The texture inhomogeneity in cross shear rolled grain oriented Si steel was investigated by means of the through thickness texture analysis. For the chosen rolling reductions (55%, 66.5%) and mismatch speed ratios (1....The texture inhomogeneity in cross shear rolled grain oriented Si steel was investigated by means of the through thickness texture analysis. For the chosen rolling reductions (55%, 66.5%) and mismatch speed ratios (1.0, 1.1, 1.3), the deformation textures in various thickness layers consist of three major components, i.e. strong γ-fiber, medium α-fiber and weak η-fiber, and they show an asymmetrical distribution throughout the thickness. The effect of reduction on the texture gradient is found to be more significant at and near the center layer; however, the effect of mismatch speed ratio is less important. In most cases, a strong {111}<112> texture component appears in the subsurface layers, that may favour the formation of a sharp Goss texture during the subsequent annealing.展开更多
The magnetic property of soft magnetic metals and alloys depends strongly on the crystallo-graphic orientation. In automated equipment for orientation research, the intensity for drawing up the pole figure is measured...The magnetic property of soft magnetic metals and alloys depends strongly on the crystallo-graphic orientation. In automated equipment for orientation research, the intensity for drawing up the pole figure is measured in detail. The present research shows that the accurate pole figure can be drawn up without measuring concretely the intensity. For directional Si steel sheet the measuring step may be 4~5 degrees. In this paper the experimental equation for defo-cusing correction was derived from the experimental data in different specimens with random orientation.展开更多
基金This work was supported by the National Natural Science Foundation of China (No. 59671037 and 50071061).
文摘The texture inhomogeneity in cross shear rolled grain oriented Si steel was investigated by means of the through thickness texture analysis. For the chosen rolling reductions (55%, 66.5%) and mismatch speed ratios (1.0, 1.1, 1.3), the deformation textures in various thickness layers consist of three major components, i.e. strong γ-fiber, medium α-fiber and weak η-fiber, and they show an asymmetrical distribution throughout the thickness. The effect of reduction on the texture gradient is found to be more significant at and near the center layer; however, the effect of mismatch speed ratio is less important. In most cases, a strong {111}<112> texture component appears in the subsurface layers, that may favour the formation of a sharp Goss texture during the subsequent annealing.
文摘The magnetic property of soft magnetic metals and alloys depends strongly on the crystallo-graphic orientation. In automated equipment for orientation research, the intensity for drawing up the pole figure is measured in detail. The present research shows that the accurate pole figure can be drawn up without measuring concretely the intensity. For directional Si steel sheet the measuring step may be 4~5 degrees. In this paper the experimental equation for defo-cusing correction was derived from the experimental data in different specimens with random orientation.