期刊文献+
共找到230篇文章
< 1 2 12 >
每页显示 20 50 100
Influencing factors and optimization on mechanical performance of solid waste-derived rapid repair mortar
1
作者 Jingwei Li Xiangshan Hou +5 位作者 Aiguang Jia Xin Xiao Xujiang Wang Yonggang Yao Ziliang Zhang Wenlong Wang 《Waste Disposal and Sustainable Energy》 EI CSCD 2023年第2期223-234,共12页
There is a great demand for high performance rapid repair mortar(RRM)because of the wide use of cement concrete.Solid-waste-based sulfoaluminate cement(WSAC)is very suitable as a green cementitious material for repair... There is a great demand for high performance rapid repair mortar(RRM)because of the wide use of cement concrete.Solid-waste-based sulfoaluminate cement(WSAC)is very suitable as a green cementitious material for repair materials because of its characteristics of high early-age strength and short setting time.However,the influence and optimization of various factors of WSAC-based RRM,such as water-to-RRM ratio,binder-to-sand ratio and additives,as well as the further solid waste replacement of aggregate,remain to be studied.This paper comprehensively studied the influence of the above factors on the performance of WSAC-based RRM and obtained a green high-performance RRM by optimizing these factors.The experimental results showed that the early and late strength of the obtained RRM is excellent,and the setting time and fluidity are appropriate,which reflected good mechanical properties and construction performance.Ordinary Portland cement(OPC)doping could not improve RRM strength.It was feasible to prepare RRM with gold tailing sand replacing part of the quartz sand.This paper provides data and a theoretical basis for the preparation of high-performance RRM based on solid waste,expanding the high value utilization of solid waste,which is conducive to the development of a low carbon society. 展开更多
