The concern with environmental preservation is a very current and relevant topic. Regarding polymers, the search for potentially ecofriendly matters has been the subject of scientific research. In this context, this w...The concern with environmental preservation is a very current and relevant topic. Regarding polymers, the search for potentially ecofriendly matters has been the subject of scientific research. In this context, this work aimed to study the effect of adding nanocellulose (nCE) with 1, 3, and 5 wt.% on poly(butylene adipate-co-butylene terephthalate) (PBAT). Thermal, structural, relaxometric, and rheological assessments were carried out. Quantitative evaluation of PBAT copolymer by high field NMR revealed 56.4 and 43.6 m.% of the butylene adipate and butylene terephthalate segments, respectively. WAXD measurement on the deconvoluted diffraction patterns identified that nCE was a mixing of Cellulose I and Cellulose II polymorph structures. At any composition, nanocellulose interfered with the PBAT crystallisation process. Also, a series of new PBAT crystallographic planes appeared as a function of nanocellulose content. PBAT hydrogen molecular relaxation varied randomly with nanocellulose content and had a strong effect on the hydrogen relaxation. PBAT cold crystallisation and melting temperatures (T<sub>cc</sub> and T<sub>m</sub>) were almost unchangeable. Although T<sub>cc</sub> did not change during polymer solidification from PBAT molten state, the sample’s degree of crystallinity varied with composition through the transcrystallization phenomenon. Nanocomposite thermal stability decreased possibly owing to the catalytic action of sulfonated amorphous cellulose chains. For the sample with 3 wt.% of nanocellulose, the highest values of complex viscosity and storage modulus were achieved.展开更多
In order to improve the wettability and biocompatibility of the poly (butylene terephthalate) non-woven (PBTNW), the method of surface modification is used to graft copolymerization of chitosan (CS) onto the PBT...In order to improve the wettability and biocompatibility of the poly (butylene terephthalate) non-woven (PBTNW), the method of surface modification is used to graft copolymerization of chitosan (CS) onto the PBTNW under alkylpolyglycoside (APG) inducing. The product is thoroughly characterized with the Fourier transform infrared spectroscopy (FrIR), the electron spectroscopy for chemical analysis (ESCA), the thermogravimetric (TG) and the scanning electron microscopy (SEM). It is found that chitosan is successfully grafted onto PBTNW. In addition, the water contact angles, hemolysis tests and cytotoxicity evaluation tests show an improvement in wettability and biocompatihility as a result of graft copolymerization of chitosan. So the CS-grafted PBTNW exhibits greater superiority than the original PBTNW. The CS-grafted PBTNW can be a candidate for blood filter materials and other medical applications.展开更多
In the present study,thermal behavior and crystal transition of pure poly(butylene adipate)(PBA)upon heating process were investigated by FTIR spectroscopy.To gain further insight into the thermal behavior alteration ...In the present study,thermal behavior and crystal transition of pure poly(butylene adipate)(PBA)upon heating process were investigated by FTIR spectroscopy.To gain further insight into the thermal behavior alteration and the phase transition of PBA,we performed two-dimensional(2D)correlation analysis.We found thatβ-form PBA crystal undergoes not only the melting process but also crystal transition upon the heating process.展开更多
In this article, the transesterification of poly(bisphenol A carbonate) (PC) with butylene terephthalate-caprolactone copolyester at a weight ratio 50/50 (BCL(21)) was thoroughly investigated by proton nuclear magneti...In this article, the transesterification of poly(bisphenol A carbonate) (PC) with butylene terephthalate-caprolactone copolyester at a weight ratio 50/50 (BCL(21)) was thoroughly investigated by proton nuclear magnetic resonance spectroscopy ('H-NMR), in conjunction with a model compound. The 1 H-NMR results of the annealed blend PC/BCL(21) show that the formation of bisphenol A-terephthalate ester units is the same as in the annealed blend of PC with PBT, and the transesterification actually occurs between PC and butylene terephthalate (BT) segments in BCL(21). By comparison with the model compound bisphenol A dibutyrate, the new signal appearing at δ= 2.56 in the 1H-NMR spectrum confirms the existence of bisphenol A caprolactone ester units resulting from the exchange reaction of PC with caprolactone (CL) segments. 1H-NMR analysis of the transesterification rates reveals that the reaction of PC with aromatic and aliphatic segments in BCL(21) proceeds in a random manner. The miscibility of the blend PC/BCL(21) copolyester is favorable for the transesterification of PC with BT segments and CL segments.展开更多
