Synthesis of benzoxazine-based phenolic resin containing furan groups 被引量:5
1
作者 Sheng Fang Li School of Chemical and Material Engineering,Huangshi Institute of Technology,Huangshi 435003,China 《Chinese Chemical Letters》 SCIE CAS CSCD 2010年第7期868-871,共4页
A novel benzoxazine-based phenolic resin containing furan groups(PFB) was synthesized via simple two-step reactions and the structure of PFB was confirmed by FTIR and ~1H NMR spectra.Differential scanning calorimetr... A novel benzoxazine-based phenolic resin containing furan groups(PFB) was synthesized via simple two-step reactions and the structure of PFB was confirmed by FTIR and ~1H NMR spectra.Differential scanning calorimetry(DSC) showed that the polybenzoxazine cured from PFB had good heat resistance and lower polymerization temperature compared with that of benzoxazine-based phenolic resins. 展开更多
关键词 BENZOXAZINE Phenolic resin furan Phenol-furfural Performance enhancement
下载PDF
Effect of praseodymium on catalytic graphitization of furan resin carbon 被引量:3
2
作者 易守军 陈金华 +2 位作者 肖雄 刘露 樊桢 《Journal of Rare Earths》 SCIE EI CAS CSCD 2010年第1期69-71,共3页
We introduced a new catalyst,rare earth element praseodymium,for the catalytic graphitization of furan resin carbon.The extent of graphitization of the furan resin carbon was examined by X-ray diffraction and Raman sp... We introduced a new catalyst,rare earth element praseodymium,for the catalytic graphitization of furan resin carbon.The extent of graphitization of the furan resin carbon was examined by X-ray diffraction and Raman spectroscopy.The morphology of furan resin carbon was characterized by scanning electron microscopy.The effects of the praseodymium content and the heat-treatment temperature on the catalytic graphitization of furan resin carbon were also investigated.The results indicated that the praseodymium c... 展开更多
关键词 catalytic graphitization PRASEODYMIUM furan resin X-ray diffraction Raman spectroscopy rare earths
下载PDF
Optimization of tensile strength for new type acetone-urea-formaldehyde furan resin using uniform design 被引量:5
3
作者 Lin Shengjun Zhao Wei +2 位作者 Li Yuancai Tong Siyi Wang Wenqing 《China Foundry》 SCIE CAS 2011年第1期30-35,共6页