关键词 Rapid repair mortar Solid-waste-based sulfoaluminate cement Ordinary Portland cement Pilot production Gold tailing sand Environmental friendliness
原文传递
水性环氧树脂-聚丙烯纤维改性水泥基快速修补砂浆性能研究
2
作者 田耀刚 鲁涛 +3 位作者 赵成 蒋静 纪括 王振军 《功能材料》 CAS CSCD 北大核心 2024年第1期1031-1037,共7页
为改善机场道面修补砂浆脆性大和粘结性能差等问题,本文利用水性环氧树脂(WER)、聚丙烯(PP)纤维和硫铝酸盐水泥(SAC)制备出一种快速修补砂浆,并对其工作性能、力学性能、阻尼性能和耐硫酸盐腐蚀性能进行研究。结果表明,PP纤维和WER可显... 为改善机场道面修补砂浆脆性大和粘结性能差等问题,本文利用水性环氧树脂(WER)、聚丙烯(PP)纤维和硫铝酸盐水泥(SAC)制备出一种快速修补砂浆,并对其工作性能、力学性能、阻尼性能和耐硫酸盐腐蚀性能进行研究。结果表明,PP纤维和WER可显著提高快速修补砂浆韧性和粘结性能,使得快速修补砂浆2 h抗压、抗折强度和粘结强度分别达到22.3,5.1和3.7MPa,满足民用机场规范要求,同时可改善快速修补砂浆的阻尼性能和抗硫酸盐侵蚀性能。 展开更多
关键词 快速修补砂浆 水性环氧树脂 聚丙烯纤维 阻尼性能 耐久性
下载PDF
低温养护对环氧树脂基砂浆早期性能的影响及机理
3
作者 吕炎 白二雷 +1 位作者 王志航 夏伟 《材料导报》 EI CAS CSCD 北大核心 2024年第5期98-103,共6页
环氧树脂基砂浆是一种快速修补材料,为研究低温养护条件对环氧树脂基砂浆工作性能及早期力学性能的影响,构建了全过程低温环境,分别进行了抗压强度、抗折强度、流动度、凝结时间以及内部温度测试,分析了环氧树脂基砂浆的微观结构。结果... 环氧树脂基砂浆是一种快速修补材料,为研究低温养护条件对环氧树脂基砂浆工作性能及早期力学性能的影响,构建了全过程低温环境,分别进行了抗压强度、抗折强度、流动度、凝结时间以及内部温度测试,分析了环氧树脂基砂浆的微观结构。结果表明:环氧树脂基砂浆性能受养护温度影响较大,当养护温度为0℃时,流动度仅为112 mm,但随着温度升高流动度增长较快;低温养护使得砂浆内部热效应减弱,延缓了凝结时间;早期强度也损失显著,0℃时,砂浆养护1 d才形成强度,说明低温环境大大减慢了体系的固化速度。微观分析表明低温养护导致砂浆内部结构疏松,裂缝及孔隙增多,说明固化反应不完全,从而降低了砂浆的性能。当养护温度为20℃时,砂浆内部结构较为致密,宏观结构也表现出较高强度。 展开更多
关键词 环氧树脂基砂浆 快速修补材料 低温养护 早期力学性能 工作性能 微观结构
下载PDF
偏高岭土基地聚物道路修补砂浆的制备和性能优化
4
作者 唐瑞军 刘杰胜 《武汉轻工大学学报》 CAS 2024年第2期56-61,84,共7页
为弥补传统水泥基修补材料的不足,利用地聚物凝结硬化快、强度高、可持续等优点来制备道路快速修补材料。从力学性能角度出发,采用偏高岭土和普通硅酸盐水泥复掺的方法,将水玻璃和NaOH作为复合碱性激发剂,制备出了力学性能优良的地聚物... 为弥补传统水泥基修补材料的不足,利用地聚物凝结硬化快、强度高、可持续等优点来制备道路快速修补材料。从力学性能角度出发,采用偏高岭土和普通硅酸盐水泥复掺的方法,将水玻璃和NaOH作为复合碱性激发剂,制备出了力学性能优良的地聚物道路修补砂浆。通过正交试验,确定了复合碱性激发剂的水玻璃模数为1.5、胶砂比为0.5的试验条件。结合SEM试验,系统地研究了水泥掺量、激胶比对地聚物道路修补砂浆早期和后期力学性能的影响。试验结果显示,当水泥掺量为40%、激胶比为0.30时,在标准养护条件下,地聚物修补砂浆在0.5 d时的抗折强度为3.8 MPa,抗压强度为21.9 MPa。在28 d龄期时,其抗折强度达到了9.7 MPa,抗压强度达到了最大值47.7 MPa。研究结果将为地聚物道路修补砂浆的可控制备和性能优化设计提供参考。 展开更多
