Properties of AA7075 aluminum alloy in aging and retrogression and reaging process 被引量:10
1
作者 Gokhan OZER Ahmet KARAASLAN 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2017年第11期2357-2362,共6页
A retrogression process was applied to AA7075alloy at180,240and320°C for1,30,50,70,90and120min.After the retrogression,aging treatment was reapplied with T6conditions(120°C,24h).The mechanical properties of ... A retrogression process was applied to AA7075alloy at180,240and320°C for1,30,50,70,90and120min.After the retrogression,aging treatment was reapplied with T6conditions(120°C,24h).The mechanical properties of aged samples were determined by V-Charpy and hardness tests and also,physical properties of samples were determined by electrical conductivity tests.Moreover,microstructural properties were characterized by light microscope and transmission electron microscope.The results show that the effects of the temperature and the duration of the retrogression and reagent on the impact toughness and hardness are related to the precipitates at the grain boundary. 展开更多
关键词 aluminum alloy precipitate behavior retrogression and reaging impact toughness HARDNESS electrical conductivity
下载PDF
Effect of Retrogression and Reaging on Stress Corrosion Cracking of Spray Formed Al Alloy 被引量:2
2
作者 Ruiming Su Yingdong Qu +2 位作者 Xiang Li Junhua You Rongde Li 《Materials Sciences and Applications》 2016年第1期1-7,共7页
Stress corrosion cracking (SCC) resistance of a spray formed Al-Zn-Mg-Cu alloy underwent retrogression and reaging (RRA) was studied by slow strain rate tests in dry air and 3.5 wt% NaCl solution. The results showed t... Stress corrosion cracking (SCC) resistance of a spray formed Al-Zn-Mg-Cu alloy underwent retrogression and reaging (RRA) was studied by slow strain rate tests in dry air and 3.5 wt% NaCl solution. The results showed that after RRA treatment, interrupted η phases at grain boundaries and slightly wide precipitate free zones could decrease SCC susceptibility of the alloy. Lots of reticular dislocations appeared in deformation process could prevent hydrogen induced cracking, and then SCC. Abundance transgranular dispersive η' phases separated out again promoted tensile strength to 759.4 MPa. The fracture ways of the specimens were dimple fracture in dry air and sub-cleavage fracture in 3.5% NaCl solution. 展开更多
关键词 Spray Forming Al-Zn-Mg-Cu Alloy retrogression and reaging Stress Corrosion Cracking
下载PDF