In this study,the 24 h tensile strength of new type acetone-urea-formaldehyde furan resin (nitrogen content 3%) was investigated by uniform design optimization.Four independent variables such as acetone:formaldehyde m... In this study,the 24 h tensile strength of new type acetone-urea-formaldehyde furan resin (nitrogen content 3%) was investigated by uniform design optimization.Four independent variables such as acetone:formaldehyde molar ratio (mol/mol),solution pH value,reaction temperature (℃) and reaction time (min) were considered in the experiments.U13(134) uniform design was employed and the equation of 24 h tensile strength model was obtained after 13 experimentations.The 24 h tensile strength was optimized by applying single factor experiments and stepwise non-linear regression analysis.Minitab (Minitab 15 trial version) and MATLAB (R2010a trial version) were used for data analysis.The t-value and p-value indicate that the major impact factors include the interaction effect of solution pH value and reaction temperature (X2X3),the linear terms of acetone:formaldehyde molar ratio (X1),reaction time (X4) followed by the square effects of acetone/formaldehyde molar ratio (X1X1).The optimized results were achieved with the acetone:formaldehyde molar ratio (mol/mol) at 3:1,solution pH value at 6.0,reaction temperature at 70℃,and reaction time at 140 min,respectively.This method can not only significantly reduce the number and cost of the tests,but also provide a good experimental design strategy for the development of furan resin.The investigation shows that the predicted results of 24 h tensile strength are consistent well with the experimental ones. 展开更多
关键词 acetone-urea-formaldehyde furan resin 24 h tensile strength single factor experiment uniform design stepwise regression
下载PDF
Emission of BTEX and PAHs from molding sands with furan cold setting resins containing different contents of free furfuryl alcohol during production of cast iron 被引量:2
4
作者 Mariusz Holtzer Sylwia Zymankowska–Kumon +1 位作者 Angelika Kmita Rafal Dańko 《China Foundry》 SCIE 2015年第6期446-450,共5页
At present, furan resin is the largest selling no-bake system of moulding sands. The most commonly used furan no-bake binders(FNB) are condensation products of furfuryl alcohol(FA) urea, formaldehyde and phenol. They ... At present, furan resin is the largest selling no-bake system of moulding sands. The most commonly used furan no-bake binders(FNB) are condensation products of furfuryl alcohol(FA) urea, formaldehyde and