关键词 地聚物 偏高岭土 道路修补砂浆 力学性能
下载PDF
一种海洋工程自流平修补砂浆的制备及其性能研究
5
作者 陈武辉 潘荣伟 +1 位作者 农玉伯 梁雅倩 《广东建材》 2024年第6期8-11,共4页
本文使用硫铝酸盐水泥为基材,针对其早凝快、抗折性不好和容易干缩开裂等缺点,探究了修补砂浆中减水剂、缓凝剂、砂子粒径级配、矿物掺合料以及其他微量添加剂等组分对于修补砂浆物理性能的影响,制备出了符合国标要求的硫铝酸盐水泥基... 本文使用硫铝酸盐水泥为基材,针对其早凝快、抗折性不好和容易干缩开裂等缺点,探究了修补砂浆中减水剂、缓凝剂、砂子粒径级配、矿物掺合料以及其他微量添加剂等组分对于修补砂浆物理性能的影响,制备出了符合国标要求的硫铝酸盐水泥基自流平修补砂浆,其28d抗压强度可达50MPa。 展开更多
关键词 硫铝酸盐水泥基 修补砂浆 自流平
下载PDF
含有安定性不良钢渣骨料的混凝土病害诊治研究
6
作者 唐坤 胡杰 +1 位作者 唐钷 纪鹏远 《建筑结构》 北大核心 2024年第10期94-99,72,共7页
某掺入钢渣的现浇混凝土高层住宅项目混凝土表面出现密集鼓起脱落,通过对从现场鼓起部位获得的块状样品和粉末状样品进行电子显微分析、能量色散谱分析和X射线荧光分析,确定混凝土鼓起的原因为混凝土中掺入了安定性不良的钢渣,并获得了... 某掺入钢渣的现浇混凝土高层住宅项目混凝土表面出现密集鼓起脱落,通过对从现场鼓起部位获得的块状样品和粉末状样品进行电子显微分析、能量色散谱分析和X射线荧光分析,确定混凝土鼓起的原因为混凝土中掺入了安定性不良的钢渣,并获得了安定性不良钢渣的典型微观形貌和元素构成。通过对236个鼓起构件进行分析统计,确定该批混凝土的碳化深度、破坏深度、破坏面直径等指标,为后续研究提供数据支撑。最后,本文建议采用先剔除钢渣和拉毛面层,再挂钢丝网和喷射高强聚合物改性水泥砂浆的处理措施来提高构件耐久性。修复完成后由房屋使用方负责日常巡检,前5年要求每年定期全面巡检1次,5年后每3年定期全面巡检1次。若发现已修补构件出现鼓起现象,应及时请有资质的单位进行检测和处理。 展开更多
关键词 钢渣混凝土 耐久性 安定性 聚合物改性水泥砂浆 修复方案
下载PDF
高性能改性聚合物修补砂浆和单组分聚脲防水涂料在小型水库防渗加固处理中的应用
7
作者 邹彦艺 戴俊 《红水河》 2024年第2期53-56,62,共5页
某小型水库坝体为浆砌石拱坝,经多年运行,坝体背水面出现了较大面积潮湿现象,存在一定的安全隐患。为及时消除安全隐患,确保坝体的整体稳定性,设计采用高性能改性聚合物修补砂浆和单组分聚脲防水涂料对坝体迎水面进行整体修复加固与防... 某小型水库坝体为浆砌石拱坝,经多年运行,坝体背水面出现了较大面积潮湿现象,存在一定的安全隐患。为及时消除安全隐患,确保坝体的整体稳定性,设计采用高性能改性聚合物修补砂浆和单组分聚脲防水涂料对坝体迎水面进行整体修复加固与防渗处理。笔者详细介绍了高性能改性聚合物修补砂浆和单组分聚脲防水涂料的性能特点,以及采用这两种材料进行防渗加固处理的施工工艺和质量控制要点。结果表明,两种材料组合使用在水库防渗加固处理中取得了良好的效果,既满足了工程应用要求,又简化了施工过程并降低了工程投资。 展开更多
关键词 小型水库 防渗加固 高性能改性聚合物修补砂浆 单组分聚脲防水涂料
下载PDF
磷酸镁水泥及其修补砂浆耐水性研究进展 被引量:2
8
作者 刘俊霞 燕依梦 +1 位作者 海然 王雪平 《水利水电科技进展》 CSCD 北大核心 2023年第3期94-100,共7页
在总结磷酸镁水泥(MPC)及其修补砂浆耐水性破坏机理的基础上,综述了水胶比、重烧氧化镁和磷酸盐的质量比(M/P)、原材料颗粒级配、矿物掺合料种类与掺量、外加剂种类和养护温湿度条件等对MPC耐水性的影响机制,分析了MPC及其修补砂浆耐水... 在总结磷酸镁水泥(MPC)及其修补砂浆耐水性破坏机理的基础上,综述了水胶比、重烧氧化镁和磷酸盐的质量比(M/P)、原材料颗粒级配、矿物掺合料种类与掺量、外加剂种类和养护温湿度条件等对MPC耐水性的影响机制,分析了MPC及其修补砂浆耐水性研究和应用等领域中亟待解决的问题,并提出了掺入矿物掺合料、纳米粒子改性和优选并提升细集料品质等改善MPC及其修补砂浆耐水性和经济性的技术途径。 展开更多
