A linear relationship has been realized between the maximum streamer length and discharge voltage of a pulsed positive streamer discharge by measuring the streamer length in water with conductivity of 100 μS cm-1usin...A linear relationship has been realized between the maximum streamer length and discharge voltage of a pulsed positive streamer discharge by measuring the streamer length in water with conductivity of 100 μS cm-1using high-speed photography. Based on Ohm's law, a quantitative equation has been derived for the dependence of the maximum streamer length on the discharge voltage of a pulsed positive streamer discharge in water. According to the equation, our results suggest that the streamers spontaneously stop propagating through water due to the voltage at the streamer head dropping below the ignition voltage of a pulsed positive streamer discharge.展开更多
A set of metallic specimens containing fatigue cracks with different sizes were tested using eddy current pulsed thermography(ECPT),therefore the relations between heating response of the crack area and the crack leng...A set of metallic specimens containing fatigue cracks with different sizes were tested using eddy current pulsed thermography(ECPT),therefore the relations between heating response of the crack area and the crack length was studied.The numerical and experimental results both showed that the increase of the crack length enhanced the crack heating response under specific test conditions.A particular form of calculated response signal,which is linearly related to the crack length,was introduced to provide a quantitative evaluation of crack length.展开更多
基金supported in part by National Natural Science Foundation of China(Nos.11635004,11275040,and 51437002)
文摘A linear relationship has been realized between the maximum streamer length and discharge voltage of a pulsed positive streamer discharge by measuring the streamer length in water with conductivity of 100 μS cm-1using high-speed photography. Based on Ohm's law, a quantitative equation has been derived for the dependence of the maximum streamer length on the discharge voltage of a pulsed positive streamer discharge in water. According to the equation, our results suggest that the streamers spontaneously stop propagating through water due to the voltage at the streamer head dropping below the ignition voltage of a pulsed positive streamer discharge.
基金supported by the Open Foundation of Key Laboratory of Nondestructive Testing of Ministry of Education of Nanchang Aeronautical University
文摘A set of metallic specimens containing fatigue cracks with different sizes were tested using eddy current pulsed thermography(ECPT),therefore the relations between heating response of the crack area and the crack length was studied.The numerical and experimental results both showed that the increase of the crack length enhanced the crack heating response under specific test conditions.A particular form of calculated response signal,which is linearly related to the crack length,was introduced to provide a quantitative evaluation of crack length.