期刊文献+
共找到460篇文章
< 1 2 23 >
每页显示 20 50 100
Effect of inclusions on the formation of acicular ferrite in Ti-bearing non quenched-and-tempered steel 被引量:6
1
作者 Ying Yang Chaobin Lai +2 位作者 Fuming Wang Zhanbing Yang Bo Song 《Journal of University of Science and Technology Beijing》 CSCD 2007年第6期501-506,共6页
Nucleation of acicular ferrite and its influence factors in non quenched-and-tempered steel was studied by using TEM and thermodynamic calculation. The results show that the complex particles with a center made of Ti ... Nucleation of acicular ferrite and its influence factors in non quenched-and-tempered steel was studied by using TEM and thermodynamic calculation. The results show that the complex particles with a center made of Ti oxide, Al2O3, and silicate and an outside made of a small quantity of mixture of TiN and MnS are able to act as ferrite nucleation nuclei. The acicular ferrite percentage changes little with Ti. When the oxygen content was 80 ppm, the volume percentage of acicular ferrite decreased due to an increase in allotriomorphic ferrite. The larger the cooling rate and the shorter the incubation time, the finer the titanium oxide and the higher the nucleation ratio of acicular ferrite. 展开更多
关键词 acicular ferrite titanium INCLUSIONS non quenched-and-tempered steel
下载PDF
Development of non-quenched and tempered bolt steel
2
作者 BAI Xifeng~(1)),ZHAO Xuebo~(1)),REN Yuhui~(1)),WANG Bingxi~(2)) and GUO Dayong~(2)) 1) Wire rod plant,Anshan Iron & Steel Co.,Ltd. 2) Technology Center,Anshan Iron & Steel Co.,Ltd.,Anshan 114021,China 《Baosteel Technical Research》 CAS 2010年第S1期62-,共1页
The 8.8 grade non-quenched and tempered bolt steel was studied according to the process conditions of wire rod plant and customer requirments.Three types of experimental steel grades were selected.10MnSiTi Nb and 20Mn... The 8.8 grade non-quenched and tempered bolt steel was studied according to the process conditions of wire rod plant and customer requirments.Three types of experimental steel grades were selected.10MnSiTi Nb and 20Mn2VTi(N) were chosen as the formal steel after several experimemts. 展开更多
关键词 non-quenched and tempered steel BOLT mechanical property
下载PDF
Theoretical calculation of the impact work in the alloying non-quenched and tempered steel 被引量:11
3
作者 LIU Zhilin1, LIN Cheng1 & GUO Yanchang2 1. Department of Materials and Chemical Engineering, Liaoning Institute of Technology, Jinzhou 121001, China 2. The Technical Center of Benxi Iron and Steel Group Corporation, Benxi 117000, China 《Science China(Technological Sciences)》 SCIE EI CAS 2006年第3期257-273,共17页
Coupled with hot-continuous rolling technology and based on the calculation of the finishing rolling impact work in the non-quenched and tempered Si-Mn steel, the calculations of the finishing rolling impact work in t... Coupled with hot-continuous rolling technology and based on the calculation of the finishing rolling impact work in the non-quenched and tempered Si-Mn steel, the calculations of the finishing rolling impact work in the alloying non-quenched and tempered steel with the elements of Cr, Ni, Mo, W, Cu, V, Nb and Ti are studied with the covalent electron number nA of the strongest bond in alloying phases, the smallest electron density difference ?ρ of phase interfaces, and the number of atom states σ (σ′) which keep the interface electron density continuous. The calculated results show that the finishing rolling impact work of the alloying non-quenched and tempered steel intensely depends on strengthening mechanisms. The solution strengthening, interface strengthening, precipita- tion strengthening of pearlite, and dispersion strengthening will result in the decrease of the finishing rolling impact work; the refinement strengthening, the precipitation strength- ening of V, Nb and Ti in α-Fe-C-V(Nb, Ti), and the residual austenite containing Ni on the boundary of α-Fe-C-Ni will increase the impact work; and the increments or decrements can be calculated with nA, ?ρ, σ (σ′) and weights of alloying elements. The calculation formulas of the finishing rolling impact work in this paper are intergraded with the sug- gested ones of the finishing rolling tensile strength, yield strength, and elongation of the non-quenched and tempered steel. The calculated results agree well with the measured ones. 展开更多
关键词 ALLOYING non-quenched and tempered steel ELECTRON structure impact work calculation.
