A poly(L-lactide)-b-poly(ethylene glycol)-b-poly(L-lactide)(PLLA-PEG-PLLA)block copolymer has great potential for use as a flexible bioplastic.Highly flexible bioplastics are required for flexible packaging applicatio...A poly(L-lactide)-b-poly(ethylene glycol)-b-poly(L-lactide)(PLLA-PEG-PLLA)block copolymer has great potential for use as a flexible bioplastic.Highly flexible bioplastics are required for flexible packaging applications.In this work,a PEG was incorporated into block copolymer as a plasticizer by solvent casting.PLLA-PEG-PLLA/PEG blends with different blend ratios were prepared,and the plasticizing effect and miscibility of PEG in block copolymer were intensively investigated compared to PLLA/PEG blends.The results indicated that the PEG was an effective plasticizer for the block copolymer.The blending of PEG decreased glass-transition temperature and accelerated the crystallization of both the PLLA and PLLA-PEG-PLLA matrices.The PEG was completely miscible when blended with block copolymer and it improved thermal stability of the block copolymer matrix but not of the PLLA matrix.Film extensibility of PLLA-PEG-PLLA/PEG blends steadily increased as the PEG ratio increased.These non-toxic and highly flexible PLLA-PEG-PLLA/PEG bioplastics are promising candidates for several applications such as biomedical devices,tissue scaffolds and packaging materials.展开更多
Structure and properties of bioabsorbable polyglycolide (PGA) and poly(glycolide-co-lactide) (PGA-co-PLA)fibers were investigated during several industrial processing stages and in vitro degradation by means of wide-a...Structure and properties of bioabsorbable polyglycolide (PGA) and poly(glycolide-co-lactide) (PGA-co-PLA)fibers were investigated during several industrial processing stages and in vitro degradation by means of wide-angle X-raydiffraction (WAXD), dynamic mechanical analysis (DMA) and mechanical property tests. In the orientation stage, the PGAfibers were found to have higher degrees of crystallinity than corresponding PGA-co-PLA samples produced under similarconditions. In the hot-stretching and post-annealing stages, after fibers were braided, PGA samples were found to gain morecrystallinity and higher T_g than PGA-co-PLA samples. The higher crystallinity in PGA fibers resulted in a slower rate ofdegradation. DMA results showed that a great deal of internal stress that was built during orientation and hot-stretchingstages was released in the post-annealing stage for a1l PGA and PGA-co-PLA samples. During earlier stages of in vitrodegradation, both PGA and PGA-co-PLA samples exhibited the typical cleavage-induced crystallization mechanism. Theheat shrinkage in the glass transition area was found to disappear after 6-8 days of degradation for all PGA and PGA-co-PLAsamples, indicating the amorphous portions of the polymers lost orientation after a short period in the buffer solution, mostlikely due to relaxation of the cleaved chains.展开更多
Poly (L-lactide) was prepared by bulk polymerization ofL-lactide at 140°C in the presence of stannous octoate. The polymer products were characterized by number average molecular weight Mn, weight average molecul...Poly (L-lactide) was prepared by bulk polymerization ofL-lactide at 140°C in the presence of stannous octoate. The polymer products were characterized by number average molecular weight Mn, weight average molecular weight Mw and molecular weight distribution MWD (M w/M n) respectively. The results showed that stannous octoate was a high effective catalyst, and coordinated insertion mechanism of the reaction was proposed.展开更多
Poly (L-lactide)-poly(ethylene glycol) multiblock copolymers with predetermined block lengths were synthesized by polycondensation of PLA diols and PEG diacids. These copolymers presented special properties, such as ...Poly (L-lactide)-poly(ethylene glycol) multiblock copolymers with predetermined block lengths were synthesized by polycondensation of PLA diols and PEG diacids. These copolymers presented special properties, such as better miscibility between the two components, low crystallinity and better hydrophilicity, which can be modulated by adjusting the block lengths of the two components.展开更多
The non-isothermal crystallization of poly(L-lactide) (PLLA) under quiescent and steady shear flow conditions was in situ investigated by using polarizing optical microscopy (POM) with a hot shear stage and wide...The non-isothermal crystallization of poly(L-lactide) (PLLA) under quiescent and steady shear flow conditions was in situ investigated by using polarizing optical microscopy (POM) with a hot shear stage and wide-angle X-ray diffraction (WAXD). The shear rate and the cooling rate both play a significant role in the final crystalline morphology and crystallinity. Under quiescent conditions, the morphology assumes different sized spherulites, and its crystallinity dramatically reduces with increasing the cooling rate. On the other hand, the shear flow increases the onset crystallization temperature, and enhances the final crystallinity. When the shear rate is above 5 s^-1, cylindrite-like crystals are observed, furthermore, their content depends on the cooling rate.展开更多
