The effects of process parameters on the depth-to-width ratio (D/W) of flux-cored wire underwater wet welding with a certain type of homemade .flux-cored wire are studied. It is found that the welding .speed, wire f...The effects of process parameters on the depth-to-width ratio (D/W) of flux-cored wire underwater wet welding with a certain type of homemade .flux-cored wire are studied. It is found that the welding .speed, wire feeding speed and torch oscillating amplitude hare significant effects on the dopth-to-width ratio (D/W) of welds. The D/W ratio of welds increases significantly with the increase of welding speed without the oscillating of welding torch. It increased (from 0. 14 to 0. 26 ) with the increase of wire feeding speed while the torch oscillating. And it decreased linearly with the increase of torch oscillating amplitude. However, the influelwe of oscillating speed, wire extension and welding voltage on the D/W ratio of welds was not obvious.展开更多
Bed morphology is the result of a dynamic response to a complex meandering river system. It is an important factor for the further development of river. Based on the meandering river characterized by a large depth-to-...Bed morphology is the result of a dynamic response to a complex meandering river system. It is an important factor for the further development of river. Based on the meandering river characterized by a large depth-to-width ratio, a theoretical model is established with the coupling of Navier-Stokes (N-S)~ sediment transport, and bed deformation equations. The flow characteristics and bed response of river are obtained with the perturbation method. The research results show that, under the effect of two- dimensional flow disturbance, the bars and pools present the regular response. For a given sinuousness, the amplitude of the bed response can be used as a criterion to judge the bedform stability. The effects of the Reynolds number, disturbance wavenumber, sinuousness, and bed morphology gradient on the bed response development are described.展开更多
In order to meet the requirement of structural inspection,the crack spacing and crack width at various heights in the tensile zone of six large depth reinforced concrete beams were measured under several loading level...In order to meet the requirement of structural inspection,the crack spacing and crack width at various heights in the tensile zone of six large depth reinforced concrete beams were measured under several loading levels of serviceability state.The effects of the depth of normal section beams on the crack spacing and crack width were analyzed,and the modified model is proposed for calculating the average crack spacing by thinking about the depth of normal section,the reinforcement arrangement and the effective reinforcement ratio.The relationships of crack widths at any position in the tensile zone and at the reinforcement level on the side surface of beam were studied.By theoretical and statistical analysis,a method is proposed to calculate the ratios of crack widths between any position and the reinforcement level on the side surface of large depth reinforced concrete beams.展开更多
In this study,adopting uniform design method established a mathematical model to prepare multi-element active flux. GH4169 superalloy plates were welded by the Nd: YAG laser equipment with the prepared active flux. Th...In this study,adopting uniform design method established a mathematical model to prepare multi-element active flux. GH4169 superalloy plates were welded by the Nd: YAG laser equipment with the prepared active flux. The results show all kinds of fluxes increase the depth to width ratio and the multi-component systems are more significant. The largest increment of the weld depth to width ratio is 159%,obtained by using of the F12 series flux. It is proved that by using of the active flux to increase the depth to width ratio of micro laser welding is feasible.展开更多
Joining metal to plastic can lighten weight of products to reduce energy consumption.However,it is difficult to achieve high-strength welding between metal and plastic.To address this problem,the methods of surface te...Joining metal to plastic can lighten weight of products to reduce energy consumption.However,it is difficult to achieve high-strength welding between metal and plastic.To address this problem,the methods of surface texture pretreatment and laser irradiation welding was proposed to achieve the high-strength connection of metal and plastic.In this study,with different parameters of laser power and texture morphology,1060 Al with surface texture treatment was joined to polyethylene terephthalate(PET)by laser irradiation welding from metal side.Study showed that as the laser power increased,the tensile shear strength of joints increased first,and decreased thereafter.Tensile shear tests demonstrated that the mechanical force of joint was strengthened contributed to mechanical anchorage formed by surface texture.The depth-width ratio of the texture grooves affected the tensile shear process of the joint.According to the result of temperature simulation,the existence of texture grooves reduced the heat transfer efficiency,and the heat dissipation at interface was also impeded in course of laser welding.Finally,the maximum tensile strength of 1060Al-PET joint reached 48.4 MPa,which was close to the strength of PET matrix.The bonding mechanism of the 1060Al-PET joints was composed of mechanical bonding and chemical bonding.This study proposes an effective method to join metal to plastic which achieved high-strength connection between metal and plastic.展开更多
文摘The effects of process parameters on the depth-to-width ratio (D/W) of flux-cored wire underwater wet welding with a certain type of homemade .flux-cored wire are studied. It is found that the welding .speed, wire feeding speed and torch oscillating amplitude hare significant effects on the dopth-to-width ratio (D/W) of welds. The D/W ratio of welds increases significantly with the increase of welding speed without the oscillating of welding torch. It increased (from 0. 14 to 0. 26 ) with the increase of wire feeding speed while the torch oscillating. And it decreased linearly with the increase of torch oscillating amplitude. However, the influelwe of oscillating speed, wire extension and welding voltage on the D/W ratio of welds was not obvious.