Rare earth (Nd, Y, La, Dy) stearates have been synthesized and used as single component catalysts for the polycondensation of dimethyl terephthalate, adipic acid and 1,4-butanediol for the first time preparing biode...Rare earth (Nd, Y, La, Dy) stearates have been synthesized and used as single component catalysts for the polycondensation of dimethyl terephthalate, adipic acid and 1,4-butanediol for the first time preparing biodegradable poly(butylene adipate-co-terephthalate) (PBAT) with high molecular weight, The microstructures of PBAT were characterized by ^1H NMR spectra. The PBAT exhibits good mechanical properties such as high tensile strength (ca. 20 MPa) and long break elongation (〉700%).展开更多
Poly(glycolic acid)(PGA)is derived from glycolide obtained by fermenting pineapples or sugarcane,which has excellent gas barrier properties and a small carbon footprint.PGA is a potential substitute for the current al...Poly(glycolic acid)(PGA)is derived from glycolide obtained by fermenting pineapples or sugarcane,which has excellent gas barrier properties and a small carbon footprint.PGA is a potential substitute for the current aluminum-plastic composite films used in high barrier packaging applications.However,its poor ductility and narrow processing window limit its application in food packaging.Herein,poly(butylene succinate-co-butylene adipate)(PBSA)was used to fabricate PGA/PBSA blend films through an in situ fibrillation technique and blown film extrusion.Under the elongational flow field used during the extrusion process,a unique hierarchical structure based on the PBSA nanofibrils and interfacially oriented PGA crystals was obtained.This structure enhances the strength,ductility and gas barrier properties of the PGA/PBSA blend film.In addition,an epoxy chain extender(ADR4468)was used as a compatibilizer to further enhance the interfacial adhesion between PGA and PBSA.70PGA/0.7ADR exhibited a very low oxygen permeability(2.34×10^(-4)Barrer)with significantly high elongating at break(604.4%),tensile strength(47.4 MPa),and transparency,which were superior to those of petroleum-based polymers.Thus,the 70PGA/0.7ADR blown films could satisfy the requirements for most instant foods such as coffee,peanuts,and fresh meat.展开更多
The pyrolysis of poly(ethylene terephthalate)(PET)/poly(butylene terephthalate)(PBT)catalyzed by five alkaline earth metal-based minerals/wastes,namely calcined dolomite,calcite,magnesite,calcium carbide slag(CCS),and...The pyrolysis of poly(ethylene terephthalate)(PET)/poly(butylene terephthalate)(PBT)catalyzed by five alkaline earth metal-based minerals/wastes,namely calcined dolomite,calcite,magnesite,calcium carbide slag(CCS),and ophicalcitum,was conducted by a pyrolyzer-gas chromatography-mass spectrometer(Py-GC-MS)with the objective of recovering benzenes-enriched oil.Compared with magnesium-based catalysts and pure CaO,the calcium-based catalysts with calcium hydroxide as the main component performed better catalytic effect,which could simultaneously promote the hydrolysis of ester products and the decarboxylation of aromatic acids after hydrolysis.For PET,the addition of solid base catalysts at 600℃promoted the complete degradation of aromatic acids and aryl esters,which accounted for 32.6%and 30.7%of the pyrolysis oil,respectively.The content of benzene in oil increased from 8.8%to 31.7%–78.8%.For PBT,the addition of solid base catalysts at 600℃completely decomposed the aromatic acids,which accounted for 67.1%of the pyrolysis oil,and the content of benzene in oil increased from 12.3%to 34.5%–81.0%.During the deoxygenation of polyester pyrolysis products,increasing temperature was more effective for the decomposition/conversion of acetone and tetrahydrofuran,while increasing the alkalinity of the reaction environment contributed to the rapid decrease in acetaldehyde and aryl ketone contents.展开更多
