oxidation behaviors,surface treatment methods to enhance oxidation resistance of these alloys should be developed.
基金Project(51575127)supported by the National Natural Science Foundation of China
文摘Cylindrical samples of Ni-based GH4037 alloy were compressed at solid temperatures(1200,1250 and 1300℃) and semi-solid temperatures(1340,1350,1360,1370 and 1380℃) with different strain rates of 0.01,0.1 and 1 s-1.High temperature deformation behavior and microstructure evolution of GH4037 alloy were investigated.The results indicated that flow stress decreased rapidly at semi-solid temperatures compared to that at solid temperatures.Besides,the flow stress continued to increase after reaching the initial peak stress at semi-solid temperatures when the strain rate was 1 s-1.With increasing the deformation temperature,the size of initial solid grains and recrystallized grains increased.At semi-solid temperatures,the grains were equiaxed,and liquid phase existed at the grain boundaries and inside the grains.Discontinuous dynamic recrystallization(DDRX) characterized by grain boundary bulging was the main nucleation mechanism for GH4037 alloy.
基金Project(2016YFB0700300)supported by the National Key Research and Development Program of ChinaProject(51774335)supported by the National Natural Science Foundation of China。
文摘To study the hot deformation behavior of a new powder metallurgy nickel-based superalloy,hot compression tests were conducted in the temperature range of 1020−1110℃ with the strain rates of 0.001−1 s^−1.It is found that the flow stress of the superalloy decreases with increasing temperature and decreasing strain rate.An accurate constitutive equation is established using a hyperbolic-sine type expression.Moreover,processing map of the alloy is constructed to optimize its hot forging parameters.Three domains of dynamic recrystallization stability and instability regions are identified from the processing map at a strain of 0.7,respectively.The adiabatic shear band,intergranular crack and a combination of intergranular crack and wedge crack are demonstrated to be responsible for the instabilities.Comprehensively analyzing the processing map and microstructure,the optimal isothermal forging conditions for the superalloy is determined to be t=1075−1105℃ andε&=10^−3−10−2.8 s^−1.
基金This work is financially supported by The National Defence Committee of ChineseTechnology(No.95-YJ-20)
文摘The surface microstructure and the surface segregation of FGH 95 nickel-basedsuperalloy powders prepared through plasma rotating electrode processing (PREP) have beeninvestigated by using SEM and AES. The results indicate that the surface microstructure of powderschanges from dendrite into cellular stricture as the particle size of powders decrease, and thepredominant precipitates solidified on the particle surfaces were identified as MC' type carbidesenriched with Nb and Ti. It was also indicated that along with the depth of particle surfaces, thesegregation layer of S, C and O elements are thick, and that of Ti, Cr elements are thin for largesire powders while they are in reverse for median size particles.
基金supported by the National Natural Science Foundation of China(No.50371042).
文摘The low-cycle fatigue (LCF) behavior of a nickel-based single crystal superalloy with [001] orientation was studied at an intermediate temperature of T0℃ and a higher temperature of To + 250℃ under a constant low strain rate of 10^-3 s^-1 in ambient atmosphere. The superalloy exhibited cyclic tension-compression asymmetry which is dependent on the temperature and applied strain amplitude. Analysis on the fracture surfaces showed that the surface and subsurface casting micropores were the major crack initiation sites. Interior Ta-rich carbides were frequently observed in all specimens. Two distinct types of fracture were suggested by fractogaphy. One type was characterized by Mode-I cracking with a microscopically rough surface at To + 250℃. Whereas the other type at lower temperature T0℃ favored either one or several of the octahedral {111} planes, in contrast to the normal Mode-I growth mode typically observed at low loading frequencies (several Hz). The failure mechanisms for two cracking modes are shearing of γ' precipitates together with the matrix at T0℃ and cracking confined in the matrix and the γ/γ'interface at To - 250℃.
基金financially supported by the Scientific Research Foundation for Ph.D.,Northwest A & F University (No.Z109021103)the Special Fund for Basic Scientific Research of Central Colleges,Northwest A & F University No.Z109021114)the fund of the State Key Laboratory of Solidification Processing in NWPU (SKLSP201220)
文摘A series of directional solidification experiments have been performed to study the effect of cooling rate on the precipitation behavior of MC carbide in nickel-based superalloy under the temperature gradient of 500 K-s^-1. Results reveal that the morphology of MC carbide changes from coarse block to fine strip, then to Chinese-script, and their sizes reduce gradually with the increasing of cooling rate from 2.53 K.s^-1 to 36.4 K.s^-1. At low cooling rates, most of these carbides are found to be located at the grain boundary and interdendritic regions, while the coupled growth of some carbides and 7 matrix in the center of 7 grains is occurred at high cooling rate. The main elements forming MC carbide are Ta, W, and Hf.