Poly(d,l-lactide-co-p-dioxanone) (P(LA-co-PDO)) copolymers with different chain microstructures were synthesized by onestep or two-step bulk ring-opening polymerizations of d,l-lactide (LA) and p-dioxanone (...Poly(d,l-lactide-co-p-dioxanone) (P(LA-co-PDO)) copolymers with different chain microstructures were synthesized by onestep or two-step bulk ring-opening polymerizations of d,l-lactide (LA) and p-dioxanone (PDO) monomers using stannous octoate [Sn(Oct)2]/n-dodecanol as the initiating system. The average sequence lengths of the lactidyl (LLA) and dioxanyl (LpDo) units were calculated from the ^1H NMR spectra. It was found that both LLA and Lpoo values from the two-step syntheses were significantly longer than those from the corresponding one-step syntheses, indicating more blocky structure achieved for the twostep copolymers. Corresponding to this difference in microstructure, the two-step copolymers were semi-crystalline, while the one-step copolymers were completely amorphous. In conclusion, the crystallinity of P(LA-co-PDO) copolymers could be adjusted conveniently to meet specific applications by changing the microstructure of the copolymers via different polymerization routes.展开更多
Bioactive and bioresorbable composite was fabricated by a solvent evaporation technique using poly-L-lactide(PLLA) and bioactive glass (average particle size: 6.8 μm). Bioactive glass granules are homogeneously distr...Bioactive and bioresorbable composite was fabricated by a solvent evaporation technique using poly-L-lactide(PLLA) and bioactive glass (average particle size: 6.8 μm). Bioactive glass granules are homogeneously distributed in the composite with microcrack structure. The formation of hydroxyapatite(HA) on the composite in simulated body fluid(SBF) was analyzed by scanning electron microscopy(SEM), energy dispersive spectroscopy(EDS), X-ray diffraction(XRD), and Raman spectra. Rod-like HA crystals deposit on the surface of PLLA/bioactive glass composite after soaking for 3 d. Both rod-like crystals and HA layer form on the surface for 14 d in SBF. The high bioactivity of PLLA/bioactive glass composite indicates the potential of materials for integration with bone.展开更多
The aim of the present study was to develop a novel long-acting Poly(lactic-co-glycolic acid)(PLGA)-based microspheres formulation of Bisdemethoxycurcum(BDMC) by emulsionsolvent evaporation method. Meanwhile, the effe...The aim of the present study was to develop a novel long-acting Poly(lactic-co-glycolic acid)(PLGA)-based microspheres formulation of Bisdemethoxycurcum(BDMC) by emulsionsolvent evaporation method. Meanwhile, the effects of the volume ratio of the dispersed phase and continuous phase, the concentration of PLGA and PVA, the theoretical drug loading and stirring speed were investigated. The mean diameter of the microspheres was 8.5 μm and the size distribution was narrow. The encapsulation efficiency(EE) and drug loading efficiency(DLE) of BDME loaded PLGA microspheres(BDMC-PLGA-MS) was 94.18% and 8.14%,respectively. In an in vitro study of drug release, it can be concluded that the BDMC-PLGAMS exhibited sustained and long-term release properties for 96 h. Stability studies suggested that the microspheres we prepared had a very good stability. Furthermore, the results of an in vivo study indicated that the BDMC-PLGA-MS had sustained release effect and was mainly distributed in the lung tissue, and less distribution in other tissues, which indicated that microspheres could be an effective parenteral carrier for the delivery of BDMC in lung cancer treatment.展开更多
Poly (lactic acid) (PLA) was synthesized by microwave-assisted ring-opening polymerization of D, L-lactide with stannous octanoate (SnOct(2)) as catalyst. Its weight-average molar mass (M-w) ranged from 39000 to 67000...Poly (lactic acid) (PLA) was synthesized by microwave-assisted ring-opening polymerization of D, L-lactide with stannous octanoate (SnOct(2)) as catalyst. Its weight-average molar mass (M-w) ranged from 39000 to 67000 and the polydispersity index from 1.3 to 1.7. The polymerization rate was much faster than that of the conventional thermal polymerization. A degradation of newly formed PLA in reaction mixture by microwave irradiation was observed.展开更多