原文传递
Theoretical calculation of the finishing rolling impact work in non-quenched and tempered Si-Mn steel 被引量:5
4
作者 LIU Zhilin1, LIN Cheng1 & WANG Ping2 1. Department of Materials and Chemical Engineering, Liaoning Institute of Technology, Jinzhou 121001, China 2. Mechanical Department, Armor technique Institute of PLA, Changchun 130117, China 《Science China(Technological Sciences)》 SCIE EI CAS 2006年第2期137-146,共10页
Based on the hot-continuous rolling technology, the finishing rolling impact work α k of the non-quenched and tempered Si-Mn steel is theoretically calculated with the covalent electron number nA of the strongest bon... Based on the hot-continuous rolling technology, the finishing rolling impact work α k of the non-quenched and tempered Si-Mn steel is theoretically calculated with the covalent electron number nA of the strongest bond in alloying phases, and the smallest interface electron density difference Δρ of alloying phase interface and the number of atom states σ which keep the interface electron density continuous. Calculations show that the solution strengthening, the precipitation strengthening, and the interface strengthening will result in the decrease of the finishing rolling impact work α k, and the effects of the number of atom states σ which keep the interface electron density continuous on the finishing rolling impact work α k are different. Taking the impact work and the number of atom states σ 0 keeping the electron density continuous of the phase interface α-Fe/α-Fe-C between α-Fe and α-Fe-C as reference values, the impact work of the interface will increase when σ of some interface is larger than σ 0; otherwise, the impact will decrease. Therefore, the finishing rolling impact work α k can be calculated with the impact value of the refined α-Fe matrix and the influence amounts caused by the solution strengthening, the precipitation strengthening, the interface strengthening, and the number of atom states σ which keep the interface electron density continuous. The calculated results agree well with the measured ones. In this paper, the effect of S on the impact work is also discussed. 展开更多