The effects of crystallization temperature and blend ratio on the polymorphic crystal structures of poly(butylene adipate) (PBA) in poly(butylene succinate) (PBS)/poly(butylene adipate) (PBS/PBA) blends we...The effects of crystallization temperature and blend ratio on the polymorphic crystal structures of poly(butylene adipate) (PBA) in poly(butylene succinate) (PBS)/poly(butylene adipate) (PBS/PBA) blends were studied by means of differential scanning calorimetry (DSC), wide-angle X-ray diffraction (XRD) and atomic force microscopy (AFM). It was revealed that the polymorphism of PBA can be regulated by the blend ratio even in a non-isothermal crystallization process. The results demonstrate that high temperature favors fiat-on α crystals, while low temperature contributes to edge-on β crystals. It was also found that the effect of blend ratio on the crystallization mechanism of PBA is well coincident with that of the crystallization temperature. The increment of PBS content in the PBS/PBA blend gives rise to more β-form crystals of PBA. For those PBS/PBA blends with low PBA content, the interlamellar phase segregation of PBA makes its molecular chains so difficult to diffuse from one isolated microdomain to another that high crystallization temperature and sufficiently long crystallization time will be required if the PBA α-type crystals are targeted.展开更多
Oriented and non-oriented Teflon films, which were found to have the same crystalline structure, but different surface morphologies, were used to sandwich poly(butylene adipate) (PBA) films during isothermal cryst...Oriented and non-oriented Teflon films, which were found to have the same crystalline structure, but different surface morphologies, were used to sandwich poly(butylene adipate) (PBA) films during isothermal crystallization. It was found that both the Teflon surface structure and the PBA polymorphic structure are the determining factors to induce epitaxial crystallization. The oriented Teflon film was able to induce epitaxial crystallization of PBA α crystal, while the non-oriented Teflon did not induce any epitaxial crystallization of PBA. Epitaxial crystallization did not occurred for PBA β crystals between neither the oriented nor the non-oriented Teflon films. The enzymatic degradation rate of PBA films was not determined by the epitaxial crystallization, in fact it was still dependent on the polymorphic crystal structure of PBA. The morphological changes of PBA films after enzymatic degradation confirmed again that the epitaxial crystallization only occurred for the PBA film with α crystal structure which was produced by being sandwiched between oriented Teflon films, and it happened only on the surface of PBA films.展开更多
The morphology of polyamide 6/poly(butylene terephthalate)(PA6/PBT, 70/30, W/W) blends filled with pristine Zinc oxide(ZnO) nanoparticles and ZnO surface-modified by γ-glycidoxypropyltrimethoxysilane(K-ZnO) was inves...The morphology of polyamide 6/poly(butylene terephthalate)(PA6/PBT, 70/30, W/W) blends filled with pristine Zinc oxide(ZnO) nanoparticles and ZnO surface-modified by γ-glycidoxypropyltrimethoxysilane(K-ZnO) was investigated. The incorporation of ZnO and K-ZnO by one-step compounding both resulted in a smaller size and narrower distribution of PBT domains and the effect of ZnO was greater than K-ZnO. To reveal the underlying mechanism, two-step compounding in which ZnO or K-ZnO was premixed with PA6 or PBT was conducted and the finest morphology was achieved when mixing PA6 with premixed PBT/ZnO. Transmission electron microscopy(TEM) demonstrated that ZnO was distributed in PBT in all cases and K-ZnO was enriched at the interface except when K-ZnO was premixed with PBT. ZnO and K-ZnO caused a deterioration in the melt rheological properties of PBT, which played a dominating role in the morphological changes. In addition, the interfacial localization of K-ZnO enhanced the dynamic rheological properties of PA6/PBT blends substantially.展开更多