文摘Bed morphology is the result of a dynamic response to a complex meandering river system. It is an important factor for the further development of river. Based on the meandering river characterized by a large depth-to-width ratio, a theoretical model is established with the coupling of Navier-Stokes (N-S)~ sediment transport, and bed deformation equations. The flow characteristics and bed response of river are obtained with the perturbation method. The research results show that, under the effect of two- dimensional flow disturbance, the bars and pools present the regular response. For a given sinuousness, the amplitude of the bed response can be used as a criterion to judge the bedform stability. The effects of the Reynolds number, disturbance wavenumber, sinuousness, and bed morphology gradient on the bed response development are described.
基金Sponsored by the Outstanding Youth Scientific Fund of Henan Province(Grant No.04120002300)Program for Innovation in University of Henan Province(Grant No.[2004]294)
文摘In order to meet the requirement of structural inspection,the crack spacing and crack width at various heights in the tensile zone of six large depth reinforced concrete beams were measured under several loading levels of serviceability state.The effects of the depth of normal section beams on the crack spacing and crack width were analyzed,and the modified model is proposed for calculating the average crack spacing by thinking about the depth of normal section,the reinforcement arrangement and the effective reinforcement ratio.The relationships of crack widths at any position in the tensile zone and at the reinforcement level on the side surface of beam were studied.By theoretical and statistical analysis,a method is proposed to calculate the ratios of crack widths between any position and the reinforcement level on the side surface of large depth reinforced concrete beams.
基金supported by National Natural Science Foundation of China(No.51565040)Science and Technology Planning Project of Jiangxi Province(20151BBE50034,20133BBE50021)Aviation Science Funds of China(2014ZE56016)
文摘In this study,adopting uniform design method established a mathematical model to prepare multi-element active flux. GH4169 superalloy plates were welded by the Nd: YAG laser equipment with the prepared active flux. The results show all kinds of fluxes increase the depth to width ratio and the multi-component systems are more significant. The largest increment of the weld depth to width ratio is 159%,obtained by using of the F12 series flux. It is proved that by using of the active flux to increase the depth to width ratio of micro laser welding is feasible.
基金Supported by Natural Science Foundation of Jilin Province,China(20200201230JC).
文摘Joining metal to plastic can lighten weight of products to reduce energy consumption.However,it is difficult to achieve high-strength welding between metal and plastic.To address this problem,the methods of surface texture pretreatment and laser irradiation welding was proposed to achieve the high-strength connection of metal and plastic.In this study,with different parameters of laser power and texture morphology,1060 Al with surface texture treatment was joined to polyethylene terephthalate(PET)by laser irradiation welding from metal side.Study showed that as the laser power increased,the tensile shear strength of joints increased first,and decreased thereafter.Tensile shear tests demonstrated that the mechanical force of joint was strengthened contributed to mechanical anchorage formed by surface texture.The depth-width ratio of the texture grooves affected the tensile shear process of the joint.According to the result of temperature simulation,the existence of texture grooves reduced the heat transfer efficiency,and the heat dissipation at interface was also impeded in course of laser welding.Finally,the maximum tensile strength of 1060Al-PET joint reached 48.4 MPa,which was close to the strength of PET matrix.The bonding mechanism of the 1060Al-PET joints was composed of mechanical bonding and chemical bonding.This study proposes an effective method to join metal to plastic which achieved high-strength connection between metal and plastic.