关键词 ELECTRON structure parameters non-quenched and tempered steel IMPACT WORK and calculation.
原文传递
Effect of Nb-V Microalloying on Microstructures and Mechanical Properties of Medium Carbon Non-Quenched and Tempered Steel 被引量:1
5
作者 CHENG Hui-jing 1,WANG Fu-ming 1,LI Chang-rong 2,ZHANG Bo 1,XIA Yun-jin 1 (1.School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing,Beijing 100083 2.School of Materials Science and Engineering,University of Science and Technology Beijing,Beijing 100083) 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2011年第S1期779-784,共6页
Based on optical microscope(OM),transmission electron microscope(TEM) and mechanical performance measurement,the microstructures and mechanical properties of Nb-V micro-alloying non-quenched and tempered steels have b... Based on optical microscope(OM),transmission electron microscope(TEM) and mechanical performance measurement,the microstructures and mechanical properties of Nb-V micro-alloying non-quenched and tempered steels have been studied.The results showed that the microstructure consists of ferrite and pearlite,in which there exists a lot of intragranular ferrite.Niobium carbide is the main form of carbonitrides,Nb-enriched carbonitrides refine grains,V-enriched carbonitrides have precipitation strengthening effect,which promotes the toughness of the studied steel.The mechanical properties for steels 1,2 and 3 have met the standards required by high load automobile crankshaft,in which the comprehensive property for No.2 is the best. 展开更多
关键词 non-quenched and tempered steel Nb-V microalloying strength and toughness-enhanced mechanism
原文传递
38MnVTi非调质钢的TTT曲线的测定与分析
6
作者 陈浩东 谢丁 陈元芳 《重庆理工大学学报(自然科学)》 CAS 北大核心 2024年第1期221-228,共8页
研究了38MnVTi非调质钢在等温冷却过程中的奥氏体转变产物及转变量与时间的关系。通过Gleeble-1 500D热模拟试验机获得不同等温温度的膨胀曲线。采用膨胀法,通过Gleeble-1 500D热模拟试验机获得不同等温温度的膨胀曲线,再计算和运用Ori... 研究了38MnVTi非调质钢在等温冷却过程中的奥氏体转变产物及转变量与时间的关系。通过Gleeble-1 500D热模拟试验机获得不同等温温度的膨胀曲线。采用膨胀法,通过Gleeble-1 500D热模拟试验机获得不同等温温度的膨胀曲线,再计算和运用Origin软件拟合得到38MnVTi非调质钢的等温转变曲线(TTT曲线)。结果表明:38MnVTi非调质钢渗碳体的析出温度为750℃、铁素体析出温度为840℃、马氏体析出温度为360℃以及马氏体转变终止温度为212℃。在540、510、480、430℃等温冷却条件下贝氏体的最大转变量分别为16.9%、26.8%、38.5%、55.3%。 展开更多
