A water-quenching technique has been adopted to evaluate thermal shock fracture and fatigue behaviors of porous Si3N4 ceramics in an air atmosphere. The high-porosity Si3N4 ceramics exhibit a higher strength retention...A water-quenching technique has been adopted to evaluate thermal shock fracture and fatigue behaviors of porous Si3N4 ceramics in an air atmosphere. The high-porosity Si3N4 ceramics exhibit a higher strength retention and a better resistance to thermal shock fatigue because of its role of the pores as crack arresters.A dense and coherent surface oxide layer leads to a significant benefit in residual strength during thermal fatigue, however, an increased fatigue number to 30 th cycle cannot cause a further influence although a thicker oxide layer presents, which is attributed to holes defect and disappearance of part intergranular phase.展开更多
Porous silicon nitride ceramics(Si3N4) were fabricated by pressureless sintering using different particle size of silicon nitride powder.Lu2O3 was used as sintering additive.According to phase relationships in the t...Porous silicon nitride ceramics(Si3N4) were fabricated by pressureless sintering using different particle size of silicon nitride powder.Lu2O3 was used as sintering additive.According to phase relationships in the ternary system Si3N4-SiO2-Lu2O3,porous Si3N4 ceramics with different phase composition were designed through the change of the content of SiO2 which was formed by the oxidation at 800℃ in air.Porous Si3N4 with different phase compositions was obtained after sintering at 1800℃ in N2atmosphere.A small content of SiO2 favored the formation of secondary phase Lu4Si2O7N2,while large content of SiO2 favored the formation of secondary phase Lu2Si2O7 and Si2N2O.Porous Si3N4 ceramics with secondary phase Lu4Si2O7N2 had a flexural strength of 207 MPa,while that with secondary phase Si2N2O and Lu2Si2O7 had lower flexural strength.展开更多
This paper presents the microwave dielectric properties of reaction bonded porous silicon nitride ceramics with variant porosity and pore size, which were prepared by adding pore-forming agent grains into the silicon ...This paper presents the microwave dielectric properties of reaction bonded porous silicon nitride ceramics with variant porosity and pore size, which were prepared by adding pore-forming agent grains into the silicon powders. The experimental results show that the dielectric constant and the dielectric loss of the samples reduce evidently with increasing porosity in the sample. When the porosity is constant, the dielectric constant and the dielectric loss of the ceramics decrease visibly as the pore size increases. Among all the obtained samples, the minimum dielectric constant is about 2.4.展开更多
Porous silicon nitride(Si_3N_4) ceramics were fabricated by low temperature pressureless sintering, using carbonized rice husk and α-Si_3N_4 powders as raw materials, and MgO-CeO_2 as sintering additives. The effec...Porous silicon nitride(Si_3N_4) ceramics were fabricated by low temperature pressureless sintering, using carbonized rice husk and α-Si_3N_4 powders as raw materials, and MgO-CeO_2 as sintering additives. The effects of CeO_2 concentration and sintering temperature on phase composition, microstructure, porosity and flexural strength of the sintered products were investigated by X-ray diffraction(XRD), scanning electronic microscopy(SEM), Archimedes' displacement method and three-point bending strength, respectively. The results suggested that MgO-CeO_2 was a much more effective sintering additive for Si_3N_4 than MgO alone. When CeO_2 concentration was 4 wt.%–5 wt.% and sintering temperatures were in a range of 1500 to 1550 oC, the obtained porous silicon nitride ceramics had the porosity of 45.78%–42.81% and flexural strength of 49.44–84.09 MPa. Moreover, when sintering temperature was 1550 oC and CeO_2 concentration was 5%, large elongated β-Si_3N_4 grains were well developed.展开更多
基金financial support of the project from the National Natural Science Foundation of China (Nos. 51272206 and 51472198)the Program for Changjiang Scholars and Innovative Research Team in University (No. IRT1280)+2 种基金the National Key Laboratory Functional Composite (No. 9140C560109130C56201)the Fundamental Research Funds for the Central University (No. xkjc2014009)the State Key Laboratory for Mechanical Behavior of Materials (No. 20121207)
文摘A water-quenching technique has been adopted to evaluate thermal shock fracture and fatigue behaviors of porous Si3N4 ceramics in an air atmosphere. The high-porosity Si3N4 ceramics exhibit a higher strength retention and a better resistance to thermal shock fatigue because of its role of the pores as crack arresters.A dense and coherent surface oxide layer leads to a significant benefit in residual strength during thermal fatigue, however, an increased fatigue number to 30 th cycle cannot cause a further influence although a thicker oxide layer presents, which is attributed to holes defect and disappearance of part intergranular phase.
基金the State Key Laboratory of Solidification Processing in NWPU(No. KB200920)the Program for New Century Excellent Talents in University
文摘Porous silicon nitride ceramics(Si3N4) were fabricated by pressureless sintering using different particle size of silicon nitride powder.Lu2O3 was used as sintering additive.According to phase relationships in the ternary system Si3N4-SiO2-Lu2O3,porous Si3N4 ceramics with different phase composition were designed through the change of the content of SiO2 which was formed by the oxidation at 800℃ in air.Porous Si3N4 with different phase compositions was obtained after sintering at 1800℃ in N2atmosphere.A small content of SiO2 favored the formation of secondary phase Lu4Si2O7N2,while large content of SiO2 favored the formation of secondary phase Lu2Si2O7 and Si2N2O.Porous Si3N4 ceramics with secondary phase Lu4Si2O7N2 had a flexural strength of 207 MPa,while that with secondary phase Si2N2O and Lu2Si2O7 had lower flexural strength.
基金supported by the National Natural Science Foundation of China under grant No.90305016.
文摘This paper presents the microwave dielectric properties of reaction bonded porous silicon nitride ceramics with variant porosity and pore size, which were prepared by adding pore-forming agent grains into the silicon powders. The experimental results show that the dielectric constant and the dielectric loss of the samples reduce evidently with increasing porosity in the sample. When the porosity is constant, the dielectric constant and the dielectric loss of the ceramics decrease visibly as the pore size increases. Among all the obtained samples, the minimum dielectric constant is about 2.4.
基金Project supported by the research fund of Collaborative Innovation Center for Ecological Building Materials(GX2015304,CP201506)Jiangsu Provincial Natural Science Foundation(BK20150427)
文摘Porous silicon nitride(Si_3N_4) ceramics were fabricated by low temperature pressureless sintering, using carbonized rice husk and α-Si_3N_4 powders as raw materials, and MgO-CeO_2 as sintering additives. The effects of CeO_2 concentration and sintering temperature on phase composition, microstructure, porosity and flexural strength of the sintered products were investigated by X-ray diffraction(XRD), scanning electronic microscopy(SEM), Archimedes' displacement method and three-point bending strength, respectively. The results suggested that MgO-CeO_2 was a much more effective sintering additive for Si_3N_4 than MgO alone. When CeO_2 concentration was 4 wt.%–5 wt.% and sintering temperatures were in a range of 1500 to 1550 oC, the obtained porous silicon nitride ceramics had the porosity of 45.78%–42.81% and flexural strength of 49.44–84.09 MPa. Moreover, when sintering temperature was 1550 oC and CeO_2 concentration was 5%, large elongated β-Si_3N_4 grains were well developed.