phenol. They are generally cured by exposure to organic sulfonic acids. FNB provide excellent mold and core strength, cure rapidly and allow the sand to be reclaimed at fairly high yields, generally 75%-80%, especially in applications where due allowance is made for the need to keep total sulfur content below 0.1%. However, due to probable carcinogenic properties of furfuryl alcohol, the EU Directive limits the content of this substance(in a monomer form in resin) to 25%. The classification of furfuryl alcohol and the resulting furan resin products has changed from "harmful" to "toxic by inhalation". The aim of this study was to determine the effect of free furfuryl alcohol content in the resin on the emission of harmful substances from the BTEX(Benzene Toluene Ethylbenzene & Xylene) and PAHs(polycyclic aromatic hydrocarbon) group exposed to high temperature and how it affects the emissions allowance of reclaimed sand in the matrix. Three resins from a leading manufacturer were examined, which contain a free furfuryl alcohol content of 71%-72%, about 50% and < 25%, respectively. The hardener for each resin was 65% aqueous solution of paratoluenesulfonic acid. Tests were carried out in semi-industrial conditions where liquid cast-iron was poured into sample sand mold at 1,350 °C. The matrix of the studied sands was reclaimed in the amount of 0, 50%, 100%, respectively.With the increase of free furfuryl alcohol content, the volume of evolved gases decreased. For all resins the main component from the BTEX group dominating in the emitted gases was benzene; however toluene also appeared in the amount of a few percentages. In contrast, ethylbenzene and xylenes occurred only in the gases emitted from resin-bonded sands with the largest furfuryl alcohol content. The increase in the share of reclaimed sands resulted in very significant increase in the volume of gas generated and participation of benzene in these gases. In terms of emission of compounds from the PAHs group virtually for all resins, the total content of these substances was comparable(within the limits of error). The main components were: fluoranthene, pyrene and benzo(a) anthracene. 展开更多
关键词 FOUNDRY free furfuryl alcohol furan resins BTEX and PAHs environmental protection
下载PDF
Substitute materials of furfuryl alcohol in furan resin used for foundry and their technical properties 被引量:1