关键词 磷酸镁水泥 修补砂浆 耐水性 水化产物 破坏机理
下载PDF
Performance of Epoxy-Repaired Corroded Reinforced Concrete Beams
9
作者 李洪明 吴瑾 +1 位作者 王喆 尚保康 《Transactions of Nanjing University of Aeronautics and Astronautics》 EI CSCD 2015年第5期579-584,共6页
Reinforcement corrosion has a serious impact on the durability and safety of reinforced concrete structures.Six reinforced concrete(RC)beam specimens are constructed.After beam specimens are subjected to accelerated c... Reinforcement corrosion has a serious impact on the durability and safety of reinforced concrete structures.Six reinforced concrete(RC)beam specimens are constructed.After beam specimens are subjected to accelerated corrosion with the constant current,beam specimens are repaired with epoxy mortar and the flexural test of beams is investigated.Then the behaviors of repaired corroded reinforced concrete beams are evaluated.The experimental results show that cracking and ultimate loads of corroded RC beams are enhanced after being repaired.And the strain distributions measured across sections of beam specimens still obey the assumption of plane section.After being repaired,the number of cracks decreases and the crack spacing increases. 展开更多
关键词 CORROSION reinforced concrete beam epoxy mortar flexural behavior repair
下载PDF
缓凝剂对PC-CSA-FDG三元胶凝体系修补砂浆性能的影响
10
作者 张国防 汪江福 +1 位作者 王向红 王培铭 《建筑材料学报》 EI CAS CSCD 北大核心 2023年第6期670-677,共8页
利用硅酸盐水泥-硫铝酸盐水泥-脱硫石膏三元胶凝体系制备修补砂浆,研究了酒石酸、硼砂及六偏磷酸钠等缓凝剂及其复掺时对修补砂浆性能的影响.结果表明:酒石酸在修补砂浆中无明显的缓凝作用,并且显著降低了修补砂浆的流动度、力学性能和... 利用硅酸盐水泥-硫铝酸盐水泥-脱硫石膏三元胶凝体系制备修补砂浆,研究了酒石酸、硼砂及六偏磷酸钠等缓凝剂及其复掺时对修补砂浆性能的影响.结果表明:酒石酸在修补砂浆中无明显的缓凝作用,并且显著降低了修补砂浆的流动度、力学性能和干燥收缩率;硼砂和六偏磷酸钠均能有效延长修补砂浆的凝结时间,改善其流动度;硼砂虽能提高修补砂浆的强度,但增大了干燥收缩率;六偏磷酸钠有利于修补砂浆的中后期强度,显著降低了干燥收缩率;3种缓凝剂均使得修补砂浆的拉伸黏结强度有所降低,复掺缓凝剂的影响介于单掺2种相应缓凝剂的作用效果之间. 展开更多
