An enriched goal-oriented error estimation method with extended degrees of freedom is developed to estimate the error in the continuum-based shell extended finite element method. It leads to high quality local error b... An enriched goal-oriented error estimation method with extended degrees of freedom is developed to estimate the error in the continuum-based shell extended finite element method. It leads to high quality local error bounds in three-dimensional fracture mechanics simulation which involves enrichments to solve the singularity in crack tip. This enriched goal-oriented error estimation gives a chance to evaluate this continuum- based shell extended finite element method simulation. With comparisons of reliability to the stress intensity factor calculation in stretching and bending, the accuracy of the continuum-based shell extended finite element method simulation is evaluated, and the reason of error is discussed. 展开更多
关键词 goal-oriented error estimation finite element analysis fracture mechanics continuum-based shell
下载PDF
Experimental research of non-burned fly-ash ceramsite
2
作者 张义顺 张超 +1 位作者 郭金敏 周少统 《Journal of Coal Science & Engineering(China)》 2005年第2期75-77,共3页
Selected non-burned method and took fly-ash as main material, together with lime and gypsum, to inspire the activity of volcanic ash, took a kind of poly-organics to re-place the clay as binder, and then made small ba... Selected non-burned method and took fly-ash as main material, together with lime and gypsum, to inspire the activity of volcanic ash, took a kind of poly-organics to re-place the clay as binder, and then made small balls with machine, wrapped slurry twice and autoclaved 8 hours at normal atmosphere, made ceramsite in this way can endure higher compression strength. Comparing with common concrete, the ceramsite concrete is about 25% lighter on weight. 展开更多
关键词 non-burned ceramsite wrapping slurry suitable strength shell structure mechanism