5
作者 Ren Yuyan Li Yingmin 《China Foundry》 SCIE CAS 2009年第4期339-342,共4页
Based on a special synthesis process of furan resin,the furfuryl alcohol(FA),the main component of typical no-bake furan resins is substituted by ethanol and xylitol mother liquor which is relatively low price and che... Based on a special synthesis process of furan resin,the furfuryl alcohol(FA),the main component of typical no-bake furan resins is substituted by ethanol and xylitol mother liquor which is relatively low price and chemically active.Through orthogonal test,the optimal amount of xylitol liquor,ethanol and modifier has been determined.Finally,the test results on technical properties show that the performance can meet the production requirement well,which indicate a success in this substituting attempt. 展开更多
关键词 furan resin furfuryl alcohol substitution test technical property
下载PDF
Investigation on synthesis of a low cost no-bake furan resin system with a high strength
6
作者 Liu Weihua Liu Shiyang Li Yingmin 《China Foundry》 SCIE CAS 2014年第5期408-411,共4页
The synthesis of a low cost no-bake furan resin with a high strength was researched in this paper. Through the analysis of main factors influencing the strength of furan resin, an orthogonal experiment was conducted t... The synthesis of a low cost no-bake furan resin with a high strength was researched in this paper. Through the analysis of main factors influencing the strength of furan resin, an orthogonal experiment was conducted to optimize synthesis of urea-formaldehyde furan resin with 3% nitrogen. The critical factors and their optimal levels were confirmed, and high strength property was obtained. Subsequently, some active substitute materials, including polyols A agent, methyl alcohol, mother liquid of xylitol, polyols B agent and ethanol, were used for partly substitution of furfural alcohol, the main material component of furan resin. A good combination of the substitute materials was determined to achieve a high strength, and the overal proportion of substitute materials to the resin is 20%. In this study, the substitution mechanism on furan resin was also characterized and analyzed by IR. 展开更多
关键词 furan resin synthesis optimization substitute of furfuryl alcohol substitution mechanism
下载PDF
Curing mechanism of furan resin modified with different agents and their thermal strength