Core-shell structured polyacrylic(named CSSP) impact modifiers consisting of a rubbery poly(n-butyl acrylate) core and a rigid poly(methyl methacrylate) shell with a size of about 353 nm were prepared by seed em...Core-shell structured polyacrylic(named CSSP) impact modifiers consisting of a rubbery poly(n-butyl acrylate) core and a rigid poly(methyl methacrylate) shell with a size of about 353 nm were prepared by seed emulsion polymerization. The CSSP modifiers with different core-shell weight ratios(90/10, 85/15, 80/20, 75/25, 70/30, 65/35 and 60/40) were used to modify the toughness of poly(butylene terephthalate)(PBT) by melt blending. It was found that the polymerization had a very high instantaneous conversion( 95.7%) and overall conversion(99.7%). The morphology of the core-shell structure was confirmed by means of transmission electron microscopy. Scanning electron microscopy was used to observe the morphology of the fractured surfaces. Differential scanning calorimeter was used to study the crystallization behaviors of PBT/CSSP blends. The dynamic mechanical analyses of PBT/CSSP blends showed two merged transition peaks of PBT matrix, with the presence of CSSP core-shell structured modifier, that were responsible for the improvement of PBT toughness. The results indicated that the notch impact strength of PBT/CSSP blends with a core-shell weight ratio of 75/25 was almost 8.64 times greater than that of pure PBT, and the mechanical properties agreed well with the SEM observation.展开更多
We successfully use a co-precipitation method to prepare inclusion complex between poly(butylene adipate) (PBA) chains (guest component) and urea molecules (host component). The PBA/urea inclusion complex is c...We successfully use a co-precipitation method to prepare inclusion complex between poly(butylene adipate) (PBA) chains (guest component) and urea molecules (host component). The PBA/urea inclusion complex is confirmed to adopt a hexagonal crystal modification with lattice parameters ofa = 8.14 A and c = 10.92 A, and the interaction between PBA chains and urea is van der Waals force. The singly isolated PBA chains are suggested to take some gauche conformation, which is different from the all-trans conformation in r-form PBA. Furthermore, we employ the isolated PBA chains which are uniformly pre-established in a specific conformation in urea channels to regulate the crystal form of PBA for the first time. After removing the host urea molecules, the coalesced PBA chains are found to solely crystallize into a-form crystals at different coalescing temperatures. By comparing the FTIR spectra, it is found that PBA chains in inclusion complex plausibly contain some similar conformers as those in a-form crystal, which is suggested to be the intrinsic reason for the sole formation of a-form crystals. This research proves that inclusion complex can be used as a very effective method to regulate polymorphism of semi-crystalline polymers.展开更多
文摘The concern with environmental preservation is a very current and relevant topic. Regarding polymers, the search for potentially ecofriendly matters has been the subject of scientific research. In this context, this work aimed to study the effect of adding nanocellulose (nCE) with 1, 3, and 5 wt.% on poly(butylene adipate-co-butylene terephthalate) (PBAT). Thermal, structural, relaxometric, and rheological assessments were carried out. Quantitative evaluation of PBAT copolymer by high field NMR revealed 56.4 and 43.6 m.% of the butylene adipate and butylene terephthalate segments, respectively. WAXD measurement on the deconvoluted diffraction patterns identified that nCE was a mixing of Cellulose I and Cellulose II polymorph structures. At any composition, nanocellulose interfered with the PBAT crystallisation process. Also, a series of new PBAT crystallographic planes appeared as a function of nanocellulose content. PBAT hydrogen molecular relaxation varied randomly with nanocellulose content and had a strong effect on the hydrogen relaxation. PBAT cold crystallisation and melting temperatures (T<sub>cc</sub> and T<sub>m</sub>) were almost unchangeable. Although T<sub>cc</sub> did not change during polymer solidification from PBAT molten state, the sample’s degree of crystallinity varied with composition through the transcrystallization phenomenon. Nanocomposite thermal stability decreased possibly owing to the catalytic action of sulfonated amorphous cellulose chains. For the sample with 3 wt.% of nanocellulose, the highest values of complex viscosity and storage modulus were achieved.
