Based on X-ray diffraction,optical microscopy and scanning electron microscopy analysis of the Dachang gold ore,it is showed that the sulfide of ore is the main carrier minerals of gold. A majority of gold is embedded...Based on X-ray diffraction,optical microscopy and scanning electron microscopy analysis of the Dachang gold ore,it is showed that the sulfide of ore is the main carrier minerals of gold. A majority of gold is embedded in pyrite and tetrahedrite as the form of inclusion and a small amount intergrowth with pyrite and gangue mineral,occasionally the presence is in form of monomer natural gold. The main factors which influence the recovery rate are sulfide mineral particle size,and the fine grained sulfide is beneficial for the dissociation and flotation of gold bearing minerals. The monomer dissociation degree of gold bearing minerals can reach91. 3%,when the grinding fineness is less than 0. 074 mm and grain level accounts as 80%. It is not conducive to the flotation of sulfide if the grinding fineness is low or high. It is difficult to completely dissociate the monomer if there is a small amount of pyrite and arsenopyrite in the ore. Therefore,before leaching the gold,it must conduct pretreatment to reach the ideal recovery rate of the gold,like roasting oxidation,pressure oxidation and biological oxidation. The fine microscopic gold has little influence on the gold recovery rate.展开更多
The extraction process of gold and silver from the gold clay ore containing arsenic and manganese was investigated.With the conventional technique,the leaching rates of gold and silver are 78.23%and 49.02%,respectivel...The extraction process of gold and silver from the gold clay ore containing arsenic and manganese was investigated.With the conventional technique,the leaching rates of gold and silver are 78.23%and 49.02%,respectively.To eliminate the negative effects of arsenic and manganese on cyanidation and increase the gold and silver leaching rates,a novel catalyst was added.The content of the catalyst used in the process was 8 g per 500 g org sample,the sample size was 60μm and the pH value was kept between 10 and 11.Leaching with the catalyst for 3-5 h under certain conditions,the gold leaching rate increased to over 90%and the silver leaching rate increased to 80%-90%.The catalyst can effectively liberate gold and silver from the enclosure of arsenic and manganese and the industrial experiment has great significance to the development and utilization of the gold clay ore containing arsenic and manganese.展开更多
Recovery of gold and silver from a sulphide concentrate by thiourea leaching was investigat-ed.The effects of various parameters on the process,such as oxidants,the initial concentrationof thiourea and acidity in solu...Recovery of gold and silver from a sulphide concentrate by thiourea leaching was investigat-ed.The effects of various parameters on the process,such as oxidants,the initial concentrationof thiourea and acidity in solutions as well as reaction temperature,were systematically exam-ined.From the results it was confirmed that(a)oxidants had no significant influence on the dis-solution of gold and silver at a fixed initial concentration of thiourea;(b)the initial concentra-tion of thiourea and acidity affected the dissolution rate only in the earliest period of leaching;(c)the rate of the process was controlled by reagent diffusion.The optimum operations wereworked out for the thiourea leaching process of the concentrate.展开更多
The Merrill-Crowe zinc-precipitation process has been applied worldwide on a large number of operations for recovering gold and silver from cyanide solutions. However, in some of the large plants this precipitate is o...The Merrill-Crowe zinc-precipitation process has been applied worldwide on a large number of operations for recovering gold and silver from cyanide solutions. However, in some of the large plants this precipitate is of low quality, because copper and especially lead are precipitated along with gold and silver resulting in a higher consumption of zinc powder, fluxes in the smelting of the precipitate, formation of mate and short life for crucibles. In this research, a method is proposed to recover lead, zinc and copper cyanide ions from barren solutions, from the Merrill-Crowe process with hydroxyapatite before the filter press. This technology is based on inducing nucleated precipitation of zinc, copper and silver ions in a serpentine reactor, using sodium sulfide as the precipitator and sulfuric acid for pH control. This procedure was successfully applied at WILLIAM Mining and BACIS Mining Group in México.展开更多
文摘Based on X-ray diffraction,optical microscopy and scanning electron microscopy analysis of the Dachang gold ore,it is showed that the sulfide of ore is the main carrier minerals of gold. A majority of gold is embedded in pyrite and tetrahedrite as the form of inclusion and a small amount intergrowth with pyrite and gangue mineral,occasionally the presence is in form of monomer natural gold. The main factors which influence the recovery rate are sulfide mineral particle size,and the fine grained sulfide is beneficial for the dissociation and flotation of gold bearing minerals. The monomer dissociation degree of gold bearing minerals can reach91. 3%,when the grinding fineness is less than 0. 074 mm and grain level accounts as 80%. It is not conducive to the flotation of sulfide if the grinding fineness is low or high. It is difficult to completely dissociate the monomer if there is a small amount of pyrite and arsenopyrite in the ore. Therefore,before leaching the gold,it must conduct pretreatment to reach the ideal recovery rate of the gold,like roasting oxidation,pressure oxidation and biological oxidation. The fine microscopic gold has little influence on the gold recovery rate.
基金supported by the National Natural Science Foundation of China(No.20877036) the Natural Science Foundation of Shaanxi Province,China(No.2006Z06)
文摘The extraction process of gold and silver from the gold clay ore containing arsenic and manganese was investigated.With the conventional technique,the leaching rates of gold and silver are 78.23%and 49.02%,respectively.To eliminate the negative effects of arsenic and manganese on cyanidation and increase the gold and silver leaching rates,a novel catalyst was added.The content of the catalyst used in the process was 8 g per 500 g org sample,the sample size was 60μm and the pH value was kept between 10 and 11.Leaching with the catalyst for 3-5 h under certain conditions,the gold leaching rate increased to over 90%and the silver leaching rate increased to 80%-90%.The catalyst can effectively liberate gold and silver from the enclosure of arsenic and manganese and the industrial experiment has great significance to the development and utilization of the gold clay ore containing arsenic and manganese.
文摘Recovery of gold and silver from a sulphide concentrate by thiourea leaching was investigat-ed.The effects of various parameters on the process,such as oxidants,the initial concentrationof thiourea and acidity in solutions as well as reaction temperature,were systematically exam-ined.From the results it was confirmed that(a)oxidants had no significant influence on the dis-solution of gold and silver at a fixed initial concentration of thiourea;(b)the initial concentra-tion of thiourea and acidity affected the dissolution rate only in the earliest period of leaching;(c)the rate of the process was controlled by reagent diffusion.The optimum operations wereworked out for the thiourea leaching process of the concentrate.
文摘The Merrill-Crowe zinc-precipitation process has been applied worldwide on a large number of operations for recovering gold and silver from cyanide solutions. However, in some of the large plants this precipitate is of low quality, because copper and especially lead are precipitated along with gold and silver resulting in a higher consumption of zinc powder, fluxes in the smelting of the precipitate, formation of mate and short life for crucibles. In this research, a method is proposed to recover lead, zinc and copper cyanide ions from barren solutions, from the Merrill-Crowe process with hydroxyapatite before the filter press. This technology is based on inducing nucleated precipitation of zinc, copper and silver ions in a serpentine reactor, using sodium sulfide as the precipitator and sulfuric acid for pH control. This procedure was successfully applied at WILLIAM Mining and BACIS Mining Group in México.