A novel biodegradable polymer--poly (ethene maleic acid ester-co-D,L-lactide acid) was synthesized by copolymerizing lactide and prepolymer, which was prepared by the condensation of maleic anhydride and glycol, usi...A novel biodegradable polymer--poly (ethene maleic acid ester-co-D,L-lactide acid) was synthesized by copolymerizing lactide and prepolymer, which was prepared by the condensation of maleic anhydride and glycol, using p-toluene sulphonic acid as a catalyst, attempting to improve the hydrophilicity, increase flexibility and modulate the degradation rate. FTIR,^1H NMR, MALLS and DSC were employed to characterize these polymers.展开更多
L-lactide was prepared from L-lactic acid with stannous octoate as the catalyst. The effects of reaction temperature and pressure on the ingredient of crude lactide were investigated. The results show that the mass fr...L-lactide was prepared from L-lactic acid with stannous octoate as the catalyst. The effects of reaction temperature and pressure on the ingredient of crude lactide were investigated. The results show that the mass fraction of meso-lactide increases with the increasing reaction temperature. Crude lactide containing 85.4% L-lactide is obtained when the reaction temperature is 200 ℃. High purity of L-lactide with a yield of 40.6 % is obtained by synthetic purifying method. The properties of L-lactide are characterized by optical purity, infrared spectrum and gas chromatogram/mass spectrum. The L-lactide samples purified by recrystallization and synthetic purifying methods are polymerized with the catalyst of stannous octoate, and the corresponding viscosity average relative molecular masses of poly(L-lactide) are 2.85 × 105 and 5.05 × 105 , respectively. This indicates that the optical purity of Llactide has great influence on the relative molecular mass of poly(L-lactide).展开更多
Poly(D,L-lactide) was synthesized by indirect method from D,L-lactic acid and characterized by infrared spectrum and proton nuclear magnetic resonance. The influences of monomer purity, initiator concentration, polyme...Poly(D,L-lactide) was synthesized by indirect method from D,L-lactic acid and characterized by infrared spectrum and proton nuclear magnetic resonance. The influences of monomer purity, initiator concentration, polymerization temperature and polymerization time on the relative molecular mass of poly(D, L-lactide) were investigated. The polylactide was made into porous materials by using solvent-casting particulate-leaching method. Under the optimized conditions, polylactides with a viscosity average molecular mass up to 1.82×105 are obtained and the results are fairly reproducible. Scanning electron microscope observation indicates that the sample is highly porous and well-distributed with good interconnections between pores and the pore size of porous materials is in the range from 200 μm to 500 μm and it can be used as scaffold for bone tissue engineering.展开更多
Poly-dl-lactide-poly(ethylene glycol) (PELA) triblock copolymers were synthesized with lanthanum acetate as the initiator. PELA microspheres with entrapped Vibrio Cholera antigen and outer membrane protein (OMP) were ...Poly-dl-lactide-poly(ethylene glycol) (PELA) triblock copolymers were synthesized with lanthanum acetate as the initiator. PELA microspheres with entrapped Vibrio Cholera antigen and outer membrane protein (OMP) were prepared by a double emulsion W/O/W based on solvent extraction methods. The obtained microspheres showed smooth and spherical surface and their size varied between 0.5 and 5.0 mu m, which are suitable for oral targeting delivery system. The distribution tests in rabbits and mice through scanning electronic micrography and fluorescence microscope indicated that microspheres have successfully reached the immunization-related tissues, such as the liver, spleen and intestinal peyer's patches, following oral administration. The PELA microspheres were also evaluated as an efficient antigen delivery system by enhancing a higher protective ratio against live Vibrios Cholera.展开更多
Poly(ethylene oxide)(PEO)-based polymer electrolytes show the prospect in all-solid-state lithium metal batteries;however,they present limitations of low room-temperature ionic conductivity,and interfacial incompatibi...Poly(ethylene oxide)(PEO)-based polymer electrolytes show the prospect in all-solid-state lithium metal batteries;however,they present limitations of low room-temperature ionic conductivity,and interfacial incompatibility with high voltage cathodes.Therefore,a salt engineering of 1,1,2,2,3,3-hexafluoropropane-1,3-disulfonimide lithium salt(LiHFDF)/LiTFSI system was developed in PEO-based electrolyte,demonstrating to effectively regulate Li ion transport and improve the interfacial stability under high voltage.We show,by manipulating the interaction between PEO matrix and TFSI^(-)-HFDF^(-),the optimized solid-state polymer electrolyte achieves maximum Li+conduction of 1.24×10^(-4)S cm^(-1)at 40℃,which is almost 3 times of the baseline.Also,the optimized polymer electrolyte demonstrates outstanding stable cycling in the LiFePO_(4)/Li and LiNi_(0.8)Mn_(0.1)Co_(0.1)O_(2)/Li(3.0-4.4 V,200 cycles)based all-solid-state lithium batteries at 40℃.展开更多
