Effects of deformation parameters on formation of pro-eutectoid cementite in hypereutectoid steels
1
作者 管仁国 赵占勇 +2 位作者 钞润泽 刘相华 C.S.LEE 《Journal of Central South University》 SCIE EI CAS 2014年第4期1256-1263,共8页
Brittle pro-eutectoid cementite that forms along prior-austenite in hypereutectoid steels is deleterious to mechanical properties. The optimum process parameters which suppress the formation of pro-eutectoid cementite... Brittle pro-eutectoid cementite that forms along prior-austenite in hypereutectoid steels is deleterious to mechanical properties. The optimum process parameters which suppress the formation of pro-eutectoid cementite in hypereutectoid steels with carbon content in the range of 0.8%-1.3% in mass fraction, were investigated. Pro-eutectoid cementite formation is effectively hindered by increasing the deformation temperature and decreasing the amount of strain. Transformation at lower temperatures close to the nose of the cooling-transformation diagram also reduces the tendency of the formation of pro-eutectoid cementite. Control of prior-austenite grain size and grain boundary conditions is important. Due to larger number of nucleation sites, finer prior-austenite grain size results in the acceleration of transformation to pro-eutectoid cementite. However, large prior-austenite and straight boundaries lead to less nucleation sites of pro-eutectoid cementite. The cooling rate and carbon content should be reduced as much as possible. The transformation temperature below 660 °C and the strain of 0.5 at deformation temperature of 850 °C are suggested. 展开更多
关键词 共析渗碳体 过共析钢 变形参数 奥氏体晶粒尺寸 奥氏体形成 最佳工艺参数 变形温度 边界条件
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部