7
作者 Huang Renhe Gao Hongmei +1 位作者 Tang Yaoji Liu Qingyun 《China Foundry》 SCIE CAS 2011年第2期161-165,共5页
The curing mechanism of furfuryl alcohol and urea-formaldehyde furan resins was investigated using infrared spectroscopy(IR) technique.The curing productions of urea-formaldehyde furan resins modified with different a... The curing mechanism of furfuryl alcohol and urea-formaldehyde furan resins was investigated using infrared spectroscopy(IR) technique.The curing productions of urea-formaldehyde furan resins modified with different agents(i.e.sorbitol,polyester polyol,phenol and acetone) and the productions of incomplete curing were characterized by differential thermal analysis(DTA) and thermal gravity analysis(TG).The results indicate that except for polyester polyol,the other modifiers have little effect on the thermal strength of urea-formaldehyde furan resin.Furthermore,the thermal strength can be improved at a temperature of higher than 550℃. 展开更多
关键词 no-bake furan resin MODIFICATION thermal gravity analysis (TG) curing mechanism thermal strength
下载PDF
呋喃基磷杂菲阻燃剂的合成及在阻燃环氧树脂中的应用
8
作者 唐刚 陶熠 +6 位作者 邓丹 张冬欣 张诗华 刘秀玉 伍强 沈海峰 孙俊杰 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2024年第4期142-150,共9页
以5-羟甲基糠醛、糠胺、三氯氧磷和9,10-二氢-9-氧杂-10-磷杂菲-10-氧化物(DOPO)为原料合成了一种呋喃基磷杂菲阻燃剂(Furan-2DOPO),并利用傅里叶变换红外光谱(FTIR)、核磁共振波谱(^(1)H NMR和^(31)P NMR)对其结构进行了表征.进一步利... 以5-羟甲基糠醛、糠胺、三氯氧磷和9,10-二氢-9-氧杂-10-磷杂菲-10-氧化物(DOPO)为原料合成了一种呋喃基磷杂菲阻燃剂(Furan-2DOPO),并利用傅里叶变换红外光谱(FTIR)、核磁共振波谱(^(1)H NMR和^(31)P NMR)对其结构进行了表征.进一步利用Furan-2DOPO对环氧树脂进行阻燃改性,得到一系列阻燃环氧固化物.考察了Furan-2DOPO的用量对阻燃环氧固化物的力学性能、热稳定性以及阻燃性能的影响.研究结果表明,当Furan-2DOPO的添加量(质量分数)仅为5%时(磷质量分数为0.47%),环氧固化物的氧指数达到31.0%,且能够通过UL-94垂直燃烧V-0级测试.与未改性环氧树脂相比,添加2.5%和5%Furan-2DOPO的环氧固化物的最大热释放速率分别下降了31%和35%.此外,2种添加Furan-2DOPO的环氧固化物的拉伸强度均比未改性环氧树脂提升了约28%.炭层分析结果表明,Furan-2DOPO具有良好的催化成炭性能,有利于减少燃烧过程中可燃性气体的逸出,从而提升阻燃性能. 展开更多
关键词 环氧树脂 呋喃基磷杂菲 阻燃剂 热降解
下载PDF
玉米淀粉-糠醛共缩聚树脂塑料的制备
9
作者 贾永波 周云霞 +5 位作者 郑露露 刘博文 张俊 邓书端 周晓剑 杜官本 《化工新型材料》 CAS CSCD 北大核心 2024年第2期110-114,119,共6页
以来自农林的廉价植物提取物——玉米淀粉和糠醛为原料,合成一款生物基塑料淀粉-糠醇-甲醛共缩聚塑料(SFFP)。通过电喷雾电离质谱(ESI-MS)和X射线衍射(XRD)测试,表明淀粉、糠醛和甲醛在酸性条件下进行了共缩聚反应。该生物基SFFP塑料的... 以来自农林的廉价植物提取物——玉米淀粉和糠醛为原料,合成一款生物基塑料淀粉-糠醇-甲醛共缩聚塑料(SFFP)。通过电喷雾电离质谱(ESI-MS)和X射线衍射(XRD)测试,表明淀粉、糠醛和甲醛在酸性条件下进行了共缩聚反应。该生物基SFFP塑料的抗压强度与酚醛(PF)塑料相近。在300℃、氮气处理条件下的重量损失为18%,与PF塑料相比,SFFP具有较好的热降解性。此外,与PF塑料相比,SFFP具有更好的疏水性,且其可再生原材料含量高达87%,具有一定的应用价值。 展开更多
