Self-ordering of the cell arrangement of the anodic porous alumina was prepared in oxalic acid solution at a constant potential of 40V and at a temperature of 20C. The honeycomb structure made by one step anodization...Self-ordering of the cell arrangement of the anodic porous alumina was prepared in oxalic acid solution at a constant potential of 40V and at a temperature of 20C. The honeycomb structure made by one step anodization method and two step anodization method is different. Pores in the alumina film prepared by two step anodization method were more ordered than those by one step anodization method.展开更多
文摘Self-ordering of the cell arrangement of the anodic porous alumina was prepared in oxalic acid solution at a constant potential of 40V and at a temperature of 20C. The honeycomb structure made by one step anodization method and two step anodization method is different. Pores in the alumina film prepared by two step anodization method were more ordered than those by one step anodization method.