基金This work was financially supported by the National Key Research and Development Program of China(No.2017YFB 0702300)the National Natural Science Foundation of China(No.51871028)the Fundamental Research Funds for the Central Universities(No.FRF-TP-19-003B2).
文摘Evaluating the recyclability of powders in additive manufacturing has been a long-term challenge.In this study,the microstructure and mechanical properties of a nickel-based superalloy fabricated by laser powder-bed fusion(LPBF)using recycled powders were investigated.Re-melted powder surfaces,satellite particles,and deformed powders were found in the recycled powders,combined with a high-oxygencontent surface layer.The increasing oxygen content led to the formation of high-density oxide inclusions;moreover,printing-induced cracks widely occurred and mainly formed along the grain boundaries in the as-built LPBF nickel-based superalloys fabricated using recycled powders.A little change in the Si or Mn content did not increase the hot cracking susceptibility(HCS)of the printed parts.The changing aspect ratio and the surface damage of the recycled powders might contribute to increasing the crack density.Moreover,the configuration of cracks in the as-built parts led to anisotropic mechanical properties,mainly resulting in extremely low ductility vertical to the building direction,and the cracks mainly propagated along the cellular boundary owing to the existence of a brittle precipitation phase.
基金financially supported by Guangdong Province Key Field R&D Program, China (No. 2019B01 0935001)the National Nature Science Foundation of China (No. 51905192)the Fundamental Research Funds for the Central Universities (No. FRT-TP-20-006A2)
文摘The Shima yield criterion used in finite element analysis for nickel-based superalloy powder compact during hot isostatic pressing(HIP) was modified through uniaxial compression experiments. The influence of cylindrical capsule characteristics on FGH4096M superalloy powder compact deformation and densification behavior during HIP was investigated through simulations and experiments. Results revealed the simulation shrinkage prediction fitted well with the experimental shrinkage including a maximum shrinkage error of 1.5%. It was shown that the axial shrinkage was 1.7% higher than radial shrinkage for a cylindrical capsule with the size of ∮50 mm × 100 mm due to the force arm difference along the axial and radial direction of the capsule. The stress deviated from the isostatic state in the capsule led to the uneven shrinkage and non-uniform densification of the powder compact. The ratio of the maximum radial displacement to axial displacement increased from0.47 to 0.75 with the capsule thickness increasing from 2 to 4 mm. The pressure transmission is related to the capsule thickness, the capsule material performance, and physical parameters in the HIP process.
基金This work was financially supported by the National Nat-ural Science Foundation of China(Nos.51921003,51775275 and 51905363)the Natural Science Foundation of Jiangsu Province(No.BK20190940)+1 种基金the National Major Science and Technology Projects of China(No.2017-VII-0002-0095)the Six Talents Summit Project in Jiangsu Province(No.JXQC-002).
文摘The service performance of the turbine blade root of an aero-engine depends on the microstructures in its superficial layer.This work investigated the surface deformation structures of turbine blade root of single crystal nickel-based superalloy produced under different creep feed grinding conditions.Gradient microstructures in the superficial layer were clarified and composed of a severely deformed layer(DFL)with nano-sized grains(48–67 nm)at the topmost surface,a DFL with submicron-sized grains(66–158 nm)and micron-sized laminated structures at the subsurface,and a dislocation accumulated layer extending to the bulk material.The formation of such gradient microstructures was found to be related to the graded variations in the plastic strain and strain rate induced in the creep feed grinding process,which were as high as 6.67 and 8.17×10^(7)s^(−1),respectively.In the current study,the evolution of surface gradient microstructures was essentially a transition process from a coarse single crystal to nano-sized grains and,simultaneously,from one orientation of a single crystal to random orientations of polycrystals,during which the dislocation slips dominated the creep feed grinding induced microstructure deformation of single crystal nickel-based superalloy.
基金financial supports from the National Natural Science Foundation of China (Nos. 52025052, 51975405)。
文摘The cyclic deformation behavior and microstructure evolution of the 55Ni−23Cr−13Co nickel-based superalloy were studied at 750℃ under the strain amplitudes from 0.35%to 0.6%.Coffin−Manson−Basquin and Smith−Watson−Topper relationships were employed,which satisfactorily predicted the fatigue life of the alloy under various strain amplitudes.The superalloy showed an initial cyclic hardening as a result of the interaction between the dislocations and the precipitates,and following cyclic softening behavior mainly due to the shearing of theγ′phase by dislocations and dislocations recovery under all strain amplitudes.Microstructure analyses showed that the M_(23)C_(6) carbides exhibited a continuous-chain distribution at lower strain amplitudes,while they showed a discontinuous distribution at higher strain amplitudes.As the strain amplitude increased,the size of theγ′phase decreased as the consequence of repeated shearing by dislocations.Fracture mechanisms were analyzed.Under higher strain amplitudes,cavities preferred to form around grain boundaries.
