In this study on the curing dynamics of phenol-formaldehyde novolac resins(PFNR) and hexamethylene tetramine(HMTA), two typical commercial PFNR were selected as examples and the curing reactions of the resins with HMT...In this study on the curing dynamics of phenol-formaldehyde novolac resins(PFNR) and hexamethylene tetramine(HMTA), two typical commercial PFNR were selected as examples and the curing reactions of the resins with HMTA were studied by differential scanning calorimetry(DSC). Based on the data calculated by the Kissinger equation and the Crane equation, a thermocuring dynamic model was established, from which the process conditions, activation energy, reaction kinetics equation and a f irst-order reaction of the curing reactions were derived.展开更多
Montmorillonite (MMT) was modified through intercalative polymerization of phenol and formaldehyde catalyzed by oxalic acid. The modified montmorillonite was delaminated at large, as demonstrated by XRD and TEM studi...Montmorillonite (MMT) was modified through intercalative polymerization of phenol and formaldehyde catalyzed by oxalic acid. The modified montmorillonite was delaminated at large, as demonstrated by XRD and TEM studies. It can disperse easily in epoxy resin to form exfoliated nanocomposites. The nanoscale silicate platelets dispersed in water can be metallized by silver deposition.展开更多
The synergistic effect of phosphorus oxynitride(PON) with a novolac-based char former modified by salification (NA-metal salt) on the flame retardance of polyamide 6(PA6) was investigated.For this purpose,variou...The synergistic effect of phosphorus oxynitride(PON) with a novolac-based char former modified by salification (NA-metal salt) on the flame retardance of polyamide 6(PA6) was investigated.For this purpose,various flame-retardant PA6 systems were melt-compounded with PON,PON/NA,PON/NA-V_2O_5 and PON/NA-Fe_2O_3,and their flame retardance was evaluated by measuring the limiting oxygen index(LOI) values and UL-94 vertical burning ratings.The results showed that,compared with the PA6/PON/NA system,the combination of two char formers(NA-V_2O_5,NA-Fe_2O_3) with PON could obviously improve the char formation and flame retardance of PA6.The flame retardance and cone calorimetric analyses showed the stronger synergism as well as the better flame retardant performance of PON/NA-Fe_2O_3 flame retardant system. The effects of different char formers on the flame retardance and thermal stability of this system were also discussed.展开更多
基金financially supported by the Fundamental Research Funds for the Central Universities of China(SWU.113003 and XDJK 2015C097)
文摘In this study on the curing dynamics of phenol-formaldehyde novolac resins(PFNR) and hexamethylene tetramine(HMTA), two typical commercial PFNR were selected as examples and the curing reactions of the resins with HMTA were studied by differential scanning calorimetry(DSC). Based on the data calculated by the Kissinger equation and the Crane equation, a thermocuring dynamic model was established, from which the process conditions, activation energy, reaction kinetics equation and a f irst-order reaction of the curing reactions were derived.
文摘Montmorillonite (MMT) was modified through intercalative polymerization of phenol and formaldehyde catalyzed by oxalic acid. The modified montmorillonite was delaminated at large, as demonstrated by XRD and TEM studies. It can disperse easily in epoxy resin to form exfoliated nanocomposites. The nanoscale silicate platelets dispersed in water can be metallized by silver deposition.
基金financially supported by the Key Project of the National Natural Science Foundation of China (No.50933005)
文摘The synergistic effect of phosphorus oxynitride(PON) with a novolac-based char former modified by salification (NA-metal salt) on the flame retardance of polyamide 6(PA6) was investigated.For this purpose,various flame-retardant PA6 systems were melt-compounded with PON,PON/NA,PON/NA-V_2O_5 and PON/NA-Fe_2O_3,and their flame retardance was evaluated by measuring the limiting oxygen index(LOI) values and UL-94 vertical burning ratings.The results showed that,compared with the PA6/PON/NA system,the combination of two char formers(NA-V_2O_5,NA-Fe_2O_3) with PON could obviously improve the char formation and flame retardance of PA6.The flame retardance and cone calorimetric analyses showed the stronger synergism as well as the better flame retardant performance of PON/NA-Fe_2O_3 flame retardant system. The effects of different char formers on the flame retardance and thermal stability of this system were also discussed.