With the rapid development of 5G information technology,thermal conductivity/dissipation problems of highly integrated electronic devices and electrical equipment are becoming prominent.In this work,“high-temperature...With the rapid development of 5G information technology,thermal conductivity/dissipation problems of highly integrated electronic devices and electrical equipment are becoming prominent.In this work,“high-temperature solid-phase&diazonium salt decomposition”method is carried out to prepare benzidine-functionalized boron nitride(m-BN).Subsequently,m-BN/poly(pphenylene benzobisoxazole)nanofiber(PNF)nanocomposite paper with nacremimetic layered structures is prepared via sol–gel film transformation approach.The obtained m-BN/PNF nanocomposite paper with 50 wt%m-BN presents excellent thermal conductivity,incredible electrical insulation,outstanding mechanical properties and thermal stability,due to the construction of extensive hydrogen bonds andπ–πinteractions between m-BN and PNF,and stable nacre-mimetic layered structures.Itsλ∥andλ_(⊥)are 9.68 and 0.84 W m^(-1)K^(-1),and the volume resistivity and breakdown strength are as high as 2.3×10^(15)Ωcm and 324.2 kV mm^(-1),respectively.Besides,it also presents extremely high tensile strength of 193.6 MPa and thermal decomposition temperature of 640°C,showing a broad application prospect in high-end thermal management fields such as electronic devices and electrical equipment.展开更多
The ring-opening polymerization of D, L-lactide in the melt was systematically investigated by using stannous octoate as the initiator. The molecular weight of poly (D, L-lactide) was characterized with M,. Mn and Mw ...The ring-opening polymerization of D, L-lactide in the melt was systematically investigated by using stannous octoate as the initiator. The molecular weight of poly (D, L-lactide) was characterized with M,. Mn and Mw respectively. The results indicated that five variables, namely purity of monomer, initiator to monomer ratio, vacuum level, polymerization temperature and polymerization time had different influences on the molecular weight and molecular weight distribution of poly(D. L-lactide).展开更多
After removal of the caries or diseased teeth,the alveolar ridge will undergo absorption and atrophy.When the amount of alveolar bone is insufficient,it will cause an inability to perform effective dental implant rest...After removal of the caries or diseased teeth,the alveolar ridge will undergo absorption and atrophy.When the amount of alveolar bone is insufficient,it will cause an inability to perform effective dental implant restoration.In order to control the absorption and promote the repair and regeneration of alveolar ridge,a method of implanting guided bone regeneration(GBR)membranes at the extraction site is often used.In this study,silk fibroin(SF)and poly-L-lactide lactone(PLCL)were used to prepare bilayered guided bone regeneration membranes,and its morphology,hydrophilicity,surface roughness and mechanical properties were studied.At the same time,the drug release behaviors and cell compatibility of the bilayered membranes were studied.The results showed that SF/PLCL bi-layered membranes had good mechanical properties and surface hydrophilicity,and the drug-loaded bi-layered membranes had good cell compatibility.The bilayered membranes fabricated in this study are of potential for applying in the oral health field to promote bone regeneration.展开更多
This work evaluates intercalation of Nortriptyline(NT)and Venlafaxine(VFX)in an interlayer gallery of Na^(+)-MMT(Montmorillonite),which was further compounded with Poly(LLactide)(PLLA)to form microcomposite spheres(MP...This work evaluates intercalation of Nortriptyline(NT)and Venlafaxine(VFX)in an interlayer gallery of Na^(+)-MMT(Montmorillonite),which was further compounded with Poly(LLactide)(PLLA)to form microcomposite spheres(MPs)for oral controlled drug delivery.The XRD patterns,thermal and spectroscopic analyses indicated intercalation of drugs into the MMT interlayer that was stabilized by electrostatic interaction.No significant changes in structural and functional properties of drugs were found in the MMT layers.In vitro drug release studies showed controlled release pattern.展开更多