关键词 淀粉-呋喃树脂 交联 糠醛 热塑性树脂 生物质塑料
下载PDF
不同添加剂配比对镁合金砂型铸造用树脂砂性能的影响研究
10
作者 黄金鑫 蔡森 王恒 《山西冶金》 CAS 2024年第7期7-8,14,共3页
针对镁合金砂型铸造中使用的树脂砂,探讨了混砂时加入树脂、固化剂、阻燃剂、硅烷等添加剂的配方及作用。通过测定树脂砂的可使用时间、起模时间、抗压强度等参数,分析了不同添加剂配比对树脂砂性能的影响。研究结果表明,在确保树脂砂... 针对镁合金砂型铸造中使用的树脂砂,探讨了混砂时加入树脂、固化剂、阻燃剂、硅烷等添加剂的配方及作用。通过测定树脂砂的可使用时间、起模时间、抗压强度等参数,分析了不同添加剂配比对树脂砂性能的影响。研究结果表明,在确保树脂砂强度的基础上,尽量减少树脂和固化剂的配比量,可减少铸件气孔缺陷,改善高温性能,提高铸件质量,降低生产成本。该研究结果可为镁合金铸件的高质量生产提供技术支持。 展开更多
关键词 镁合金 呋喃树脂 砂型低压铸造 化学黏结剂砂造型
下载PDF
新型高活性无氮呋喃树脂母液的开发 被引量:1
11
作者 林生军 谢美芳 +2 位作者 罗志波 袁端鹏 李远才 《铸造》 CAS CSCD 北大核心 2015年第8期717-722,共6页
针对铸造用无氮呋喃树脂,设计出了一种新型树脂母液合成工艺,提出了一种新型无氮呋喃树脂制备方法。通过系统的试验研究和分析,得到了性能较好的低糠醇含量的无氮呋喃树脂,具有较好的应用前景。研究表明:加成阶段p H值为7.7、高温加成... 针对铸造用无氮呋喃树脂,设计出了一种新型树脂母液合成工艺,提出了一种新型无氮呋喃树脂制备方法。通过系统的试验研究和分析,得到了性能较好的低糠醇含量的无氮呋喃树脂,具有较好的应用前景。研究表明:加成阶段p H值为7.7、高温加成阶段温度为83℃、高温加成阶段时间为1.71 h;低温聚合阶段温度和时间分别为73℃和0.5 h、高温聚合阶段时间为2.1 h时得到的无氮呋喃树脂母液性能最好。 展开更多
关键词 无氮呋喃树脂 母液制备工艺 定制实验 模拟验证
下载PDF
呋喃树脂改性煤沥青的机理及热行为研究 被引量:12
12
作者 杨琴 李铁虎 +1 位作者 王娟 江元汝 《煤炭转化》 CAS CSCD 北大核心 2006年第1期66-68,72,共4页
以呋喃树脂为改性剂对煤沥青进行了改性,采用傅立叶红外光谱(FT-IR)和扫描电镜(SEM)对呋喃树脂改性煤沥青的机理进行了分析;采用热重和示差扫描量热技术(TG-DSC)对改性前后煤沥青的热解行为进行了分析.实验结果表明,呋喃树脂在煤沥青中... 以呋喃树脂为改性剂对煤沥青进行了改性,采用傅立叶红外光谱(FT-IR)和扫描电镜(SEM)对呋喃树脂改性煤沥青的机理进行了分析;采用热重和示差扫描量热技术(TG-DSC)对改性前后煤沥青的热解行为进行了分析.实验结果表明,呋喃树脂在煤沥青中起增塑作用,其增塑过程通过四步完成,呋喃树脂与煤沥青发生增塑作用时需要吸收热量;呋喃树脂改性煤沥青的耐热性提高,呋喃树脂对煤沥青的残炭率影响不大. 展开更多
关键词 煤沥青 呋喃树脂 机理 热行为
下载PDF
呋喃树脂对煤沥青流变性能的影响 被引量:12
13
作者 杨琴 李铁虎 +1 位作者 林起浪 单玲 《新型炭材料》 SCIE EI CAS CSCD 北大核心 2005年第1期67-70,共4页
采用旋转黏度计测定了含有不同比例呋喃树脂的煤沥青的表观黏度.考察了呋喃树脂对煤沥青表观黏度、残炭率及软化点的影响.同时,采用扫描电镜(SEM)研究了添加呋喃树脂后煤沥青的表面形貌.结果表明,添加质量分数为3.6%~9.0%的呋喃树脂使... 采用旋转黏度计测定了含有不同比例呋喃树脂的煤沥青的表观黏度.考察了呋喃树脂对煤沥青表观黏度、残炭率及软化点的影响.同时,采用扫描电镜(SEM)研究了添加呋喃树脂后煤沥青的表面形貌.结果表明,添加质量分数为3.6%~9.0%的呋喃树脂使煤沥青在达到相同黏度值时温度下降5℃~15℃,而残炭率不下降;由于呋喃树脂使煤沥青分子隔开从而改善了煤沥青的流动性能;另外加入适量的呋喃树脂可降低煤沥青的黏流活化能,有利于煤沥青在较宽温度范围内进行工艺操作. 展开更多
关键词 呋喃树脂 表观黏度 结焦值 流变性能 煤沥青 多核缩合芳烃 分子量 温度
下载PDF
碳/碳复合材料的基体前驱体研究进展 被引量:10
14
作者 付东升 张康助 +1 位作者 孙福林 姚冬梅 《化工新型材料》 CAS CSCD 2003年第6期19-21,29,共4页
本文综述了国内外碳 /碳复合材料基体前驱体的研究进展状况。讨论了不同物质 ,其中包括工业沥青、酚醛树脂、呋喃树脂、缩合多核芳香 (COPNA)树脂以及聚芳基乙炔树脂作为碳 /碳复合材料基体前驱体的特点。
关键词 碳/碳复合材料 基体前驱体 研究进展 沥青 酚醛树脂 呋喃树脂
下载PDF
高水分呋喃树脂的合成 被引量:4
15
作者 邱文革 李传强 +2 位作者 白广梅 王睿颖 宋秀庆 《北京工业大学学报》 EI CAS CSCD 北大核心 2009年第6期800-804,共5页
研究了脲醛改性呋喃树脂合成过程中反应温度、甲醛与尿素的物质的量之比、pH值、加料方式及改性剂等因素对产品性能的影响,给出了合成高水分呋喃树脂的较佳工艺条件.通过工艺控制和添加改性剂,制得了树脂砂黏结强度为2.28MPa,水的质量... 研究了脲醛改性呋喃树脂合成过程中反应温度、甲醛与尿素的物质的量之比、pH值、加料方式及改性剂等因素对产品性能的影响,给出了合成高水分呋喃树脂的较佳工艺条件.通过工艺控制和添加改性剂,制得了树脂砂黏结强度为2.28MPa,水的质量分数为18.9%,游离甲醛的质量分数为0.23%,黏度(20℃)为31mPa·s,外观为棕红色透明液体的呋喃树脂. 展开更多