关键词 修补砂浆 缓凝剂 三元胶凝体系 凝结时间 强度 干燥收缩率
下载PDF
大口径排水管涵修复技术与修复材料
11
作者 孙振平 金惠玲 +6 位作者 李欢欢 刘嘉颖 郁片红 董家宴 郑琨鹏 羊省 李志林 《混凝土世界》 2023年第6期66-70,共5页
综述了原位固化(Cured In Place Pipe,CIPP)法、穿插法、内衬法、无机防腐砂浆喷涂法、套环法、注浆法和Pipere-100内涨圈柔性内修复法共7种国内常用大口径管涵非开挖修复技术,以及Rib Loc螺旋缠绕技术和Pattem Flooring技术等国外常用... 综述了原位固化(Cured In Place Pipe,CIPP)法、穿插法、内衬法、无机防腐砂浆喷涂法、套环法、注浆法和Pipere-100内涨圈柔性内修复法共7种国内常用大口径管涵非开挖修复技术,以及Rib Loc螺旋缠绕技术和Pattem Flooring技术等国外常用大口径管涵非开挖修复技术,并结合文献和作者的研究成果,提出用于水上部分修复的快速修复砂浆和用于水下部分修复的水下抗分散修复砂浆。 展开更多
关键词 大口径排水管涵 非开挖修复技术 快速修复砂浆 水下抗分散修复砂浆
下载PDF
偏高岭土在人造水硬性石灰修复砂浆中的应用研究 被引量:1
12
作者 顾立龙 商怀帅 +2 位作者 吴亚月 孟维广 侯关豪 《硅酸盐通报》 CAS 北大核心 2023年第12期4351-4359,4367,共10页
为研制一种适用于历史建筑修复的绿色无机修复材料,本文基于青岛多栋砖砌体结构历史建筑黏结材料的XRD测试结果,通过掺偏高岭土制备了基于人造水硬性石灰的修复砂浆,测试了人造水硬性石灰砂浆的流动度、凝结时间、质量损失率、干燥收缩... 为研制一种适用于历史建筑修复的绿色无机修复材料,本文基于青岛多栋砖砌体结构历史建筑黏结材料的XRD测试结果,通过掺偏高岭土制备了基于人造水硬性石灰的修复砂浆,测试了人造水硬性石灰砂浆的流动度、凝结时间、质量损失率、干燥收缩率以及力学性能等指标,研究了偏高岭土对人造水硬性石灰砂浆的影响。结果表明:偏高岭土可降低人造水硬性石灰砂浆的流动度,缩短凝结时间,降低收缩率,提高抗压强度及黏结强度。当掺量为5.0%和7.5%(质量分数)时,人造水硬性石灰砂浆的56 d抗压强度分别提升了66.8%和94.3%,黏结强度分别提升了22.2%和25.9%。采用XRD和SEM对材料的微观结构进行测试分析发现,偏高岭土能使人造水硬性石灰砂浆性能提升的主要原因是偏高岭土中的活性SiO_(2)和Al_(2)O_(3)与石灰发生直接反应并消耗Ca(OH)_(2),促进了水泥水化,增强了水化产物与骨料间的黏结力。 展开更多
关键词 偏高岭土 水硬性石灰 修复砂浆 历史建筑 物理力学性能 微观结构
下载PDF
界面处理对硫铝酸盐水泥修补砂浆黏结性能的影响
13
作者 王业民 张贤 +1 位作者 卢晓磊 杜鹏 《混凝土与水泥制品》 2023年第8期6-9,14,共5页
基于水灰比对硫铝酸盐水泥(SAC)修补砂浆界面弯拉强度的影响,确定了SAC修补砂浆最佳配合比,并研究了增大粗糙度、不同溶液浸润的界面处理方式对SAC修补砂浆新旧界面弯拉强度的影响。结果表明:SAC修补砂浆的3 d界面弯拉强度随着水灰比的... 基于水灰比对硫铝酸盐水泥(SAC)修补砂浆界面弯拉强度的影响,确定了SAC修补砂浆最佳配合比,并研究了增大粗糙度、不同溶液浸润的界面处理方式对SAC修补砂浆新旧界面弯拉强度的影响。结果表明:SAC修补砂浆的3 d界面弯拉强度随着水灰比的减小逐渐增大,当水灰比为0.35时,SAC修补砂浆界面弯拉强度达到最高,为3.82 MPa;对界面进行粗糙处理可显著提高SAC修补砂浆1、3、28 d新旧界面弯拉强度,相较于界面未进行处理组分别提高了1.03、1.08、0.64 MPa;与粗糙处理方式相比,对界面进行水浸润或碱溶液浸润处理均对SAC修补砂浆的新旧界面弯拉强度不利。 展开更多
