THE ROLE OF NIOBIUM IN NICKEL-BASED SUPERALLOYS AND CHARACTERIZATION OF PM ALLOY EP741NP
1
作者 T. Carneiro J. Radavich D. Furrer 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2005年第4期468-478,共11页
The role of niobium in nickel-based superalloys is reviewed. The importance of niobium as a strengthener is discussed. New developments in nickel-based superalloys are also briefly mentioned, including some results th... The role of niobium in nickel-based superalloys is reviewed. The importance of niobium as a strengthener is discussed. New developments in nickel-based superalloys are also briefly mentioned, including some results that show improved resistance to sulfidation by niobium. Research results from a current program on the role of niobium in the Russian powder metallurgy alloy EP741NP are presented. Future research plans on the role of niobium in superalloys are also discussed. 展开更多
关键词 niobium superalloy alloy ep741np powder metallurgy superalloy nickel-based superalloy disk material
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部