关键词 非调质钢 TTT曲线 膨胀法 热模拟
下载PDF
硼对Mn-Si-Cr系贝氏体型非调质钢过冷奥氏体连续转变行为的影响
7
作者 徐晓春 惠卫军 《现代交通与冶金材料》 CAS 2024年第6期87-94,共8页
本文采用热膨胀法结合硬度法及金相法研究了添加0.0016%(质量分数)的B与未加B的Mn⁃Si⁃Cr系贝氏体型非调质钢在不同冷却速度(0.02~44℃/s)下过冷奥氏体的连续冷却转变行为。结果表明,B元素的添加使得高温铁素体+珠光体转变受到明显抑制... 本文采用热膨胀法结合硬度法及金相法研究了添加0.0016%(质量分数)的B与未加B的Mn⁃Si⁃Cr系贝氏体型非调质钢在不同冷却速度(0.02~44℃/s)下过冷奥氏体的连续冷却转变行为。结果表明,B元素的添加使得高温铁素体+珠光体转变受到明显抑制而促进了中温贝氏体转变,降低了贝氏体开始转变温度和形成贝氏体的冷却速度,使得实验钢获得最大贝氏体体积分数(约80%)的冷却速度由未加B钢的~0.17℃/s降到添加B钢的~0.13℃/s。B的添加能够提高实验钢的硬度,硬度增量随着冷却速度的增加呈现先增大后减小的趋势,并在0.28℃/s时硬度增量达到峰值为55 HV5。在目前的成分体系下,很难获得体积分数接近100%的贝氏体组织,需要进一步优化实验钢的成分体系,以便在尽可能宽的冷却速度范围内获得尽可能多的贝氏体组织。 展开更多
关键词 贝氏体型非调质钢 连续冷却转变曲线 冷却速度 微观组织 硬度
下载PDF
35CrMo钢蓄能器开裂原因
8
作者 聂志川 《理化检验(物理分册)》 CAS 2024年第2期56-59,共4页
某公司生产的蓄能器在使用1 a后发生开裂现象。采用宏观观察、化学成分分析、力学性能测试、扫描电镜分析、金相检验等方法对蓄能器的开裂原因进行分析。结果表明:制做蓄能器壳体的35CrMo钢存在微裂纹;蓄能器工作时,内部介质气体和液压... 某公司生产的蓄能器在使用1 a后发生开裂现象。采用宏观观察、化学成分分析、力学性能测试、扫描电镜分析、金相检验等方法对蓄能器的开裂原因进行分析。结果表明:制做蓄能器壳体的35CrMo钢存在微裂纹;蓄能器工作时,内部介质气体和液压油产生的压力使微裂纹逐步扩展并贯穿管壁,导致蓄能器开裂。 展开更多
关键词 35CRMO钢 非金属夹杂物 晶粒度 调质处理 穿孔
下载PDF
8.8级非调紧固件用10B21盘条研究与开发
9
作者 孔祥伟 白云 张剑锋 《特殊钢》 2024年第1期23-26,共4页
采用转炉→精炼炉→真空脱气→方坯连铸→加热→粗轧→中轧→精轧→减定径→吐丝→XDWP(Xingcheng Direct Water Patenting)冷却→斯太尔摩风冷冷却的方式试验生产基于10B21钢的8.8级非调紧固件用热轧盘条。通过控制减定径温度为813℃,... 采用转炉→精炼炉→真空脱气→方坯连铸→加热→粗轧→中轧→精轧→减定径→吐丝→XDWP(Xingcheng Direct Water Patenting)冷却→斯太尔摩风冷冷却的方式试验生产基于10B21钢的8.8级非调紧固件用热轧盘条。通过控制减定径温度为813℃,吐丝温度为828℃,斯太尔摩辊道速率设置为0.75 m/s,在连续经过XDWP冷却和斯太尔摩风冷后获得的热轧盘条抗拉强度达到680 MPa,断后伸长率为23.6%,断面收缩率为75%,力学性能完全满足GB/T 29087―2012的要求。且经过1/4冷顶锻和25%的大减面率拉拔试验,其结果满足紧固件用户使用要求。 展开更多
关键词 8.8级非调紧固件 10B21钢 XDWP 贝氏体
下载PDF
汽车零部件用非调质钢切削性能改进
10
作者 邓向阳 庞卓纯 +1 位作者 李仕超 李大明 《理化检验(物理分册)》 CAS 2024年第11期22-26,共5页
钢的化学成分、显微组织、力学性能、硫化物形貌等是影响材料切削性能的重要因素。通过碲改质处理可以改善硫化物的形貌,改质后生成的MnTe-MnS共晶化合物可以使硫化物呈椭球体状。结果表明:碲改质后,长宽比小于2的硫化物占比接近50%,90... 钢的化学成分、显微组织、力学性能、硫化物形貌等是影响材料切削性能的重要因素。通过碲改质处理可以改善硫化物的形貌,改质后生成的MnTe-MnS共晶化合物可以使硫化物呈椭球体状。结果表明:碲改质后,长宽比小于2的硫化物占比接近50%,90%的硫化物长宽比小于6;碲改质后,材料切削阻抗力降低、刀具磨损量减少、材料表面粗糙度降低,材料的切削性能提高。 展开更多
关键词 非调质钢 切削性能 硫化物 碲改质处理 刀具磨损量
下载PDF
一种汽车用微合金非调质钢的连续冷却转变
11
作者 赵楠 孙晓冉 +2 位作者 王程明 郭维超 赵剑磊 《理化检验(物理分册)》 CAS 2024年第4期1-4,共4页