关键词 硫铝酸盐水泥 修补砂浆 水灰比 界面 粗糙处理 界面弯拉强度
下载PDF
潮湿环境下原位聚合修补砂浆的黏接性能及增黏机理
14
作者 邵丽静 冯攀 +3 位作者 刘明星 王伟 洪锦祥 缪昌文 《东南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2023年第5期749-755,共7页
为了提高潮湿恶劣环境下水泥基修补材料的修复效果,通过在水泥基修补砂浆中掺入有机物单体、引发剂和交联剂等使其在砂浆中原位发生聚合.利用抗拉黏接强度测试探究了原位聚合改性砂浆对干燥和潮湿界面黏接性能的影响,同时通过流动性和... 为了提高潮湿恶劣环境下水泥基修补材料的修复效果,通过在水泥基修补砂浆中掺入有机物单体、引发剂和交联剂等使其在砂浆中原位发生聚合.利用抗拉黏接强度测试探究了原位聚合改性砂浆对干燥和潮湿界面黏接性能的影响,同时通过流动性和凝结时间测试探究砂浆的工作性能.研究结果表明:原位聚合改性砂浆具有良好的工作性能和较短的凝结时间,且能够显著增强砂浆与基体的界面黏接性能;相对于空白组,其28 d的干燥和潮湿界面黏接强度最高可增加3.7倍和13.0倍;由于聚合后在潮湿界面的钉扎锚固作用,其潮湿界面的黏接强度最高可达干燥界面的1.6倍,表明了原位聚合改性修补砂浆在潮湿环境下具有良好的修补效果. 展开更多
关键词 修补砂浆 原位聚合 潮湿环境 界面黏接性能
下载PDF
稻壳灰掺量对修补砂浆流变性能及力学性能的影响规律及机理分析
15
作者 段培培 李绍纯 王培军 《材料导报》 CSCD 北大核心 2023年第S02期247-253,共7页
采用600℃烧制的稻壳灰(RHA)制备了基于RHA的修补砂浆,研究了不同掺量下稻壳灰对修补砂浆力学性能和流变性能的影响,同时结合水化热、水化产物、微观形貌、孔隙结构等分析稻壳灰对水泥水化的影响及其对砂浆强度的增强机理。结果表明:随... 采用600℃烧制的稻壳灰(RHA)制备了基于RHA的修补砂浆,研究了不同掺量下稻壳灰对修补砂浆力学性能和流变性能的影响,同时结合水化热、水化产物、微观形貌、孔隙结构等分析稻壳灰对水泥水化的影响及其对砂浆强度的增强机理。结果表明:随着RHA掺量的增加,修补砂浆的流动度不断降低,但修补砂浆的屈服应力和塑性黏度增大,RHA的掺入并未改变水泥浆体的流变类型。RHA的掺入降低了修补砂浆早期的力学性能,但明显提升了修补砂浆的中后期强度,当RHA掺量为6%时,修补砂浆28 d力学性能达到最好。收缩性能研究表明,当RHA掺量为10%时,水泥砂浆的干燥收缩值最小。RHA对水泥早期(<1d)的水化过程有抑制作用,但是对后期(>1d)的水化过程具有一定的促进作用,且随着RHA掺量越高,水泥水化速率逐渐加快。RHA中高活性的SiO_(2)促进水泥水化的同时也参与水泥的二次水化反应,生成大量的C⁃S⁃H凝胶和钙矾石,C⁃S⁃H凝胶将内部串联成一个整体,使得水泥砂浆内部的物质能更好地连接在一起,从而提高修补砂浆的强度。 展开更多
关键词 稻壳灰 力学性能 修补砂浆 流变 干燥收缩 微观分析
下载PDF
机械活化煤矸石在路面修补材料中的应用研究 被引量:2
16
作者 何建能 王雷 +3 位作者 邱宏科 王长安 李娜 牛洪薪 《中国建材科技》 CAS 2023年第3期62-65,共4页
研究了不同机械活化煤矸石掺量对道路路面用修补砂浆工作性、力学性能和耐久性能的影响。结果表明,当用机械活化煤矸石替代矿粉时,随着掺量的增加,所制备修补砂浆的工作性能有较好改善。煤矸石在低掺量时对修补砂浆的力学性能影响较小,... 研究了不同机械活化煤矸石掺量对道路路面用修补砂浆工作性、力学性能和耐久性能的影响。结果表明,当用机械活化煤矸石替代矿粉时,随着掺量的增加,所制备修补砂浆的工作性能有较好改善。煤矸石在低掺量时对修补砂浆的力学性能影响较小,但当替代矿粉掺量超过50%后,修补砂浆抗折和抗压强度的降幅较大。同时,随着煤矸石掺量的增加,修补砂浆的黏结强度和收缩性能降低。 展开更多
关键词 修补砂浆 活化煤矸石 强度 收缩
下载PDF
无碱液体速凝剂对修补砂浆性能的影响 被引量:1
17
作者 王武锁 袁倩男 +5 位作者 宋心 赵世冉 王欢 任双倩 张强 徐潇 《新型建筑材料》 2023年第2期63-65,73,共4页