文摘The present research aims to establish a quantitative relation between microstructure and chemical composition (i.e., Ti, Al, and Nb) of newly designed nickel-based superalloys. This research attempts to identify an optimum microstructure at which the minimum quanti- fies of γ/γ' and γ/γ" compounds are achieved and the best castability is predicted. The results demonstrate that the highest quantity of inter- metallic eutectics (i.e., 41.5wt%) is formed at 9.8wt% (Ti + A1). A significant quantity of intermetallics formed in superalloy 1 (with a com- position of7 - 9.8wt% (Ti + A1)), which can deteriorate its castability. The type and morphology of the eutectics changed and the amount considerably decreased with decreasing Ti + A1 content in superalloy 2 (with a composition ofy - 7.6wt% (Ti + A1), 1.Swt% Nb). Thus, it is predicted that the castability would improve for superalloy 2. The same trend was observed for superalloy 4 (with a composition of 7 - 3.7wt% (Ti + A1), 4.4wt% Nb). This means that the amount of Laves increases with increasing Nb (to 4.4wt%) and decreasing Ti + A1 (to 3.7wt%) in su- peralloy 4. The best castability was predicted for superalloy 3 (with a composition ofy - 5.7wt% (Ti + A1), 2.8wt% Nb).
基金financial support of Science and Technology Program of Jiangsu Province (Nos. BE2015144 and BE2015145)
文摘The oxidation behavior of a nickel-based superalloy at 1000°C in air was investigated through X-ray diffraction, scanning electron microscopy, and energy-dispersive spectroscopy analysis. A series of oxides, including external oxide scales(Cr_2O_3,(TiO_2 + Mn Cr_2O_4)) and internal oxides(Al_2O_3,Ti N), were formed on the surface or sub-surface of the substrate at 1000°C in experimental still air. The oxidation resistance of the alloy was dependent on the stability of the surface oxide layer. The continuity and density of the protective Cr_2O_3 scale were affected by minor alloying elements such as Ti and Mn. The outermost oxide scale was composed of TiO_2 rutile and Mn Cr_2O_4 spinel, and the growth of TiO_2 particles was controlled by the outer diffusion of Ti ions through the pre-existing oxide layer. Severe internal oxidation occurred beneath the external oxide scale, consuming Al and Ti of the strength phase γ′(Ni_3(Al,Ti)) and thereby severely deteriorating the surface mechanical properties. The depth of the internal oxidation region was approximately 35 μm after exposure to experimental air at 1000°C for 80 h.
文摘Grain growth, mechanical properties, and fracture mechanism of nickel-based GH4099 superalloy are investigated using heat treatments, tensile tests, optical microscopy (OM), and scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDS). The OM observation shows that the matrix grains (γ-grains) undergo an apparent growth during the solution treatment. The grain size diameter increases from 100 to 174 μm when the solution temperature rises from 1100℃ to 1160℃ for 30 min. When the holding time increases from 15 to 60 min at 1140℃, the grain size diameter increases from 140 to 176 μm, indicating that the γ-grain growth is more sensitive to temperature than time. Standard deviation, <em>S</em><sub>v</sub>, and the grain size distribution are utilized to characterize the microstructural uniformity. To predict the grain size more accurately, we develop the grain growth kinetics and find that the growth index is close to 5. The yield strength (<em>R</em><sub>p0.2</sub>), tensile strength (<em>R</em><sub>m</sub>), and ductility (<em>A</em><sub>f</sub>) are also measured. It is found that the effect decreases in the order cooling rate, solution temperature, time. <em>R</em><sub>p0.2</sub> reduces by 47% with the increase in the cooling rate from 1℃ to 8000℃/min, while both strength and ductility exhibit little changes with time. The SEM results show that the fracture surfaces have typical mixed brittle and ductile characteristics when specimens are subjected to water quenching and air cooling. However, a complete brittle fracture occurs under furnace cooling conditions. The EDS analysis indicates that the brittle γ' (Ni<sub>3</sub>Ti) phase precipitates around the γ-grain boundary during the slow cooling process, which is the main factor yielding the complete brittle fracture. Finally, the optimal solution treatment scheme for the GH4099 superalloy is proposed—a temperature of 1140℃ for 30 min followed by air cooling.