测定了一种汽车用微合金非调质钢的过冷奥氏体连续冷却转变曲线,研究了冷却速率对相变组织及显微硬度的影响。结果表明:试验钢的临界点A c3为838℃,A c1为732℃;当冷却速率小于0.2℃/s时,试验钢的连续冷却转变产物为铁素体、珠光体和贝... 测定了一种汽车用微合金非调质钢的过冷奥氏体连续冷却转变曲线,研究了冷却速率对相变组织及显微硬度的影响。结果表明:试验钢的临界点A c3为838℃,A c1为732℃;当冷却速率小于0.2℃/s时,试验钢的连续冷却转变产物为铁素体、珠光体和贝氏体;当冷却速率为0.2℃/s时,转变产物中出现马氏体;当冷却速率为5℃/s时,铁素体、珠光体消失,转变产物为贝氏体和马氏体;随着冷却速率的增大,马氏体含量逐渐增多,贝氏体含量逐渐减少,甚至完全消失;当冷却速率增大至20℃/s时,转变产物均为马氏体;随着冷却速率的增大,试验钢的显微硬度呈先快速增长,后增长速率变缓的趋势。 展开更多
关键词 微合金非调质钢 连续冷却转变曲线 临界点 显微组织 显微硬度
下载PDF
锻前加热次数对C70S6非调质钢连杆组织与性能的影响
12
作者 韩亚辉 陈荣标 +1 位作者 姜爱龙 伍启华 《金属加工(热加工)》 2024年第11期128-132,共5页
连杆生产时,经常出现坯料被反复加热的情况,反复加热的坯料是否能再次利用,则关系到原材料成本。以C70S6非调质钢为研究对象,将其进行反复加热,探究了加热次数对C70S6钢连杆组织与性能的影响。结果表明:加热次数低于4次的坯料可以正常使... 连杆生产时,经常出现坯料被反复加热的情况,反复加热的坯料是否能再次利用,则关系到原材料成本。以C70S6非调质钢为研究对象,将其进行反复加热,探究了加热次数对C70S6钢连杆组织与性能的影响。结果表明:加热次数低于4次的坯料可以正常使用,加热次数对C70S6连杆的力学性能影响不大,抗拉强度始终>950MPa,屈服强度始终>550MPa;随着加热次数的增加,C70S6钢连杆中铁素体尺寸增大,珠光体片层间距也逐渐增大,抗拉强度和屈服强度逐渐减小。 展开更多
关键词 C70S6非调质钢 加热次数 力学性能
下载PDF
活塞杆电镀后表面缺陷原因分析
13
作者 何健楠 钟芳华 +2 位作者 冯宝 程强 刘年富 《南方金属》 CAS 2024年第1期32-35,共4页
针对非调钢活塞杆电镀后表面缺陷,通过宏观、金相、扫描电镜等分析,发现表面缺陷为磨削工序中的铁屑经超声碱洗未清除,电镀后与基体结合力不良,在抛光工序中镀层脱落形成的镀层起皮缺陷。在活塞杆电镀前加强表面清洗、表面检查,对表面... 针对非调钢活塞杆电镀后表面缺陷,通过宏观、金相、扫描电镜等分析,发现表面缺陷为磨削工序中的铁屑经超声碱洗未清除,电镀后与基体结合力不良,在抛光工序中镀层脱落形成的镀层起皮缺陷。在活塞杆电镀前加强表面清洗、表面检查,对表面存在的氧化皮、粘附异物进行清理和去除,可有效减少活塞杆表面镀层起皮缺陷。 展开更多
关键词 非调钢 活塞杆 电镀表面缺陷 镀层起皮
下载PDF
轧后冷却工艺对含硼贝氏体钢组织和力学性能的影响
14
作者 赵燕青 石帅 +4 位作者 高云哲 弓俊杰 禹青霄 和晓民 吴艳阳 《河北冶金》 2024年第6期17-19,75,共4页
含硼贝氏体钢具有高强度、高韧性和良好的焊接性能。本文采用拉伸试验机、冲击试验机及扫描电镜研究了轧后冷却工艺对含硼贝氏体钢组织和力学性能的影响。结果表明:轧后冷却工艺对轧态、淬火态和回火态试验钢的组织和力学性能有明显的... 含硼贝氏体钢具有高强度、高韧性和良好的焊接性能。本文采用拉伸试验机、冲击试验机及扫描电镜研究了轧后冷却工艺对含硼贝氏体钢组织和力学性能的影响。结果表明:轧后冷却工艺对轧态、淬火态和回火态试验钢的组织和力学性能有明显的影响。轧后空冷工艺下回火态试验钢的-20℃冲击功为268 J,轧后水冷工艺下回火态试验钢的-20℃冲击功为280 J,轧后水冷工艺下回火态试验钢的冲击性能最佳;轧后空冷工艺下轧态试验钢的组织主要为粒状贝氏体,轧后水冷工艺下轧态试验钢的组织主要为板条贝氏体和少量的粒状贝氏体,轧后空冷和水冷工艺下淬火态试验钢的组织均为板条贝氏体,轧后空冷和水冷工艺下回火态试验钢的组织均为回火索氏体。相较于轧后空冷工艺,轧后水冷工艺下试验钢轧态、淬火态和回火态的组织均得到细化。 展开更多
关键词 贝氏体钢 空冷 水冷 淬火 回火索氏体 冲击功
下载PDF
贝氏体型非调质钢的试制 被引量:11
15
作者 胡淑娥 唐立东 +1 位作者 冯勇 王祥宾 《钢铁钒钛》 CAS 北大核心 2003年第1期66-70,共5页
为降低钢结构件的成本,开发了一种新型的贝氏体高强度钢。该钢种属普通低碳合金钢,其特点是以价格较低的V,Mn,Cr取代昂贵的Ni,Mo,B等进行合金化,勿需热处理,生产工艺简单。铸坯的加热和压下制度与其它钢种类似,采用控温轧制和轧后空冷... 为降低钢结构件的成本,开发了一种新型的贝氏体高强度钢。该钢种属普通低碳合金钢,其特点是以价格较低的V,Mn,Cr取代昂贵的Ni,Mo,B等进行合金化,勿需热处理,生产工艺简单。铸坯的加热和压下制度与其它钢种类似,采用控温轧制和轧后空冷提高钢的强度和韧性。结果表明:试验钢板的抗拉强度较高,均在860MPa以上;且随着终轧温度的提高,钢的冲击韧性得到改善。 展开更多