研究了无碱液体速凝剂对水泥基修补砂浆凝结时间、抗压、抗折及拉伸粘结强度的影响规律,对掺加无碱液体速凝剂的修补砂浆的水化放热行为进行了分析。结果表明,无碱液体速凝剂的掺入加速了修补砂浆早期的水化进程,缩短了修补砂浆的凝结时... 研究了无碱液体速凝剂对水泥基修补砂浆凝结时间、抗压、抗折及拉伸粘结强度的影响规律,对掺加无碱液体速凝剂的修补砂浆的水化放热行为进行了分析。结果表明,无碱液体速凝剂的掺入加速了修补砂浆早期的水化进程,缩短了修补砂浆的凝结时间,提高了修补砂浆的抗压、抗折和拉伸粘结强度;在速凝剂掺量为0~7%时,随着无碱液体速凝剂掺量的增加,修补砂浆的抗压、抗折和拉伸粘结强度均有所提高。 展开更多
关键词 修补砂浆 无碱液体速凝剂 凝结时间 力学性能
下载PDF
聚合物防水修复砂浆机械化施工性能研究与应用 被引量:1
18
作者 李波 王星尧 +3 位作者 亓帅 刘畅 张晓 蒋亚军 《中国建筑防水》 2023年第1期21-25,共5页
研究了不同助剂用量及不同水灰比对聚合物水泥防水修复砂浆力学性能和抗渗性能的影响,进一步通过专用的输送阻力测试装置定量研究了不同助剂用量及不同水灰比下砂浆的输送阻力,分析了实际喷涂施工难易程度与砂浆输送阻力值的相对关系,... 研究了不同助剂用量及不同水灰比对聚合物水泥防水修复砂浆力学性能和抗渗性能的影响,进一步通过专用的输送阻力测试装置定量研究了不同助剂用量及不同水灰比下砂浆的输送阻力,分析了实际喷涂施工难易程度与砂浆输送阻力值的相对关系,以指导此类砂浆的实际喷涂施工应用。 展开更多
关键词 聚合物水泥防水修复砂浆 喷涂施工 力学性能 输送阻力
下载PDF
混凝土裂缝修补施工技术探讨 被引量:2
19
作者 蔡志航 《江西建材》 2023年第2期187-188,191,共3页
文中以某建筑工程为背景,结合实际情况,通过修补界面清理、拌制丙乳砂浆修补料、修补料涂装以及修补界面处理,完成建筑工程中混凝土裂缝的修补施工。通过混凝土渗透试验与抗剪测试证明,采用新技术修补后的混凝土抗渗性能与抗剪性能均得... 文中以某建筑工程为背景,结合实际情况,通过修补界面清理、拌制丙乳砂浆修补料、修补料涂装以及修补界面处理,完成建筑工程中混凝土裂缝的修补施工。通过混凝土渗透试验与抗剪测试证明,采用新技术修补后的混凝土抗渗性能与抗剪性能均得到有效提升,裂缝修补效果良好,具有一定的应用价值。 展开更多
关键词 建筑工程 混凝土 裂缝修补 丙乳砂浆 抗渗性能 力学性能
下载PDF
复合矿物掺合料对砂浆自修复性能的影响 被引量:2
20
作者 常洪雷 李晨聪 +4 位作者 王晓龙 王剑宏 王云飞 曲明月 刘健 《材料导报》 EI CAS CSCD 北大核心 2023年第2期58-64,共7页
为了增强水泥基材料的自修复能力,通过在砂浆中复掺三种不同类型的矿物掺合料探究其共同作用的效果。通过对比裂缝宽度、透水率以及抗压强度恢复情况评估试件的自修复效果,并利用扫描电镜-能谱分析(SEM-EDS)研究裂缝处自修复物质的物相... 为了增强水泥基材料的自修复能力,通过在砂浆中复掺三种不同类型的矿物掺合料探究其共同作用的效果。通过对比裂缝宽度、透水率以及抗压强度恢复情况评估试件的自修复效果,并利用扫描电镜-能谱分析(SEM-EDS)研究裂缝处自修复物质的物相组成及微观形貌。掺加复合矿物掺合料可有效提升砂浆的自修复能力,具体表现为裂缝宽度减小、透水性降低和抗压强度显著恢复。其中,掺料组合膨胀剂+硅灰+生石灰和膨胀剂+生石灰+Na_(2)CO_(3)的修复效果最好,裂缝在14 d内可以实现完全愈合,透水率分别降低92.7%和87.4%,在养护28 d后抗压强度分别恢复79.1%和80.1%,且浸水环境更有利于提高砂浆的自修复效果。而掺料组合膨胀剂+硅灰+Na_(2)CO_(3)和膨胀剂+偏高岭土+Na_(2)CO_(3)的修复效果较差,不利于砂浆裂缝的修复和抗压强度的恢复。此外,微观分析结果显示,裂缝中的修复物质除含有水化生成的C-S-H和C-A-H外,碳化生成的碳酸钙也是主要的修复物质之一。 展开更多
关键词 砂浆 自修复 矿物掺和料 裂缝 修复程度
下载PDF