To develop a new generation of absorbable fracture fixation devices with enhanced biocompatibility, the biodegradation mechanism and its influence on the cellular response at the tissue/implant interface of hydroxyapa...To develop a new generation of absorbable fracture fixation devices with enhanced biocompatibility, the biodegradation mechanism and its influence on the cellular response at the tissue/implant interface of hydroxyapatite/ poly DL lactide (HA/PDLLA) composites were investigated in vitro and in vivo.HA/PDLLA rods were immersed in phosphate buffered saline,or implanted in muscle and bony tissue for 52 weeks.Scanning electron microscopic and histological studies were done.The degradation rate was the slowest in vitro,slower in muscle tissue and fast in bone.In vitro, the composites degraded heterogeneously and a hollow structure was formed.In bone,the limited clearing capacity leads to the accumulation of oligomeric debris,which contribute totally to the autocatalytic effect.So,the fastest degradation and intense tissue response were seen.In muscle tissue,oligomeric debris migrated into vicinal fibers over a long distance from the original implant cavity and the tissue reactions were,however, quite moderate.For the same size organic/inorganic composite,the environment where it was placed is the major factor in determining its biodegradation process and cellular reaction.In living tissue,factors such as cells,enzymes and mechanical stress have an obvious influence on the biodegradation and biological process at the tissue/implant interface.The biocompatibility of the HA/PDLLA composites is enhanced with the incorporating of the resorbable HA microparticles.展开更多
基金financially supported by Mahasarakham University。
文摘A poly(L-lactide)-b-poly(ethylene glycol)-b-poly(L-lactide)(PLLA-PEG-PLLA)block copolymer has great potential for use as a flexible bioplastic.Highly flexible bioplastics are required for flexible packaging applications.In this work,a PEG was incorporated into block copolymer as a plasticizer by solvent casting.PLLA-PEG-PLLA/PEG blends with different blend ratios were prepared,and the plasticizing effect and miscibility of PEG in block copolymer were intensively investigated compared to PLLA/PEG blends.The results indicated that the PEG was an effective plasticizer for the block copolymer.The blending of PEG decreased glass-transition temperature and accelerated the crystallization of both the PLLA and PLLA-PEG-PLLA matrices.The PEG was completely miscible when blended with block copolymer and it improved thermal stability of the block copolymer matrix but not of the PLLA matrix.Film extensibility of PLLA-PEG-PLLA/PEG blends steadily increased as the PEG ratio increased.These non-toxic and highly flexible PLLA-PEG-PLLA/PEG bioplastics are promising candidates for several applications such as biomedical devices,tissue scaffolds and packaging materials.
基金This research was made possible by a Johnson & Johnson CORD Internship Award funded by Ethicon. BH and BF thank the National Science Foundation for partial financial support (DMR-0098104).
文摘Structure and properties of bioabsorbable polyglycolide (PGA) and poly(glycolide-co-lactide) (PGA-co-PLA)fibers were investigated during several industrial processing stages and in vitro degradation by means of wide-angle X-raydiffraction (WAXD), dynamic mechanical analysis (DMA) and mechanical property tests. In the orientation stage, the PGAfibers were found to have higher degrees of crystallinity than corresponding PGA-co-PLA samples produced under similarconditions. In the hot-stretching and post-annealing stages, after fibers were braided, PGA samples were found to gain morecrystallinity and higher T_g than PGA-co-PLA samples. The higher crystallinity in PGA fibers resulted in a slower rate ofdegradation. DMA results showed that a great deal of internal stress that was built during orientation and hot-stretchingstages was released in the post-annealing stage for a1l PGA and PGA-co-PLA samples. During earlier stages of in vitrodegradation, both PGA and PGA-co-PLA samples exhibited the typical cleavage-induced crystallization mechanism. Theheat shrinkage in the glass transition area was found to disappear after 6-8 days of degradation for all PGA and PGA-co-PLAsamples, indicating the amorphous portions of the polymers lost orientation after a short period in the buffer solution, mostlikely due to relaxation of the cleaved chains.
文摘Poly (L-lactide) was prepared by bulk polymerization ofL-lactide at 140°C in the presence of stannous octoate. The polymer products were characterized by number average molecular weight Mn, weight average molecular weight Mw and molecular weight distribution MWD (M w/M n) respectively. The results showed that stannous octoate was a high effective catalyst, and coordinated insertion mechanism of the reaction was proposed.
基金The authors are Indebted to the National Basic Science Rescarch and Development Grants(973)(No.1999054306).
文摘Poly (L-lactide)-poly(ethylene glycol) multiblock copolymers with predetermined block lengths were synthesized by polycondensation of PLA diols and PEG diacids. These copolymers presented special properties, such as better miscibility between the two components, low crystallinity and better hydrophilicity, which can be modulated by adjusting the block lengths of the two components.