文摘In order to improve the wettability and biocompatibility of the poly (butylene terephthalate) non-woven (PBTNW), the method of surface modification is used to graft copolymerization of chitosan (CS) onto the PBTNW under alkylpolyglycoside (APG) inducing. The product is thoroughly characterized with the Fourier transform infrared spectroscopy (FrIR), the electron spectroscopy for chemical analysis (ESCA), the thermogravimetric (TG) and the scanning electron microscopy (SEM). It is found that chitosan is successfully grafted onto PBTNW. In addition, the water contact angles, hemolysis tests and cytotoxicity evaluation tests show an improvement in wettability and biocompatihility as a result of graft copolymerization of chitosan. So the CS-grafted PBTNW exhibits greater superiority than the original PBTNW. The CS-grafted PBTNW can be a candidate for blood filter materials and other medical applications.
文摘In the present study,thermal behavior and crystal transition of pure poly(butylene adipate)(PBA)upon heating process were investigated by FTIR spectroscopy.To gain further insight into the thermal behavior alteration and the phase transition of PBA,we performed two-dimensional(2D)correlation analysis.We found thatβ-form PBA crystal undergoes not only the melting process but also crystal transition upon the heating process.
文摘In this article, the transesterification of poly(bisphenol A carbonate) (PC) with butylene terephthalate-caprolactone copolyester at a weight ratio 50/50 (BCL(21)) was thoroughly investigated by proton nuclear magnetic resonance spectroscopy ('H-NMR), in conjunction with a model compound. The 1 H-NMR results of the annealed blend PC/BCL(21) show that the formation of bisphenol A-terephthalate ester units is the same as in the annealed blend of PC with PBT, and the transesterification actually occurs between PC and butylene terephthalate (BT) segments in BCL(21). By comparison with the model compound bisphenol A dibutyrate, the new signal appearing at δ= 2.56 in the 1H-NMR spectrum confirms the existence of bisphenol A caprolactone ester units resulting from the exchange reaction of PC with caprolactone (CL) segments. 1H-NMR analysis of the transesterification rates reveals that the reaction of PC with aromatic and aliphatic segments in BCL(21) proceeds in a random manner. The miscibility of the blend PC/BCL(21) copolyester is favorable for the transesterification of PC with BT segments and CL segments.
基金Project supported by the National Natural Science Foundation of China (No. 20434020), the Major State Basic Research Development Program (No. 2005CB623802), and China Postdoctor Science Foundation (No. 20060390334).
文摘Rare earth (Nd, Y, La, Dy) stearates have been synthesized and used as single component catalysts for the polycondensation of dimethyl terephthalate, adipic acid and 1,4-butanediol for the first time preparing biodegradable poly(butylene adipate-co-terephthalate) (PBAT) with high molecular weight, The microstructures of PBAT were characterized by ^1H NMR spectra. The PBAT exhibits good mechanical properties such as high tensile strength (ca. 20 MPa) and long break elongation (〉700%).
基金the National Key Research and Development Program of China(No.2022YFB3704900)the National Natural Science Foundation of China(No.52073004)China National Tobacco Corporation Guizhou Company(No.2023XM24)。
文摘Poly(glycolic acid)(PGA)is derived from glycolide obtained by fermenting pineapples or sugarcane,which has excellent gas barrier properties and a small carbon footprint.PGA is a potential substitute for the current aluminum-plastic composite films used in high barrier packaging applications.However,its poor ductility and narrow processing window limit its application in food packaging.Herein,poly(butylene succinate-co-butylene adipate)(PBSA)was used to fabricate PGA/PBSA blend films through an in situ fibrillation technique and blown film extrusion.Under the elongational flow field used during the extrusion process,a unique hierarchical structure based on the PBSA nanofibrils and interfacially oriented PGA crystals was obtained.This structure enhances the strength,ductility and gas barrier properties of the PGA/PBSA blend film.In addition,an epoxy chain extender(ADR4468)was used as a compatibilizer to further enhance the interfacial adhesion between PGA and PBSA.70PGA/0.7ADR exhibited a very low oxygen permeability(2.34×10^(-4)Barrer)with significantly high elongating at break(604.4%),tensile strength(47.4 MPa),and transparency,which were superior to those of petroleum-based polymers.Thus,the 70PGA/0.7ADR blown films could satisfy the requirements for most instant foods such as coffee,peanuts,and fresh meat.