关键词 试制 非调质钢 贝氏体钢 微合金元素 强度 韧性
下载PDF
变形温度和冷却方法对粒状贝氏体组织形态的影响 被引量:9
16
作者 曹杰 刘雅政 +4 位作者 阎军 章静 孙维 于同仁 柳美玲 《材料热处理学报》 EI CAS CSCD 北大核心 2011年第7期62-66,共5页
为控制粒状贝氏体的组织形态,在热模拟试验机上对新研制的非调质冷镦用钢进行了研究。主要分析了变形温度和冷却方法对粒状贝氏体组织中岛状物的影响。结果表明,在给定的变形温度和冷却条件下可以得到完全的粒状贝氏体组织;变形温度和... 为控制粒状贝氏体的组织形态,在热模拟试验机上对新研制的非调质冷镦用钢进行了研究。主要分析了变形温度和冷却方法对粒状贝氏体组织中岛状物的影响。结果表明,在给定的变形温度和冷却条件下可以得到完全的粒状贝氏体组织;变形温度和冷却方法对粒状贝氏体组织中的岛状物有明显影响。低温变形和采用快冷+缓冷的双冷速方法可细化粒状贝氏体组织中的岛状物,使岛状物的数量增加,但体积分数减少。 展开更多
关键词 非调质钢 粒状贝氏体 M/A岛 硬度
下载PDF
非调质钢中钛氧化物冶金行为 被引量:25
17
作者 杨颖 王福明 +2 位作者 宋波 罗志涛 杨占兵 《北京科技大学学报》 EI CAS CSCD 北大核心 2005年第5期540-544,共5页
通过热力学计算及实验,研究了含钛汽车用非调质钢在液态和凝固过程中含钛夹杂物的析出规律.研究表明,通过调整非调质钢中O,Al和Ti的含量,可以控制夹杂的形态和尺寸,从而得到细小、弥散非金属夹杂物作为针状铁素体的形核核心,细化钢的组... 通过热力学计算及实验,研究了含钛汽车用非调质钢在液态和凝固过程中含钛夹杂物的析出规律.研究表明,通过调整非调质钢中O,Al和Ti的含量,可以控制夹杂的形态和尺寸,从而得到细小、弥散非金属夹杂物作为针状铁素体的形核核心,细化钢的组织,提高钢的强度和韧性. 展开更多
关键词 非调质钢 夹杂物 晶内铁素体 钛氧化物
下载PDF
回火温度和时间对贝氏体型非调质钢力学性能的影响 被引量:11
18
作者 彭金明 罗毅 +1 位作者 汪宏斌 吴晓春 《上海金属》 CAS 2009年第3期16-19,共4页
通过常规力学性能测试设备和SEM,XRD研究了回火温度和回火时间对贝氏体型非调质钢力学性能的影响。研究结果表明:在300~600℃不同温度保温2h的回火处理后,屈服强度在350℃达到峰值,在450℃落到谷值;抗拉强度随回火温度的提高一直下降;... 通过常规力学性能测试设备和SEM,XRD研究了回火温度和回火时间对贝氏体型非调质钢力学性能的影响。研究结果表明:在300~600℃不同温度保温2h的回火处理后,屈服强度在350℃达到峰值,在450℃落到谷值;抗拉强度随回火温度的提高一直下降;硬度在550℃以上才明显下降;而冲击韧性在325℃达到峰值,在450℃落到谷值。在350℃不同时间回火后,屈服强度和抗拉强度并没有随回火时间的延长明显下降,而冲击韧性在保温2h时达最大值,之后急剧下降。 展开更多
关键词 贝氏体型非调质钢 回火温度 回火时间 力学性能
下载PDF
V-Ti-N微合金非调质无缝油井管钢中碳氮化物的热力学计算 被引量:14
19
作者 王安东 刘国权 +4 位作者 刘胜新 杨才福 李长荣 向嵩 韩庆礼 《北京科技大学学报》 EI CAS CSCD 北大核心 2006年第9期823-829,895,共8页
用包括奥氏体γ相和两个碳氮化物相三相溶解度间隙平衡处理的方法计算了V-Ti-N微合金非调质油井管钢中的碳氮化物析出.计算结果表明,此钢奥氏体中的析出模式为1473℃时TiN即开始析出;其后部分TiN逐渐转变为复合(TixV1-x)(CyN1-y)颗粒,... 用包括奥氏体γ相和两个碳氮化物相三相溶解度间隙平衡处理的方法计算了V-Ti-N微合金非调质油井管钢中的碳氮化物析出.计算结果表明,此钢奥氏体中的析出模式为1473℃时TiN即开始析出;其后部分TiN逐渐转变为复合(TixV1-x)(CyN1-y)颗粒,而其他的TiN直到低温仍保持其化学性质;最后富V-C的V(CxN1-x)在846℃开始析出.实验数据验证了这种析出模式.计算结果支持了中碳含钒微合金钢中800℃以下奥氏体中的析出对其后的奥氏体分解相变具有明显的调控作用的观点. 展开更多
关键词 微合金非调质钢 碳氮化物 析出 热力学计算
下载PDF
VN合金在非调质钢中的应用 被引量:12
20
作者 卢向阳 刘明 +3 位作者 贾斌 董军 董成瑞 崔润炯 《钢铁钒钛》 CAS 北大核心 2000年第3期29-33,共5页
简要介绍了VN合金在F35MnVN钢中的应用 ,对钒、氮的作用和钢水增氮方法进行了研究。结果表明 ,为发挥钒的作用 ,应增加含钒非调质钢中氮的含量 ;加氮的最好办法是采用VN合金。
关键词 VN合金 财质钢 微合金化 钢水增氮
下载PDF