基金supported by the National Natural Science Foundation of China(No.50527301)
文摘The non-isothermal crystallization of poly(L-lactide) (PLLA) under quiescent and steady shear flow conditions was in situ investigated by using polarizing optical microscopy (POM) with a hot shear stage and wide-angle X-ray diffraction (WAXD). The shear rate and the cooling rate both play a significant role in the final crystalline morphology and crystallinity. Under quiescent conditions, the morphology assumes different sized spherulites, and its crystallinity dramatically reduces with increasing the cooling rate. On the other hand, the shear flow increases the onset crystallization temperature, and enhances the final crystallinity. When the shear rate is above 5 s^-1, cylindrite-like crystals are observed, furthermore, their content depends on the cooling rate.
基金supported by the National Natural Sciences Fund of China(No.50603025)the Opening Project of State Key Laboratory of Polymer Materials Engineering(Sichuan University).
文摘Poly(d,l-lactide-co-p-dioxanone) (P(LA-co-PDO)) copolymers with different chain microstructures were synthesized by onestep or two-step bulk ring-opening polymerizations of d,l-lactide (LA) and p-dioxanone (PDO) monomers using stannous octoate [Sn(Oct)2]/n-dodecanol as the initiating system. The average sequence lengths of the lactidyl (LLA) and dioxanyl (LpDo) units were calculated from the ^1H NMR spectra. It was found that both LLA and Lpoo values from the two-step syntheses were significantly longer than those from the corresponding one-step syntheses, indicating more blocky structure achieved for the twostep copolymers. Corresponding to this difference in microstructure, the two-step copolymers were semi-crystalline, while the one-step copolymers were completely amorphous. In conclusion, the crystallinity of P(LA-co-PDO) copolymers could be adjusted conveniently to meet specific applications by changing the microstructure of the copolymers via different polymerization routes.
基金Project(50174059) supported by the National Natural Science Foundation of China
文摘Bioactive and bioresorbable composite was fabricated by a solvent evaporation technique using poly-L-lactide(PLLA) and bioactive glass (average particle size: 6.8 μm). Bioactive glass granules are homogeneously distributed in the composite with microcrack structure. The formation of hydroxyapatite(HA) on the composite in simulated body fluid(SBF) was analyzed by scanning electron microscopy(SEM), energy dispersive spectroscopy(EDS), X-ray diffraction(XRD), and Raman spectra. Rod-like HA crystals deposit on the surface of PLLA/bioactive glass composite after soaking for 3 d. Both rod-like crystals and HA layer form on the surface for 14 d in SBF. The high bioactivity of PLLA/bioactive glass composite indicates the potential of materials for integration with bone.
文摘The aim of the present study was to develop a novel long-acting Poly(lactic-co-glycolic acid)(PLGA)-based microspheres formulation of Bisdemethoxycurcum(BDMC) by emulsionsolvent evaporation method. Meanwhile, the effects of the volume ratio of the dispersed phase and continuous phase, the concentration of PLGA and PVA, the theoretical drug loading and stirring speed were investigated. The mean diameter of the microspheres was 8.5 μm and the size distribution was narrow. The encapsulation efficiency(EE) and drug loading efficiency(DLE) of BDME loaded PLGA microspheres(BDMC-PLGA-MS) was 94.18% and 8.14%,respectively. In an in vitro study of drug release, it can be concluded that the BDMC-PLGAMS exhibited sustained and long-term release properties for 96 h. Stability studies suggested that the microspheres we prepared had a very good stability. Furthermore, the results of an in vivo study indicated that the BDMC-PLGA-MS had sustained release effect and was mainly distributed in the lung tissue, and less distribution in other tissues, which indicated that microspheres could be an effective parenteral carrier for the delivery of BDMC in lung cancer treatment.
文摘Poly (lactic acid) (PLA) was synthesized by microwave-assisted ring-opening polymerization of D, L-lactide with stannous octanoate (SnOct(2)) as catalyst. Its weight-average molar mass (M-w) ranged from 39000 to 67000 and the polydispersity index from 1.3 to 1.7. The polymerization rate was much faster than that of the conventional thermal polymerization. A degradation of newly formed PLA in reaction mixture by microwave irradiation was observed.
文摘A novel biodegradable polymer--poly (ethene maleic acid ester-co-D,L-lactide acid) was synthesized by copolymerizing lactide and prepolymer, which was prepared by the condensation of maleic anhydride and glycol, using p-toluene sulphonic acid as a catalyst, attempting to improve the hydrophilicity, increase flexibility and modulate the degradation rate. FTIR,^1H NMR, MALLS and DSC were employed to characterize these polymers.