基金would like to gratefully acknowledge the National Key Research and Development Program(No.2018YFC1901300)the Key Research and Development Program of Zhejiang Province(No.2020C03084).
文摘The pyrolysis of poly(ethylene terephthalate)(PET)/poly(butylene terephthalate)(PBT)catalyzed by five alkaline earth metal-based minerals/wastes,namely calcined dolomite,calcite,magnesite,calcium carbide slag(CCS),and ophicalcitum,was conducted by a pyrolyzer-gas chromatography-mass spectrometer(Py-GC-MS)with the objective of recovering benzenes-enriched oil.Compared with magnesium-based catalysts and pure CaO,the calcium-based catalysts with calcium hydroxide as the main component performed better catalytic effect,which could simultaneously promote the hydrolysis of ester products and the decarboxylation of aromatic acids after hydrolysis.For PET,the addition of solid base catalysts at 600℃promoted the complete degradation of aromatic acids and aryl esters,which accounted for 32.6%and 30.7%of the pyrolysis oil,respectively.The content of benzene in oil increased from 8.8%to 31.7%–78.8%.For PBT,the addition of solid base catalysts at 600℃completely decomposed the aromatic acids,which accounted for 67.1%of the pyrolysis oil,and the content of benzene in oil increased from 12.3%to 34.5%–81.0%.During the deoxygenation of polyester pyrolysis products,increasing temperature was more effective for the decomposition/conversion of acetone and tetrahydrofuran,while increasing the alkalinity of the reaction environment contributed to the rapid decrease in acetaldehyde and aryl ketone contents.
基金financially supported by the National Natural Science Foundation of China(Nos.21204045 and 21276151)Natural Science Basic Research Plan in Shaanxi Province of China(No.2011JQ2004)Key Scientific Research Group of Shaanxi Province(No.2013KCT-08)
文摘The effects of crystallization temperature and blend ratio on the polymorphic crystal structures of poly(butylene adipate) (PBA) in poly(butylene succinate) (PBS)/poly(butylene adipate) (PBS/PBA) blends were studied by means of differential scanning calorimetry (DSC), wide-angle X-ray diffraction (XRD) and atomic force microscopy (AFM). It was revealed that the polymorphism of PBA can be regulated by the blend ratio even in a non-isothermal crystallization process. The results demonstrate that high temperature favors fiat-on α crystals, while low temperature contributes to edge-on β crystals. It was also found that the effect of blend ratio on the crystallization mechanism of PBA is well coincident with that of the crystallization temperature. The increment of PBS content in the PBS/PBA blend gives rise to more β-form crystals of PBA. For those PBS/PBA blends with low PBA content, the interlamellar phase segregation of PBA makes its molecular chains so difficult to diffuse from one isolated microdomain to another that high crystallization temperature and sufficiently long crystallization time will be required if the PBA α-type crystals are targeted.
基金financially supported by the National Natural Science Foundation of China(No.51025314)the Oticon Foundation in Denmark
文摘Oriented and non-oriented Teflon films, which were found to have the same crystalline structure, but different surface morphologies, were used to sandwich poly(butylene adipate) (PBA) films during isothermal crystallization. It was found that both the Teflon surface structure and the PBA polymorphic structure are the determining factors to induce epitaxial crystallization. The oriented Teflon film was able to induce epitaxial crystallization of PBA α crystal, while the non-oriented Teflon did not induce any epitaxial crystallization of PBA. Epitaxial crystallization did not occurred for PBA β crystals between neither the oriented nor the non-oriented Teflon films. The enzymatic degradation rate of PBA films was not determined by the epitaxial crystallization, in fact it was still dependent on the polymorphic crystal structure of PBA. The morphological changes of PBA films after enzymatic degradation confirmed again that the epitaxial crystallization only occurred for the PBA film with α crystal structure which was produced by being sandwiched between oriented Teflon films, and it happened only on the surface of PBA films.