关键词 呋喃树脂 铸造 游离甲醛
下载PDF
糠醇替代材料对呋喃树脂自硬砂强度的影响 被引量:5
16
作者 任玉艳 李英民 +2 位作者 刘伟华 刘柄言 刘军 《铸造》 CAS CSCD 北大核心 2008年第11期1199-1201,共3页
呋喃树脂是一种具有优良工艺性能的铸造用粘结剂,但呋喃树脂主要成分糠醇的快速涨价,限制了呋喃树脂的推广应用。分别采用相对糠醇价格便宜且性质活泼的材料:改性木质素、乙醇、山梨醇、木糖醇母液来对制备铸造用自硬呋喃树脂的主要成... 呋喃树脂是一种具有优良工艺性能的铸造用粘结剂,但呋喃树脂主要成分糠醇的快速涨价,限制了呋喃树脂的推广应用。分别采用相对糠醇价格便宜且性质活泼的材料:改性木质素、乙醇、山梨醇、木糖醇母液来对制备铸造用自硬呋喃树脂的主要成分糠醇进行部分替代。以抗拉强度为主要检测指标,确定了各个替代材料的用量。替代后的树脂强度高于或接近原树脂强度。 展开更多
关键词 铝硅合金 真空造型 铸造工艺
下载PDF
利用XRD研究呋喃树脂制备玻璃炭过程中的结构变化 被引量:13
17
作者 邱海鹏 赵根祥 《新型炭材料》 SCIE EI CAS CSCD 1999年第2期49-53,共5页
根据热失重曲线和运用X射线衍射(XRD)所测得的实验结果,讨论了聚糠醇(PFA)和聚糠酮(PFK)两种呋喃树脂在氮气气氛中热解过程中的结构变化。结果表明,两种试样在450℃以前,随着炭化温度的升高,聚合物分子的原有序... 根据热失重曲线和运用X射线衍射(XRD)所测得的实验结果,讨论了聚糠醇(PFA)和聚糠酮(PFK)两种呋喃树脂在氮气气氛中热解过程中的结构变化。结果表明,两种试样在450℃以前,随着炭化温度的升高,聚合物分子的原有序态结构逐渐被破坏;450℃以后,随着炭化温度的升高。 展开更多
关键词 呋喃树脂 热解过程 XRD 结构 玻璃炭
下载PDF
呋喃树脂固化体系及其固化机理研究进展 被引量:10
18
作者 夏宇 蔺向阳 +1 位作者 杜震 况方舟 《材料导报》 EI CAS CSCD 北大核心 2014年第19期79-83,共5页
呋喃树脂是重要的粘合剂之一,呋喃树脂的使用性能除了和呋喃树脂本身的性能有关外,还与呋喃树脂固化剂体系有很大的关系。主要介绍了国内外呋喃树脂固化剂体系的研究进展,总结归纳了各种固化剂的优缺点,并对它们的固化性能作了对比。从... 呋喃树脂是重要的粘合剂之一,呋喃树脂的使用性能除了和呋喃树脂本身的性能有关外,还与呋喃树脂固化剂体系有很大的关系。主要介绍了国内外呋喃树脂固化剂体系的研究进展,总结归纳了各种固化剂的优缺点,并对它们的固化性能作了对比。从这些对比中可以得出结论,在生产实践中,固化剂的使用必须根据生产条件和要求进行合理选择,以期发挥出各固化剂自身的优点,降低生产和使用成本。同时,还介绍了酸催化下呋喃树脂的固化机理的研究进展,并展望了呋喃树脂固化剂的发展方向。 展开更多
关键词 呋喃树脂 固化剂 固化机理
下载PDF
天然黑荆树皮单宁—糠醇木材胶黏剂的研究 被引量:11
19
作者 张俊 杜官本 周晓剑 《森林与环境学报》 CSCD 北大核心 2016年第4期500-505,共6页
通过天然黑荆树皮单宁与来自玉米及小麦剩余提取物的糠醇在酸性条件下反应,制备出一种新型无污染的热固性生物质木材胶黏剂。通过基质辅助激光解吸电离飞行时间质谱(MALDI-TOF-MS)及傅里叶红外光谱(FT-IR)对树脂的结构进行表征;采用静... 通过天然黑荆树皮单宁与来自玉米及小麦剩余提取物的糠醇在酸性条件下反应,制备出一种新型无污染的热固性生物质木材胶黏剂。通过基质辅助激光解吸电离飞行时间质谱(MALDI-TOF-MS)及傅里叶红外光谱(FT-IR)对树脂的结构进行表征;采用静态热机械性能分析(TMA)对树脂的玻璃转化温度及弹性模量进行表征;通过制备胶合板的胶合强度对树脂的胶合性能进行表征。结果表明:在酸性条件下,糠醇中的羟甲基能够且主要与单宁结构单体A环上的6或8号位上的C连接而缩聚成具有一定粘度的大分子化合物。同时,与基于脲醛树脂改性尿素—甲醛—糠醇树脂相比较,单宁—糠醇树脂具有更高的弹性模量及玻璃转化温度,且基于单宁—糠醇树脂制备胶合板的胶合性能优于尿素—甲醛—糠醇树脂。 展开更多
关键词 生物质树脂 单宁-糠醇树脂 胶合强度 共缩聚 木材胶黏剂
下载PDF
有色合金用呋喃树脂砂溃散性的研究 被引量:7
20
作者 凌宏江 戴绪绮 +1 位作者 魏华胜 王文清 《特种铸造及有色合金》 CAS CSCD 北大核心 1995年第2期12-15,共4页
呋喃树脂砂用于有色合金铸造时,由于浇注温度低,型芯的演散性较差。对于薄壁铝合金铸件和厚大型芯该问题尤其明显。为解决这个问题,作者以KJN-Ⅲ型呋喃树脂自硬砂为对象,就其在不同加热温度下的温度场、残留强度及热强度进行了... 呋喃树脂砂用于有色合金铸造时,由于浇注温度低,型芯的演散性较差。对于薄壁铝合金铸件和厚大型芯该问题尤其明显。为解决这个问题,作者以KJN-Ⅲ型呋喃树脂自硬砂为对象,就其在不同加热温度下的温度场、残留强度及热强度进行了系统的研究。通过对树脂添加剂与残留强度之间关系的研究,得到几种较好的树脂添加剂。在合适的加入量下,可使呋喃树脂砂的残留强度下降40%~80%,取得了令人满意的结果。 展开更多
关键词 溃散性 呋喃树脂砂 铸造 有色金属合金