文摘L-lactide was prepared from L-lactic acid with stannous octoate as the catalyst. The effects of reaction temperature and pressure on the ingredient of crude lactide were investigated. The results show that the mass fraction of meso-lactide increases with the increasing reaction temperature. Crude lactide containing 85.4% L-lactide is obtained when the reaction temperature is 200 ℃. High purity of L-lactide with a yield of 40.6 % is obtained by synthetic purifying method. The properties of L-lactide are characterized by optical purity, infrared spectrum and gas chromatogram/mass spectrum. The L-lactide samples purified by recrystallization and synthetic purifying methods are polymerized with the catalyst of stannous octoate, and the corresponding viscosity average relative molecular masses of poly(L-lactide) are 2.85 × 105 and 5.05 × 105 , respectively. This indicates that the optical purity of Llactide has great influence on the relative molecular mass of poly(L-lactide).
基金Project(50174059) supported by the National Natural Science Foundation of China
文摘Poly(D,L-lactide) was synthesized by indirect method from D,L-lactic acid and characterized by infrared spectrum and proton nuclear magnetic resonance. The influences of monomer purity, initiator concentration, polymerization temperature and polymerization time on the relative molecular mass of poly(D, L-lactide) were investigated. The polylactide was made into porous materials by using solvent-casting particulate-leaching method. Under the optimized conditions, polylactides with a viscosity average molecular mass up to 1.82×105 are obtained and the results are fairly reproducible. Scanning electron microscope observation indicates that the sample is highly porous and well-distributed with good interconnections between pores and the pore size of porous materials is in the range from 200 μm to 500 μm and it can be used as scaffold for bone tissue engineering.
基金The project was supported by the National Natural Science Foundation of China(No.29774034).
文摘Poly-dl-lactide-poly(ethylene glycol) (PELA) triblock copolymers were synthesized with lanthanum acetate as the initiator. PELA microspheres with entrapped Vibrio Cholera antigen and outer membrane protein (OMP) were prepared by a double emulsion W/O/W based on solvent extraction methods. The obtained microspheres showed smooth and spherical surface and their size varied between 0.5 and 5.0 mu m, which are suitable for oral targeting delivery system. The distribution tests in rabbits and mice through scanning electronic micrography and fluorescence microscope indicated that microspheres have successfully reached the immunization-related tissues, such as the liver, spleen and intestinal peyer's patches, following oral administration. The PELA microspheres were also evaluated as an efficient antigen delivery system by enhancing a higher protective ratio against live Vibrios Cholera.
基金supported by National Natural Science Foundation of China(Grant No.U1930113),ChinaNational Natural Science Foundation of China(52072036)
文摘Poly(ethylene oxide)(PEO)-based polymer electrolytes show the prospect in all-solid-state lithium metal batteries;however,they present limitations of low room-temperature ionic conductivity,and interfacial incompatibility with high voltage cathodes.Therefore,a salt engineering of 1,1,2,2,3,3-hexafluoropropane-1,3-disulfonimide lithium salt(LiHFDF)/LiTFSI system was developed in PEO-based electrolyte,demonstrating to effectively regulate Li ion transport and improve the interfacial stability under high voltage.We show,by manipulating the interaction between PEO matrix and TFSI^(-)-HFDF^(-),the optimized solid-state polymer electrolyte achieves maximum Li+conduction of 1.24×10^(-4)S cm^(-1)at 40℃,which is almost 3 times of the baseline.Also,the optimized polymer electrolyte demonstrates outstanding stable cycling in the LiFePO_(4)/Li and LiNi_(0.8)Mn_(0.1)Co_(0.1)O_(2)/Li(3.0-4.4 V,200 cycles)based all-solid-state lithium batteries at 40℃.
基金The authors are grateful for the support and funding from the Foundation of National Natural Science Foundation of China(52373089 and 51973173)Startup Foundation of Chongqing Normal University(23XLB011),Science and Technology Research Program of Chongqing Municipal Education Commission(KJQN202300561)Fundamental Research Funds for the Central Universities。
文摘With the rapid development of 5G information technology,thermal conductivity/dissipation problems of highly integrated electronic devices and electrical equipment are becoming prominent.In this work,“high-temperature solid-phase&diazonium salt decomposition”method is carried out to prepare benzidine-functionalized boron nitride(m-BN).Subsequently,m-BN/poly(pphenylene benzobisoxazole)nanofiber(PNF)nanocomposite paper with nacremimetic layered structures is prepared via sol–gel film transformation approach.The obtained m-BN/PNF nanocomposite paper with 50 wt%m-BN presents excellent thermal conductivity,incredible electrical insulation,outstanding mechanical properties and thermal stability,due to the construction of extensive hydrogen bonds andπ–πinteractions between m-BN and PNF,and stable nacre-mimetic layered structures.Itsλ∥andλ_(⊥)are 9.68 and 0.84 W m^(-1)K^(-1),and the volume resistivity and breakdown strength are as high as 2.3×10^(15)Ωcm and 324.2 kV mm^(-1),respectively.Besides,it also presents extremely high tensile strength of 193.6 MPa and thermal decomposition temperature of 640°C,showing a broad application prospect in high-end thermal management fields such as electronic devices and electrical equipment.