文摘The morphology of polyamide 6/poly(butylene terephthalate)(PA6/PBT, 70/30, W/W) blends filled with pristine Zinc oxide(ZnO) nanoparticles and ZnO surface-modified by γ-glycidoxypropyltrimethoxysilane(K-ZnO) was investigated. The incorporation of ZnO and K-ZnO by one-step compounding both resulted in a smaller size and narrower distribution of PBT domains and the effect of ZnO was greater than K-ZnO. To reveal the underlying mechanism, two-step compounding in which ZnO or K-ZnO was premixed with PA6 or PBT was conducted and the finest morphology was achieved when mixing PA6 with premixed PBT/ZnO. Transmission electron microscopy(TEM) demonstrated that ZnO was distributed in PBT in all cases and K-ZnO was enriched at the interface except when K-ZnO was premixed with PBT. ZnO and K-ZnO caused a deterioration in the melt rheological properties of PBT, which played a dominating role in the morphological changes. In addition, the interfacial localization of K-ZnO enhanced the dynamic rheological properties of PA6/PBT blends substantially.
基金financially supported by Program for Changjiang Scholars and Innovative Research Team in University-IRT13060Key Lab for Micro-and Nano-Scale Boron Nitride Materials in Hebei Province
文摘Core-shell structured polyacrylic(named CSSP) impact modifiers consisting of a rubbery poly(n-butyl acrylate) core and a rigid poly(methyl methacrylate) shell with a size of about 353 nm were prepared by seed emulsion polymerization. The CSSP modifiers with different core-shell weight ratios(90/10, 85/15, 80/20, 75/25, 70/30, 65/35 and 60/40) were used to modify the toughness of poly(butylene terephthalate)(PBT) by melt blending. It was found that the polymerization had a very high instantaneous conversion( 95.7%) and overall conversion(99.7%). The morphology of the core-shell structure was confirmed by means of transmission electron microscopy. Scanning electron microscopy was used to observe the morphology of the fractured surfaces. Differential scanning calorimeter was used to study the crystallization behaviors of PBT/CSSP blends. The dynamic mechanical analyses of PBT/CSSP blends showed two merged transition peaks of PBT matrix, with the presence of CSSP core-shell structured modifier, that were responsible for the improvement of PBT toughness. The results indicated that the notch impact strength of PBT/CSSP blends with a core-shell weight ratio of 75/25 was almost 8.64 times greater than that of pure PBT, and the mechanical properties agreed well with the SEM observation.
基金financially supported by the National Natural Science Foundation of China(No.21674128)China University of Petroleum(Beijing)
文摘We successfully use a co-precipitation method to prepare inclusion complex between poly(butylene adipate) (PBA) chains (guest component) and urea molecules (host component). The PBA/urea inclusion complex is confirmed to adopt a hexagonal crystal modification with lattice parameters ofa = 8.14 A and c = 10.92 A, and the interaction between PBA chains and urea is van der Waals force. The singly isolated PBA chains are suggested to take some gauche conformation, which is different from the all-trans conformation in r-form PBA. Furthermore, we employ the isolated PBA chains which are uniformly pre-established in a specific conformation in urea channels to regulate the crystal form of PBA for the first time. After removing the host urea molecules, the coalesced PBA chains are found to solely crystallize into a-form crystals at different coalescing temperatures. By comparing the FTIR spectra, it is found that PBA chains in inclusion complex plausibly contain some similar conformers as those in a-form crystal, which is suggested to be the intrinsic reason for the sole formation of a-form crystals. This research proves that inclusion complex can be used as a very effective method to regulate polymorphism of semi-crystalline polymers.