A hydrometallurgical process for refractory gold-bearing arsenosulfide concentrates at ambient temperature and pressure was presented, including fine grinding with intensified alkali-leaching (FGIAL), enhanced agita... A hydrometallurgical process for refractory gold-bearing arsenosulfide concentrates at ambient temperature and pressure was presented, including fine grinding with intensified alkali-leaching (FGIAL), enhanced agitation alkali-leaching (EAAL), thiosulfate leaching and displacement. Experimental results on a refractory gold concentrate showed that the total consumption of NaOH in alkaline leaching is only 41% of those theoretically calculated under the conditions of full oxidization for the same amount of arse- nides and sulfides transformed into arsenates and sulfates, and 72.3% of gold is synchro-dissoluted by thiosulfate self-generated during alkaline leaching. After alkaline leaching, thiosulfate leaching was carried out for 24 h. The dissolution of gold is increased to 91.9% from 4.6% by cyanide without the pretreatment. The displacement of gold by zinc powder in the solution gets to 99.2%. Due to an amount of thiosulfate self-generated during alkaline leaching, the reagent addition in thiosulfate leaching afterwards is lower than the normal. 展开更多
关键词 refractory gold-bearing arsenosulfide concentrates PRETREATMENT alkaline leaching self-leaching of gold thiosulfate leaching
下载PDF
A new extraction process of refractory gold arsenosulfide concentrates 被引量:3
2
作者 YuqunMeng TaoJin +2 位作者 MinjieWu ShaolingSu LongbaoWang 《Journal of University of Science and Technology Beijing》 CSCD 2003年第5期9-14,共6页
A new hydrometallurgical process for the refractory gold arsenosulfideconcentrates under normal temperature and pressure was presented. The experimental results of arefractory gold concentrate show that the total cons... A new hydrometallurgical process for the refractory gold arsenosulfideconcentrates under normal temperature and pressure was presented. The experimental results of arefractory gold concentrate show that the total consumption of NaOH in alkaline leaching is only 40%of those theoretically calculated under the conditions of full oxidization at the same oxidation ofarsenic to ar-senate and sulfur to sulfate. After alkaline leaching, cyanidation and adsorptionwere carried out for 24 h. The dissolution of gold by NaCN is increased to 95.3% from 12.8% beforepretreatment, and meanwhile 99.3% of the adsorption of gold by activated charcoal. The consumptionof NaCN for one ton ore is 10 kg, which is 1.2 times less than that before pretreatment. As it iscarried out under normal temperature and pressure, the investment of installations is alsodecreased. 展开更多
关键词 refractory gold arsenosulfide concentrates normal temperature and pressure PRETREATMENT
下载PDF
难浸砷金精矿的碱性常温常压预氧化 被引量:14
3
作者 孟宇群 《贵金属》 CAS CSCD 2004年第3期1-5,共5页
本文提供了1种难浸金精矿的湿法预氧化新工艺,它包括细磨、强化碱浸预氧化、氰化和炭吸附。在螺旋搅拌式塔式磨浸机中,先将目的难浸金精矿细磨至98%<37μm,然后在40%的矿浆质量浓度、11℃的环境温度和0.1MPa的环境压力下强化碱浸24h,... 本文提供了1种难浸金精矿的湿法预氧化新工艺,它包括细磨、强化碱浸预氧化、氰化和炭吸附。在螺旋搅拌式塔式磨浸机中,先将目的难浸金精矿细磨至98%<37μm,然后在40%的矿浆质量浓度、11℃的环境温度和0.1MPa的环境压力下强化碱浸24h,NaOH的消耗量为88kg/t矿,仅为相同氧化率条件下将砷硫氧化成砷酸盐和硫酸盐所需理论碱耗量的30%。预氧化完成后经36h的氰化浸出和炭吸附,金的浸出率从预氧化前的24.6%提高到95.4%,金的吸附率99.2%,NaCN的消耗4kg/t矿。整个提金工艺的成本约300元/t矿。 展开更多