基金Funded by the Key Project of the Ministry of Science and Technology (No. 96 - 920 - 20 - 21)
文摘The ring-opening polymerization of D, L-lactide in the melt was systematically investigated by using stannous octoate as the initiator. The molecular weight of poly (D, L-lactide) was characterized with M,. Mn and Mw respectively. The results indicated that five variables, namely purity of monomer, initiator to monomer ratio, vacuum level, polymerization temperature and polymerization time had different influences on the molecular weight and molecular weight distribution of poly(D. L-lactide).
基金Natural Science Foundation for Key Program of the Jiangsu Higher Education Institutions,China(No.19KJA610004)Natural Science Foundation of Jiangsu Province,China(No.BK20161254)+1 种基金China Postdoctoral Science Foundation(No.2019M651947)Mandatory Projects of Nantong Municipal Science and Technology Plan,China(No.JC2018004)
文摘After removal of the caries or diseased teeth,the alveolar ridge will undergo absorption and atrophy.When the amount of alveolar bone is insufficient,it will cause an inability to perform effective dental implant restoration.In order to control the absorption and promote the repair and regeneration of alveolar ridge,a method of implanting guided bone regeneration(GBR)membranes at the extraction site is often used.In this study,silk fibroin(SF)and poly-L-lactide lactone(PLCL)were used to prepare bilayered guided bone regeneration membranes,and its morphology,hydrophilicity,surface roughness and mechanical properties were studied.At the same time,the drug release behaviors and cell compatibility of the bilayered membranes were studied.The results showed that SF/PLCL bi-layered membranes had good mechanical properties and surface hydrophilicity,and the drug-loaded bi-layered membranes had good cell compatibility.The bilayered membranes fabricated in this study are of potential for applying in the oral health field to promote bone regeneration.
基金Authors are thankful to Director,CSMCRI,Bhavnagar for pro-viding necessary infrastructure facilities and the Council of Scientific and Industrial Research,Government of India,New Delhi,India(CSIR)for Senior research fellowship awarded to BDK,and funding under Network Project:NWP 0010.
文摘This work evaluates intercalation of Nortriptyline(NT)and Venlafaxine(VFX)in an interlayer gallery of Na^(+)-MMT(Montmorillonite),which was further compounded with Poly(LLactide)(PLLA)to form microcomposite spheres(MPs)for oral controlled drug delivery.The XRD patterns,thermal and spectroscopic analyses indicated intercalation of drugs into the MMT interlayer that was stabilized by electrostatic interaction.No significant changes in structural and functional properties of drugs were found in the MMT layers.In vitro drug release studies showed controlled release pattern.
文摘To develop a new generation of absorbable fracture fixation devices with enhanced biocompatibility, the biodegradation mechanism and its influence on the cellular response at the tissue/implant interface of hydroxyapatite/ poly DL lactide (HA/PDLLA) composites were investigated in vitro and in vivo.HA/PDLLA rods were immersed in phosphate buffered saline,or implanted in muscle and bony tissue for 52 weeks.Scanning electron microscopic and histological studies were done.The degradation rate was the slowest in vitro,slower in muscle tissue and fast in bone.In vitro, the composites degraded heterogeneously and a hollow structure was formed.In bone,the limited clearing capacity leads to the accumulation of oligomeric debris,which contribute totally to the autocatalytic effect.So,the fastest degradation and intense tissue response were seen.In muscle tissue,oligomeric debris migrated into vicinal fibers over a long distance from the original implant cavity and the tissue reactions were,however, quite moderate.For the same size organic/inorganic composite,the environment where it was placed is the major factor in determining its biodegradation process and cellular reaction.In living tissue,factors such as cells,enzymes and mechanical stress have an obvious influence on the biodegradation and biological process at the tissue/implant interface.The biocompatibility of the HA/PDLLA composites is enhanced with the incorporating of the resorbable HA microparticles.